CN106433459A - Environment-friendly waterproof tung oil and preparation method thereof - Google Patents
Environment-friendly waterproof tung oil and preparation method thereof Download PDFInfo
- Publication number
- CN106433459A CN106433459A CN201610587314.5A CN201610587314A CN106433459A CN 106433459 A CN106433459 A CN 106433459A CN 201610587314 A CN201610587314 A CN 201610587314A CN 106433459 A CN106433459 A CN 106433459A
- Authority
- CN
- China
- Prior art keywords
- tung oil
- environment
- ginseng
- powder
- friendly waterproof
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an environment-friendly waterproof tung oil and a preparation method thereof. The environment-friendly waterproof tung oil is prepared by mixing of the following components by mass percentage: 92%-96% of tung oil, 2%-4% of tuoshen, and 2%-4% of tuzi. The preparation method of the environment-friendly waterproof tung oil includes the steps of: a. selecting high-quality tung oil, tuoshen and tuzi, and washing tuoshen and tuzi for standby use; b. processing the washed tuoshen and tuzi into powder respectively for standby use; c. putting bancoul nuts into a steamer, introducing steam, and controlling the pressure at 0.14-0.25MPa; d. adding tuoshen powder into the steamer, controlling the temperature at 85-95DEG C, and observing the concentration; and e. performing cooling, and adding tuzi powder so as to be usable. Compared with existing tung oil, the environment-friendly waterproof tung oil provided by the invention has no lead or mercury, is harmless to the human body, is more reliable than other tung oil in waterproof aspect, and greatly increases the service life.
Description
Technical field
The present invention relates to timber floor manufacture field, more particularly, to a kind of environment-friendly waterproof tung oil and preparation method thereof.
Background technology
Natural timber is a kind of traditional furniture material, and making for furniture has very long history.But it is natural
Timber has inborn deficiency on antiseptic property.Wood furniture is susceptible to rot, significantly after making moist
Shorten the service life of wood furniture.In order to improve the antiseptic property of wood furniture, can be in wood furniture surface smear oil
Paint.But paint can add numerous artificial synthesized compounds in manufacture and use, and these compounds more or less can be to human body
Produce harm.
Tung oil is the local product resource of China's sustainable development, is yield highest in traditional oil tree, has high exploitation
The natural oilseed plant of environmental, the economical dual-use function being worth, is to squeeze to obtain from tung tree fruit.Tung oil can be made
For a kind of anticorrosive paint of natural timber, after being applied to wood furniture surface, can effectively prevent wood material from making moist.Paulownia simultaneously
Oil is applied to wood furniture surface, after complete xeroma, has stronger light resistance, ageing resistance, service life is longer.It
It is to manufacture paint, the primary raw material of ink, be used as in a large number the building, waterproof of machinery, weapons, car and boat, fishing gear, electrical equipment, anti-corrosion, anti-
Rust coating, and oilcloth, oilpaper, soap, agricultural chemicals and pharmaceutical nauseant, agrochemical can be made.Rapid with China's economy
Development, increasing to the demand of the energy, energy supply and demand contradiction increasingly manifests, using tung oil tree be main biomass energy as
Alternative energy source will be the inevitable choice of China, in addition the development of China's industrial or agricultural, fishery, and the raising of living standards of the people is domestic
Tung oil demand will greatly increase.
Content of the invention
The invention provides a kind of environment-friendly waterproof tung oil and preparation method thereof, the unleaded mercury of environment-friendly waterproof tung oil of the present invention, ring
Protect, to human body fanout free region, more relatively reliable than other tung oil waterproof aspects, and considerably increase service life.
The purpose of the present invention is achieved through the following technical solutions:
A kind of environment-friendly waterproof tung oil, is mixed by mass percentage by following components:
Tung oil 92%~96%, the ginseng that sticks together 2%~4%, native seed 2%~4%.
The described ginseng that sticks together is powder with native seed.
A kind of preparation method of environment-friendly waterproof tung oil, comprises the following steps:
A, the tung oil from high-quality, the ginseng that sticks together and native seed, and will stick together ginseng and native seed is cleaned, standby;
B, by clean stick together ginseng and native seed is respectively processed into powder, standby;
C, bancoul nuts are put in steamer, in steamer, be passed through steam, pressure is 0.14-0.25MPa;
D, add in steamer and stick together ginseng powder, control temperature at 85~95 DEG C, observe concentration;
Add native seed powder can use after e, cooling.
Compared with prior art, the present invention at least has advantages below:
By the technical scheme of the invention described above, compared with existing tung oil, tung oil of the present invention adds during steaming
The ginseng that sticks together and the native big raw material of seed two, by the mixed proportion of precise control tung oil, the ginseng that sticks together and native seed, control the pressure during steaming
And temperature, so that the ginseng that sticks together of powder is merged completely with tung oil with native seed, formed and there is certain density tung oil product, using this
The waterproof tung oil that bright method is obtained does not contain chemical toxic substances, and natural environmental-protective, to human body fanout free region, than other tung oil waterproof aspects
Relatively reliable, and considerably increase service life.
Specific embodiment
Technical scheme in the present invention will be clearly and completely described below it is clear that described embodiment only
It is a part of embodiment of the present invention, rather than whole embodiments.Based on the embodiment in the present invention, ordinary skill
The every other embodiment that personnel are obtained under the premise of not making creative work, broadly falls into the scope of protection of the invention.
Embodiment one
The embodiment of the present invention one provides a kind of environment-friendly waterproof tung oil, is mixed by mass percentage by following components:Paulownia
Oil 93%, stick together ginseng~4%, native seed 3%.
Preferably, the ginseng that sticks together and native seed are powder.
Further, the present invention also provides a kind of preparation method of environment-friendly waterproof tung oil, comprises the following steps:
A, the tung oil from high-quality, the ginseng that sticks together and native seed, and will stick together ginseng and native seed is cleaned, standby;
B, by clean stick together ginseng and native seed is respectively processed into powder, standby;
C, bancoul nuts are put in steamer, in steamer, be passed through steam, O.16MPa pressure be;
D, add in steamer and stick together ginseng powder, control temperature at 93 DEG C, observe concentration;
Add native seed powder can use after e, cooling.
Embodiment two
The embodiment of the present invention two provides the another embodiment of the present invention one to provide a kind of environment-friendly waterproof tung oil, presses matter by following components
Amount percentage mixes:Tung oil 95%, stick together ginseng~3%, native seed 2%.
Preferably, the ginseng that sticks together and native seed are powder.
Further, the present invention also provides a kind of preparation method of environment-friendly waterproof tung oil, comprises the following steps:
A, the tung oil from high-quality, the ginseng that sticks together and native seed, and will stick together ginseng and native seed is cleaned, standby;
B, by clean stick together ginseng and native seed is respectively processed into powder, standby;
C, bancoul nuts are put in steamer, in steamer, be passed through steam, pressure is 0.22MPa;
D, add in steamer and stick together ginseng powder, control temperature at 87 DEG C, observe concentration;
Add native seed powder can use after e, cooling.
Compared with prior art, the present invention at least has advantages below:
By the technical scheme of the invention described above, compared with existing tung oil, tung oil of the present invention adds during steaming
The ginseng that sticks together and the native big raw material of seed two, by the mixed proportion of precise control tung oil, the ginseng that sticks together and native seed, control the pressure during steaming
And temperature, so that the ginseng that sticks together of powder is merged completely with tung oil with native seed, formed and there is certain density tung oil product, using this
The waterproof tung oil that bright method is obtained does not contain chemical toxic substances, and natural environmental-protective, to human body fanout free region, than other tung oil waterproof aspects
Relatively reliable, and considerably increase service life.
More than, the only present invention preferably specific embodiment, but protection scope of the present invention is not limited thereto, and any
Those familiar with the art the invention discloses technical scope in, the change or replacement that can readily occur in, all answer
It is included within the scope of the present invention.Therefore, protection scope of the present invention with the protection domain of claims should be
Accurate.
Claims (3)
1. a kind of environment-friendly waterproof tung oil is it is characterised in that be to be mixed by mass percentage by following components:
Tung oil 92%~96%, the ginseng that sticks together 2%~4%, native seed 2%~4%.
2. environment-friendly waterproof tung oil as claimed in claim 1 it is characterised in that:The described ginseng that sticks together is powder with native seed.
3. a kind of preparation method of the environment-friendly waterproof tung oil as described in claim 1-2 is it is characterised in that comprise the following steps:
A, the tung oil from high-quality, the ginseng that sticks together and native seed, and will stick together ginseng and native seed is cleaned, standby;
B, by clean stick together ginseng and native seed is respectively processed into powder, standby;
C, bancoul nuts are put in steamer, in steamer, be passed through steam, pressure is 0.14-0.25MPa;
D, add in steamer and stick together ginseng powder, control temperature at 85~95 DEG C, observe concentration;
Add native seed powder can use after e, cooling.