- CN106441750B CN106441750B CN201610893668.2A CN201610893668A CN106441750B CN 106441750 B CN106441750 B CN 106441750B CN 201610893668 A CN201610893668 A CN 201610893668A CN 106441750 B CN106441750 B CN 106441750B
- Authority
- CN
- China
- Prior art keywords
- spring
- height
- rectangular section
- hours
- compressed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01M—TESTING STATIC OR DYNAMIC BALANCE OF MACHINES OR STRUCTURES; TESTING OF STRUCTURES OR APPARATUS, NOT OTHERWISE PROVIDED FOR
- G01M5/00—Investigating the elasticity of structures, e.g. deflection of bridges or air-craft wings
- G01M5/0041—Investigating the elasticity of structures, e.g. deflection of bridges or air-craft wings by determining deflection or stress
- G01M5/005—Investigating the elasticity of structures, e.g. deflection of bridges or air-craft wings by determining deflection or stress by means of external apparatus, e.g. test benches or portable test systems
Landscapes
- Engineering & Computer Science (AREA)
- Aviation & Aerospace Engineering (AREA)
- Physics & Mathematics (AREA)
- General Physics & Mathematics (AREA)
- Springs (AREA)
- Investigating Strength Of Materials By Application Of Mechanical Stress (AREA)
Abstract
一种高强度车制矩形截面弹簧间歇式强压试验工艺方法,将弹簧经过4次紧压试验,每次紧压试验时间由4小时递减为3小时,最后2小时,完成间歇式强压试验。本发明大大提高了高强度车制矩形截面弹簧的弹力P1值、P2值、刚度值的一次交验合格率。
Description
技术领域
本发明属于零件机械性能试验技术领域,特别涉及一种高强度车制矩形截面弹簧间歇式强压试验方法。
背景技术
弹簧必须通过预应力处理来提高弹簧的承载能力及稳定几何尺寸,预应力处理的工艺方法分为立定处理、强压(强拉、强扭)处理、加温强压(强拉、强扭) 处理。
预应力处理必须在热处理(包括消除应力回火)、吹砂处理或喷丸处理之后进行才能充分发挥强化效果,当弹簧承受的应力超过材料的弹性极限时,弹簧产生永久变形后才会对弹簧产生强化作用。
立定处理,对压缩弹簧,是把弹簧压缩到工作极限高度或并紧高度数次。
强压处理:对压缩弹簧是把弹簧压至材料层的应力超过屈服点,使表面产生负剩余应力,心部产生正剩余应力。其工艺方法有两种,一种是静强压,即把弹簧高度压缩至工作极限或并紧高度数小时,一般24至48小时,然后放来弹簧恢复自由高度;由于对高强度车制矩形截面弹簧公差要求高,对弹簧力P2 值影响因素多,当弹簧经会发生一定数量的弹簧静紧压过头,不能恢复到公差范围的自由高度H0,造成合格率降低;
另一种工艺方法是用较慢速度(约1分钟)把弹簧压至规定高度,然后缓慢放开约1分钟,使弹簧产生塑性变形,随后在该高度下进行立定处理。经常出现压过规定高度,使弹簧不能恢复到公差范围的自由高度,且操作工艺复杂,对操作者要求高。
发明内容
本发明的目的就是为了克服上述背景技术的不足,而提供一种高强度车制矩形截面弹簧间歇式强压试验方法。
本发明所涉及的高强度车制矩形截面弹簧间歇式强压试验方法,其步骤如下:
1)将热处理合格后的高强度车制矩形截面弹簧串入特制的心轴中,将弹簧放在专用压力机压头下;
2)启动压力机将弹簧高度压缩到工作极限高度H3处,保持4小时;
3)卸载,测量弹簧的自由高度H0;
4)若自由高度H0高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持3小时;
5)卸载,第二次测量弹簧的自由高度H0;
6)若自由高度H0仍高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持2小时;
7)卸载,第三次测量弹簧的自由高度H0,若自由高度H0仍高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持2小时,直至H0合格为止;
8)在专用检测设备上检测弹簧弹力P1值、P2值、刚度值。
本发明大大提高了高强度车制矩形截面弹簧的弹力P1值、P2值、刚度值的一次交验合格率。
附图说明:
图1是本发明专利的弹簧间歇式强压试验工艺曲线图,
图2是本发明专利的弹簧间歇式强压试验示意图,
其中:1弹簧紧压芯轴;2上垫圈;3矩形截面弹簧;4下垫圈;
图3是弹簧紧压后弹簧高度被压缩到H3的示意图;
图4为零件最终形状。
具体实施方式
下面结合附图和实例对本发明进一步说明。
实施例
我厂某一高强度车制矩形截面弹簧零件218号,零件名称:缓冲弹簧,材料:65Si2MnWA,原材料状态:棒料。零件经过十余道机加工序后成为为图4 的最终零件形状,经过热处理淬火回火后,进行弹簧间歇式强压试验,弹簧的技术要求为:如图4所示,
1.旋向:右旋。
2.有效圈数:n=15。
3.总圈数:n1=16.5。
4.热处理:48HRC-53HRC。
5.表面处理;磷化。
6.压缩到各圈接触时进行压紧试验。
7.制造与验收技术条件按WJ532-75Ⅱ组。
检测弹簧零件218号络氏硬度,在硬度合格后,将弹簧(3)串入特制的心轴(1)中,弹簧两端面垫入上垫圈(2)和下垫圈(4),将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,使弹簧各圈之间紧密接触并保持4 小时,卸载,按图1间歇式强压试验工艺曲线图进行,直至弹簧的自由高度合格为止,在专用的弹簧检测设备进行P1值、P2值测试;最后弹簧进行吹砂处理,表面磷化处理。
Claims (1)
1.一种高强度车制矩形截面弹簧间歇式强压试验方法,其特征是该方法步骤如下:
1)将热处理合格后的高强度车制矩形截面弹簧串入特制的心轴中,将弹簧放在专用压力机压头下;
2)启动压力机将弹簧高度压缩到工作极限高度H3处,保持4小时;
3)卸载,测量弹簧的自由高度H0;
4)若自由高度H0高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持3小时;
5)卸载,第二次测量弹簧的自由高度H0;
6)若自由高度H0仍高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持2小时;
7)卸载,第三次测量弹簧的自由高度H0,若自由高度H0仍高于弹簧的技术要求,则再次将弹簧放在专用压力机压头下,启动压力机将弹簧高度压缩到工作极限高度H3处,保持2小时,直至H0合格为止;
8)在专用检测设备上检测弹簧弹力P1值、P2值、刚度值。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610893668.2A CN106441750B (zh) | 2016-10-13 | 2016-10-13 | 高强度车制矩形截面弹簧间歇式强压试验方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610893668.2A CN106441750B (zh) | 2016-10-13 | 2016-10-13 | 高强度车制矩形截面弹簧间歇式强压试验方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
CN106441750A CN106441750A (zh) | 2017-02-22 |
CN106441750B true CN106441750B (zh) | 2019-02-05 |
Family
ID=58173975
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201610893668.2A Expired - Fee Related CN106441750B (zh) | 2016-10-13 | 2016-10-13 | 高强度车制矩形截面弹簧间歇式强压试验方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN106441750B (zh) |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN1712548A (zh) * | 2005-04-28 | 2005-12-28 | 长安汽车(集团)有限责任公司 | 车制缓冲簧短压强化处理方法 |
CN103343203A (zh) * | 2013-06-14 | 2013-10-09 | 上海核工碟形弹簧制造有限公司 | 一种碟形弹簧的强压方式及其装置 |
CN103717775A (zh) * | 2011-08-11 | 2014-04-09 | 日本发条株式会社 | 压缩螺旋弹簧及其制造方法 |
CN105834333A (zh) * | 2016-05-06 | 2016-08-10 | 江西昌河航空工业有限公司 | 一种弹簧强压用快速定位夹具 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2004144132A (ja) * | 2002-10-22 | 2004-05-20 | Nhk Spring Co Ltd | 皿ばね及び皿ばねの製造方法 |
KR20110024977A (ko) * | 2009-09-03 | 2011-03-09 | 한국과학기술연구원 | 형상기억합금 코일스프링 제조방법 |
-
2016
- 2016-10-13 CN CN201610893668.2A patent/CN106441750B/zh not_active Expired - Fee Related
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN1712548A (zh) * | 2005-04-28 | 2005-12-28 | 长安汽车(集团)有限责任公司 | 车制缓冲簧短压强化处理方法 |
CN103717775A (zh) * | 2011-08-11 | 2014-04-09 | 日本发条株式会社 | 压缩螺旋弹簧及其制造方法 |
CN103343203A (zh) * | 2013-06-14 | 2013-10-09 | 上海核工碟形弹簧制造有限公司 | 一种碟形弹簧的强压方式及其装置 |
CN105834333A (zh) * | 2016-05-06 | 2016-08-10 | 江西昌河航空工业有限公司 | 一种弹簧强压用快速定位夹具 |
Non-Patent Citations (2)
Title |
---|
弹簧强压处理简易装置设计;吴应东;《产品开发与设计》;20150331;第42卷(第3期);第56-60页 |
强压弹簧研究;何献忠等;《北京工业学院学报》;19830228(第2期);第90-105页 |
Also Published As
Publication number | Publication date |
---|---|
CN106441750A (zh) | 2017-02-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2016198791A (ja) | プレス加工方法、プレス加工装置、プレス成形体、プレス加工品 | |
CN106441750B (zh) | 高强度车制矩形截面弹簧间歇式强压试验方法 | |
CN102489943A (zh) | 制造波形弹簧的方法 | |
JP2012212569A (ja) | 電池ケースの蓋体製造方法 | |
CN102380755A (zh) | 一种柴油机泵喷嘴柱塞弹簧的加工工艺 | |
JP4246804B2 (ja) | 加熱・加圧処理装置 | |
CN105364429B (zh) | 一种厚壁双相不锈钢封头的制造方法 | |
CN109648265A (zh) | 一种高效加工生产精密机械的方法 | |
CN101920287A (zh) | 精冲模具及其实现精冲的方法 | |
CN105619032B (zh) | 一种碟形弹簧加工方法 | |
JP2005140285A (ja) | 金属ベローズおよびその製造方法並びにアキュムレータ | |
US2666723A (en) | Method of manufacturing helical coil compression springs | |
GB201213097D0 (en) | Method of manufacturing a coining die | |
EP3798329A1 (en) | Method and apparatus for remedying a non-conforming feature of an aluminum alloy part | |
CN104203447A (zh) | 渐进成形方法 | |
CN204657916U (zh) | 锁芯阿门装配组装机 | |
CN111496121A (zh) | 简单压力容器深拉成型封头材料选择方法及封头成型工艺 | |
JP2009050859A (ja) | 2つの部品、例えばインナー部品とアウター部品の製造方法 | |
CN106595995A (zh) | 高强度车制矩形截面弹簧间歇式强压试验方法 | |
CN202392105U (zh) | 一种自紧型锥形环密封结构 | |
CN209364436U (zh) | 一种主从式圆周异形壳体防护材料装配工装 | |
CN110988135A (zh) | 一种无约束振动处理下疲劳损伤修复振动参数的确定方法 | |
KR101425465B1 (ko) | 타이어 가류금형의 밴트장치 제조방법 | |
RU2506136C1 (ru) | Способ штамповки эластичной средой | |
JP2009106961A (ja) | プレス成形方法及びプレス成形型 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
GR01 | Patent grant | ||
GR01 | Patent grant | ||
CF01 | Termination of patent right due to non-payment of annual fee |
Granted publication date: 20190205 Termination date: 20191013 |
|
CF01 | Termination of patent right due to non-payment of annual fee |