CN107794790A - A kind of method for improving waterproof polyester-cotton fabric color fastness - Google Patents

A kind of method for improving waterproof polyester-cotton fabric color fastness Download PDF

Info

Publication number
CN107794790A
CN107794790A CN201711104853.XA CN201711104853A CN107794790A CN 107794790 A CN107794790 A CN 107794790A CN 201711104853 A CN201711104853 A CN 201711104853A CN 107794790 A CN107794790 A CN 107794790A
Authority
CN
China
Prior art keywords
waterproof
cotton fabric
polyester
color fastness
waterproof polyester
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711104853.XA
Other languages
Chinese (zh)
Inventor
何佳乐
尚军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xinxiang Xinke Protection Technology Co Ltd
Original Assignee
Xinxiang Xinke Protection Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xinxiang Xinke Protection Technology Co Ltd filed Critical Xinxiang Xinke Protection Technology Co Ltd
Priority to CN201711104853.XA priority Critical patent/CN107794790A/en
Publication of CN107794790A publication Critical patent/CN107794790A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of method for improving waterproof polyester-cotton fabric color fastness, detailed process is:Waterproof polyester-cotton fabric is subjected to boiling in the dye vat containing detergent 6501 first, boiling cleaning is then carried out in pure water, addition chlorine-resistant color fixing agent F 323 makes chlorine-resistant color fixing agent F 323 be impregnated with waterproof polyester-cotton fabric after carrying out cold water wash at once again, then waterproof polyester-cotton fabric is taken out from dye vat and is dried and baked successively, finally so that waterproof polyester-cotton fabric color fastness is obviously improved on the premise of waterproof polyester-cotton fabric water proofing property is not influenceed.Of the invention effectively realize effectively improves its color fastness rank on the premise of waterproof polyester-cotton fabric water proofing property is not influenceed, and has preferable using effect, and this method technique is simple and easy to operate, is advantageous to further genralrlization application.

Description

A kind of method for improving waterproof polyester-cotton fabric color fastness
Technical field
The invention belongs to the technical field of improvement of waterproof polyester-cotton fabric, and in particular to one kind improves waterproof polyester-cotton fabric color jail The method of degree.
Background technology
Existing waterproof polyester-cotton fabric is widely used in real life such as:Umbrella, tent and some protective garments etc., but do It is higher such as 4 grades or 5 grades of waterproof fabrics to cross the polyester-cotton fabric of waterproof, particularly classification of waterproof, then goes to pad working solution, almost Without band liquid measure.If it is bad to do the polyester-cotton fabric color fastness after waterproof, its performance, such as daily life will be had a strong impact on In umbrella, once just fades by drenching with rain, outward appearance will extremely unsightly at leisure.Effectively carried therefore, it is necessary to design one kind The method of high waterproof polyester-cotton fabric color fastness is effectively to solve above-mentioned technical problem.
The content of the invention
Present invention solves the technical problem that there is provided, a kind of technique is simple, cost is cheap and easy to operate raising waterproof The method of polyester-cotton fabric color fastness.
The present invention is to solve above-mentioned technical problem to adopt the following technical scheme that, a kind of raising waterproof polyester-cotton fabric color fastness Method, it is characterised in that detailed process is:Waterproof polyester-cotton fabric is subjected to boiling in the dye vat containing detergent 6501 first, Boiling cleaning is then carried out in pure water, then add chlorine-resistant color fixing agent F-323 after progress cold water wash at once to make chlorine-resistant fixation Agent F-323 is impregnated with waterproof polyester-cotton fabric, and then waterproof polyester-cotton fabric is taken out from dye vat and is dried and is baked successively, most Eventually so that waterproof polyester-cotton fabric color fastness is obviously improved on the premise of waterproof polyester-cotton fabric water proofing property is not influenceed.
Further preferably, the method for improving waterproof polyester-cotton fabric color fastness, it is characterised in that concretely comprise the following steps:First Waterproof polyester-cotton fabric is incubated to 90 DEG C of cleaning 1h in the dye vat containing detergent 6501, the mass concentration of the detergent 6501 is 15g/L, then cleans 3 in 90 DEG C of pure water, and per pass is respectively washed 30min, then carries out adding after cold water wash at once resistance to Chlorine color fixing agent F-323 makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof polyester-cotton fabric, and chlorine-resistant color fixing agent F-323 mass concentration is 10g/L, then waterproof polyester-cotton fabric is taken out from dye vat in 100-120 DEG C of drying, bakes 40s then at 165 DEG C, it is tentering, pre- Contracting finally gives waterproof rank and the higher waterproof polyester-cotton fabric of color fastness rank.
Further preferably, the method for improving waterproof polyester-cotton fabric color fastness, it is characterised in that concretely comprise the following steps:By T/ C fabrics pad Teflon C6 waterproofing agents, and the wherein mass concentration of C6 waterproofing agents is 80g/L, are dried then at 100-120 DEG C, then 40s is baked in 165 DEG C, finally gives 5 grades of waterproof, 3 grades of dry friction color fastness, the waterproof T/C fabrics of 2 grades of wet friction color fastness; Obtained waterproof T/C fabrics are incubated to 90 DEG C of cleaning 1h, the quality of the detergent 6501 in the dye vat containing detergent 6501 Concentration is 15g/L, and 3 are then cleaned in 90 DEG C of pure water, and per pass is respectively washed 30min, then at once after progress cold water wash Adding chlorine-resistant color fixing agent F-323 makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof polyester-cotton fabric, chlorine-resistant color fixing agent F-323 quality Concentration is 10g/L, then takes out waterproof T/C fabrics in 100-120 DEG C of drying from dye vat, 40s is baked then at 165 DEG C, draw Width, preshrunk finally give waterproof 4-5 levels, dry friction color fastness 4-5 levels, the waterproof T/C fabrics of 3 grades of wet friction color fastness.
The present invention has the advantages that compared with prior art:Of the invention effectively realize is not influenceing waterproof polyester-cotton blend Its color fastness rank is effectively improved on the premise of fabric waterproof, there is preferable using effect, and this method technique is simple And it is easy to operate, be advantageous to further genralrlization application.
Embodiment
The particular content of the present invention is described in detail in conjunction with the embodiments.
Embodiment
1st, T/C12*12 black cloth is padded into Teflon C6 waterproofing agents, the wherein mass concentration of C6 waterproofing agents is 80g/L, then In 100-120 DEG C of drying, 40s then is baked in 165 DEG C, finally gives 5 grades of waterproof, 3 grades of dry friction color fastness, wet friction color jail The waterproof T/C fabrics of 2 grades of degree, the color fastness of waterproof T/C fabrics are poor.
2nd, because waterproof T/C fabrics had done waterproof, chlorine-resistant color fixing agent F-323 is directly padded, colorfastness to rubbing is not It can get a promotion.On the other hand, using following PROCESS FOR TREATMENT:By obtained waterproof T/C fabrics in the dye vat containing detergent 6501 90 DEG C of cleaning 1h of insulation, the mass concentration of the detergent 6501 is 15g/L, 3 is then cleaned in 90 DEG C of pure water, per pass point 30min is not cleaned, then adding chlorine-resistant color fixing agent F-323 after progress cold water wash at once makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof Polyester-cotton fabric, chlorine-resistant color fixing agent F-323 mass concentration is 10g/L, then by waterproof polyester-cotton fabric taken out from dye vat in 100-120 DEG C of drying, bakes 40s then at 165 DEG C, tentering, preshrunk finally give waterproof 4-5 levels, dry friction color fastness 4-5 levels, The waterproof T/C fabrics of 3 grades of wet friction color fastness.
This technique washes away the loose colour of web surface using detergent 6501, fabric again through HIGH TEMPERATURE PURGE in the case of, its table The water proofing property in face is destroyed, and cold water wash reduces the cloth cover temperature of fabric, and adding chlorine-resistant color fixing agent F-323 makes chlorine-resistant fixation Inside agent F-323 infiltration fabrics, got a promotion by the color fastness for drying waterproof polyester-cotton fabric, now measure waterproof T/C Fabric waterproof 2-3 levels, dry friction color fastness 4-5 levels, 3 grades of wet friction color fastness.Waterproof T/C faces in the case of being washed due to high temperature The mode of material is destroyed, it is necessary to be baked, and now the water proofing property of waterproof T/C fabrics gets a promotion, and measures waterproof 4-5 Level, so while waterproof T/C fabrics color fastness is lifted, and does not influence the water proofing property of waterproof T/C fabrics.
Have been shown and described above the general principle of the present invention, principal character and advantage, do not depart from spirit of the invention and On the premise of scope, the present invention also has various changes and modifications, and these changes and improvements both fall within claimed invention Scope.

Claims (3)

  1. A kind of 1. method for improving waterproof polyester-cotton fabric color fastness, it is characterised in that detailed process is:First by waterproof polyester-cotton blend face Material carries out boiling in the dye vat containing detergent 6501, boiling cleaning is then carried out in pure water, then carry out cold water at once Chlorine-resistant color fixing agent F-323 is added after cleaning makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof polyester-cotton fabric, then by waterproof polyester-cotton fabric Taken out from dye vat and dried and baked successively, finally caused on the premise of waterproof polyester-cotton fabric water proofing property is not influenceed anti- Water polyester-cotton fabric color fastness is obviously improved.
  2. 2. the method according to claim 1 for improving waterproof polyester-cotton fabric color fastness, it is characterised in that concretely comprise the following steps:It is first Waterproof polyester-cotton fabric is first incubated to 90 DEG C of cleaning 1h, the mass concentration of the detergent 6501 in the dye vat containing detergent 6501 For 15g/L, 3 are then cleaned in 90 DEG C of pure water, per pass is respectively washed 30min, then is added after carrying out cold water wash at once Chlorine-resistant color fixing agent F-323 makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof polyester-cotton fabric, chlorine-resistant color fixing agent F-323 mass concentration For 10g/L, then waterproof polyester-cotton fabric is taken out from dye vat in 100-120 DEG C of drying, bakes 40s then at 165 DEG C, tentering, Preshrunk finally gives waterproof rank and the higher waterproof polyester-cotton fabric of color fastness rank.
  3. 3. the method according to claim 1 or 2 for improving waterproof polyester-cotton fabric color fastness, it is characterised in that specific steps For:T/C fabrics are padded into Teflon C6 waterproofing agents, the wherein mass concentration of C6 waterproofing agents is 80g/L, then at 100-120 DEG C of baking It is dry, 40s then is baked in 165 DEG C, finally gives 5 grades of waterproof, 3 grades of dry friction color fastness, the waterproof T/ of 2 grades of wet friction color fastness C fabrics;Obtained waterproof T/C fabrics are incubated to 90 DEG C of cleaning 1h, the detergent 6501 in the dye vat containing detergent 6501 Mass concentration be 15g/L, 3 are then cleaned in 90 DEG C of pure water, per pass is respectively washed 30min, then carries out cold water at once Chlorine-resistant color fixing agent F-323 is added after cleaning makes chlorine-resistant color fixing agent F-323 be impregnated with waterproof polyester-cotton fabric, chlorine-resistant color fixing agent F-323 Mass concentration be 10g/L, then by waterproof T/C fabrics taken out from dye vat in 100-120 DEG C drying, baked then at 165 DEG C 40s, tentering, preshrunk finally give waterproof 4-5 levels, dry friction color fastness 4-5 levels, the waterproof T/C faces of 3 grades of wet friction color fastness Material.
CN201711104853.XA 2017-11-10 2017-11-10 A kind of method for improving waterproof polyester-cotton fabric color fastness Pending CN107794790A (en)