CN107523657A - 一种延长水渣方型槽使用寿命的方法 - Google Patents

一种延长水渣方型槽使用寿命的方法 Download PDF

Info

Publication number
CN107523657A
CN107523657A CN201710698757.6A CN201710698757A CN107523657A CN 107523657 A CN107523657 A CN 107523657A CN 201710698757 A CN201710698757 A CN 201710698757A CN 107523657 A CN107523657 A CN 107523657A
Authority
CN
China
Prior art keywords
wear
draw point
square groove
hexsteel
resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710698757.6A
Other languages
English (en)
Inventor
于涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xinjiang Bayi Iron and Steel Co Ltd
Original Assignee
Baosteel Group Xinjiang Bayi Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Baosteel Group Xinjiang Bayi Iron and Steel Co Ltd filed Critical Baosteel Group Xinjiang Bayi Iron and Steel Co Ltd
Priority to CN201710698757.6A priority Critical patent/CN107523657A/zh
Publication of CN107523657A publication Critical patent/CN107523657A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种延长水渣方型槽使用寿命的方法,首先在方型槽的底面以及底面左右两侧的方型槽两侧内壁上均布间隔焊接锚固件,锚爪高1.5‑2cm,间宽5‑7cm,然后在所述三面槽体内壁上覆盖厚度为30mm规格的龟甲网,再选用其中含有钢针的耐高温陶瓷耐磨浇注料对龟甲网进行喷涂或浇筑构成耐磨防护层,耐磨防护层的厚度为10mm,其中所述钢针的长度为8mm、钢针的直径为0.5‑1mm,钢针的重量占所述的耐磨浇注料重量的10%,夏季养护6‑8小时即可投入使用。

Description

一种延长水渣方型槽使用寿命的方法
技术领域
本发明涉及一种延长水渣方型槽使用寿命的方法。
背景技术
现水渣系统使用的方型槽一般采用18—24mm热轧钢板采用焊接方式制成,由于水渣系统的输送介质为渣水混合物,且作业温度较高(80℃左右),一般在使用9-12个月就会出现局部磨穿漏水、漏渣现象,越到后期磨穿频次越高,增加了维护工的劳动强度,增加了企业生产成本。
发明内容
本发明的目的在于提供一种延长水渣方型槽使用寿命的方法,能够延长水渣方型槽的使用寿命,降低生产成本。
本发明的目的是这样实现的,一种延长水渣方型槽使用寿命的方法,首先在方型槽的底面以及底面左右两侧的方型槽两侧内壁上均布间隔焊接锚固件,锚爪高1.5-2cm,间宽5-7cm,然后在所述三面槽体内壁上覆盖厚度为30mm规格的龟甲网,龟甲网与所述的锚固件固定连接在一起。再选用其中含有钢针的耐高温陶瓷耐磨浇注料对龟甲网进行填充、浇筑、抹平构成耐磨防护层,耐磨防护层高出龟甲网的厚度为10mm,其中所述钢针的长度为8mm、钢针的直径为0.5-1mm,钢针的重量占所述的耐磨浇注料重量的10%,钢针与耐磨浇注料均匀搅拌在一起,夏季养护6-8小时即可投入使用;养护时,用湿麻袋或湿席子盖在浇注料表面并及时洒水以保持湿润状态。
本发明通过在某钢铁公司第二高炉分厂B高炉南场方型槽试用,水渣方型槽的耐磨效果大幅度提高,至少可使用18个月以上,且可以重复喷涂使用,大大减少了更换方型槽时的人力、资材的投入,极大地降低了企业生产成本。
具体实施方式
一种延长水渣方型槽使用寿命的方法,首先在方型槽的底面以及底面左右两侧的方型槽两侧内壁上均布间隔焊接锚固件,锚爪高1.5-2cm,间宽5-7cm,然后在所述三面槽体内壁上覆盖厚度为30mm规格的龟甲网,龟甲网与所述的锚固件固定连接在一起。再选用其中含有钢针的耐高温陶瓷耐磨浇注料对龟甲网进行填充、浇筑、抹平构成耐磨防护层,耐磨防护层高出龟甲网的厚度为10mm,其中所述钢针的长度为8mm、钢针的直径为0.5-1mm,钢针的重量占所述的耐磨浇注料重量的10%,钢针与耐磨浇注料均匀搅拌在一起。耐磨浇注料市场上有售。夏季养护6-8小时即可投入使用。养护时,可用湿麻袋或湿席子盖在浇注料表面并及时洒水以保持湿润状态。

Claims (2)

1.一种延长水渣方型槽使用寿命的方法,其特征在于首先在方型槽的底面以及底面左右两侧的方型槽两侧内壁上均布间隔焊接锚固件,锚爪高1.5-2cm,间宽5-7cm,然后在所述三面槽体内壁上覆盖厚度为30mm规格的龟甲网,龟甲网与所述的锚固件固定连接在一起。
2.再选用其中含有钢针的耐高温陶瓷耐磨浇注料对龟甲网进行填充、浇筑、抹平构成耐磨防护层,耐磨防护层高出龟甲网的厚度为10mm,其中所述钢针的长度为8mm、钢针的直径为0.5-1mm,钢针的重量占所述的耐磨浇注料重量的10%,钢针与耐磨浇注料均匀搅拌在一起,夏季养护6-8小时即可投入使用;养护时,用湿麻袋或湿席子盖在浇注料表面并及时洒水以保持湿润状态。
CN201710698757.6A 2017-08-15 2017-08-15 一种延长水渣方型槽使用寿命的方法 Pending CN107523657A (zh)