CN107099192A - 一种炫彩棒的制备方法 - Google Patents
一种炫彩棒的制备方法 Download PDFInfo
- Publication number
- CN107099192A CN107099192A CN201710450416.7A CN201710450416A CN107099192A CN 107099192 A CN107099192 A CN 107099192A CN 201710450416 A CN201710450416 A CN 201710450416A CN 107099192 A CN107099192 A CN 107099192A
- Authority
- CN
- China
- Prior art keywords
- mass parts
- colorful
- rod
- preparation
- green
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种炫彩棒的制备方法,该方法包括以下步骤:取100质量份的水加热至90℃,将30‑50质量份的瓜尔豆胶加入溶解,然后加入40‑60质量份的硬脂酸钠、25‑35质量份的丙二醇、25‑35质量份的甘油、3‑10质量份的颜料,搅拌均匀,经过扎料后加热溶解,浇铸成型即得炫彩棒。本发明一种炫彩棒的制备方法制备的炫彩棒具有良好的手感、水溶性、流畅性、可擦拭性和光滑度等,以及合适的硬度,具有环保、无毒等性能,有广阔的市场前景。
Description
技术领域
本发明涉及绘画用品制备领域,尤其涉及一种炫彩棒的制备方法。
背景技术
炫彩棒是一种新型的绘画用品,日本、韩国最先发展,后来在国内也得到了较快的发展,并且进行了技术改进;水溶彩棒一般有一个塑料外壳,多采用口红式旋转方式,相比传统的蜡笔和油画棒,水溶彩棒绘画时阻力小,涂层更佳,而且有水溶性效果,易擦洗不污染环境的特点,越来越受到市场的欢迎。相比较传统的蜡笔和油画棒,水溶彩棒手感超滑,完全没有阻力的感觉;色泽艳丽,涂层分明,主要填料为无毒环保材料,更加安全。水溶彩棒又特别容易清洗,即便不小心画到衣物上面也不用担心,用清水就能洗干净。而且由于材质的进步,水溶彩棒不仅能在纸上作画,而且能在毛玻璃,地砖甚至人体上作画。由于有一个塑料外壳,手不会直接接触蜡芯,干净卫生。
虽然水溶性炫彩棒问世已经近十年,但是因为技术问题及成本问题,并没有被广大消费者接受,只是在上海等地区流行。但是,随着收入的增加,人们对环保的要求增加,对文具安全的重视,以及炫彩棒本身具有的独特优势,将相当程度上代替蜡笔和油画棒。
发明内容
为了克服现有技术中的缺陷,提供一种炫彩棒的制备方法。
本发明通过下述方案实现:
一种炫彩棒的制备方法,该方法包括以下步骤:取100质量份的水加热至90℃,将30-50质量份的瓜尔豆胶加入溶解,然后加入40-60质量份的硬脂酸钠、25-35质量份的丙二醇、25-35质量份的甘油、3-10质量份的颜料,搅拌均匀,经过扎料后加热溶解,浇铸成型即得炫彩棒。
所述颜料是中黄、淡黄、橄榄绿、粉绿、土黄、土红、赭石、桔黄、群青、钴蓝、湖蓝、紫罗兰、柠檬黄、玫瑰红、深红、青莲、钛白粉、碱性玫瑰精、铁黄、酞青绿、橡胶大红中的一种或者数种。
本发明的有益效果为:
本发明一种炫彩棒的制备方法制备的炫彩棒具有良好的手感、水溶性、流畅性、可擦拭性和光滑度等,以及合适的硬度,具有环保、无毒等性能,有广阔的市场前景。
具体实施方式
下面结合具体实施例对本发明进一步说明:
实施例1
取100质量份的的水加热至90℃,首先将30质量份的的瓜尔豆胶加入溶解、然后加入40质量份的的硬脂酸钠,25质量份的的丙二醇,25质量份的的甘油,3质量份的的玫瑰红颜料,搅拌均匀,最后在在三辊机上扎料2遍,再次加热溶解后浇铸成型即得炫彩棒。
实施例2
取100质量份的的水加热至90℃,首先将36质量份的的瓜尔豆胶加入溶解、然后加入45质量份的的硬脂酸钠,28质量份的的丙二醇,27质量份的的甘油,5质量份的的碱性玫瑰精颜料,搅拌均匀,最后在在三辊机上扎料2遍,再次加热溶解后浇铸成型即得炫彩棒。
实施例3
取100质量份的的水加热至90℃,首先将40质量份的的瓜尔豆胶加入溶解、然后加入50质量份的的硬脂酸钠,30质量份的的丙二醇,30质量份的的甘油,7质量份的的紫罗兰颜料,搅拌均匀,最后在在三辊机上扎料2遍,再次加热溶解后浇铸成型即得炫彩棒。
实施例4
取100质量份的的水加热至90℃,首先将50质量份的的瓜尔豆胶加入溶解、然后加入60质量份的的硬脂酸钠,35质量份的的丙二醇,35质量份的的甘油,10质量份的的粉绿颜料,搅拌均匀,最后在在三辊机上扎料2遍,再次加热溶解后浇铸成型即得炫彩棒。
表1是本发明四个实施例的性能指标的比较,其中指标的衡量数字1、2、3、4、5分别代表差、较差、中等、较好、好。
表1四个实施例的性能指标
在实际使用中,本发明的颜料是中黄、淡黄、橄榄绿、粉绿、土黄、土红、赭石、桔黄、群青、钴蓝、湖蓝、紫罗兰、柠檬黄、玫瑰红、深红、青莲、钛白粉、碱性玫瑰精、铁黄、酞青绿、橡胶大红中的一种或者数种。
本发明以瓜尔豆胶为锁水剂和成膜物质,以硬脂酸钠为炫彩棒主体填料,通过调整甘油、丙二醇含量调整整体的流畅性、硬度、光泽性等因素,制备的具有优良的综合性能的炫彩棒,具有广泛的市场需求。
尽管已经对本发明的技术方案做了较为详细的阐述和列举,应当理解,对于本领域技术人员来说,对上述实施例做出修改或者采用等同的替代方案,这对本领域的技术人员而言是显而易见,在不偏离本发明精神的基础上所做的这些修改或改进,均属于本发明要求保护的范围。
Claims (2)
1.一种炫彩棒的制备方法,其特征在于,该方法包括以下步骤:取100质量份的水加热至90℃,将30-50质量份的瓜尔豆胶加入溶解,然后加入40-60质量份的硬脂酸钠、25-35质量份的丙二醇、25-35质量份的甘油、3-10质量份的颜料,搅拌均匀,经过扎料后加热溶解,浇铸成型即得炫彩棒。
2.根据权利要求1所述的一种炫彩棒的制备方法,其特征在于:所述颜料是中黄、淡黄、橄榄绿、粉绿、土黄、土红、赭石、桔黄、群青、钴蓝、湖蓝、紫罗兰、柠檬黄、玫瑰红、深红、青莲、钛白粉、碱性玫瑰精、铁黄、酞青绿、橡胶大红中的一种或者数种。