CN107192599A - 一种自然交联绝缘料快速制样方法 - Google Patents
一种自然交联绝缘料快速制样方法 Download PDFInfo
- Publication number
- CN107192599A CN107192599A CN201610725814.0A CN201610725814A CN107192599A CN 107192599 A CN107192599 A CN 107192599A CN 201610725814 A CN201610725814 A CN 201610725814A CN 107192599 A CN107192599 A CN 107192599A
- Authority
- CN
- China
- Prior art keywords
- insulation material
- material thickness
- natural
- rapid prototyping
- prototyping method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种自然交联绝缘料快速制样方法,将试样放入85℃‑120℃的烘箱之内,烘烤时间按照线芯绝缘料厚度可分别为:绝缘料厚度0.6mm‑1.0mm为3‑6h,绝缘料厚度1.0mm‑1.4mm为5‑8h,绝缘料厚度1.4mm‑1.8mm为7‑12h;该自然交联绝缘料快速制样方法能够解决10kV以下硅烷可交联聚乙烯绝缘料在使用过程中快速获得交联度数据的问题。
Description
技术领域
本发明涉及一种自然交联绝缘料快速制样方法。
背景技术
随着10kV以下硅烷可交联聚乙烯绝缘料在生产中的广泛应用,省去了交联电缆生产过程中绝缘层催化交联的工序,同时也缩短了电缆的交货周期,但10kV以下硅烷可交联聚乙烯绝缘料的自交联过程比较缓慢,通常需要15天左右的时间才能达到正常交联度,这给生产中的中间检验带来一定的困难。
发明内容
本发明要解决的技术问题是提供一种能够解决10KV以下硅烷可交联聚乙烯绝缘料在使用过程中快速获得交联度数据的问题的自然交联绝缘料快速制样方法。
为解决上述问题,本发明采用如下技术方案:
一种自然交联绝缘料快速制样方法,将试样放入85℃-120℃的烘箱之内,烘烤时间按照线芯绝缘料厚度可分别为:绝缘料厚度0.6mm-1.0mm为 3-6h,绝缘料厚度1.0mm-1.4mm为5-8h,绝缘料厚度1.4mm-1.8mm为7-12h。
将所需试验的样品放置于烘箱当中,然后提高烘箱温度通过一段时间的烘烤,最后得到所需的试验样品,就可以正常进行相关实验。
本发明的有益效果为:在提供较为准确的试验数据的同时可节省大量的中间检验时间,缩短中间检验时间,提高产品的生产效率。
具体实施方式
为使对本发明的结构特征及所达成的功效有更进一步的了解与认识,用以较佳的实施例详细的说明,说明如下:
采用以下两种制样方法:
1、将试样放入85℃的烘箱之内,烘烤时间按照线芯绝缘料厚度可分别为:绝缘料厚度0.6mm-1.0mm为6小时,绝缘料厚度1.0mm-1.4mm为8小时,绝缘料厚度1.4mm-1.8mm为12小时。
2、将试样放入120℃的烘箱之内,烘烤时间按照线芯绝缘料厚度可分别为:绝缘料厚度0.6mm-1.0mm为3小时,绝缘料厚度1.0mm-1.4mm为5小时,绝缘料厚度1.4mm-1.8mm为7小时。
经过大量实验验证通过以上制样方法,大约可以得到自然放置情况下14 至20天的自然交联绝缘料的交联度数据,为产品的中间检验提供真实的试验样品。
试样热延伸数据对比:
生产设备:Ф65型挤塑机(在这里设备不做限定)
由以上对比数据可以看出,85℃烘烤制样方法与120℃烘烤制样方法所得试验样品与自然放置14天的试验样品试验数据较为接近,但相比之下 85℃烘烤制样方法所得数据更为准确。所以建议120℃烘烤制样方法仅用于急需得到结果的试验。
本发明的有益效果为:在提供较为准确的试验数据的同时可节省大量的中间检验时间,缩短中间检验时间,提高产品的生产效率。
以上所述,仅为本发明的具体实施方式,但本发明的保护范围并不局限于此,任何不经过创造性劳动想到的变化或替换,都应涵盖在本发明的保护范围之内。
Claims (1)
1.一种自然交联绝缘料快速制样方法,其特征在于:将试样放入85℃-120℃的烘箱之内,烘烤时间按照线芯绝缘料厚度可分别为:绝缘料厚度0.6mm-1.0mm为3-6h,绝缘料厚度1.0mm-1.4mm为5-8h,绝缘料厚度1.4mm-1.8mm为7-12h。