CN106982520A - A kind of riveting method for improving riveted precision - Google Patents

A kind of riveting method for improving riveted precision Download PDF

Info

Publication number
CN106982520A
CN106982520A CN201710289048.2A CN201710289048A CN106982520A CN 106982520 A CN106982520 A CN 106982520A CN 201710289048 A CN201710289048 A CN 201710289048A CN 106982520 A CN106982520 A CN 106982520A
Authority
CN
China
Prior art keywords
riveted
rivet
rivet hole
boards
edges
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710289048.2A
Other languages
Chinese (zh)
Inventor
欧阳�
汪广明
戴勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangmen Suntak Circuit Technology Co Ltd
Original Assignee
Jiangmen Suntak Circuit Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangmen Suntak Circuit Technology Co Ltd filed Critical Jiangmen Suntak Circuit Technology Co Ltd
Priority to CN201710289048.2A priority Critical patent/CN106982520A/en
Publication of CN106982520A publication Critical patent/CN106982520A/en
Pending legal-status Critical Current

Abstract

The present invention relates to board production technical field, specially a kind of riveting method for improving riveted precision.The present invention passes through the placement positioning pin in the rivet hole of another edges of boards, each flaggy that pilot pin can be fixed in laminate structure respectively at grade with red needle, it can avoid sliding between core plate and causing layer inclined during riveted, even if the variable thickness of two core plates is caused in laminate structure, also it can ensure that homework precision is not influenceed by laminate structure, also can equally ensure its precision during batch production during riveted.If pilot pin can not be inserted in tacking nail, it can tentatively confirm that the rivet hole has been rushed partially, so as to realize the problem of whether rivet hole rushes inclined is being would know that during riveted.Can will occur the inclined scrappage of layer after riveted by the inventive method and be reduced to zero, significantly reduce product rejection rate, improve production efficiency, reduce production cost.

Description

A kind of riveting method for improving riveted precision
Technical field
The present invention relates to board production technical field, more particularly to a kind of riveting method for improving riveted precision.
Background technology
The process for pressing of multilayer printed wiring board can be divided into pin positioning laminating technology according to the localization method between each layer (PIN-LAM) and without pin positioning laminating technology (MASS-LAM), the former positioning precision is high, but efficiency is low, cost is high, is only applicable In the production of high-layer, high-precision multilayer printed wiring board, although and the latter's positioning precision is relatively low, efficiency high, cost is low, Therefore this method is that current most domestic producer carries out the process that multi-layer sheet production in enormous quantities is commonly used.
When pressing working procedure is pressed using MASS-LAM, needed before pressing using the first riveted laminate structure of rivet driver, and twin shaft The homework precision of rivet driver and three axle rivet drivers is limited, when running into the laminate structure for having task difficulty (such as comprising thickness copper or Structure of pseudobed plate etc.) or 8 layers and more than 8 layers of operation production plate when, easily produce layer scrap partially.Existing riveted flow is such as Under:The technique for riveting flow of existing use twin shaft rivet driver or three axle rivet drivers is as follows:1st, in core plate and the edges of boards of prepreg Bore at least eight rivet hole (wherein long side at least three, short side at least one is as shown in Figure 1);2nd, according to lamination order by core plate with Prepreg is stacked together, and core plate is corresponded with the rivet hole on prepreg, forms laminate structure;3rd, twin shaft or three axles Two or three rivet holes that the red needle of rivet driver is inserted on laminate structure one side simultaneously carry out riveted, then riveted lamination knot one by one Other rivet holes on structure.There is problems with above-mentioned riveting method:1st, because the rivet hole of riveted first is in straight line On, it is impossible to a plane is fixed.When operation is to the laminate structure for having production difficulty, at the first hole of riveted, different cores The plane of plate may produce relative slip, cause layer to scrap partially.2nd, after due to two axles and three axle rivet driver long-time uses, its Stability can gradually be deteriorated, even if operation does not have the laminate structure of difficulty or the initial workpiece of the difficult laminate structure of operation not to occur When layer is inclined, homework precision when can not also ensure follow-up batch production is not in deviation, and is only partially by X-RAY detection layers A kind of detection method, any raising is not had to its homework precision;Prior art uses biaxial plane or three axle rivet machine operations, when The larger laminate structure layer scrappage about 30% partially of task difficulty is run into, is also occurred even if the common laminate structure of operation scattered Layer scrap partially.3rd, when previous process bores rivet hole to core material, if the rivet hole of the same position of two core plates has been offset, It can not ensure that process is inclined by drift before being found in operation using existing riveting method.
The content of the invention
The present invention, which is directed to, to be had the inclined scrappage height of layer using existing riveting method and riveting can not be known during riveted The problem of whether nail rushes inclined would know that whether rivet hole rushes inclined riveting during riveted precision and riveted there is provided a kind of improve Conjunction method.
To achieve the above object, the present invention uses following technical scheme.
A kind of riveting method for improving riveted precision, comprises the following steps:
S1, according to lamination order the prepreg that core plate and edges of boards that edges of boards have bored rivet hole have bored rivet hole is layered in Together, laminate structure is formed;The edges of boards of the core plate and prepreg are respectively provided with least eight rivet holes.
S2, two or three rivets by same edges of boards on two of rivet driver or three red needle correspondence insertion laminate structures In hole.
It is preferred that, the rivet driver is twin shaft rivet driver or three axle rivet drivers.
S3, in laminate structure in a rivet hole of another edges of boards insert a pilot pin, the rivet hole be referred to as positioning Rivet hole.
It is preferred that, the pilot pin is rivet.
S4, by rivet driver simultaneously the above-mentioned rivet hole for having inserted red needle of riveted.
S5, pass through rivet driver remaining rivet hole of riveted in addition to tacking nail one by one.
It is preferred that, the rivet hole of long edges of boards in preferential riveted laminate structure, then riveted short slab side rivet hole;Same edges of boards Rivet hole then first riveted two ends rivet hole, then the rivet hole in the middle of riveted.
S6, the pilot pin taken out in tacking nail, pass through rivet driver riveted tacking nail.
Above-mentioned riveting method is preferred, in step s 2, by two of rivet driver or three red needles correspondence insertion lamination knots On structure in two or three rivet holes of same long edges of boards;In step s3, the quilting rivet hole position is in another long edges of boards.
It is furthermore preferred that the quilting rivet hole position is in the centre of another long edges of boards.
Compared with prior art, the beneficial effects of the invention are as follows:The present invention in the rivet hole of another edges of boards by placing Pilot pin, each flaggy that pilot pin and red needle can be fixed in laminate structure respectively at grade, during can avoiding riveted Slided between core plate and cause layer partially, even if the variable thickness of two core plates is caused in laminate structure, can also ensure homework precision during riveted Do not influenceed by laminate structure, also can equally ensure its precision during batch production.If pilot pin can not be inserted in tacking nail, It then can tentatively confirm that the rivet hole has been rushed partially, so as to realize the problem of whether rivet hole rushes inclined is being would know that during riveted. Can will occur the inclined scrappage of layer after riveted by the inventive method and be reduced to zero, significantly reduce product rejection rate, improve Production efficiency, reduces production cost.
Brief description of the drawings
Fig. 1 is the structural representation for the core plate that edges of boards are drilled with 8 rivet holes;
Fig. 2 is the top view of laminate structure in embodiment 1.
Embodiment
In order to more fully understand the technology contents of the present invention, with reference to specific embodiment to technical scheme It is described further and illustrates.
Embodiment 1
Reference picture 1-2, the present embodiment provides a kind of riveting method for improving riveted precision.
Comprise the following steps that:
(1) provide for being subsequently pressed into multiple-plate core plate and prepreg, respectively in core plate and the plate of prepreg Rivet hole is bored on side, and when core plate is overlapping with prepreg, the rivet hole on both is overlapping one by one.Core plate is rectangle, in two length Three rivet holes are bored on side respectively, a rivet hole are bored respectively on two short sides, as shown in Figure 1.In other embodiments, often Rivet hole number on block plate can be more than eight, the long rivet hole of side at least three and short side at least one rivet hole.
(2) it is according to lamination order that core plate and prepreg is stacked together, form laminate structure 10.
(3) three red needles correspondence of three axle rivet drivers is inserted in laminate structure 10 in three rivet holes of same long edges of boards 11st, 12,13, as shown in Figure 2.
(4) pilot pin is inserted in a rivet hole in laminate structure in the middle of another long edges of boards, the rivet hole claims The rivet used for tacking nail 14, the pilot pin when being riveted.
(5) by three axle rivet drivers while above-mentioned three rivet holes 11,12,13 for having inserted red needle of riveted.
(6) by remaining rivet hole on three axle rivet drivers one by one riveted laminate structure 10 in addition to tacking nail 14, and And in preferential riveted laminate structure 10 long edges of boards rivet hole, then riveted short slab side rivet hole;The rivet hole of same edges of boards is then The rivet hole at first riveted two ends, then the rivet hole in the middle of riveted.
(7) pilot pin in tacking nail 14 is taken out, passes through three axle rivet driver riveted tacking nail.
The present embodiment is by the placement positioning pin in the rivet hole of another edges of boards in laminate structure, and pilot pin and red needle can be Each flaggy fixed respectively in laminate structure on same plane, can avoid sliding between core plate and causing layer partially during riveted, i.e., The variable thickness of two core plates in laminate structure is caused, can also ensure that homework precision is not influenceed by laminate structure during riveted, batch Also its precision can equally be ensured during production.
If pilot pin can not be inserted in tacking nail, it can tentatively confirm that the rivet hole has been rushed partially, so as to realize in riveting The problem of whether rivet hole rushes inclined is would know that during conjunction.
Can will occur the inclined scrappage of layer after riveted by the inventive method and be reduced to zero, significantly reduce product rejection Rate, improves production efficiency, reduces production cost.
Embodiment 2
The present embodiment provides a kind of riveting method for improving riveted precision.
Comprise the following steps that:
(1) provide for being subsequently pressed into multiple-plate core plate and prepreg, respectively in core plate and the plate of prepreg Rivet hole is bored on side, and when core plate is overlapping with prepreg, the rivet hole on both is overlapping one by one.Core plate is rectangle, in two length Three rivet holes are bored on side respectively, a rivet hole are bored respectively on two short sides, as shown in Figure 1.In other embodiments, often Rivet hole number on block plate can be more than eight, the long rivet hole of side at least three and short side at least one rivet hole.
(2) it is according to lamination order that core plate and prepreg is stacked together, form laminate structure 10.
(3) two red needles correspondence of twin shaft rivet driver is inserted in laminate structure in two rivet holes of same long edges of boards.
(4) pilot pin is inserted in a rivet hole in laminate structure in the middle of another long edges of boards, the rivet hole claims The rivet used for tacking nail, the pilot pin when being riveted.
(5) by twin shaft rivet driver while above-mentioned two rivet holes for having inserted red needle of riveted.
(6) by remaining rivet hole on twin shaft rivet driver one by one riveted laminate structure in addition to tacking nail, and it is excellent The rivet hole of long edges of boards in first riveted laminate structure, then riveted short slab side rivet hole;The rivet hole of same edges of boards then first riveted The rivet hole at two ends, then the rivet hole in the middle of riveted.
(7) pilot pin in tacking nail is taken out, passes through twin shaft rivet driver riveted tacking nail.
The present embodiment is by the placement positioning pin in the rivet hole of another edges of boards in laminate structure, and pilot pin and red needle can be Each flaggy fixed respectively in laminate structure on same plane, can avoid sliding between core plate and causing layer partially during riveted, i.e., The variable thickness of two core plates in laminate structure is caused, can also ensure that homework precision is not influenceed by laminate structure during riveted, batch Also its precision can equally be ensured during production.
If pilot pin can not be inserted in tacking nail, it can tentatively confirm that the rivet hole has been rushed partially, so as to realize in riveting The problem of whether rivet hole rushes inclined is would know that during conjunction.
Can will occur the inclined scrappage of layer after riveted by the inventive method and be reduced to zero, significantly reduce product rejection Rate, improves production efficiency, reduces production cost.
The technology contents described above that the present invention is only further illustrated with embodiment, in order to which reader is easier to understand, But embodiments of the present invention are not represented and are only limitted to this, and any technology done according to the present invention extends or recreated, and is sent out by this Bright protection.

Claims (6)

1. a kind of riveting method for improving riveted precision, it is characterised in that comprise the following steps:
S1, according to lamination order the prepreg that core plate and edges of boards that edges of boards have bored rivet hole have bored rivet hole is layered in one Rise, form laminate structure;The edges of boards of the core plate and prepreg are respectively provided with least eight rivet holes;
S2, two or three rivet holes by same edges of boards on two of rivet driver or three red needle correspondence insertion laminate structures It is interior;
S3, a pilot pin is inserted in a rivet hole of another edges of boards in laminate structure, the rivet hole is referred to as quilting rivet Hole;
S4, by rivet driver simultaneously the above-mentioned rivet hole for having inserted red needle of riveted;
S5, pass through rivet driver remaining rivet hole of riveted in addition to tacking nail one by one;
S6, the pilot pin taken out in tacking nail, pass through rivet driver riveted tacking nail.
2. a kind of riveting method for improving riveted precision according to claim 1, it is characterised in that in step S5, preferentially The rivet hole of long edges of boards in riveted laminate structure, then riveted short slab side rivet hole;The rivet hole of same edges of boards then first riveted two The rivet hole at end, then the rivet hole in the middle of riveted.
3. a kind of riveting method for improving riveted precision according to claim 1, it is characterised in that in step S2, by riveting In two of nailing machine or three red needles correspondence insertion laminate structures in two or three rivet holes of same long edges of boards;Step S3 In, the quilting rivet hole position is in another long edges of boards.
4. a kind of riveting method for improving riveted precision according to claim 3, it is characterised in that described in step S3 Quilting rivet hole position is in the centre of another long edges of boards.
5. a kind of riveting method for improving riveted precision according to claim 1, it is characterised in that the pilot pin is riveting Nail.
6. a kind of riveting method for improving riveted precision according to claim 1, it is characterised in that the rivet driver is three Axle rivet driver or twin shaft rivet driver.
CN201710289048.2A 2017-04-27 2017-04-27 A kind of riveting method for improving riveted precision Pending CN106982520A (en)