CN110344556A - Ecological moss wall of the soft dress in a kind of interior and preparation method thereof - Google Patents
Ecological moss wall of the soft dress in a kind of interior and preparation method thereof Download PDFInfo
- Publication number
- CN110344556A CN110344556A CN201910749999.2A CN201910749999A CN110344556A CN 110344556 A CN110344556 A CN 110344556A CN 201910749999 A CN201910749999 A CN 201910749999A CN 110344556 A CN110344556 A CN 110344556A
- Authority
- CN
- China
- Prior art keywords
- moss
- dedicated
- interior
- scape
- parts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The present invention relates to indoor soft dress technical field, a kind of soft dress ecology moss wall in interior and preparation method thereof is specifically provided, comprising the following steps: (1) fixation medium density fiberboard;(2) fixed dead wood, lightweight volcanic rock;(3) the fixed glue of dedicated moss is coated;(4) the dedicated moss of scape is made in filled chamber;(5) it after making the dedicated moss material filling of scape to interior, removes interior and makes the moss fragment and extra colloid being mingled in the dedicated moss material of scape, and fix ornament on dead wood;(6) dry solidification 24 hours under natural conditions.Bryophyte used in the soft dress moss wall is through processing afterwards without late maintainings such as illumination, irrigation, fertilisings, it being capable of the original color of long sustaining and texture, landscape effect novel and unique, and also have the characteristics that frivolous, fade-proof, moisture-proof, easy construction, applied widely with the moss wall that this method makes.
Description
Technical field
The present invention relates to indoor soft dress technical fields, more particularly to a kind of ecological moss wall of the soft dress in interior and its preparation side
Method.
Background technique
In recent years, application of the bryophyte in vertical planting is more and more wider, and bryophyte element is gradually dissolved into wall
Landscape, courtyard landscape design, in rainforest landscape, bryophyte landscape is also increasingly subject to pursuing for people.Traditional moss wall scape
The way of sight be with irrigate, light filling equipment is that fresh and alive bryophyte builds suitable growing environment, but exist maintenance difficulty compared with
Greatly, the disadvantages of manpower and material resources investment is high.Occur recent years not needing " immortal moss " material of maintenance on the market, for interior
Soft dress provides new thinking.
" immortal moss " is in fact not moss material, but with a kind of small shrub shape lichen of entitled deer stamen
It is made for raw material is processed.The material can keep color and form for a long time, gradually be used as wall body decoration, but
Product quality on the market is irregular, is limited by processing technology, and some " immortal moss " materials take off there are the easy moisture absorption, easily
Color has the defects of peculiar smell.Therefore, in face of the great demand in indoor soft dress moss market, develop it is a kind of it is more practical, effect is more longlasting
Moss wall production method, have important application value.
Summary of the invention
The purpose of the invention is to provide ecological moss wall of the soft dress in a kind of interior and preparation method thereof, the present invention is used
Technical solution be:
The soft preparation method for filling ecological moss wall in a kind of interior, comprising the following steps: (1) in having been tailored according to design drawing
Fine plate is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element;It (2) will be withered
Wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) it is coated specially in each color block areas of medium density fiberboard
Glue is fixed with moss;(4) the dedicated moss material of scape is made by color filling to corresponding color block areas in processed interior, uses hand
It makes the dedicated moss material of scape and its root and the fixed glue of dedicated moss is in close contact in pressing interior;(5) to make scape to interior dedicated
After moss material is filled, removes interior and make the moss fragment and extra colloid being mingled in the dedicated moss material of scape, and
Ornament is fixed on dead wood;(6) dry solidification 24 hours under natural conditions.
Preferably, the fixing means of dead wood described in step (2), lightweight volcanic rock are as follows: on dead wood, lightweight volcanic rock
It punches respectively, the pre-buried nylon expansion tube of corresponding position on metope, the hole on dead wood or lightweight volcanic rock is then passed through with screw
And it is screwed into expansion tube fixed.
Preferably, medium density fiberboard with a thickness of 2.5mm.
Preferably, the fixed glue of dedicated moss with a thickness of 2-3mm.
Preferably, when making the dedicated moss material of scape in step (4) in filled chamber, the dedicated moss of scape is made in selected interior
The thickness of material is close, and to hide the seam at two pieces of different color blocks Local handovers.
Preferably, the fixed glue of dedicated moss by the hydroxypropyl methyl celluloses of 10-15 parts by weight, 2-4 parts by weight poly- third
Acrylamide, the food-grade dextrin of 5-8 parts by weight, the polyvinyl alcohol of 3-5 parts by weight, the dehydroactic acid sodium of 1-2 parts by weight, 1-2 weight
Measure part concentration lemon extract and 1000-1500 parts by weight pure water compound after heated, cool down it is obtained.
Preferably, it is white hair moss or big hypnum moss by screening, removal of impurities, high pressure that the dedicated moss material of scape is made in the interior
Made from moise-heat sterilization inactivation treatment, reagent processing and air-dried processing.
A kind of ecological moss wall of the soft dress in the interior according to obtained by the above method.
Compared with the prior art, the present invention has the following advantages: bryophyte used in the soft dress moss wall is through processing
Afterwards without the late maintainings such as illumination, irrigation, fertilising, can the original color of long sustaining and texture, landscape effect novel and unique,
And also has the characteristics that frivolous, fade-proof, moisture-proof, easy construction, applied widely with the moss wall that this method makes.
Specific embodiment
With reference to embodiment, the specific embodiment of the present invention is further described.Following embodiment is only used for more
Add and clearly demonstrate technical solution of the present invention, and not intended to limit the protection scope of the present invention.
Specific embodiments of the present invention are:
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard, fixing means are as follows: dead wood,
It is punched respectively on lightweight volcanic rock, the pre-buried nylon expansion tube of corresponding position on metope, then passes through dead wood or lightweight with screw
Hole on volcanic rock is simultaneously screwed into expansion tube fixed;(3) consolidate in the dedicated moss that each color block areas of medium density fiberboard coats 2-3mm thickness
Determine glue;(4) the dedicated moss material of scape is made by color filling to corresponding color block areas in processed interior, is pressed with hand indoor
Making the dedicated moss material of scape is in close contact its root and the fixed glue of dedicated moss, and the fixed glue of dedicated moss can be clung with moment
The dedicated moss material of scape is made in interior, in the short time colloid will not desiccation, can arbitrarily remove or be bonded again;(5) it is made to interior
The dedicated moss material filling of scape finishes post-processing detailed problem, and such as it is broken to make the moss being mingled in the dedicated moss material of scape for removing interior
Piece and extra colloid, polishing seam etc., and ornament is fixed on dead wood, such as Tillandsia;(6) dry solid under natural conditions
Change 24 hours, must not firmly be squeezed in this 24 hours or the dedicated moss material of scape is made in touching interior, to the fixed glue of dedicated moss
More violent external force could be resisted after thorough dry solidification.Being made in the later period maintenance of scape ecology moss wall indoors should be avoided spray
Water avoids being in it in wet environment for a long time.
When making the dedicated moss material of scape in step (4) in filled chamber, the dedicated moss material of scape is made into the interior of gap two sides
Expect to squeeze to gap direction, the seam between moss material is hidden with this, meanwhile, selected interior makes the dedicated moss material of scape
The thickness of material is close, to avoid apparent height fall is generated.
The fixed glue of dedicated moss in step (3) is by the hydroxypropyl methyl celluloses of 10-15 parts by weight, 2-4 parts by weight
Polyacrylamide, the food-grade dextrin of 5-8 parts by weight, the polyvinyl alcohol of 3-5 parts by weight, the dehydroactic acid sodium of 1-2 parts by weight, 1-
The concentration lemon extract of 2 parts by weight and the pure water composition of 1000-1500 parts by weight.The fixed glue of dedicated moss the preparation method comprises the following steps:
Hydroxypropyl methyl cellulose, the polyacrylamide, food-grade dextrin, polyvinyl alcohol, dehydroactic acid of above-mentioned parts by weight are weighed respectively
Sodium, concentration lemon extract, obtain pulvis after mixing, then prepare a certain amount of pure water with reverse osmosis water purification machine;By pulvis
Be added in 35 DEG C of pure water, be sufficiently stirred until solution become translucent paste, then at room temperature cool down.
It is white hair moss or big hypnum moss by screening, removal of impurities, disinfection with high pressure steam inactivation that the dedicated moss material of scape is made in interior
Made from processing, reagent processing and air-dried processing.Comprise the concrete steps that: screening: choose plant it is complete, it is homogeneous, without lesion
Bryophyte material;Removal of impurities: the sundries of bryophyte material surface and root is rejected;Disinfection with high pressure steam inactivation treatment;Examination
Agent processing: dedicated moss reagent treatment is sprayed at bryophyte material surface in spraying form;Air-dry processing: dry logical
Natural air drying under the conditions of wind.Wherein dedicated moss reagent treatment is by 78 parts of colorant, 52 parts of filler, 15 parts of bonding
Agent, 3 parts of lubricant, 2 parts of preservative and 1000 parts of pure water compounding are made.Dedicated moss reagent treatment is by 78 parts
Colorant, 52 parts of filler, 15 parts of binder, 3 parts of lubricant, 2 parts of preservative after mixing, on a small quantity in multiple times
It is added in the pure water of 1000ml, heats while stirring, stop heating when solution is warming up to 85 DEG C, be cooled to room temperature to solution
When up to dedicated moss reagent treatment.
Embodiment 1
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each color lump of medium density fiberboard
Coat the fixed glue of dedicated moss of 2mm thickness in region;(4) by processed interior make the dedicated moss material of scape by color filling to pair
The color block areas answered makes the dedicated moss material of scape with hand pressing interior and its root and dedicated moss is made to fix glue close contact;
(5) the dedicated moss material filling of scape being made to interior and finishing post-processing detailed problem, removing interior, which is made in the dedicated moss material of scape, to press from both sides
Miscellaneous moss fragment and extra colloid, polishing seam etc., and Tillandsia is fixed on dead wood;(6) dry under natural conditions
Solidification 24 hours.
The fixed glue of dedicated moss the preparation method comprises the following steps: weighing 10 parts of hydroxypropyl methyl cellulose, 4 parts of polypropylene respectively
Amide, 5 parts of food-grade dextrin, 5 parts of polyvinyl alcohol, 1 part of dehydroactic acid sodium, 2 parts of concentration lemon extract are uniformly mixed
After obtain pulvis, then with reverse osmosis water purification machine prepare 1000ml pure water;Pulvis is added in 40 DEG C of pure water, is sufficiently stirred
Until solution becomes translucent paste, then cool down at room temperature.
The preparation method that the dedicated moss material of scape is made in interior is: screening: choose plant it is complete, it is homogeneous, without lesion
Bryophyte material;Removal of impurities: the sundries of bryophyte material surface and root is rejected;Disinfection with high pressure steam inactivation treatment;Examination
Agent processing: dedicated moss reagent treatment is sprayed at bryophyte material surface in spraying form;Air-dry processing: dry logical
Natural air drying under the conditions of wind.Wherein, dedicated moss reagent treatment is by 78 parts of colorant, 52 parts of filler, 15 parts
Binder, 3 parts of lubricant, 2 parts of preservative after mixing, are added in the pure water of 1000ml in multiple times on a small quantity, while stirring
Side heating is mixed, stops heating when solution is warming up to 85 DEG C, up to dedicated moss reagent treatment when solution is cooled to room temperature.
Embodiment 2
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each color lump of medium density fiberboard
Coat the fixed glue of dedicated moss of 3mm thickness in region;(4) by processed interior make the dedicated moss material of scape by color filling to pair
The color block areas answered makes the dedicated moss material of scape with hand pressing interior and its root and dedicated moss is made to fix glue close contact;
(5) the dedicated moss material filling of scape being made to interior and finishing post-processing detailed problem, removing interior, which is made in the dedicated moss material of scape, to press from both sides
Miscellaneous moss fragment and extra colloid, polishing seam etc., and Tillandsia is fixed on dead wood;(6) dry under natural conditions
Solidification 24 hours.
The fixed glue of dedicated moss the preparation method comprises the following steps: weighing 15 parts of hydroxypropyl methyl cellulose, 2 parts of polypropylene respectively
Amide, 8 parts of food-grade dextrin, 3 parts of polyvinyl alcohol, 2 parts of dehydroactic acid sodium, 1 part of concentration lemon extract are uniformly mixed
After obtain pulvis, then with reverse osmosis water purification machine prepare 1500ml pure water;Pulvis is added in 30 DEG C of pure water, is sufficiently stirred
Until solution becomes translucent paste, then cool down at room temperature.
The dedicated moss material of scape and dedicated moss reagent treatment are made in interior, and the preparation method is the same as that of Example 1.
Embodiment 3
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each color lump of medium density fiberboard
Coat the fixed glue of dedicated moss of 2.5mm thickness in region;(4) the dedicated moss material of scape is made in processed interior to arrive by color filling
Corresponding color block areas, is made the dedicated moss material of scape its root is made to fix glue with dedicated moss and closely connect with hand pressing interior
Touching;(5) the dedicated moss material filling of scape is made to interior and finish post-processing detailed problem, remove interior and make in the dedicated moss material of scape
The moss fragment and extra colloid that are mingled with, polishing seam etc., and Tillandsia is fixed on dead wood;(6) it is done under natural conditions
Dry solidification 24 hours.
The fixed glue of dedicated moss the preparation method comprises the following steps: weighing 12 parts of hydroxypropyl methyl cellulose, 3 parts of polypropylene respectively
Amide, 6 parts of food-grade dextrin, 4 parts of polyvinyl alcohol, 1 part of dehydroactic acid sodium, 2 parts of concentration lemon extract are uniformly mixed
After obtain pulvis, then with reverse osmosis water purification machine prepare 1200ml pure water;Pulvis is added in 35 DEG C of pure water, is sufficiently stirred
Until solution becomes translucent paste, then cool down at room temperature.
The dedicated moss material of scape is made in interior, and the preparation method is the same as that of Example 1.
Embodiment 4
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each color lump of medium density fiberboard
Coat the fixed glue of dedicated moss of 2mm thickness in region;(4) by processed interior make the dedicated moss material of scape by color filling to pair
The color block areas answered makes the dedicated moss material of scape with hand pressing interior and its root and dedicated moss is made to fix glue close contact;
(5) the dedicated moss material filling of scape being made to interior and finishing post-processing detailed problem, removing interior, which is made in the dedicated moss material of scape, to press from both sides
Miscellaneous moss fragment and extra colloid, polishing seam etc., and Tillandsia is fixed on dead wood;(6) dry under natural conditions
Solidification 24 hours.
The fixed glue of dedicated moss the preparation method comprises the following steps: weighing 14 parts of hydroxypropyl methyl cellulose, poly- the third of 3.5 parts respectively
Acrylamide, 7 parts of food-grade dextrin, 5 parts of polyvinyl alcohol, 2 parts of dehydroactic acid sodium, 1 part of concentration lemon extract, mixing are equal
Pulvis is obtained after even, then prepares 1300ml pure water with reverse osmosis water purification machine;Pulvis is added in 38 DEG C of pure water, is sufficiently stirred
Mix until solution become translucent paste, then at room temperature cool down.
The dedicated moss material of scape is made in interior, and the preparation method is the same as that of Example 1.
Embodiment 5
A kind of interior soft preparation method for filling ecological moss wall, comprising the following steps: (1) will have been tailored according to design drawing
The medium density fiberboard of 2.5mm thickness is fixed on metope, the point for sketching out each color block areas in medium density fiberboard with marking pen, respectively making scape element
Position;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each color lump of medium density fiberboard
Coat the fixed glue of dedicated moss of 3mm thickness in region;(4) by processed interior make the dedicated moss material of scape by color filling to pair
The color block areas answered makes the dedicated moss material of scape with hand pressing interior and its root and dedicated moss is made to fix glue close contact;
(5) the dedicated moss material filling of scape being made to interior and finishing post-processing detailed problem, removing interior, which is made in the dedicated moss material of scape, to press from both sides
Miscellaneous moss fragment and extra colloid, polishing seam etc., and Tillandsia is fixed on dead wood;(6) dry under natural conditions
Solidification 24 hours.
The fixed glue of dedicated moss the preparation method comprises the following steps: weighing 15 parts of hydroxypropyl methyl cellulose, 3 parts of polypropylene respectively
Amide, 6 parts of food-grade dextrin, 5 parts of polyvinyl alcohol, 1.5 parts of dehydroactic acid sodium, 1.5 parts of concentration lemon extract, mixing
Pulvis is obtained after uniformly, then prepares 1500ml pure water with reverse osmosis water purification machine;Pulvis is added in 40 DEG C of pure water, sufficiently
Stirring becomes translucent paste up to solution, then cools down at room temperature.
The dedicated moss material of scape is made in interior, and the preparation method is the same as that of Example 1.
What has been described above is only a preferred embodiment of the present invention, it is noted that for those skilled in the art,
Without depart from that overall concept of the invention, several changes and improvements can also be made, these also should be considered as of the invention
Protection scope.
Claims (8)
1. a kind of soft preparation method for filling ecological moss wall in interior, it is characterised in that: the following steps are included: (1) will be according to design
The medium density fiberboard that drawing has been tailored is fixed on metope, is sketched out each color block areas in medium density fiberboard with marking pen, is respectively made Jing Yuansu
Point;(2) dead wood, lightweight volcanic rock are separately fixed at the point for making scape element in medium density fiberboard;(3) in each of medium density fiberboard
Color block areas coats the fixed glue of dedicated moss;(4) the dedicated moss material of scape is made by color filling to correspondence in processed interior
Color block areas, make that the dedicated moss material of scape makes its root and dedicated moss fixes glue and is in close contact with hand pressing interior;(5)
After making scape dedicated moss material filling to interior, removes interior and make the moss fragment being mingled in the dedicated moss material of scape and more
Remaining colloid, and ornament is fixed on dead wood;(6) dry solidification 24 hours under natural conditions.
2. a kind of soft preparation method for filling ecological moss wall in interior according to claim 1, it is characterised in that: step (2)
Described in dead wood, lightweight volcanic rock fixing means are as follows: punched respectively on dead wood, lightweight volcanic rock, it is corresponding on metope
Then the pre-buried nylon expansion tube in position passes through the hole on dead wood or lightweight volcanic rock with screw and is screwed into expansion tube fixed.
3. a kind of soft preparation method for filling ecological moss wall in interior according to claim 1, it is characterised in that: in described
Fine plate with a thickness of 2.5mm.
4. a kind of soft preparation method for filling ecological moss wall in interior according to claim 2, it is characterised in that: described is special
With moss fix glue with a thickness of 2-3mm.
5. a kind of soft preparation method for filling ecological moss wall in interior according to claim 4, it is characterised in that: the step
When making the dedicated moss material of scape in (4) in filled chamber suddenly, the thickness that the dedicated moss material of scape is made in selected interior is close, and
Hide the seam at two pieces of different color blocks Local handovers.
6. a kind of soft preparation method for filling ecological moss wall in interior according to claim 5, it is characterised in that: described is special
Glue is fixed by the hydroxypropyl methyl cellulose of 10-15 parts by weight, the polyacrylamide of 2-4 parts by weight, 5-8 parts by weight with moss
Food-grade dextrin, the polyvinyl alcohol of 3-5 parts by weight, the dehydroactic acid sodium of 1-2 parts by weight, 1-2 parts by weight concentration lemon extract
It is obtained with being heated, being cooled down after the pure water compounding of 1000-1500 parts by weight.
7. a kind of soft preparation method for filling ecological moss wall in interior according to claim 5, it is characterised in that: the room
Inside make the dedicated moss material of scape be white hair moss or big hypnum moss by screening, removal of impurities, disinfection with high pressure steam inactivation treatment, reagent at
Made from reason and air-dried processing.
8. a kind of ecological moss wall of the soft dress in interior, it is characterised in that: the ecological moss wall of the soft dress in interior is wanted according to right
It asks made from any preparation method of 1-7.