CN106244018A - Water quick-drying industrial paint - Google Patents

Water quick-drying industrial paint Download PDF

Info

Publication number
CN106244018A
CN106244018A CN201610841038.0A CN201610841038A CN106244018A CN 106244018 A CN106244018 A CN 106244018A CN 201610841038 A CN201610841038 A CN 201610841038A CN 106244018 A CN106244018 A CN 106244018A
Authority
CN
China
Prior art keywords
agent
water
base resin
deionized water
industrial paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610841038.0A
Other languages
Chinese (zh)
Inventor
张文斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FOSHAN MERLIN COATING Co Ltd
Original Assignee
FOSHAN MERLIN COATING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by FOSHAN MERLIN COATING Co Ltd filed Critical FOSHAN MERLIN COATING Co Ltd
Priority to CN201610841038.0A priority Critical patent/CN106244018A/en
Publication of CN106244018A publication Critical patent/CN106244018A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of water quick-drying industrial paint, it is characterized in that, its composition of raw materials includes water-base resin 50 60%, dimethylethanolamine 0.1 0.5%, propylene glycol 0.5 1.5%, deionized water 13 18%, dispersion moisture agent 0.1 0.8%, defoamer 0.05 0.15%, anti-sudden strain of a muscle rust agent 0.1 0.5%, titanium dioxide 13 18%, potassium phosphate 3 8%, blanc fixe 8 14%, anti-settling agent 0.1 0.8%, substrate wetting agents 0.1 0.5%, alkali swelling thickening agent 0.2 0.8%, polyurethane thickener 0.1 0.8% by weight percentage.The present invention is prepared conveniently, and low cost, compared to the product of same type, more environmentally-friendly, performance is more superior.

Description

Water quick-drying industrial paint
Technical field
The present invention relates to industrial coating technical field, especially relate to a kind of rapid-curing cutback industrial paint.
Background technology
The article surfaces such as paint is a kind of common industrial coating goods, is applied to various metal, timber.The biggest on the market Most common paint are all to need the most some hours, the most even up to the solidification of a few days, air-dried cycle.When special at some Under the conditions of need fast rapid-curing cutback solidifying occasion just cannot meet demand.
Summary of the invention
The one that the purpose of the present invention is contemplated to solve the deficiency of prior art and provides is prepared simply, environmental protection, The water quick-drying industrial paint that rate of drying is fast.
The present invention is to use following technical solution to be attained in that a kind of water quick-drying industrial paint, its feature Being, its composition of raw materials includes water-base resin 50-60%, dimethylethanolamine 0.1-0.5%, propylene glycol by weight percentage 0.5-1.5%, deionized water 13-18%, dispersion moisture agent 0.1-0.8%, defoamer 0.05-0.15%, anti-sudden strain of a muscle rust agent 0.1- 0.5%, titanium dioxide 13-18%, potassium phosphate 3-8%, blanc fixe 8-14%, anti-settling agent 0.1-0.8%, substrate wetting agents 0.1-0.5%, alkali swelling thickening agent 0.2-0.8%, polyurethane thickener 0.1-0.8%.
Further illustrating as such scheme, its composition of raw materials include by weight percentage water-base resin 50-58%, Dimethylethanolamine 0.1-0.4%, propylene glycol 0.5-1.3%, deionized water 12-17%, dispersion moisture agent 0.1-0.7%, disappear Infusion 0.05-0.15%, anti-sudden strain of a muscle rust agent 0.1-0.4%, titanium dioxide 13-17%, potassium phosphate 3-7%, blanc fixe 8-13%, Anti-settling agent 0.2-0.7%, substrate wetting agents 0.1-0.5%, alkali swelling thickening agent 0.2-0.6%, polyurethane thickener 0.1- 0.6%.
Preferably, its composition of raw materials includes water-base resin 52%, dimethylethanolamine 0.2%, third by weight percentage Glycol 1%, deionized water 14.7%, dispersion moisture agent 0.5%, defoamer 0.1%, anti-dodge rust agent 0.2%, titanium dioxide 15%, Potassium phosphate 5%, blanc fixe 10%, anti-settling agent 0.5%, substrate wetting agents 0.2%, alkali swelling thickening agent 0.4%, polyurethane Thickening agent 0.2%.
Further, described water-base resin and deionized water add at twice, add first water-base resin 25% and go from Sub-water 13%, second time adds water-base resin 27% and deionized water 1.7%.
The present invention uses above-mentioned technical solution can reach to provide the benefit that:
The present invention uses water-base resin, dimethylethanolamine, propylene glycol, deionized water, dispersion moisture agent, titanium dioxide, phosphorus Acid the preparation of raw material such as potassium, blanc fixe water quick-drying paint, solidify, air-dry the cycle short, rapid draing, environmental protection.
Detailed description of the invention
The present invention is a kind of water quick-drying industrial paint, and its composition of raw materials includes water-base resin 50-by weight percentage 60%, dimethylethanolamine 0.1-0.5%, propylene glycol 0.5-1.5%, deionized water 13-18%, dispersion moisture agent 0.1- 0.8%, defoamer 0.05-0.15%, anti-sudden strain of a muscle rust agent 0.1-0.5%, titanium dioxide 13-18%, potassium phosphate 3-8%, sulfate precipitate Barium 8-14%, anti-settling agent 0.1-0.8%, substrate wetting agents 0.1-0.5%, alkali swelling thickening agent 0.2-0.8%, polyurethane thickening Agent 0.1-0.8%.
Below in conjunction with specific embodiment, the technical program is explained in detail.
Embodiment 1
In the present embodiment, its composition of raw materials includes water-base resin 52%, dimethylethanolamine by weight percentage 0.2%, propylene glycol 1%, deionized water 14.7%, dispersion moisture agent 0.5%, defoamer 0.1%, anti-sudden strain of a muscle rust agent 0.2%, titanium white Powder 15%, potassium phosphate 5%, blanc fixe 10%, anti-settling agent 0.5%, substrate wetting agents 0.2%, alkali swelling thickening agent 0.4%, polyurethane thickener 0.2%.Water-base resin and deionized water add at twice, add water-base resin 25% first and go Ionized water 13%, second time adds water-base resin 27% and deionized water 1.7%.
Embodiment 2
In the present embodiment, its composition of raw materials includes water-base resin 54%, dimethylethanolamine by weight percentage 0.1%, propylene glycol 1.1%, deionized water 13%, dispersion moisture agent 0.3%, defoamer 0.1%, anti-sudden strain of a muscle rust agent 0.3%, titanium white Powder 14.7%, potassium phosphate 4%, blanc fixe 11%, anti-settling agent 0.5%, substrate wetting agents 0.3%, alkali swelling thickening agent 0.3%, polyurethane thickener 0.3%.
Compared with prior art, employing includes water-base resin, dimethylethanolamine, propylene glycol, deionized water, divides the present invention Dissipate wetting agent, defoamer, anti-sudden strain of a muscle rust agent, titanium dioxide, potassium phosphate, blanc fixe, anti-settling agent, substrate wetting agents, the increasing of alkali swelling Thick dose, the water quick-drying paint of the preparation of raw material of polyurethane thickener, and its formula is carried out strict design so that it is solidifying Gu, air-dry the cycle short, rapid draing, environmental protection.
Above-described is only the preferred embodiment of the present invention, it is noted that for those of ordinary skill in the art For, without departing from the concept of the premise of the invention, it is also possible to make some deformation and improvement, these broadly fall into the present invention Protection domain.

Claims (4)

1. a water quick-drying industrial paint, it is characterised in that its composition of raw materials includes water-base resin 50-by weight percentage 60%, dimethylethanolamine 0.1-0.5%, propylene glycol 0.5-1.5%, deionized water 13-18%, dispersion moisture agent 0.1- 0.8%, defoamer 0.05-0.15%, anti-sudden strain of a muscle rust agent 0.1-0.5%, titanium dioxide 13-18%, potassium phosphate 3-8%, sulfate precipitate Barium 8-14%, anti-settling agent 0.1-0.8%, substrate wetting agents 0.1-0.5%, alkali swelling thickening agent 0.2-0.8%, polyurethane thickening Agent 0.1-0.8%.
Water quick-drying industrial paint the most according to claim 1, it is characterised in that its composition of raw materials wraps by weight percentage Include water-base resin 50-58%, dimethylethanolamine 0.1-0.4%, propylene glycol 0.5-1.3%, deionized water 12-17%, dispersion Wetting agent 0.1-0.7%, defoamer 0.05-0.15%, anti-sudden strain of a muscle rust agent 0.1-0.4%, titanium dioxide 13-17%, potassium phosphate 3- 7%, blanc fixe 8-13%, anti-settling agent 0.2-0.7%, substrate wetting agents 0.1-0.5%, alkali swelling thickening agent 0.2- 0.6%, polyurethane thickener 0.1-0.6%.
Water quick-drying industrial paint the most according to claim 1, it is characterised in that its composition of raw materials wraps by weight percentage Include water-base resin 52%, dimethylethanolamine 0.2%, propylene glycol 1%, deionized water 14.7%, dispersion moisture agent 0.5%, disappear Infusion 0.1%, anti-sudden strain of a muscle rust agent 0.2%, titanium dioxide 15%, potassium phosphate 5%, blanc fixe 10%, anti-settling agent 0.5%, base material Wetting agent 0.2%, alkali swelling thickening agent 0.4%, polyurethane thickener 0.2%.
Water quick-drying industrial paint the most according to claim 1, it is characterised in that described water-base resin and deionization moisture two Secondary interpolation, adds water-base resin 25% and deionized water 13% first, and second time adds water-base resin 27% and deionized water 1.7%.
CN201610841038.0A 2016-09-22 2016-09-22 Water quick-drying industrial paint Pending CN106244018A (en)