CN1071182C - 铝塑管变径套结法 - Google Patents

铝塑管变径套结法 Download PDF

Info

Publication number
CN1071182C
CN1071182C CN99116611A CN99116611A CN1071182C CN 1071182 C CN1071182 C CN 1071182C CN 99116611 A CN99116611 A CN 99116611A CN 99116611 A CN99116611 A CN 99116611A CN 1071182 C CN1071182 C CN 1071182C
Authority
CN
China
Prior art keywords
pipe
aluminium
diameter
plastic
sleeve joint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN99116611A
Other languages
English (en)
Other versions
CN1243926A (zh
Inventor
粟幼特
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN99116611A priority Critical patent/CN1071182C/zh
Publication of CN1243926A publication Critical patent/CN1243926A/zh
Application granted granted Critical
Publication of CN1071182C publication Critical patent/CN1071182C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明提供一种铝塑管变径套结法,主要用于建筑铝塑管加工工艺。其方法是铝管内径与塑管外径相同,但铝管内径为负公差,塑管外径为正公差,使之常温下为过盈配合,然后将铝管加热,也可同时塑管降温,使两管温差达70-90℃,再用专用设备将塑管拉入铝管中,自然冷却。该方法工艺简单、造价低,不会因温度变化而松脱和滑动,寿命长、无污染。

Description

铝塑管变径套结法
本发明涉及一种铝塑管变径套结法,属于建筑铝塑管生产工艺。
铝塑管由于耐腐蚀、无污染、已成为政策性替代产品。但因生产工艺需将两管套结,工艺难度大。现有生产工艺用粘结剂拉套法使两管结合,因此成本高,粘结剂对水有污染,因热胀冷缩使两管间结合面有间隙,而出现松脱,滑动,对其强度及寿命造成不良影响。经检索专利申请98110415即是此种例证。
本发明的目的是研究一种工艺简单、而铝塑两管结合而无间隙,不松脱的套结工艺。
本发明的技术方案是在常温时,内管外径与外管内径相等,将外铝管内壁取为负公差,将内塑管外壁取为正公差,使之过盈公差为0.30mm-0.00mm之间,然后将铝管加热,使铝塑两管温差达70°-90℃时用专用设备将塑管拉入铝管。
上述工艺过程中一般铝管内壁负公差为-0.10mm,塑管外径正公差为+0.20mm,总过盈公差最大为+0.30mm。
温差主要是加热铝管,可用热水及蒸汽加热,加热至90-100℃,当环境温度高时,可用冰等方法降低塑管温度。
本发明的优点是,用过盈配合温差法套结,工艺简单,温度一致后两管自然紧密贴合,不会随温度变化产生松脱和滑动现象,同时不用粘结剂对水质无污染,使用寿命长。
实施例:如DN15-DN50的管材,将铝管内径公差定为-0.10mm,将塑管外径公差定为+0.20mm,用热水及蒸汽法将铝管加热至90-100℃,塑管用冰降至0--10℃,迅速将塑管拉入铝管,自然冷却即可。

Claims (3)

1、一种铝塑管变径套结法,主要工艺是设计上内管外径与外管内径相等,将外层铝管的内壁加工为负公差,将内管塑管外壁加工为正公差,使之公差总和为0.00mm-0.30mm,然后将铝管加热,使铝塑两管温差达70-90℃时再用专用设备将塑管拉入铝管。
2、根据权利要求1所述的铝塑管变径套结法,其特征是铝管内壁负公差为-0.10mm,塑管外径正公差为+0.20mm,使公差过盈值在+0.30mm。
3、根据权利要求1或2所述的铝塑管变径套结法,其特征是温差主要是将铝管加热至90-100℃,当环境温度高时,可同时降低塑管温度。
CN99116611A 1999-08-25 1999-08-25 铝塑管变径套结法 Expired - Fee Related CN1071182C (zh)