CN100517419C - Archaized door frame mark brand processing method - Google Patents
Archaized door frame mark brand processing method Download PDFInfo
- Publication number
- CN100517419C CN100517419C CNB2007100244580A CN200710024458A CN100517419C CN 100517419 C CN100517419 C CN 100517419C CN B2007100244580 A CNB2007100244580 A CN B2007100244580A CN 200710024458 A CN200710024458 A CN 200710024458A CN 100517419 C CN100517419 C CN 100517419C
- Authority
- CN
- China
- Prior art keywords
- sign board
- doorframe
- wolline
- embryo
- groove
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a manufacturing method of imitation antique door signboard, which comprises the following steps: sintering the signboard through acetylene and oxygen under high temperature between 150 deg.c and 200 deg.c for 10-15s along the surface; adopting frosted paper to mill the signboard after the surface of signboard is carbonized and blackened; inserting the character content on the signboard after the signboard surface displays sequent fringe and the color becomes brown black; painting the character groove for 2-3 times. The invention simplifies the carbonizing method with low cost, which increases the appearance effect for sign door board.
Description
Technical field
The present invention relates to the job operation of Sign Board, specifically a kind of job operation of archaized door frame mark brand.
Background technology
In office building, between Office Area, Sign Board is set on door usually for the difference in functionality zone.Be used to handle official business for wooden frame structure, adopt Sign Board modelled after an antique usually, Sign Board modelled after an antique can increase the decorative effect of doorframe, can coordinate mutually with wooden frame structure again simultaneously.The doorframe Sign Board will obtain effect modelled after an antique, generally needs to handle through charing.Have many advantages through the timber after the charing processing, for example have favorable durability, termite-proof, anti-rotten, the anti-fungi of energy; Because the carbonization of wood is pure physical process, does not add any chemical agent, therefore has good environmental protection characteristic; Have good stable, moisture resistance etc. in addition.Simultaneously, have surperficial silk quality gloss, clean mark, have appearance modelled after an antique through the timber of charing.In the prior art, to carry out that charing handles be the process of a relative complex to opposite house frame Sign Board: at first be that high temperature is heated to 130 ℃, the timber dewatering drying; Mandatory then thermal treatment, carbonization temperature are controlled in 185 ℃ to the 230 ℃ scopes; Be surface treatment etc. at last.The job operation more complicated of this archaized door frame mark brand, antique effect is not good, and the cost cost is higher.
Summary of the invention
The objective of the invention is to propose a kind of process of simplifying, cut down finished cost, improve the job operation of the archaized door frame mark brand of appearance modelled after an antique.
Purpose of the present invention can be achieved through the following technical solutions:
A kind of job operation of archaized door frame mark brand may further comprise the steps:
1. according to the design font size on the doorframe Sign Board, determine the apparent size size of doorframe Sign Board, and make corresponding wolline embryo doorframe Sign Board with timber;
2. step 1. the wolline embryo doorframe Sign Board reverse side of made offer mounting groove;
3. use acetylene and oxygen high temperature sintering wolline embryo doorframe Sign Board, the temperature of combustion that makes wolline embryo doorframe Sign Board is 150 ℃~200 ℃, and along the surface calcination of wolline embryo doorframe Sign Board, calcination time is 10 seconds~15 seconds, when treating wolline embryo doorframe Sign Board superficial charring blackout, stop calcination;
4. adopt dry sanding paper polishing calcination back door frame Sign Board, treat that doorframe Sign Board surface presents orderly striped, when color is brownish black, stop polishing;
5. the word content with sign is embedded on the doorframe Sign Board, and adopts design colours coating to be filled in the font groove;
6. on the doorframe Sign Board, smear varnish 2~3 times.
Purpose of the present invention can also further realize by following technical measures:
The job operation of aforesaid a kind of archaized door frame mark brand, wherein said step 1. in, timber can be selected pinus sylvestris var. mongolica, masson pine, China fir for use.
The job operation of aforesaid a kind of archaized door frame mark brand, wherein said step 2. in, respectively open a groove at wolline embryo doorframe Sign Board reverse side two ends, groove is made up of inside groove and water jacket, inside groove is positioned at the upper end, water jacket is positioned at the lower end, and connect by level trough, inside groove, 3 millimeters~5 millimeters of the groove depths of water jacket and level trough, the water jacket diameter is 10 millimeters~15 millimeters, the inside groove diameter is 12 millimeters~18 millimeters, the vertical distance at interior groove center and wolline embryo doorframe Sign Board edge be wolline embryo doorframe Sign Board wide 1/4~1/3, the horizontal range at outer groove center and wolline embryo doorframe Sign Board edge be wolline embryo doorframe Sign Board long 1/5~1/4.
Advantage of the present invention is: the present invention is with using acetylene and oxygen high temperature sintering Sign Board, and making the temperature of combustion of wolline embryo doorframe Sign Board is 150 ℃ to 200 ℃, and along surperficial calcination, calcination time is 10 seconds~15 seconds, treats that Sign Board superficial charring blackout gets final product; Then, adopt dry sanding paper polishing Sign Board, this moment, the Sign Board surface presented orderly striped, and color is brownish black; Once more, the word content that identifies is embedded on Sign Board, and adopts design colours coating to be filled in the font groove; At last, on Sign Board, smear varnish 2~3 times, be installed on the door after the drying.The present invention has simplified the method for production of charing, and job operation had both reduced and manufactured cost, increases the appearance of sign doorplate again.In addition, have two mounting grooves at the Sign Board reverse side, each mounting groove all is made up of water jacket and inside groove, thereby the archaized door frame mark brand that makes the present invention process is easy for installation.
Description of drawings
Fig. 1 is the structural representation of doorframe Sign Board reverse side.
Embodiment
Embodiment one
Present embodiment is a kind of job operation of archaized door frame mark brand, carries out according to the following steps:
(1), determines the apparent size size of doorframe Sign Board, and makes corresponding wolline embryo that timber can be selected pinus sylvestris var. mongolica, masson pine, China fir etc. for use with timber according to the design font size on the Sign Board.Usually, Sign Board adopts Chinese and English font, and adopting semicircle lead angle, the length of Sign Board around the Sign Board is 150 millimeters, and wide is 50 millimeters, and thick is 10 millimeters.
(2) because Sign Board need hang on the door, therefore the nested mode of screw is adopted in the installation of Sign Board, open two grooves at the reverse side of Sign Board, as shown in Figure 1, two grooves 1,2 dark 3 millimeters, groove 1,2 all is made up of water jacket 3 and inside groove 4, and connects by level trough 5, water jacket 3 diameters are 12 millimeters, and inside groove 4 diameters are 10 millimeters.The horizontal range L1 at water jacket 3 centre distance Sign Board edges be about Sign Board long 1/5, the vertical distance L 2 at inside groove 4 centre distance Sign Board edges be about Sign Board wide 1/4.
(3) with acetylene and oxygen high temperature sintering Sign Board, making the temperature of combustion of wolline embryo doorframe Sign Board is 150 ℃, and along Sign Board surface calcination, calcination time is 15 seconds, when treating Sign Board superficial charring blackout, stops calcination.
(4) Sign Board after the employing dry sanding paper polishing calcination treats that the Sign Board surface presents orderly striped, when color is brownish black, stops polishing.
(5) word content with sign is embedded on Sign Board, and adopts design colours coating to be filled in the font groove.
(6) on the doorframe Sign Board, smear varnish 2~3 times, be installed on the door after the drying.During installation, according to the fluting spacing of Sign Board, two antirust screws of rotation are embedded in Sign Board on the screw then on door.
Embodiment two
Present embodiment is a kind of job operation of archaized door frame mark brand, carries out according to the following steps:
(1), determines the apparent size size of doorframe Sign Board, and makes corresponding wolline embryo that timber can be selected pinus sylvestris var. mongolica, masson pine, China fir etc. for use with timber according to the design font size on the Sign Board.Usually, Sign Board adopts Chinese and English font, and adopting semicircle lead angle, the length of Sign Board around the Sign Board is 170 millimeters, and wide is 80 millimeters, and thick is 12 millimeters.
(2) because Sign Board need hang on the door, therefore the nested mode of screw is adopted in the installation of Sign Board, open two grooves at the reverse side of Sign Board, as shown in Figure 1, two grooves 1,2 dark 4 millimeters, groove 1,2 all is made up of water jacket 3 and inside groove 4, and connects by level trough 5, water jacket 3 diameters are 16 millimeters, and inside groove 4 diameters are 13 millimeters.The horizontal range L1 at water jacket 3 centre distance Sign Board edges be about Sign Board long 1/4, the vertical distance L 2 at inside groove 4 centre distance Sign Board edges be about Sign Board wide 1/3.
(3) with acetylene and oxygen high temperature sintering Sign Board, making the temperature of combustion of wolline embryo doorframe Sign Board is 180 ℃, and along Sign Board surface calcination, calcination time is 12 seconds, when treating Sign Board superficial charring blackout, stops calcination.
(4) Sign Board after the employing dry sanding paper polishing calcination treats that the Sign Board surface presents orderly striped, when color is brownish black, stops polishing.
(5) word content with sign is embedded on Sign Board, and adopts design colours coating to be filled in the font groove.
(6) on the doorframe Sign Board, smear varnish 2~3 times, be installed on the door after the drying.During installation, according to the fluting spacing of Sign Board, two antirust screws of rotation are embedded in Sign Board on the screw then on door.
Embodiment three
Present embodiment is a kind of job operation of archaized door frame mark brand, carries out according to the following steps:
(1), determines the apparent size size of doorframe Sign Board, and makes corresponding wolline embryo that timber can be selected pinus sylvestris var. mongolica, masson pine, China fir etc. for use with timber according to the design font size on the Sign Board.Usually, Sign Board adopts Chinese and English font, and adopting semicircle lead angle, the length of Sign Board around the Sign Board is 200 millimeters, and wide is 100 millimeters, and thick is 15 millimeters.
(2) because Sign Board need hang on the door, therefore the nested mode of screw is adopted in the installation of Sign Board, open two grooves at the reverse side of Sign Board, as shown in Figure 1, two grooves 1,2 dark 5 millimeters, groove 1,2 all is made up of water jacket 3 and inside groove 4, and connects by level trough 5, water jacket 3 diameters are 18 millimeters, and inside groove 4 diameters are 15 millimeters.The horizontal range L1 at water jacket 3 centre distance Sign Board edges be about Sign Board long 1/4, the vertical distance L 2 at inside groove 4 centre distance Sign Board edges be about Sign Board wide 1/3.
(3) with acetylene and oxygen high temperature sintering Sign Board, making the temperature of combustion of wolline embryo doorframe Sign Board is 200 ℃, and along Sign Board surface calcination, calcination time is 10 seconds, when treating Sign Board superficial charring blackout, stops calcination.
(4) Sign Board after the employing dry sanding paper polishing calcination treats that the Sign Board surface presents orderly striped, when color is brownish black, stops polishing.
(5) word content with sign is embedded on Sign Board, and adopts design colours coating to be filled in the font groove.
(6) on the doorframe Sign Board, smear varnish 2~3 times, be installed on the door after the drying.During installation, according to the fluting spacing of Sign Board, two antirust screws of rotation are embedded in Sign Board on the screw then on door.
The present invention can also have other embodiment, and the technical scheme that equal replacement of all employings or equivalent transformation form all drops within the scope of protection of present invention.
Claims (3)
1. the job operation of an archaized door frame mark brand is characterized in that: may further comprise the steps:
1. according to the design font size on the doorframe Sign Board, determine the apparent size size of doorframe Sign Board, and make corresponding wolline embryo doorframe Sign Board with timber;
2. step 1. the wolline embryo doorframe Sign Board reverse side of made offer mounting groove;
3. use acetylene and oxygen high temperature sintering wolline embryo doorframe Sign Board, the temperature of combustion that makes wolline embryo doorframe Sign Board is 150 ℃~200 ℃, and along the surface calcination of wolline embryo doorframe Sign Board, calcination time is 10 seconds~15 seconds, when treating wolline embryo doorframe Sign Board superficial charring blackout, stop calcination;
4. adopt dry sanding paper polishing calcination back door frame Sign Board, treat that doorframe Sign Board surface presents orderly striped, when color is brownish black, stop polishing;
5. the word content with sign is embedded on the doorframe Sign Board, and adopts design colours coating to be filled in the font groove;
6. on the doorframe Sign Board, smear varnish 2~3 times.
2. the job operation of a kind of archaized door frame mark brand as claimed in claim 1 is characterized in that: described step 1. in, timber can be selected pinus sylvestris var. mongolica, masson pine, China fir for use.
3. the job operation of a kind of archaized door frame mark brand as claimed in claim 1, it is characterized in that: described step 2. in, respectively open a groove at wolline embryo doorframe Sign Board reverse side two ends, groove is made up of inside groove and water jacket, inside groove is positioned at the upper end, water jacket is positioned at the lower end, and connect by level trough, described inside groove, 3 millimeters~5 millimeters of the groove depths of water jacket and level trough, the water jacket diameter is 10 millimeters~15 millimeters, the inside groove diameter is 12 millimeters~18 millimeters, the vertical distance at interior groove center and wolline embryo doorframe Sign Board edge be wolline embryo doorframe Sign Board wide 1/4~1/3, the horizontal range at outer groove center and wolline embryo doorframe Sign Board edge be wolline embryo doorframe Sign Board long 1/5~1/4.