CN108625618A - It is a kind of not tear brick quick service method open for the rupture infiltration of toilet warterproof layer - Google Patents

It is a kind of not tear brick quick service method open for the rupture infiltration of toilet warterproof layer Download PDF

Info

Publication number
CN108625618A
CN108625618A CN201810644960.XA CN201810644960A CN108625618A CN 108625618 A CN108625618 A CN 108625618A CN 201810644960 A CN201810644960 A CN 201810644960A CN 108625618 A CN108625618 A CN 108625618A
Authority
CN
China
Prior art keywords
brickwork joint
toilet
quick service
joint
infiltration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201810644960.XA
Other languages
Chinese (zh)
Other versions
CN108625618B (en
Inventor
赵晟煜
陈俊华
高珊珊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Yi Bird Technology Co Ltd
Original Assignee
Chengdu Yi Bird Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Yi Bird Technology Co Ltd filed Critical Chengdu Yi Bird Technology Co Ltd
Priority to CN201810644960.XA priority Critical patent/CN108625618B/en
Publication of CN108625618A publication Critical patent/CN108625618A/en
Application granted granted Critical
Publication of CN108625618B publication Critical patent/CN108625618B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Brick quick service method is not torn open for the rupture infiltration of toilet warterproof layer, including (1) uses original adhering material in the ceramic tile brickwork joint of raked joint tool removal accomodation ground and metope the invention discloses a kind of;(2) remaining fine slag in brickwork joint is cleaned with water;(3) the uniform brushing organosilicon moisture repellent in the brickwork joint cleared up, makes it permeate and cures base in brickwork joint;(4) bicomponent epoxy resin glue is injected in backward brickwork joint to be dried, and is compacted;(5) after to be dried on remaining brickwork joint coating filling waterproof jointing agent;(6) after to be dried, quick service is completed.The ingenious water-resistance, crack resistance and high adhesiveness that epoxide resin material is utilized of the present invention; waterproofing protection is re-established at tiles in toilet brickwork joint; in conjunction with the extremely low characteristic of tiles in toilet surface permeability rate itself; build new toilet waterproofing structure layer; toilet warterproof performance, efficient quick can also be restored by not destroying toilet and integrally fitting up to achieving the effect that not tear open brick.

Description

It is a kind of not tear brick quick service method open for the rupture infiltration of toilet warterproof layer
Technical field
The present invention relates to toilet warterproof treatment technologies, in particular, being to be related to one kind to rupture for toilet warterproof layer Brick quick service method is not torn in infiltration open.
Background technology
For domestic premises, especially now high-rise or multilayer folk building, wherein the space of common water, as toilet, Kitchen etc. is required for carrying out water-proofing treatment, generated in normal water utilizing process to avoid resident family leaching to resident family of lower layer or its The house of his resident family impacts.Building immersion leak is not only to the concrete of the support of building structure itself and wall and metope Structure is impacted and is destroyed, but also causes irreversible damage to indoor furniture, seriously affects the quality of life of resident family.Cause This, for the big place of this kind of water consumption in toilet, the water-proofing treatment in finishing is most important.
However, some building building times are remote, limited by general waterproof material service life, along with some uses The influence of the external factor such as improper, the toilet warterproof layer in the building that some can be made more old rupture, Jin Eryin Send out percolating water situation;On the other hand, the construction party of some buildings or finishing person are because the problems such as sense of responsibility is inadequate, is to toilet mode Processing is not proper, and toilet warterproof layer rupture event also occurs after certain usage time and causes percolating water, to resident family itself And neighbours generate bad adventure in daily life.
It in the prior art, the problem of percolating water being caused for the rupture of toilet warterproof layer, often can only be by removing health Between, waterproof layer is set up again to solve.This scheme is although feasible effective, but time-consuming and laborious and cost is very high, removes health Between not only the equipment Removal disposed in toilet, also to retract ceramic tile, wipe extra filling off, be equivalent to again finishing health Between workload, the time of cost, and during this, resident family can not all use toilet at least at one week or more, ten Divide the costs such as packing material, new ceramic tile, the labour cost for influencing to live, and be related in the process also very high.
Invention content
To overcome the above problem in the prior art, a kind of novel, ingenious in design, energy of present invention offer is quickly and effectively Ground solve toilet warterproof layer rupture seepage problem and cost it is relatively low have no effect on live do not tear brick quick service method open.
The design of the present invention is established extremely low in full ceramic tile and general the tiles in toilet permeability rate of toilet laying itself On the basis of, due to the self-characteristic of tiles in toilet, the substantially impervious water in porcelain surface, the leakage of daily water consumption is substantially logical The splicing gap crossed between ceramic tile enters bottom, and inventor is creatively had found by the research to the direction, by using spy These gaps of other materials repairing, new waterproof layer is established based on ceramic tile surface, can equally reach waterproof effect, and realization is not torn open Except the quick effect for repairing toilet warterproof ability of sanitary equipment and ceramic tile.
To achieve the goals above, the technical solution adopted by the present invention is as follows:
It is a kind of not tear brick quick service method open for the rupture infiltration of toilet warterproof layer, include the following steps:
(1) original adhering material in the ceramic tile brickwork joint of raked joint tool removal accomodation ground and metope is used, exposing Brickwork joint depth at least 4mm, width are not less than 2mm;
(2) it cleans remaining fine slag in brickwork joint with water, ensures in brickwork joint without fine slag;
(3) the uniform brushing organosilicon moisture repellent in the brickwork joint cleared up, makes it permeate and cures base in brickwork joint, every meter The organosilicon moisture repellent dosage of brickwork joint is 45-55ml;
(4) after organosilicon moisture repellent drying, bicomponent epoxy resin glue is injected into brickwork joint, and be compacted, control compacting The surface of epoxide-resin glue afterwards keeps 1mm ± 0.2mm distances with ceramic tile surface;
(5) after epoxide-resin glue is completely dried, coating filling waterproof jointing agent, makes waterproof jointing on remaining brickwork joint Agent is combined with ceramic tile surface edge, and the waterproof jointing agent filled is not higher than ceramic tile surface;
(6) after the drying of waterproof jointing agent, quick service is completed;
Wherein, before quick service completion, apparent water mark cannot occur in accomodation ground and metope.
Specifically, the raked joint tool is chisel, perching knife or abrasive machine.
Specifically, when removing original adhering material in ceramic tile brickwork joint in the step (1), ceramic tile ontology is avoided damage to.
Specifically, in the step (2), fine slag is cleaned with water using brush or/and hair-dryer.
Specifically, the glue group and solidification group of bicomponent epoxy resin glue are uniform using hybrid nozzle in the step (4) It is injected after mixing.
Specifically, it in the step (4), is rolled successively along brickwork joint trend using tooled joint ball and all is molded with two component epoxy The brickwork joint of resin glue makes its compacting.
Specifically, after the quick service is completed 4 hours, normal use toilet.
Compared with prior art, the invention has the advantages that:
(1) the ingenious water-resistance, crack resistance and high adhesiveness that epoxide resin material is utilized of the present invention, in tiles in toilet Waterproofing protection is re-established at brickwork joint, in conjunction with the extremely low characteristic of tiles in toilet surface permeability rate itself, builds new toilet Waterproof structural course, toilet warterproof performance, phase can also be restored by not destroying toilet and integrally fitting up to achieving the effect that not tear open brick Than previous toilet warterproof layer rupture maintenance mode, the present invention be greatly reduced toilet warterproof repair when time, space, Material, cost of labor, efficient quick repair field in toilet warterproof and are with a wide range of applications, be suitble to promote and apply.
(2) present invention provides space by original adhering material in removing ceramic tile brickwork joint for quick service packing material, former Some adhering materials are generally concrete mortar and the joint filling cream of beautification, these materials do not have any help to waterproof, and Brickwork joint part is also exactly the permeable intermediate portions in toilet surface layer, it is therefore desirable to it is especially handled, and the porcelain on ceramic tile because Permeability rate is extremely low to have certain fire resistance characteristic, can be used, enable the waterproof bonding material newly injected and ceramic tile porcelain Matter is effectively bonded the effective new waterproof layer of formation, while ensureing the epoxy for, without fine slag, avoiding influencing to inject in the brickwork joint handled out The adhesive strength of resin glue.
(3) present invention also builds waterproof matrix by organosilicon moisture repellent before injecting epoxide-resin glue in brickwork joint, adds The strong bond strength of epoxide-resin glue and brickwork joint, improves the intensity and service life of the waterproof layer of epoxide-resin glue structure.
(4) present invention realizes the filling to brickwork joint waterproof by injecting epoxide-resin glue in brickwork joint, the ring after filling Oxygen resin glue is combined with ceramic tile porcelain edge, forms effective waterproof layer, and the manufacturing process of ceramic tile can be such that its porcelain part removes Front is completely covered outer can all have a small amount of extension, epoxide-resin glue preferably to dock porcelain after compaction generally at lateral edge The porcelain part of brick lateral edge, therefore compaction process treated epoxide-resin glue can form in upper surface and be similar to arc Shape forms the groove profile of 1mm or so depth with ceramic tile surface, take into account waterproof with it is Nian Jie and reserve centainly for the jointing of brickwork joint surface Space.
(5) present invention also covers one layer of waterproof jointing agent on the surface of epoxide-resin glue, is on the one hand by the anti-of multilayer Water protects the water resistance for strengthening the water resistance of brickwork joint part and being docked with ceramic tile porcelain part, on the other hand can rise To the effect of beautification brickwork joint, while not above ceramic tile surface after requiring waterproof jointing agent to fill, and should make as possible between ceramic tile Transition keep smooth-going, with ensure toilet just common water when water discharge will not hindered and water it is remaining poly- at brickwork joint Collection.
Specific implementation mode
With reference to embodiment, the invention will be further described, and embodiments of the present invention include but not limited to following reality Apply example.
Embodiment
This does not tear brick quick service method open, the repair place of percolating water phenomenon occurs after being ruptured primarily directed to toilet warterproof layer Reason occurred that when the repair of such case resident family toilet decoration can only be removed, and did waterproof layer in accomodation ground base again in the past, Restore toilet decoration again, not only quantities is big, and what is needed is of long duration, of high cost, and influences very much resident family to toilet Normal use, so that there is the resident family of such case all to this prodigious complaint.Applicant is for the angle for improving customer experience Degree, studies the construction and water resistance of toilet, the characteristics of infiltration based on existing toilet, creatively proposes this hair Bright waterproof restorative procedure finds that repairing effect is especially good after actual tests.
This method comprises the following steps:
(1) original adhering material in the ceramic tile brickwork joint of raked joint tool removal accomodation ground and metope is used, exposing Brickwork joint depth at least 4mm, width are not less than 2mm;Used raked joint tool is chisel, perching knife or abrasive machine, while in raked joint When should avoid damage to ceramic tile ontology, should shovel out or scrape original adhering material such as successively along brickwork joint with chisel or perching knife Joint filling cream, concrete etc. should be also repeated at least once more when the depth for once shoveling out or scraping is less than 4mm, it is made to meet institute The brickwork joint depth and width requirement needed;When original adhering material more fastens, first abrasive machine can also be used in brickwork joint Material carries out grinding process, so that it is become relatively softer, is then rooted out or struck off with chisel or perching knife again, wherein sand The grinding wheel that turbine is configured should harder and thickness should not be wide and brickwork joint cannot be stretched into.
(2) it cleans remaining fine slag in brickwork joint with water, ensures without fine slag, to avoid the bonding for influencing epoxide-resin glue strong in brickwork joint Degree;It cleans tool with water and preferentially selects brush, good operability, flexibly and easily, cost are relatively low, can also be configured hair-dryer and are carried out to brickwork joint Purging or brush are used cooperatively with hair-dryer.
(3) the uniform brushing organosilicon moisture repellent in the brickwork joint cleared up, makes it permeate and cures base in brickwork joint, every meter The organosilicon moisture repellent dosage of brickwork joint is 45-55ml, can make organosilicon moisture repellent base's infiltration 1mm ± 0.4mm in brickwork joint Thickness forms waterproof matrix.
(4) after organosilicon moisture repellent drying, normal flash-off time is 20 minutes or so;Then double groups are injected into brickwork joint Part epoxide-resin glue, the glue group and solidification group of the bicomponent epoxy resin glue are noted after evenly mixing using hybrid nozzle It penetrates, to ensure curing rate, the epoxide-resin glue finished surface after injection is from ceramic tile surface about 1mm between left and right every then using pressure Seam ball along brickwork joint trend roll successively all brickwork joints for being molded with bicomponent epoxy resin glue make its compacting (tooled joint ball be industry it is special With tool, diameter and the suitable round end chopsticks replacement of radian can also be used in this tool), the table of the epoxide-resin glue after control compacting Face keeps 1mm ± 0.2mm distances with ceramic tile surface, while being formed and being docked with the side porcelain part of ceramic tile.
(5) after epoxide-resin glue is completely dried, normal flash-off time is 2 hours or so, passes through finger or auxiliary at this time Tool presses the epoxide-resin glue in brickwork joint, observes whether it deformation occurs, if undeformed, shows that it has been completely dried, otherwise Extend flash-off time and tests its drying regime in due course;Then the coating filling waterproof jointing agent on remaining brickwork joint, makes waterproof Jointing agent is combined with ceramic tile surface edge, and the waterproof jointing agent filled is not higher than ceramic tile surface.
(6) after the drying of waterproof jointing agent, normal flash-off time is 1 hour or so, completes quick service.
Wherein, in the entire work progress before quick service completion, apparent water mark cannot occur in accomodation ground and metope. After construction is completed 4 hours, bright water can be used in toilet.
The entire construction processing time of the present invention is no more than 8 hours (containing drying time is waited for), that is, does not exceed a work Make Time of Day, take short, one week construction time, processing time contract significantly easily compared to previous toilet warterproof method for repairing and mending It is short.The present invention in construction will not substantial damage toilet whole finishing, cleaning processing only is carried out to brickwork joint, in the process The fine slag dust and other impurities for only needing cleaning to strike off, workload is small, needs to remove the dress in toilet compared to previous method for repairing and mending These finishings are simultaneously restored in the finishings such as decorations, ceramic tile part after the repair has been completed, and workload greatly reduces.The present invention uses in construction Few reagent material of quantity such as organosilicon moisture repellent, bicomponent epoxy resin glue, waterproof jointing agent etc., cost is not high, and with Past method for repairing and mending wants the materials such as additional waterproof layer material, concrete mortar, joint filling cream, and the ceramic tile damaged when removing also needs Extra purchase ceramic tile etc., construction cost substantially reduces.The cost of labor accordingly generated is also reduced significantly.It realizes anti-to toilet Brick quick service is not torn in water layer rupture infiltration open.
Applicant also carries out common test, test condition mould to the toilet warterproof layer service life of quick service method processing Quasi- toilet practical service environment, and burin-in process test is carried out to test material.It passs, surveys by normal time in common test 3 months ne-leakage water meters of examination are existing;In burin-in process test, material is equivalent to 2 year of normal use, same ne-leakage water meter It is existing.According to material aging characteristic, theoretically the quick service method is not in the case where tiles in toilet is damaged, it is ensured that normal use 5-8 is water-tight.
Above-described embodiment is merely a preferred embodiment of the present invention, and it is not intended to limit the protection scope of the present invention, as long as using The design principle of the present invention, and the non-creative variation worked and made is carried out on this basis, it should all belong to the present invention's Within protection domain.

Claims (7)

1. a kind of not tearing brick quick service method open for the rupture infiltration of toilet warterproof layer, which is characterized in that include the following steps:
(1) original adhering material in the ceramic tile brickwork joint of raked joint tool removal accomodation ground and metope, the brickwork joint of exposing are used Depth at least 4mm, width are not less than 2mm;
(2) it cleans remaining fine slag in brickwork joint with water, ensures in brickwork joint without fine slag;
(3) the uniform brushing organosilicon moisture repellent in the brickwork joint cleared up, makes it permeate and cures base in brickwork joint, every meter of brickwork joint Organosilicon moisture repellent dosage be 45-55ml;
(4) after organosilicon moisture repellent drying, bicomponent epoxy resin glue is injected into brickwork joint, and be compacted, after control compacting The surface of epoxide-resin glue keeps 1mm ± 0.2mm distances with ceramic tile surface;
(5) after epoxide-resin glue is completely dried, the coating filling waterproof jointing agent on remaining brickwork joint, make waterproof jointing agent with Ceramic tile surface edge is combined, and the waterproof jointing agent filled is not higher than ceramic tile surface;
(6) after the drying of waterproof jointing agent, quick service is completed;
Wherein, before quick service completion, apparent water mark cannot occur in accomodation ground and metope.
2. it is according to claim 1 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, the raked joint tool is chisel, perching knife or abrasive machine.
3. it is according to claim 1 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, ceramic tile ontology is avoided damage to when original adhering material in removal ceramic tile brickwork joint in the step (1).
4. it is according to claim 1 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, in the step (2), fine slag is cleaned with water using brush or/and hair-dryer.
5. it is according to claim 1 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, the glue group and solidification group of bicomponent epoxy resin glue are carried out after evenly mixing using hybrid nozzle in the step (4) Injection.
6. it is according to claim 1 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, in the step (4), all bricks for being molded with bicomponent epoxy resin glue is rolled using tooled joint ball successively along brickwork joint trend Seam makes its compacting.
7. it is according to claim 6 it is a kind of for toilet warterproof layer rupture infiltration do not tear brick quick service method, feature open It is, after the quick service is completed 4 hours, normal use toilet.
CN201810644960.XA 2018-06-21 2018-06-21 Quick repair method for water seepage caused by rupture of waterproof layer of bathroom without disassembling bricks Active CN108625618B (en)