CN1079484C - 一种调整注水井吸水剖面的方法 - Google Patents

一种调整注水井吸水剖面的方法 Download PDF

Info

Publication number
CN1079484C
CN1079484C CN99113190A CN99113190A CN1079484C CN 1079484 C CN1079484 C CN 1079484C CN 99113190 A CN99113190 A CN 99113190A CN 99113190 A CN99113190 A CN 99113190A CN 1079484 C CN1079484 C CN 1079484C
Authority
CN
China
Prior art keywords
water
blocking agent
water injection
plugging
stage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN99113190A
Other languages
English (en)
Other versions
CN1248663A (zh
Inventor
白云渡
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN99113190A priority Critical patent/CN1079484C/zh
Publication of CN1248663A publication Critical patent/CN1248663A/zh
Application granted granted Critical
Publication of CN1079484C publication Critical patent/CN1079484C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明涉及一种用于调整注水井吸水剖面、改善油层开采状况的方法。该方法乃是采用分别用以封堵大孔道、大裂缝和小孔道、小裂缝的两个阶段性堵剂配方,且在注入两个阶段性堵剂之间加入一个注水阶段。采用该方法可以获得良好的调剖效果和较长的有效期,改善油井生产和油层开采状况。该方法简单易行,效果良好,所用堵剂皆为现成产品,尤其适用于低渗透、油层发育不均或断裂、裂缝发育的油田。

Description

一种调整注水井吸水剖面的方法
本发明涉及一种用于调整注水井吸水剖面、改善油层开采状况的工艺方法。
由于油层发育不均,当油田投入注水开发后注入水沿高渗透层突进,导致油井含水迅速上升,产量急剧下降,低渗透层动用程度甚低,严重影响着油井生产和油田开发效果。上述情况是国内外油田在开发过程中经常遇到的难题之一。另外,在高渗透层即主力吸水层中存在着高渗透带和低渗透带,在正常注水的情况下,高渗透带吸水,水线沿高渗透带指进,而低渗透带不吸水,因而很难得到动用。目前,现场通常采用调整分层注水量、低渗透层压裂酸化改造、高渗透层堵水调整吸水剖面等措施来解决这一问题。然而,目前采用的用粘土、水泥以及体膨型或交联型堵剂按常规工艺进行的注水井井调剖虽然施工后初期取得一定效果,但有效期短,且措施后的增产量逐轮下降。
本发明的目的在于提供一种能够使各种堵剂在不同时间段产生不同作用,从而获得良好调剖效果并保持较长有效期的调整注水井吸水剖面的方法。
本发明提供的调整注水井吸水剖面的方法是这样实现的。该方法的关键所在乃是采用两个阶段性堵剂配方,分别用以封堵大孔道、大裂缝和小孔道、小裂缝,且在注入两个阶段性堵剂之间加入一个注水阶段,让已堵堵的高渗透层中原不吸水的低渗透带吸水。亦即该调剖方法将整个施工分成三个阶段:1、注体膨型聚丙烯酰胺或橡胶颗粒堵剂阶段;2、注水阶段;3、注交联型聚丙烯酰胺或粘土堵剂阶段,其实施步骤及过程如下:
1、注用以封堵大孔道、大裂缝的体膨型聚丙烯酰胺或橡胶颗粒堵剂阶段。在地面容积为10m3的调剖剂罐中,按10%的体积浓度加入体膨型聚丙烯酰胺堵剂,其余加水;或者配制体积浓度10%的橡胶颗粒堵剂;将该堵剂用水泥车打入地层,直至爬坡压力上升2--3MPa停止。
2、注水阶段。第一种堵剂打完后,候凝1-2天,然后按略高于正常配注的注入量注水,直至注水压力由步骤1实施完毕后初期注水压力值下降1-2MPa时为止;
3、注用以封堵小孔道、小裂缝的交联型聚丙烯酰胺或粘土堵剂阶段。在地面10m3调剖剂罐中加入体积浓度1.2%的聚丙烯酰胺、1.3‰的重铬酸钠、1.7‰的亚硫酸钠,其余加水;或者配制体积浓度30%的粘土堵剂,用水泥车将该堵剂打入地层,直至爬坡压力上升4-5MPa时停止;
4、关井候凝3-5天。
本发明所提供的调整注水井吸水剖面的方法采用分阶段注入不同类型堵剂分别封堵大孔道、大裂缝和小孔道、小裂缝,并在其间注入一定量水的做法,可以获得良好的调剖效果和较长的有效期,改善油井生产和油层开采状况。该方法简单易行,效果良好,所用堵剂皆为现成产品,尤其适用于低渗透、油层发育不均或断裂、裂缝发育的油田,对于此类油田该方法可获得较好的调剖效果。

Claims (1)

1、一种调整注水井吸水剖面的方法,其特征在于:该方法包括以下步骤:
1)注用以封堵大孔道、大裂缝体膨型聚丙烯酰胺或橡胶颗粒堵剂阶段:在地面容积10m3的调剖剂罐中,按10%的体积浓度加入体膨型聚丙烯酰胺堵剂,其余加水;或者配制体积浓度10%的橡胶颗粒堵剂;将该堵剂用水泥车打入地层,直至爬坡压力上升2-3MPa停止;
2)注水阶段:第一种堵剂打完后停凝1-2天,然后按高于正常配注的注入量注水,直至注水压力由步骤1实施完毕后初期注水压力值下降1-2MPa时为止;
3)注用以封堵小孔道小裂缝的交联型聚丙烯酰胺或粘土堵剂阶段:在地面调剖剂罐中加入体积浓度1.2%的聚丙烯酰胺、1.3‰的重铬酸钠、1.7‰的亚硫酸钠,其余加水;或者配制体积浓度30%的粘土堵剂,用水泥车将该堵剂打入地层直至爬坡压力上升4-5MPa时停止;
4)关井候凝3-5天。
CN99113190A 1999-08-19 1999-08-19 一种调整注水井吸水剖面的方法 Expired - Fee Related CN1079484C (zh)