CN114349582A - Safe and reliable toy hammer and preparation method thereof - Google Patents
Safe and reliable toy hammer and preparation method thereof Download PDFInfo
- Publication number
- CN114349582A CN114349582A CN202111551767.XA CN202111551767A CN114349582A CN 114349582 A CN114349582 A CN 114349582A CN 202111551767 A CN202111551767 A CN 202111551767A CN 114349582 A CN114349582 A CN 114349582A
- Authority
- CN
- China
- Prior art keywords
- powder
- safe
- hammer
- striker
- red phosphorus
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a safe and reliable toy hammer and a preparation method thereof, and the formula comprises: potassium chlorate powder, red phosphorus powder, paste and calcium carbonate powder, and the preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing; in the first step, the raw materials are stirred in a manual kneading and mixing mode, in the second step, a filter screen used by a filtering device is 100 meshes, in the third step, the injection amount of a single container material ring is 0.016g, in the third step, a paper card is provided with blister oil, and in the fourth step, the natural air drying temperature is 25-30 ℃.
Description
Technical Field
The invention relates to the technical field of toy manufacturing, in particular to a safe and reliable toy hammer and a preparation method thereof.
Background
Gunpowder is one of four inventions in ancient China, is commonly used for manufacturing weapons and toys, gunpowder plays fireworks, crackers, toy guns and the like, and generates fire sound and smoke by burning the gunpowder, but the existing gunpowder toys need to generate an explosion effect by combining black gunpowder and a lead wire, have low safety, and are easy to generate safety accidents in the processes of production, transportation, storage and use.
Disclosure of Invention
The invention aims to provide a safe and reliable toy striker and a preparation method thereof, so as to solve the problems in the background technology.
In order to achieve the purpose, the invention provides the following technical scheme: a safe and reliable toy striker, the formula of which comprises: potassium chlorate powder, red phosphorus powder, paste and calcium carbonate powder, wherein the mass percent of each component is as follows: 73% of potassium chlorate powder, 24% of red phosphorus powder, 1.5% of paste and 1.5% of calcium carbonate powder.
Preferably, the red phosphorus powder has a particle size of more than 200 mesh.
A safe and reliable toy hammer preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing;
in the first step, 73% of potassium chlorate powder, 24% of red phosphorus powder, 1.5% of paste and 1.5% of calcium carbonate powder are weighed for later use according to the sum of the mass percentages of the components being 1, the potassium chlorate powder is soaked in a proper amount of water, the red phosphorus powder, the paste and the calcium carbonate powder are added, and then the materials are repeatedly stirred until the materials are uniformly mixed to obtain a mixture;
in the second step, the mixture prepared in the first step is transferred into a filtering device and repeatedly filtered until the mixture becomes a gummy fluid medicament;
in the third step, the fluid medicine prepared in the second step is taken, firstly, the fluid medicine is injected into a material ring of a container through a medicine injection machine, then 80g of kraft paper is covered, and the paper card is bonded with a PVC film for thermoplastic packaging to obtain a semi-finished product hammer;
in the fourth step, the hammer prepared in the third step is naturally dried to obtain a finished product hammer, and finally, the finished product hammer is packaged and stored according to the technological specification.
Preferably, in the first step, the raw materials are stirred by manually kneading and mixing the raw materials.
Preferably, in the second step, the filter screen used by the filtering device is 100 meshes.
Preferably, in the third step, the amount of the injection material of the single container material ring is 0.016 g.
Preferably, in the third step, the paper card is provided with plastic uptake oil.
Preferably, in the fourth step, the natural air drying temperature is 25-30 ℃.
Compared with the prior art, the invention has the beneficial effects that: compared with the existing black powder toy, the novel hammer toy is designed into the hammer toy, the price of the medicine of the hammer toy is low, the fire sound and a small amount of medicine smoke are generated after the hammer is fired, the safety is high, the medicine of the hammer toy is packaged in the plastic groove, the transportation and the storage are convenient, and the novel hammer toy is safe and practical.
Drawings
FIG. 1 is a flow chart of a method of the present invention;
FIG. 2 is a pictorial representation of the present invention.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Referring to fig. 1, a technical solution provided by the present invention:
example 1:
a safe and reliable toy striker, the formula of which comprises: potassium chlorate powder, red phosphorus powder, paste and calcium carbonate powder, wherein the mass percent of each component is as follows: 73 percent of potassium chlorate powder, 24 percent of red phosphorus powder, 1.5 percent of paste and 1.5 percent of calcium carbonate powder, wherein the granularity of the red phosphorus powder is more than 200 meshes.
A safe and reliable toy hammer preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing;
in the first step, 73% of potassium chlorate powder, 24% of red phosphorus powder, 1.5% of paste and 1.5% of calcium carbonate powder are weighed for later use according to the sum of the mass percentages of the components being 1, the potassium chlorate powder is soaked in a proper amount of water, the red phosphorus powder, the paste and the calcium carbonate powder are added, then the raw materials are stirred in a manual kneading and mixing mode, and the stirring is repeated until the raw materials are uniformly mixed, so that a mixture is obtained;
in the second step, the mixture prepared in the first step is transferred into a filtering device, and the filtering is repeated until the mixture becomes a sticky fluid medicament, and a filter screen used by the filtering device is 100 meshes;
in the third step, the fluid medicine prepared in the second step is taken, the fluid medicine is firstly injected into the material rings of the containers through a medicine injection machine, the injection amount of each material ring of the container is 0.016g, 80g of kraft paper is covered, a paper card with blister oil is bonded with the PVC film, and thermoplastic packaging is carried out to obtain a semi-finished product hammer;
in the fourth step, the hammer prepared in the third step is naturally dried at 25 ℃ to obtain a finished product hammer, and finally, the finished product hammer is packaged and stored according to the process specification.
Example 2:
a safe and reliable toy striker, the formula of which comprises: potassium chlorate powder, red phosphorus powder, paste and calcium carbonate powder, wherein the mass percent of each component is as follows: 72 percent of potassium chlorate powder, 24 percent of red phosphorus powder, 2 percent of paste and 2 percent of calcium carbonate powder, wherein the granularity of the red phosphorus powder is more than 200 meshes.
A safe and reliable toy hammer preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing;
in the first step, 72% of potassium chlorate powder, 24% of red phosphorus powder, 2% of paste and 2% of calcium carbonate powder are weighed for later use according to the sum of the mass percentages of the components being 1, the potassium chlorate powder is soaked in a proper amount of water, the red phosphorus powder, the paste and the calcium carbonate powder are added, then the raw materials are stirred in a manual kneading and mixing mode, and the raw materials are repeatedly stirred until the raw materials are uniformly mixed to obtain a mixture;
in the second step, the mixture prepared in the first step is transferred into a filtering device, and the filtering is repeated until the mixture becomes a sticky fluid medicament, and a filter screen used by the filtering device is 100 meshes;
in the third step, the fluid medicine prepared in the second step is taken, the fluid medicine is firstly injected into the material rings of the containers through a medicine injection machine, the injection amount of each material ring of the container is 0.016g, 80g of kraft paper is covered, a paper card with blister oil is bonded with the PVC film, and thermoplastic packaging is carried out to obtain a semi-finished product hammer;
in the fourth step, the hammer prepared in the third step is naturally dried at the temperature of 27 ℃ to obtain a finished product hammer, and finally, the finished product hammer is packaged and stored according to the process specification.
Example 3:
a safe and reliable toy striker, the formula of which comprises: potassium chlorate powder, red phosphorus powder, paste and calcium carbonate powder, wherein the mass percent of each component is as follows: 74 percent of potassium chlorate powder, 24 percent of red phosphorus powder, 1 percent of paste and 1 percent of calcium carbonate powder, wherein the granularity of the red phosphorus powder is more than 200 meshes.
A safe and reliable toy hammer preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing;
in the first step, 74% of potassium chlorate powder, 24% of red phosphorus powder, 1% of paste and 1% of calcium carbonate powder are weighed for later use according to the sum of the mass percentages of the components being 1, the potassium chlorate powder is soaked in a proper amount of water, the red phosphorus powder, the paste and the calcium carbonate powder are added, then the raw materials are stirred in a manual kneading and mixing mode, and the raw materials are repeatedly stirred until the raw materials are uniformly mixed to obtain a mixture;
in the second step, the mixture prepared in the first step is transferred into a filtering device, and the filtering is repeated until the mixture becomes a sticky fluid medicament, and a filter screen used by the filtering device is 100 meshes;
in the third step, the fluid medicine prepared in the second step is taken, the fluid medicine is firstly injected into the material rings of the containers through a medicine injection machine, the injection amount of each material ring of the container is 0.016g, 80g of kraft paper is covered, a paper card with blister oil is bonded with the PVC film, and thermoplastic packaging is carried out to obtain a semi-finished product hammer;
in the fourth step, the hammer prepared in the third step is naturally dried at 30 ℃ to obtain a finished product hammer, and finally, the finished product hammer is packaged and stored according to the process specification.
The properties of the examples are compared in the following table:
example 1 | Example 2 | Example 3 | |
Potassium chlorate powder addition/%) | 73 | 72 | 74 |
Red phosphorus powder addition amount/%) | 24 | 24 | 24 |
Amount of paste added/%) | 1.5 | 2 | 1 |
Calcium carbonate powder addition amount/%) | 1.5 | 2 | 1 |
Air drying temperature/. degree.C | 25 | 27 | 30 |
Based on the above, the invention utilizes the chemical characteristic that potassium chloride, red phosphorus and calcium carbonate powder are easy to explode due to friction or impact after being mixed and dried to prepare the safe and reliable hammer, the product has good stability and low cost, and the product is filled in a material ring, has high safety and is convenient to transport.
It will be evident to those skilled in the art that the invention is not limited to the details of the foregoing illustrative embodiments, and that the present invention may be embodied in other specific forms without departing from the spirit or essential attributes thereof. The present embodiments are therefore to be considered in all respects as illustrative and not restrictive, the scope of the invention being indicated by the appended claims rather than by the foregoing description, and all changes which come within the meaning and range of equivalency of the claims are therefore intended to be embraced therein. Any reference sign in a claim should not be construed as limiting the claim concerned.
Claims (8)
1. A safe and reliable toy striker, the formula of which comprises: potassium chlorate powder, red phosphorus powder, thick liquid and calcium carbonate powder, its characterized in that: the mass percentage of each component is as follows: 73% of potassium chlorate powder, 24% of red phosphorus powder, 1.5% of paste and 1.5% of calcium carbonate powder.
2. A safe and reliable toy striker as claimed in claim 1, wherein: the particle size of the red phosphorus powder is larger than 200 meshes.
3. A safe and reliable toy hammer preparation method comprises the steps of firstly, premixing raw materials; step two, filtering and screening; step three, preparing a hammer; step four, drying and storing; the method is characterized in that:
in the first step, 73% of potassium chlorate powder, 24% of red phosphorus powder, 1.5% of paste and 1.5% of calcium carbonate powder are weighed for later use according to the sum of the mass percentages of the components being 1, the potassium chlorate powder is soaked in a proper amount of water, the red phosphorus powder, the paste and the calcium carbonate powder are added, and then the materials are repeatedly stirred until the materials are uniformly mixed to obtain a mixture;
in the second step, the mixture prepared in the first step is transferred into a filtering device and repeatedly filtered until the mixture becomes a gummy fluid medicament;
in the third step, the fluid medicine prepared in the second step is taken, firstly, the fluid medicine is injected into a material ring of a container through a medicine injection machine, then 80g of kraft paper is covered, and the paper card is bonded with a PVC film for thermoplastic packaging to obtain a semi-finished product hammer;
in the fourth step, the hammer prepared in the third step is naturally dried to obtain a finished product hammer, and finally, the finished product hammer is packaged and stored according to the technological specification.
4. A method of making a safe and reliable toy striker as claimed in claim 3, wherein: in the first step, the raw materials are stirred in a manual kneading and mixing mode.
5. A method of making a safe and reliable toy striker as claimed in claim 3, wherein: in the second step, the filter screen used by the filtering equipment is 100 meshes.
6. A method of making a safe and reliable toy striker as claimed in claim 3, wherein: in the third step, the amount of the injected material of the material ring of the single container is 0.016 g.
7. A method of making a safe and reliable toy striker as claimed in claim 3, wherein: and in the third step, the paper card is provided with the plastic uptake oil.
8. A method of making a safe and reliable toy striker as claimed in claim 3, wherein: in the fourth step, the natural air drying temperature is 25-30 ℃.