CN107354580A - A kind of preparation method and its industrial washing technique of the filler of water-fastness pillow - Google Patents

A kind of preparation method and its industrial washing technique of the filler of water-fastness pillow Download PDF

Info

Publication number
CN107354580A
CN107354580A CN201710479460.0A CN201710479460A CN107354580A CN 107354580 A CN107354580 A CN 107354580A CN 201710479460 A CN201710479460 A CN 201710479460A CN 107354580 A CN107354580 A CN 107354580A
Authority
CN
China
Prior art keywords
pillow
water
filler
washing
fastness
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710479460.0A
Other languages
Chinese (zh)
Inventor
张华�
季美芬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Sidefu Textile Ltd By Share Ltd
Original Assignee
Jiangsu Sidefu Textile Ltd By Share Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Sidefu Textile Ltd By Share Ltd filed Critical Jiangsu Sidefu Textile Ltd By Share Ltd
Priority to CN201710479460.0A priority Critical patent/CN107354580A/en
Publication of CN107354580A publication Critical patent/CN107354580A/en
Priority to PCT/CN2017/117009 priority patent/WO2018233247A1/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of preparation method and its industrial washing technique of the filler of water-fastness pillow, the filler of the pillow is mixed by 1.2dtex × 38mm fine count fibers of 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helical coils are curved " superfine fibre of 45 55 parts of weight, 3dtex × 51mm doughnuts of 25 35 parts of weight, 15 25 parts of weight.The present invention solves the problems, such as hotel's pillow washing property difference, improves the presentation quality (fiber does not wind, do not united, be not hardened) of pillow, pillow is possessed more preferable water-wash resistance, bulkiness and flexibility.

Description

A kind of preparation method and its industrial washing technique of the filler of water-fastness pillow
Technical field
The invention belongs to pillow manufacturing field, and in particular to a kind of preparation method and its work of the filler of water-fastness pillow Industry washing process.
Background technology
As the improvement of people's living standards, sleep quality when people are to trip also progressively has higher requirement, by There is the characteristics of flow of personnel is big, and composition is unstable in hotel, hotel's textile can all be used by different people daily, if Clean not in time, the various materials concealed in filler readily penetrate through the cross-infection that guest is caused by bedding sack, pillowcase.At present, Pillow packing material includes nodular fibrous (pearl cotton), sheet cotton by form point and combs cotton, wherein nodular fibrous (pearl cotton) It is washable with flocculus shape cotton, and comb cotton and be difficult to wash.
Nodular fibrous:3 D stereo crimped polyester cellucotton, globulate shape cotton is processed by special balling-up technology.Pearl cotton Ball boring, there is larger ventilation space, warmth retention property and gas permeability are stronger, and have hole, bullet in pearl cotton balls polyester fiber Property it is good, its product after quilting, can automatic expansion, it is prevented from caking, even if machine washing will not also deform, be used for the filling material of pillow Material.But this kind of core class product surface is uneven, it is necessary to wrapped up using thick close material outside it, and cost is higher.
Flocculus shape cotton:Flocculus is process by mixing → fibrillation → combing → lapping → dryness finalization technique.Currently, Domestic more production methods using heat bonding, it must select two or more fiber to mix, wherein there is a kind of fiber It is meldable fibre as binder fibre, its fusing point is lower than the fusing point of other composite fibre, enters drying when fiber combs networking After machine, drying temperature is higher than the fusing point of meldable fibre, and soften fusing, is then bonded together with other high-melting fibres, shape Into flocculus.Flocculus shape cotton is washable, uniform and smooth, but the density for sheet-shaped fillers of wadding a quilt with cotton is high, dosage multi-processing cost is high and fluffy Looseness is inadequate.
Comb cotton:Combing formula cotton is process by shredding → mixed cotton → combing → lapping → encapsulation technique.Comb cotton Fiber easy softening transform when packing material product is washed, it is not close due to being combined between fiber, it is easily broken off between fiber, mutually Winding, so as to which core class product formation lumps, became uneven is even.But it is fluffy, soft to comb cotton packing material product, market accounting Greatly, filling dosage is small and processing cost is relatively inexpensive.
The patent No.:201410087049.5 patent name is:A kind of production technology of multicomponent fibre mixture fabric it is special It is in the curved composite fibre of ∞ disjunctor helical coils by regenerated celulose fibre and ultra-fine polyester fiber mixture, in weaving process in profit In, hair compares general cotton product height again, will not produce looped pile and excessively lodge, influence the phenomenon of the plentiful degree of fabric outward appearance, make With long lifespan, fiber fluffy degree and pliability are good.
The content of the invention
Goal of the invention:It is an object of the invention to provide a kind of preparation method and its industry water of the filler of water-fastness pillow Technique is washed, solves the problems, such as hotel pillow washing property difference, improving the presentation quality of pillow, (fiber do not wind, do not unite, not plate Knot), pillow is possessed more preferable water-wash resistance, bulkiness and flexibility.
Technical scheme:A kind of preparation method of the filler of water-fastness pillow, comprises the following steps:
(1) raw material prepares:The filler of the pillow by 45-55 part weight 3.6dtex × 30mm terylene/regenerated fiber Plain " ∞ disjunctor helical coils are curved " superfine fibre, 3dtex × 51mm doughnuts of 25-35 part weight, 15-25 part weight 1.2dtex × 38mm fine count fibers mix;
(2) prepare:By the different fiber mixed of three of the above length, thickness, curly form together, it is well mixed laggard Row rubbing, 1.2dtex × 38mm fine count fibers are inserted partially into 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor spirals In curled " superfine fibre so that have certain mutual winding between fiber, while there is certain dispersiveness;
(3) wrap up:Filler is filled into pillow, the pillow parcel fabric selects 40s×40sBleaching plain weave face Material, through close 110 pieces/inch, 90 pieces/inch of filling density.
The industrial washing technique of filler prepared by a kind of preparation method of the filler of the water-fastness pillow described in basis, Using full-automatic industrial washing machine, water-washing step is followed successively by:Washing (normal temperature 3 minutes) for the first time → → second washing of soaping → Dehydration → drying;Concrete operations are as follows:
1) soap:The washing of 18-22g neutral laundry liquids is injected in soap cup 1, low water level is added water to, is heated to wash temperature 45 DEG C -55 DEG C, rotating speed 40-50rpm, wash time 12-18min are washed, washing turns to stop comparing 20s/8s;
2) second of washing:High water level, wash time 3min are added water to, motor main story enters uniform, dewatering time 1- 4min, dehydrating speed 435-445r/min;Low water level wash time 2-5min is added water to,
3) it is dehydrated:Motor main story enters uniform, dewatering time 1-4min;
4) dry:56-64 DEG C of drying temperature, drying time 27-33min.
As optimization:The low water level is 18L-22L.
As optimization:The high water level is 22L-28L.
Beneficial effect:The present invention solves the problems, such as that hotel pillow washes property difference, and improving the presentation quality of pillow, (fiber is not Wind, do not unite, be not hardened), pillow is possessed more preferable water-wash resistance, bulkiness and flexibility.
Embodiment
Specific embodiment 1
A kind of preparation method of the filler of water-fastness pillow, comprises the following steps:
(1) raw material prepares:The filler of the pillow by 45 parts of weight 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helical coils are curved " superfine fibre, 3dtex × 51mm doughnuts of 25 parts of weight, 15 parts of weight 1.2dtex × 38mm fine count fibers mix;
(2) prepare:By the different fiber mixed of three of the above length, thickness, curly form together, it is well mixed laggard Row rubbing, 1.2dtex × 38mm fine count fibers are inserted partially into 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor spirals In curled " superfine fibre so that have certain mutual winding between fiber, while there is certain dispersiveness;
(3) wrap up:Filler is filled into pillow, the pillow parcel fabric selects 40s×40sBleaching plain weave face Material, through close 110 pieces/inch, 90 pieces/inch of filling density.
The industrial washing technique of filler prepared by a kind of preparation method of the filler of the water-fastness pillow described in basis, Using full-automatic industrial washing machine, water-washing step is followed successively by:Washing (normal temperature 3 minutes) for the first time → → second washing of soaping → Dehydration → drying;Concrete operations are as follows:
1) soap:The washing of 18g neutral laundry liquids is injected in soap cup 1, low water level is added water to, is heated to 45 DEG C of wash temperature, Rotating speed 40rpm, wash time 12min are washed, washing turns to stop comparing 20s/8s;
2) second of washing:High water level, wash time 3min are added water to, motor main story enters uniform, dewatering time 1min, Dehydrating speed 435r/min;Low water level wash time 2min is added water to,
3) it is dehydrated:Motor main story enters uniform, dewatering time 1min;
4) dry:56 DEG C of drying temperature, drying time 27min.
In the present embodiment, the low water level is 18L.The high water level is 22L.
Specific embodiment 2
A kind of preparation method of the filler of water-fastness pillow, comprises the following steps:
(1) raw material prepares:The filler of the pillow by 55 parts of weight 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helical coils are curved " superfine fibre, 3dtex × 51mm doughnuts of 35 parts of weight, 25 parts of weight 1.2dtex × 38mm fine count fibers mix;
(2) prepare:By the different fiber mixed of three of the above length, thickness, curly form together, it is well mixed laggard Row rubbing, 1.2dtex × 38mm fine count fibers are inserted partially into 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor spirals In curled " superfine fibre so that have certain mutual winding between fiber, while there is certain dispersiveness;
(3) wrap up:Filler is filled into pillow, the pillow parcel fabric selects 40S*40S bleaching plain weave face Material, through close 110 pieces/inch, 90 pieces/inch of filling density.
The industrial washing technique of filler prepared by a kind of preparation method of the filler of the water-fastness pillow described in basis, Using full-automatic industrial washing machine, water-washing step is followed successively by:Washing (normal temperature 3 minutes) for the first time → → second washing of soaping → Dehydration → drying;Concrete operations are as follows:
1) soap:The washing of 22g neutral laundry liquids is injected in soap cup 1, low water level is added water to, is heated to 55 DEG C of wash temperature, Rotating speed 50rpm, wash time 18min are washed, washing turns to stop comparing 20s/8s;
2) second of washing:High water level, wash time 3min are added water to, motor main story enters uniform, dewatering time 4min, Dehydrating speed 445r/min;Low water level wash time 5min is added water to,
3) it is dehydrated:Motor main story enters uniform, dewatering time 4min;
4) dry:64 DEG C of drying temperature, drying time 33min.
In the present embodiment, the low water level is 22L.The high water level is 28L.
Specific embodiment 3
A kind of preparation method of the filler of water-fastness pillow, comprises the following steps:
(1) raw material prepares:The filler of the pillow by 50 parts of weight 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helical coils are curved " superfine fibre, 3dtex × 51mm doughnuts of 30 parts of weight, 20 parts of weight 1.2dtex × 38mm fine count fibers mix;
(2) prepare:By the different fiber mixed of three of the above length, thickness, curly form together, it is well mixed laggard Row rubbing, 1.2dtex × 38mm fine count fibers are inserted partially into 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor spirals In curled " superfine fibre so that have certain mutual winding between fiber, while 3dtex × 51mm doughnuts have necessarily Dispersiveness;
(3) wrap up:Filler is filled into pillow, the pillow parcel fabric selects 40s×40sBleaching plain weave face Material, through close 110 pieces/inch, 90 pieces/inch of filling density.
The industrial washing technique of filler prepared by a kind of preparation method of the filler of the water-fastness pillow described in basis, Using full-automatic industrial washing machine, water-washing step is followed successively by:Washing (normal temperature 3 minutes) for the first time → → second washing of soaping → Dehydration → drying;Concrete operations are as follows:
1) soap:The washing of 20g neutral laundry liquids is injected in soap cup 1, low water level is added water to, is heated to 50 DEG C of wash temperature, Rotating speed 45rpm, wash time 15min are washed, washing turns to stop comparing 20s/8s;
2) second of washing:High water level, wash time 3min are added water to, motor main story enters uniform, dewatering time 2min, Dehydrating speed 440r/min;Low water level wash time 4min is added water to,
3) it is dehydrated:Motor main story enters uniform, dewatering time 2min;
4) dry:60 DEG C of drying temperature, drying time 30min.
In the present embodiment, the low water level is 20L.The high water level is 25L.
Technical scheme in the embodiment of the present invention is clearly and completely described the above, so that the skill of this area Art personnel can be better understood from advantages and features of the invention, so as to make apparent boundary to protection scope of the present invention It is fixed.Embodiment described in the invention is only part of the embodiment of the present invention, rather than whole embodiments, based on the present invention In embodiment, the every other implementation that those of ordinary skill in the art are obtained on the premise of creative work is not made Example, belongs to the scope of protection of the invention.

Claims (4)

  1. A kind of 1. preparation method of the filler of water-fastness pillow, it is characterised in that:Comprise the following steps:
    (1) raw material prepares:The filler of the pillow by 45-55 part weight 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helical coils are curved " superfine fibre, 3dtex × 51mm doughnuts of 25-35 part weight, 15-25 part weight 1.2dtex × 38mm fine count fibers mix;
    (2) prepare:By the different fiber mixed of three of the above length, thickness, curly form together, rubbed with the hands after being well mixed Rub, 1.2dtex × 38mm fine count fibers are inserted partially into 3.6dtex × 30mm terylene/regenerated cellulose " ∞ disjunctor helix-coils In type " superfine fibre so that have certain mutual winding between fiber, while there is certain dispersiveness;
    (3) wrap up:Filler is filled into pillow, the pillow parcel fabric selects 40s×40sBleaching plain fabric, warp Close 110 pieces/inch, 90 pieces/inch of filling density.
  2. 2. the industry water of filler prepared by a kind of preparation method of filler of water-fastness pillow according to claim 1 Wash technique, it is characterised in that:Using full-automatic industrial washing machine, water-washing step is followed successively by:Washing (normal temperature 3 minutes) for the first time → Soap → second washing → dehydration → drying;Concrete operations are as follows:
    1) soap:The washing of 18-22g neutral laundry liquids is injected in soap cup 1, low water level is added water to, is heated to wash temperature 45 DEG C -55 DEG C, rotating speed 40-50rpm, wash time 12-18min are washed, washing turns to stop comparing 20s/8s;
    2) second of washing:High water level, wash time 3min are added water to, motor main story enters uniform, dewatering time 1-4min, de- Water rotating speed 435-445r/min;Low water level wash time 2-5min is added water to,
    3) it is dehydrated:Motor main story enters uniform, dewatering time 1-4min;
    4) dry:56-64 DEG C of drying temperature, drying time 27-33min.
  3. 3. the industrial washing technique of the filler of water-fastness pillow according to claim 2, it is characterised in that:The low water Position is 18L-22L.
  4. 4. the industrial washing technique of the filler of water-fastness pillow according to claim 2, it is characterised in that:The Gao Shui Position is 22L-28L.
CN201710479460.0A 2017-06-22 2017-06-22 A kind of preparation method and its industrial washing technique of the filler of water-fastness pillow Pending CN107354580A (en)