CN106769386A - A kind of method for quick of woodcare paint glossiness - Google Patents

A kind of method for quick of woodcare paint glossiness Download PDF

Info

Publication number
CN106769386A
CN106769386A CN201611156495.2A CN201611156495A CN106769386A CN 106769386 A CN106769386 A CN 106769386A CN 201611156495 A CN201611156495 A CN 201611156495A CN 106769386 A CN106769386 A CN 106769386A
Authority
CN
China
Prior art keywords
glass plate
glossiness
paint
quick
woodcare paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201611156495.2A
Other languages
Chinese (zh)
Inventor
曾龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Paint Chengdu Co Ltd
Original Assignee
Nippon Paint Chengdu Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Paint Chengdu Co Ltd filed Critical Nippon Paint Chengdu Co Ltd
Priority to CN201611156495.2A priority Critical patent/CN106769386A/en
Publication of CN106769386A publication Critical patent/CN106769386A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of method for quick of woodcare paint glossiness, it is comprised the following steps:Get the raw materials ready, scratch, toast and measure.A kind of method for quick of woodcare paint glossiness that the present invention is provided, sample, obtained film thickness are uniform using scratching on a glass for the method, are conducive to the precision of accurate measurement detection;The method for quick of the woodcare paint glossiness that the present invention is provided substantially reduces detection time on the premise of accuracy of detection is ensured, detection time typically only needs 1~3h, improves production efficiency;A kind of method for quick of woodcare paint glossiness that the present invention is provided is simple to operate, it is easy to control, and measurement is accurate, is easy to promote.

Description

A kind of method for quick of woodcare paint glossiness
Technical field
The invention belongs to paint film detection field, a kind of method for quick of woodcare paint glossiness is specifically related to.
Background technology
Woodcare paint refers to, for the resinoid paint on woodwork, there is polyester, polyurethane paint etc., can be divided into aqueous and oil Property.Natural woodcare paint is commonly called as lacquer, there is the title of " state's paint " again.The juice for getting off referred to as Chinese lacquer or former bucket are tapped from lacquer tree Paint, filters off impurity and is referred to as raw lacquer with calico.China's woodwork coating is mainly used in two big fields, one be for Furniture manufacture factory, Two is that, for interior decoration decoration, according to the different field of employment of woodwork, can be divided into following type.
1. wood furniture:The main application fields of woodwork coating, are that medium-to-high grade woodenware is applied based on factorial praluction application Expect the competition place of factory.
2. interior decoration:It is main construction means with manual brushing, suitable proportion is occupied in market sale, is low and middle-grade The competition place of coating material production factory.
3. timber floor:It is the woodwork coating application field occurred after factorial praluction timber floor, is with photocureable coating It is main.
4. wooden toy:Based on opaque covering with paint, its content of beary metal can not exceeded be main quality index.
5. pencil coating:It is the special woodwork coating of the opaque covering with paint of a class, in addition to quick-drying is required, content of beary metal is not yet Can be exceeded.
6. outdoor woodwork:The woodworks such as the chair class that is used for places such as park, swimming pool, sandy beaches are referred mainly to, its It is required that being have certain weatherability.
Film, also known as paint film.The solid-state continuous film that coating application is formed in the one or multi-channel coating on ground.Generally Film is made up of multi-layer coating, and the number of coating is determined according to the requirement of coated article part.Generally comprise prime coat, inter coat And top coat layer.Film embodies the effect that coatings system is used.Glossiness is journey of the umerical body surface close to minute surface Degree, is one significant feature of paint film, very big to coating decoration performance impact.Therefore, the detection to glossiness just very must Will.Current detection method time of measuring is more long, reduces production efficiency, and easily cause film thickness not during plate is sprayed Uniformly, inspection result is influenceed.Therefore, the detection to gloss of film degree has very big room for improvement.
The content of the invention
A kind of shortcoming it is an object of the invention to overcome prior art, there is provided quick detection side of woodcare paint glossiness Method, the method is simple to operate, it is easy to controls, measure accurate, is easy to promote.
The purpose of the present invention is achieved through the following technical solutions:A kind of method for quick of woodcare paint glossiness, it Comprise the following steps:
S1. get the raw materials ready:Woodcare paint sample to be detected 3~7g is taken, it is standby;Clean, dry glass plate is taken, plate face level is put Put, the glass plate has the glass plate of Berlin black for the back side;
S2. scratch:Woodcare paint sample drop to be detected is used into 80~120 μm of wire winding rod in glass plate top with dropper On a glass, the blade coating is from top to bottom uniformly to scratch to blade coating, and is completed in 2~3S, obtains making the glass of paint film Plate;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 100~140 DEG C of baking ovens, constant temperature baking 1~3h, the paint film glass plate after being toasted;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value of detection 4~6 times is taken, that is, obtains the glossiness of woodcare paint.
Further, the length of glass plate is respectively 150mm × 100mm × 5mm described in step S1.
Further, the viscosity of woodcare paint sample described in step S1 is 27~33 seconds.The condition of viscosity measurements is temperature 25 DEG C, humidity 65%, with T-4# glasss of detection.
The present invention has advantages below:A kind of method for quick of woodcare paint glossiness that the present invention is provided, the method Using sample is scratched on a glass, obtained film thickness is uniform, is conducive to the precision of accurate measurement detection;The present invention is provided Woodcare paint glossiness method for quick ensure accuracy of detection on the premise of, detection time is substantially reduced, during detection Between it is general only need 1~3h, improve production efficiency;A kind of method for quick operation of woodcare paint glossiness that the present invention is provided Simply, it is easy to control, measure accurate, be easy to promote.
Specific embodiment
With reference to embodiment, the present invention will be further described, and protection scope of the present invention is not limited to following institute State:
Embodiment 1:A kind of method for quick of woodcare paint glossiness, it is comprised the following steps:
S1. get the raw materials ready:Two Dai Yong get Li ultrawhite semi-gloss woodware white paints 3g are taken, it is standby;Take clean, dry glass plate, plate face Horizontal positioned;The viscosity of the sample is:27 seconds (T-4# glasss, temperature:25 DEG C, humidity:65%);The glass plate has for the back side The glass plate of Berlin black, and the length of glass plate is respectively 150mm × 100mm × 5mm;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 80 μm of wire winding rods with dropper On glass plate, the blade coating is from top to bottom uniformly to scratch, and is completed in 2S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 100 DEG C of baking ovens, constant temperature baking 1h is obtained Paint film glass plate after to baking;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value for detecting 4 times is taken, that is, obtains the glossiness of testing sample.
Embodiment 2:A kind of method for quick of woodcare paint glossiness, it is comprised the following steps:
S1. get the raw materials ready:PU matt varnish JD-P2025 samples 7g is taken, it is standby;Take clean, dry glass plate, plate face water Placing flat;The viscosity of the sample is:33 seconds (T-4# glasss, temperature:25 DEG C, humidity:65%);The glass plate whether there is for the back side The pitch-dark glass plate of light, and the length of glass plate is respectively 150mm × 100mm × 5mm;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 120 μm of wire winding rods with dropper On a glass, the blade coating is from top to bottom uniformly to scratch, and is completed in 3S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 140 DEG C of baking ovens, constant temperature baking 3h is obtained Paint film glass plate after to baking;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value for detecting 6 times is taken, that is, obtains the glossiness of testing sample.
Embodiment 3:A kind of method for quick of woodcare paint glossiness, it is comprised the following steps:
S1. get the raw materials ready:PU matt varnish JD-P2023 samples 5g is taken, it is standby;Take clean, dry glass plate, plate face water Placing flat;The viscosity of the sample is:30 seconds (T-4# glasss, temperature:25 DEG C, humidity:65%);The glass plate whether there is for the back side The pitch-dark glass plate of light, and the length of glass plate is respectively 150mm × 100mm × 5mm;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 100 μm of wire winding rods with dropper On a glass, the blade coating is from top to bottom uniformly to scratch, and is completed in 2S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 120 DEG C of baking ovens, constant temperature baking 2h is obtained Paint film glass plate after to baking;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value for detecting 5 times is taken, that is, obtains the glossiness of testing sample.
Embodiment 4:A kind of method for quick of woodcare paint glossiness, it is comprised the following steps:
S1. get the raw materials ready:Golden clothes limpid refined environmentally friendly semi-gloss woodenware lacquer sample 6g is taken, it is standby;Clean, dry glass plate is taken, Plate face horizontal positioned;The viscosity of the sample is:28 seconds (T-4# glasss, temperature:25 DEG C, humidity:65%);The glass plate is the back of the body There is the glass plate of Berlin black in face, and the length of glass plate is respectively 150mm × 100mm × 5mm;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 90 μm of wire winding rods with dropper On glass plate, the blade coating is from top to bottom uniformly to scratch, and is completed in 3S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 110 DEG C of baking ovens, constant temperature baking 1.5h, Paint film glass plate after being toasted;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value for detecting 6 times is taken, that is, obtains the glossiness of testing sample.
Embodiment 5:A kind of method for quick of woodcare paint glossiness, it is comprised the following steps:
S1. get the raw materials ready:Golden clothes anti-formaldehyde environmental protection semi-gloss woodenware lacquer sample 4g is taken, it is standby;Clean, dry glass plate is taken, Plate face horizontal positioned;The viscosity of the sample is:32 seconds (T-4# glasss, temperature:25 DEG C, humidity:65%);The glass plate is the back of the body There is the glass plate of Berlin black in face, and the length of glass plate is respectively 150mm × 100mm × 5mm;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 110 μm of wire winding rods with dropper On a glass, the blade coating is from top to bottom uniformly to scratch, and is completed in 2S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 130 DEG C of baking ovens, constant temperature baking 2.5h, Paint film glass plate after being toasted;
S4. measure:Use the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness The average value for detecting 5 times is taken, that is, obtains the glossiness of testing sample.
The detection data of above-mentioned 5 embodiments is as follows:

Claims (3)

1. a kind of method for quick of woodcare paint glossiness, it is characterised in that it is comprised the following steps:
S1. get the raw materials ready:Woodcare paint sample to be detected 3~7g is taken, it is standby;Take clean, dry glass plate, plate face horizontal positioned, institute Stating glass plate has the glass plate of Berlin black for the back side;
S2. scratch:Woodcare paint sample drop to be detected is scratched in glass plate top using 80~120 μm of wire winding rods with dropper On a glass, the blade coating is from top to bottom uniformly to scratch, and is completed in 2~3S, obtains making the glass plate of paint film;
S3. toast:The glass plate for making paint film that step S2 is obtained is positioned in 100~140 DEG C of baking ovens, constant temperature baking 1~ 3h, the paint film glass plate after being toasted;
S4. measure:Using the glossiness of paint film glass plate after the baking that glossometer detecting step S3 is obtained, the glossiness takes inspection The average value of 4~6 times is surveyed, that is, obtains the glossiness of woodcare paint.
2. a kind of method for quick of woodcare paint glossiness as claimed in claim 1, it is characterised in that described in step S1 The length of glass plate is respectively 150mm × 100mm × 5mm.
3. a kind of method for quick of woodcare paint glossiness as claimed in claim 1, it is characterised in that described in step S1 The viscosity of woodcare paint sample is 27~33 seconds.
CN201611156495.2A 2016-12-14 2016-12-14 A kind of method for quick of woodcare paint glossiness Pending CN106769386A (en)