CN1147549C - Bright enamel paint for inner wall and its production process - Google Patents
Bright enamel paint for inner wall and its production processInfo
- Publication number
- CN1147549C CN1147549C CNB011281642A CN01128164A CN1147549C CN 1147549 C CN1147549 C CN 1147549C CN B011281642 A CNB011281642 A CN B011281642A CN 01128164 A CN01128164 A CN 01128164A CN 1147549 C CN1147549 C CN 1147549C
- Authority
- CN
- China
- Prior art keywords
- kilograms
- add
- kilogram
- water
- polyvinyl alcohol
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present invention discloses a high-brightness cold enamel paint for coating inner walls and a production method thereof. The present invention is characterized in that water is added to corn starch and sodium hydroxide to prepare a corn starch adhesive, and water is added to cellulose and sodium benzoate to prepare a cellulose adhesive; water is added to polyvinyl alcohol and borax to prepare a polyvinyl alcohol adhesive; and the three kinds of adhesives, light calcium carbonate powder, hydrate lime powder, ground limestone powder, talcum powder and an auxiliary agent are uniformly stirred and ground to prepare the high-brightness cold enamel paint for coating inner walls. The high-brightness cold enamel paint has the characteristics of no toxicity or odor, no pollution to environment and no nuisance, and a coating layer has the advantages of high smoothness and hardness, high brightness and strong adhesive force; therefore, the high-brightness cold enamel paint can replace the existing paint for coating inner walls.
Description
Technical field
The present invention relates to buildings decoration material technical field, particularly a kind of bright enamel paint for inner wall and production method thereof.
Background technology
At present, the decoration material that construction market is used is various in style, and demand is also more and more.The same expense of the interior wall coating of buildings is more and more, but the sizing material that most of interior wall coating uses all is milky white adhesive, and the free aldehyde of milky white adhesive is slowly release in buildings, causes the room air pollution of buildings, and people's living environment is damaged.Chinese patent application number is 93110860, the day for announcing is on July 21st, 1993, " a kind of novel method of making ceramic imitation interior wall paint " disclosed, it is by water structure closely and be the colloidal resin after the cooling, has certain bounding force and water-soluble or be partially soluble in the composite powder of water and water-ground limestone and stir and form.
Summary of the invention
The purpose of this invention is to provide a kind of bright enamel paint for inner wall and production method thereof, this interior wall Spreed coated paint does not contain formaldehyde resin, helps environment protection.
Bright enamel paint for inner wall is characterized in that: it is to add 7 kilograms of W-Gums for 100 kilograms by water, adds 1.7 kilograms of Corn Starch Glue of making of sodium hydroxide; Add 3.3 kilograms of Mierocrystalline celluloses for 100 kilograms by water, add Sodium Benzoate again and make cellulose gum for 0.6 kilogram; Add 3.8 kilograms of polyvinyl alcohol for 100 kilograms by water, add borax again and make polyvinyl alcohol glue for 0.2 kilogram; Above-mentioned three kinds of glue and 40 kilograms in light calcium carbonate powder, 60 kilograms of grey calcium powders, 75 kilograms of heavy calcium carbonates, 100 kilograms of 600 order talcum powder add auxiliary agent again, stir, grind the back bright enamel paint for inner wall.
The production method of above-mentioned bright enamel paint for inner wall is characterized in that:
1, at first, fetching water 100 kilograms adds 7 kilograms of W-Gums, adds with 1.7 kilograms of sodium hydroxide of little water dissolving again, puts into the stirrer stirring and makes Corn Starch Glue;
2,3.3 kilograms of Mierocrystalline celluloses of 100 kilograms of addings of water intaking, Sodium Benzoate are put into the stirrer stirring for 0.6 kilogram and are made cellulose gum;
3, water intaking is heated to 100 ℃ for 100 kilograms, adds 3.8 kilograms of polyvinyl alcohol, 0.2 kilogram of borax, boils and makes polyvinyl alcohol glue;
4, get 104 kilograms of polyvinyl alcohol glues, add 60 kilograms of ash charge calcium powders, 40 kilograms in light calcium carbonate powder, 75 kilograms of heavy calcium carbonates, 100 kilograms of 600 order talcum powder, putting into stirrer stirs, add 108.7 kilograms of Corn Starch Glue while stirring, add 103.9 kilograms of cellulose gums again, continue to stir liquid in the pasty state;
5, pasty liquid is added 0.15 kilogram in whitening agent, 0.15 kilogram of stirring of ultramarine, add 0.08 kilogram of dibutyl phthalate, 0.08 kilogram of stirring of ethylene glycol simultaneously, add 0.5 kilogram of thickening material, 0.15 kilogram of pearlescence, stir well, add 5 kilograms of water glass, stir well, add 0.5 kilogram of reinforcing agent again, stir well, make dense thick body of paste, pack after dense thick body of paste is ground product of the present invention.
The characteristics of bright enamel paint for inner wall of the present invention are that nonpoisonous and tasteless, environmentally safe, nuisanceless is scraped the coating smooth, hard, smooth light, strong adhesion, the difficult pollution.Resistivity against fire, alkali resistance, resistance to salt water, thermotolerance, weather resisteant, freeze-thaw resistance, crashworthiness punching performance are good, can replace the inner wall decoration of ceramic tile, are the regeneration products of interior wall Spreed coated paint.Producing and manufacturing technique is easy, less investment is operated easily.
Embodiment
Bright enamel paint for inner wall, it is to add 7 kilograms of W-Gums for 100 kilograms by water, adds 1.7 kilograms of Corn Starch Glue of making of sodium hydroxide; Add 3.3 kilograms of Mierocrystalline celluloses for 100 kilograms by water, add Sodium Benzoate again and make cellulose gum for 0.6 kilogram; Add 3.8 kilograms of polyvinyl alcohol for 100 kilograms by water, add borax again and make polyvinyl alcohol glue for 0.2 kilogram; (the ten thousand li stone flour factories in Haicheng City Ba Li town, Liaoning Province produce for above-mentioned three kinds of glue and light calcium carbonate powder, address: Haicheng City eight Li Erdao villages) 40 kilograms, 60 kilograms of grey calcium powders (Lishu County, Jilin mine Building Materials Factory product), 75 kilograms of heavy calcium carbonates (the intelligent roc in Shijiazhuang City Jingxing company limited), 100 kilograms of 600 order talcum powder, add auxiliary agent again, stir, grind the back bright enamel paint for inner wall.
The production method of above-mentioned bright enamel paint for inner wall is,
1, at first, fetching water 100 kilograms adds 7 kilograms of W-Gums, adds with 1.7 kilograms of sodium hydroxide of little water dissolving again, puts into the stirrer stirring and makes Corn Starch Glue;
2,3.3 kilograms of Mierocrystalline celluloses of 100 kilograms of addings of water intaking, Sodium Benzoate are put into the stirrer stirring for 0.6 kilogram and are made cellulose gum;
3, water intaking is heated to 100 ℃ for 100 kilograms, adds 3.8 kilograms of polyvinyl alcohol, 0.2 kilogram of borax, boils and makes polyvinyl alcohol glue;
4, get 104 kilograms of polyvinyl alcohol glues, add 60 kilograms of ash charge calcium powders, 40 kilograms in light calcium carbonate powder, 75 kilograms of heavy calcium carbonates, 100 kilograms of 600 order talcum powder, putting into stirrer stirs, add 108.7 kilograms of Corn Starch Glue while stirring, add 103.9 kilograms of cellulose gums again, continue to stir liquid in the pasty state;
5, pasty liquid is added 0.15 kilogram in whitening agent, 0.15 kilogram of stirring of ultramarine, add 0.08 kilogram of dibutyl phthalate, 0.08 kilogram of stirring of ethylene glycol simultaneously, add 0.5 kilogram of thickening material, 0.15 kilogram of pearlescence, stir well, add 5 kilograms of water glass, stir well, add 0.5 kilogram of reinforcing agent again, stir well, make dense thick body of paste, pack after dense thick body of paste is ground product of the present invention.
Claims (2)
1, bright enamel paint for inner wall is characterized in that: it is to add 7 kilograms of W-Gums for 100 kilograms by water, adds 1.7 kilograms of Corn Starch Glue of making of sodium hydroxide; Add 3.3 kilograms of Mierocrystalline celluloses for 100 kilograms by water, add Sodium Benzoate again and make cellulose gum for 0.6 kilogram; Add 3.8 kilograms of polyvinyl alcohol for 100 kilograms by water, add borax again and make polyvinyl alcohol glue for 0.2 kilogram; Above-mentioned three kinds of glue and 40 kilograms in light calcium carbonate powder, 60 kilograms of grey calcium powders, 75 kilograms of heavy calcium carbonates, 100 kilograms of 600 order talcum powder add auxiliary agent again, stir, grind the back bright enamel paint for inner wall.
2, the production method of the bright enamel paint for inner wall of claim 1 is characterized in that:
1), at first, fetching water 100 kilograms adds 7 kilograms of W-Gums, adds with 1.7 kilograms of sodium hydroxide of little water dissolving again, puts into the stirrer stirring and makes Corn Starch Glue;
2), 3.3 kilograms of Mierocrystalline celluloses of 100 kilograms of addings of water intaking, Sodium Benzoate are put into the stirrer stirring for 0.6 kilogram and are made cellulose gum;
3), water intaking is heated to 100 ℃ for 100 kilograms, adds 3.8 kilograms of polyvinyl alcohol, 0.2 kilogram of borax, boil and make polyvinyl alcohol glue;
4), get 104 kilograms of polyvinyl alcohol glues, add 60 kilograms of ash charge calcium powders, 40 kilograms in light calcium carbonate powder, 75 kilograms of heavy calcium carbonates, 100 kilograms of 600 order talcum powder, putting into stirrer stirs, add 108.7 kilograms of Corn Starch Glue while stirring, add 103.9 kilograms of cellulose gums again, continue to stir liquid in the pasty state;
5), pasty liquid is added 0.15 kilogram in whitening agent, 0.15 kilogram of stirring of ultramarine, add 0.08 kilogram of dibutyl phthalate, 0.08 kilogram of stirring of ethylene glycol simultaneously, add 0.5 kilogram of thickening material, 0.15 kilogram of pearlescence, stir well, add 5 kilograms of water glass, stir well, add 0.5 kilogram of reinforcing agent again, stir well, make dense thick body of paste, pack after dense thick body of paste is ground product of the present invention.