CN109868009A - A kind of water-soluble lipid wax crayon artistic oil painting stick and preparation method thereof - Google Patents
A kind of water-soluble lipid wax crayon artistic oil painting stick and preparation method thereof Download PDFInfo
- Publication number
- CN109868009A CN109868009A CN201910214103.0A CN201910214103A CN109868009A CN 109868009 A CN109868009 A CN 109868009A CN 201910214103 A CN201910214103 A CN 201910214103A CN 109868009 A CN109868009 A CN 109868009A
- Authority
- CN
- China
- Prior art keywords
- parts
- oil painting
- wax
- wax crayon
- painting stick
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to the preparation fields of water soluble crayon artistic oil painting stick, provide a kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material includes at least, 5-15 parts of peregals, 20-40 parts of waxes, 5-15 parts of builders, 1-6 parts of color filling material, 1-12 parts of titanium dioxides, 15-30 parts of filler materials;Additionally provide the preparation method of lipid wax crayon artistic oil painting stick.
Description
Technical field
The present invention relates to the preparation field of water soluble crayon artistic oil painting stick, further relate to a kind of water-soluble lipid wax crayon artistic oil painting stick and
Preparation method.
Background technique
Currently, children's paintbrush product is relatively more, such as children's wax crayon, and artistic oil painting stick, the products comparative maturity such as watercolor pencil, but it is raw
Material is produced, technology is still more traditional;Their function is relatively single, has nothing in common with each other.Two kinds of drawing works of wax crayon and artistic oil painting stick
Tool is widely used at present, but is limited by conventional formulation, and that there are color densities is not high for wax crayon, and color is not firm and not full,
The disadvantages of color is not beautiful enough.Although artistic oil painting stick color density is high, color is beautiful, is easy to pollute user.It is domestic
There are many artistic oil painting stick, but are all waxes and cannot dissolve mostly, and lines are thick, therefore paintings are inflexible stiff.
Summary of the invention
The first aspect of the invention provides a kind of water-soluble lipid wax crayon oil in order to solve the above technical problems
Stick is drawn, by weight, raw material includes at least, 5-15 parts of peregals, 20-40 parts of waxes, 5-15 parts of builders, and 1-6 parts of colors are filled out
Charge, 1-12 parts of titanium dioxides, 15-30 parts of filler materials.
As a kind of perferred technical scheme, heretofore described lipid wax crayon artistic oil painting stick, by weight, raw material is extremely
It less include 10-13 parts of peregals, 25-35 parts of waxes, 8-12 parts of builders, 2-5 parts of color filling material, 3-9 parts of titanium dioxides, 20-25
Part filler material.
As a kind of perferred technical scheme, heretofore described lipid wax crayon artistic oil painting stick, by weight, raw material is extremely
It less include 11 parts of peregals, 30 parts of waxes, 10 parts of builders, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials.
As a kind of perferred technical scheme, heretofore described wax is one of microwax, paraffin, liquid wax or a variety of
Combination.
As a kind of perferred technical scheme, the weight ratio between heretofore described paraffin and the liquid wax is 1:
(0.1-0.8)。
As a kind of perferred technical scheme, heretofore described builder is OP-10.
As a kind of perferred technical scheme, the weight ratio between heretofore described color filling material and titanium dioxide is
1:(1-2).
As a kind of perferred technical scheme, heretofore described filler material is selected from talcum powder, land plaster, lithopone, light
One of calcium powder or a variety of combinations.
As a kind of perferred technical scheme, the granularity of heretofore described light calcium carbonate powder is 800-2500 mesh;The vertical moral
Powder Particle Size is 1000-2000 mesh;The flexural strength of the land plaster is 1-10MPa;The granularity of the talcum powder is 500-3500
Mesh.
The second aspect of the invention provides a kind of preparation method of lipid wax crayon artistic oil painting stick, includes at least following
Step:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 90-100 DEG C, is sufficiently stirred, and reacts
1-3 hours, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 80 DEG C -90 DEG C, is kept for 80 DEG C -90 DEG C and inserts titanium dioxide, filling into reaction kettle
Material, color filling material are sufficiently stirred, and stirring obtains final mixture in 0.5-2 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
The utility model has the advantages that
The present invention provides a kind of lipid wax crayon artistic oil painting stick, raw material is easily selected and is easy to get, and preparation process is simple, and very ring
It protects, it is non-toxic and tasteless not damage user's skin;Wax crayon artistic oil painting stick shape provided in the present invention looks like kind of a wax crayon, Ke Yiyong
Carry out making crayon drawing as wax crayon, it is not only neither too hard, nor too soft, it is smooth in use process and fine and smooth, and by the paintings hand finished dip in water or
Paintbrush dips in crayon drawing is further depicted as after water after, will form and become a kind of watercolor, colorfulness has been more than traditional oil painting stick, more
Space rich in imagination space and performance facilitates children and generates interest to drawing.
Each side's region feature, content described in previous section in the present invention and excellent is easier to understand with reference to following details
Point.
Specific embodiment
Unless otherwise indicated, from context cues or belong to the convention of the prior art, otherwise number all in the application
It is all based on weight with percentage, and test and characterizing method used is all synchronous with the submission date of the application.If existing
There is the definition particularly belonged to disclosed in technology inconsistent with any definition provided herein, then with provided herein
Subject to term definition.
Technical characteristic in technical solution provided by the invention is made With reference to embodiment further clear, complete
Description, not to the limitation of its protection scope.
Word " preferred ", " preferred ", " preferably " in the present invention etc. refer to, can provide certain in some cases
The embodiment of the present invention of a little beneficial effects.However, other embodiments may also under identical circumstances or in the case of other
It is preferred.In addition, do not imply that other schemes are unavailable to the statement of one or more preferred embodiments, also not purport
It is excluded except the scope of the present invention by other embodiments.The source of unmentioned component is commercially available in the present invention.
The first aspect of the invention provides a kind of water-soluble lipid wax crayon artistic oil painting stick, and by weight, raw material is extremely
It less include 5-15 parts of peregals, 20-40 parts of waxes, 5-15 parts of builders, 1-6 parts of color filling material, 1-12 parts of titanium dioxides, 15-30
Part filler material.
In some embodiments, the lipid wax crayon artistic oil painting stick, by weight, raw material includes at least, and 10-13 parts flat
It is flat to add, 25-35 parts of waxes, 8-12 parts of builders, 2-5 parts of color filling material, 3-9 parts of titanium dioxides, 20-25 parts of filler materials.
In some embodiments, the lipid wax crayon artistic oil painting stick, by weight, raw material includes at least, and 11 parts average
Add, 30 parts of waxes, 10 parts of builders, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials.
Peregal
Heretofore described peregal can buy the ten thousand new material Co., Ltd from Guangzhou, and model O-25 can also
To buy from other sources.
Wax
In some embodiments, it is one of microwax, paraffin, liquid wax or a variety of groups that the wax, which is the wax,
It closes;Preferably, the wax is one of paraffin, liquid wax or a variety of combinations;It is furthermore preferred that the wax is paraffin, liquid wax
Combination.
In some embodiments, the weight ratio between the paraffin and the liquid wax is 1:(0.1-0.8);Preferably,
Weight ratio between the paraffin and the liquid wax is 1:(0.2-0.6);It is furthermore preferred that between the paraffin and the liquid wax
Weight ratio is 1:0.4.
Heretofore described paraffin can purchase from Suzhou Chen Hang Fine Chemical Co., Ltd, paraffin-crystal form wax, and the trade mark is
58# can also be bought from other companies.
Heretofore described liquid wax is commercially available from Guangzhou Jin Quan Chemical Co., Ltd., and trade mark 300# can also be bought certainly
Other companies.
Builder
In some embodiments, the builder is OP-10.
The OP-10 is polyoxethylene octylphenyl phenol ether -10, be can purchase from the prosperous Yu Da trade Co., Ltd in Jinan, can also
To buy from other companies.
Color filling material
In some embodiments, the color filling material is dyestuff and/or pigment;Preferably, the color filling material
For dyestuff.
In some embodiments, the pigment is selected from chrome yellow, phthalocyanine blue, phthalocyanine green, bright red, permanent yellow, ultramarine, charcoal
At least one of black, forever solid orange, permanent yellow.
Heretofore described dye colour does not do particular determination, it is preferred that the dyestuff be selected from transparent yellow, transparent blue, thoroughly
It is bright at least one of red.
In some embodiments, the various colors of the dyestuff can be deployed in proportion by transparent yellow, transparent blue, transparent red
Out.
Titanium dioxide
In some embodiments, the weight ratio between the color filling material and titanium dioxide is 1:(1-2);It is preferred that
, the weight ratio between the color filling material and titanium dioxide is 1:(1.5-1.8);It is furthermore preferred that the color filling material
Weight ratio between titanium dioxide is 1:1.75.
Heretofore described titanium dioxide is selected from one of anatase thpe white powder, rutile titanium white powder or a variety of combinations;
Preferably, the titanium dioxide is rutile titanium white powder.
Filler material
In some embodiments, the filler material be selected from one of talcum powder, land plaster, lithopone, light calcium carbonate powder or
A variety of combinations;Preferably, the filler material is selected from one of lithopone, light calcium carbonate powder or a variety of combinations;It is furthermore preferred that institute
State the combination that filler material is lithopone, light calcium carbonate powder.
In some embodiments, the lithopone, light calcium carbonate powder weight ratio be 1:(4-10);Preferably, the vertical moral
Powder, light calcium carbonate powder weight ratio be 1:(6-8);It is furthermore preferred that the weight ratio of the lithopone, light calcium carbonate powder is 1:7.
In some embodiments, the granularity of the light calcium carbonate powder is 800-2500 mesh;The lithopone granularity is 1000-
2000 mesh;The flexural strength of the land plaster is 1-10MPa;The granularity of the talcum powder is 500-3500 mesh.
In some preferred embodiments, the granularity of the light calcium carbonate powder is 1000-1500 mesh;The lithopone granularity is
1200-1800 mesh;The flexural strength of the land plaster is 2.3-9.5MPa;The granularity of the talcum powder is 1250-2000 mesh.
In some further preferred embodiments, the granularity of the light calcium carbonate powder is 1250 mesh;The lithopone granularity is
1500 mesh;The flexural strength of the land plaster is 5.1MPa;The granularity of the talcum powder is 1500 mesh.
The second aspect of the invention provides a kind of preparation method of lipid wax crayon artistic oil painting stick, includes at least following
Step:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 90-100 DEG C, is sufficiently stirred, and reacts
1-3 hours, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 80 DEG C -90 DEG C, is kept for 80 DEG C -90 DEG C and inserts titanium dioxide, filling into reaction kettle
Material, color filling material are sufficiently stirred, and stirring obtains final mixture in 0.5-2 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
In some preferred embodiments, the preparation method of the lipid wax crayon artistic oil painting stick, at least includes the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 95-100 DEG C, is sufficiently stirred, and reacts
1.5-2.5 hour is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 85 DEG C -90 DEG C, is kept for 85 DEG C -90 DEG C and inserts titanium dioxide, filling into reaction kettle
Material, color filling material are sufficiently stirred, and stirring obtains final mixture in 1-1.5 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
In some preferred embodiments, the preparation method of the lipid wax crayon artistic oil painting stick includes at least following step
It is rapid:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
The present invention provides a kind of lipid wax crayon artistic oil painting stick, raw material is easily selected and is easy to get, and preparation process is simple, and very ring
It protects, it is non-toxic and tasteless not damage user's skin;And the present invention solves wax crayon and artistic oil painting stick is limited by conventional formulation, in color
The disadvantages of color aspect seems not firm and not full, and color is not beautiful enough, wax crayon artistic oil painting stick shape provided in the present invention seems
It is kind of a wax crayon, may be used as wax crayon and draw a picture, not only neither too hard, nor too soft, smooth and fine and smooth in use process, applicant speculates, this
The liquid wax of invention in the feed can be not only used in compounding with paraffin, can be improved the hardness of wax crayon artistic oil painting stick, be write it
Carry out more delicate and smooth, and it is found by the applicant that wax crayon oil can be improved under the action of liquid wax after titanium dioxide and dyestuff compounding
The coloring degree of stick is drawn, not only degree of scatter of the color filling material in wax crayon artistic oil painting stick improves, and makes it than common wax crayon in face
It more full can enrich, be in bright colors, and using effect is finer and smoother, applicant surprisingly sends out in addition to this in terms of colour saturation
Crayon drawing is described after now dipping in water by the paintings of wax crayon or artistic oil painting stick progress paintbrush or dip in water with hand, will form and become a kind of watercolor
Draw, colorfulness has been more than traditional oil painting stick, due to color can changeable and various colors can for child juvenile in painting process
There is the space of bigger imagination space and performance, facilitates children and interest is generated to drawing, possible cause is to be added in the feed
A certain amount of OP-10 and peregal generate the coloring properties of excellent concertedness and dyestuff, can not only improve each group in raw material
The dissolubility of part in water, additionally it is possible to keep component dispersibility in its raw material more preferable, therefore appear more like watercolor and color of light
It is bright-coloured beautiful.
The present invention is specifically described below by embodiment, once embodiment is only used for the present invention and does further
Illustrate, can not be interpreted as the limitation that the present invention protects, professional and technical personnel in the field makes according to the content of foregoing invention
Nonessential correction and adjustment, still fall within the range of protection of the invention.
Embodiment 1
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 11 parts of peregals, 30 parts of waxes, 10 parts are helped
Lotion, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.4;It is described to help
Lotion is OP-10;The color filling material is transparent red;The titanium dioxide is rutile titanium white powder;The color filling material and
Weight ratio between titanium dioxide is 1:1.75;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium
The weight ratio of powder is 1:7;The lithopone granularity is 1500 mesh;The granularity of the light calcium carbonate powder is 1250 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 2
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material includes 5 parts of peregals, 20 parts of waxes, and 5 parts are helped and wash
Agent, 1 part of color filling material, 1 part of titanium dioxide, 15 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.1;It is described to help
Lotion is OP-10;The color filling material is transparent yellow;The titanium dioxide is rutile titanium white powder;The color filling material and
Weight ratio between titanium dioxide is 1:1;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder
Weight ratio is 1:4;The lithopone granularity is 1000 mesh;The granularity of the light calcium carbonate powder is 800 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 90 DEG C, is sufficiently stirred, and reaction 1 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 80 DEG C, is kept for 80 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 0.5 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 3
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 15 parts of peregals, 40 parts of waxes, 15 parts are helped
Lotion, 6 parts of color filling material, 12 parts of titanium dioxides, 30 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.8;It is described to help
Lotion is OP-10;The color filling material is transparent blue;The titanium dioxide is rutile titanium white powder;The color filling material and
Weight ratio between titanium dioxide is 1:2;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder
Weight ratio is 1:10;The lithopone granularity is 2000 mesh;The granularity of the light calcium carbonate powder is 2500 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 3 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 2 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 4
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 10 parts of peregals, 25 parts of waxes, 8 parts are helped
Lotion, 2 parts of color filling material, 3 parts of titanium dioxides, 20 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.2;It is described to help
Lotion is OP-10;The color filling material is phthalocyanine blue;The titanium dioxide is rutile titanium white powder;The color filling material and
Weight ratio between titanium dioxide is 1:1.5;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder
Weight ratio be 1:6;The lithopone granularity is 1200 mesh;The granularity of the light calcium carbonate powder is 1000 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 95 DEG C, is sufficiently stirred, and reaction 1.5 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 85 DEG C, is kept for 85 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 5
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 13 parts of peregals, 35 parts of waxes, 12 parts are helped
Lotion, 5 parts of color filling material, 9 parts of titanium dioxides, 25 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.6;It is described to help
Lotion is OP-10;The color filling material is phthalocyanine green;The titanium dioxide is rutile titanium white powder;The color filling material and
Weight ratio between titanium dioxide is 1:1.8;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder
Weight ratio be 1:8;The lithopone granularity is 1800 mesh;The granularity of the light calcium carbonate powder is 1500 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, reaction 2.5
Hour, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1.5 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 6
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 11 parts of peregals, 30 parts of waxes, 10 parts are helped
Lotion, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials;
The wax is paraffin;The builder is OP-10;The color filling material is transparent yellow, transparent blue, ratio 5:1;
The titanium dioxide is rutile titanium white powder;The filler material is the combination of lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder
Weight ratio is 1:7;The lithopone granularity is 1500 mesh;The granularity of the light calcium carbonate powder is 1250 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 7
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 11 parts of peregals, 30 parts of waxes, 10 parts are helped
Lotion, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:1.5;It is described to help
Lotion is OP-10;The color filling material is transparent yellow, transparent blue ratio 4:1;The titanium dioxide is rutile titanium white powder;Institute
State the combination that filler material is lithopone, light calcium carbonate powder;The lithopone, light calcium carbonate powder weight ratio be 1:7;The lithopone granularity is
1500 mesh;The granularity of the light calcium carbonate powder is 1250 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 8
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material includes 11 parts of peregals, 30 parts of waxes, 4 parts of face
Color filler material, 7 parts of titanium dioxides, 22 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.4;The face
Color filler material is transparent yellow, transparent blue weight ratio 3:1;The titanium dioxide is rutile titanium white powder;The filler material is vertical moral
The combination of powder, light calcium carbonate powder;The lithopone, light calcium carbonate powder weight ratio be 1:7;The lithopone granularity is 1500 mesh;It is described light
The granularity of calcium powder is 1250 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reacts 2 hours, preparation
At the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 9
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 11 parts of peregals, 30 parts of waxes, 10 parts are helped
Lotion, 4 parts of color filling material, 12 parts of titanium dioxides, 22 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.4;It is described to help
Lotion is OP-10;The color filling material is transparent red, transparent blue weight ratio 5:1;The titanium dioxide is rutile titanium white
Powder;Weight ratio between the color filling material and titanium dioxide is 1:3;The filler material is the combination of lithopone, light calcium carbonate powder;
The lithopone, light calcium carbonate powder weight ratio be 1:7;The lithopone granularity is 1500 mesh;The granularity of the light calcium carbonate powder is 1250
Mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Embodiment 10
A kind of water-soluble lipid wax crayon artistic oil painting stick, by weight, raw material include that 11 parts of peregals, 30 parts of waxes, 10 parts are helped
Lotion, 4 parts of color filling material, 2 parts of titanium dioxides, 22 parts of filler materials;
The wax is the combination of paraffin, liquid wax;Weight ratio between the paraffin and the liquid wax is 1:0.4;It is described to help
Lotion is OP-10;The color filling material is transparent yellow, transparent red, weight ratio 4:1;The titanium dioxide is rutile titanium white
Powder;Weight ratio between the color filling material and titanium dioxide is 1:0.5;The filler material is the group of lithopone, light calcium carbonate powder
It closes;The lithopone, light calcium carbonate powder weight ratio be 1:7;The lithopone granularity is 1500 mesh;The granularity of the light calcium carbonate powder is
1250 mesh;
The preparation method of the lipid wax crayon artistic oil painting stick, comprising the following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 100 DEG C, is sufficiently stirred, and reaction 2 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 90 DEG C, is kept for 90 DEG C and filling titanium dioxide, filler material, color are filled out into reaction kettle
Charge is sufficiently stirred, and stirring obtains final mixture in 1 hour;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.
Performance test
(1) degree of staining is tested: to the test that wax crayon artistic oil painting stick is coloured prepared by embodiment 1-10, it is divided into 5 grades,
Grade distinction standard is according to differentiation as follows:
Change of drawing on rubber material gently can adhere on rubber material, and degree of staining is good, be 5 grades;
It slightly exerts oneself, that is, can adhere on rubber material on rubber material, degree of staining is preferable, is 4 grades;
It slightly exerts oneself on rubber material, can just be attached on rubber material, degree of staining is general, is 3 grades;
It on rubber material, need to firmly can just be attached on rubber material, degree of staining is poor, is 2 grades;
When streaking on rubber material, biggish power need to be used, degree of staining is poor, is 1 grade;
Test result is as shown in table 1.
(2) the wax crayon artistic oil painting stick in embodiment 1-10 is subjected to fracture resistence force test, detection method is according to " wax crayon industry industry
Standard " it is detected;Test result is as shown in table 1.
(3) the wax crayon artistic oil painting stick in embodiment 1-10 is carried out using uniformity and smooth performance test;Use is sentenced later
Break its whether uniformly, it is whether smooth, whether have mark of break, whether color thick and heavy gorgeous, and test result is as shown in table 1.
(4) it dips in color effect after water: according to embodiment 1 and embodiment 2, embodiment 1 and embodiment 3, embodiment 1 and implementing
Example 4, embodiment 1 and embodiment 5, embodiment 6 and embodiment 3, embodiment 7 and embodiment 2, embodiment 8 and embodiment 2 are implemented
Example 9 is grouped with embodiment 2, embodiment 10 and embodiment 2, and picture two lines are adjacent, later with the white wax crayon oil painting for dipping in water
Stick draws lines between both threads, and observation dips in whether color uniformity, amalgamation and color after water is drawn are bright-coloured, and test is tied
Fruit is as shown in table 2.
1 the performance test results of table
Table 2 dips in the measure of merit after water
Embodiment combination | Effect after dipping in water |
Embodiment 1 and embodiment 2 | Uniform in color, amalgamation are excellent, bright in luster |
Embodiment 1 and embodiment 3 | Color uniformity is general, amalgamation is general, color is general |
Embodiment 1 and embodiment 4 | Color is general, amalgamation is general, color is general |
Embodiment 1 and embodiment 5 | Uniform in color, amalgamation are preferable, color is general |
Embodiment 6 and embodiment 3 | Uniform in color is bad, amalgamation is poor, color difference |
Embodiment 7 and embodiment 2 | Uniform in color is general, amalgamation is general, color is general |
Embodiment 8 and embodiment 2 | Uniform in color is bad, amalgamation is poor, color is poor |
Embodiment 9 and embodiment 2 | Uniform in color is bad, amalgamation is poor, color is poor |
Embodiment 10 and embodiment 2 | Uniform in color is general, amalgamation is general, color is general |
Example above-mentioned is merely illustrative, some features of the feature for explaining the disclosure.The attached claims
It is intended to the range as wide as possible for requiring to be contemplated that, and embodiments as presented herein is only according to all possible embodiment
Combined selection embodiment explanation.Therefore, the purpose of applicant is that the attached claims are not illustrated the present invention
Feature exemplary selectional restriction.And the progress in science and technology will be formed language express it is inaccurate due to and not
The possible equivalent being presently considered or son replacement, and these variations should also be interpreted in the conceived case by appended
Claim covering.
Claims (10)
1. a kind of water-soluble lipid wax crayon artistic oil painting stick, which is characterized in that by weight, raw material includes at least, and 5-15 parts average
Add, 20-40 parts of waxes, 5-15 parts of builders, 1-6 parts of color filling material, 1-12 parts of titanium dioxides, 15-30 parts of filler materials.
2. lipid wax crayon artistic oil painting stick as described in claim 1, which is characterized in that by weight, raw material includes at least, 10-
13 parts of peregals, 25-35 parts of waxes, 8-12 parts of builders, 2-5 parts of color filling material, 3-9 parts of titanium dioxides, 20-25 parts of filler materials.
3. lipid wax crayon artistic oil painting stick as described in claim 1, which is characterized in that by weight, raw material includes at least, and 11 parts
Peregal, 30 parts of waxes, 10 parts of builders, 4 parts of color filling material, 7 parts of titanium dioxides, 22 parts of filler materials.
4. lipid wax crayon artistic oil painting stick as described in any one of claims 1-3, which is characterized in that the wax be microwax, paraffin,
One of liquid wax or a variety of combinations.
5. lipid wax crayon artistic oil painting stick as claimed in claim 4, which is characterized in that the weight between the paraffin and the liquid wax
Than for 1:(0.1-0.8).
6. lipid wax crayon artistic oil painting stick as described in any one of claims 1-3, which is characterized in that the builder is OP-10.
7. lipid wax crayon artistic oil painting stick as described in any one of claims 1-3, which is characterized in that the color filling material and titanium white
Weight ratio between powder is 1:(1-2).
8. lipid wax crayon artistic oil painting stick as described in any one of claims 1-3, which is characterized in that the filler material is selected from talcum
One of powder, land plaster, lithopone, light calcium carbonate powder or a variety of combinations.
9. lipid wax crayon artistic oil painting stick as described in any one of claims 1-3, which is characterized in that the granularity of the light calcium carbonate powder is
800-2500 mesh;The lithopone granularity is 1000-2000 mesh;The flexural strength of the land plaster is 1-10MPa;The talcum
The granularity of powder is 500-3500 mesh.
10. a kind of preparation method of the lipid wax crayon artistic oil painting stick as described in claim any one of 1-9, which is characterized in that at least wrap
Include following steps:
(1) peregal, wax, builder are added in reaction kettle, hot melt is warming up to 90-100 DEG C, is sufficiently stirred, and reaction 1-3 is small
When, it is prepared into the first coagulated raw material;
(2) temperature of reaction kettle restores to 80 DEG C -90 DEG C, keep 80 DEG C -90 DEG C and into reaction kettle insert titanium dioxide, filler material,
Color filling material is sufficiently stirred, and stirring obtains final mixture in 0.5-2 hours;
(3) mixture being stirred is injected into automatic wax crayon artistic oil painting stick or wax crayon machine is produced in batches.