CN105885808A - 一种钻井液用无铬磺化褐煤 - Google Patents
一种钻井液用无铬磺化褐煤 Download PDFInfo
- Publication number
- CN105885808A CN105885808A CN201610323314.4A CN201610323314A CN105885808A CN 105885808 A CN105885808 A CN 105885808A CN 201610323314 A CN201610323314 A CN 201610323314A CN 105885808 A CN105885808 A CN 105885808A
- Authority
- CN
- China
- Prior art keywords
- chromium
- drilling fluid
- sulfonated lignite
- sodium humate
- prepared
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供了一种钻井液用无铬磺化褐煤,由以下步骤制得:(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;(2)磺甲基化剂与腐植酸钠进行反应;(3)将钛溶液,喷淋到反应混合物中,最后烘干制得。本发明用钛离子取代了铬离子,产品中不含铬,避免了在钻井的过程中对水造成的铬污染。
Description
技术领域
本发明涉及一种石油天然气钻探领域,具体属于一种钻井液添加剂。
背景技术
磺化褐煤(又叫磺甲基褐煤)SMC,是钻井液添加剂(或叫泥浆处理剂),用于降滤失作用的一种性能很好的处理剂。该处理剂自发明以来得到了广泛的使用,并深受好评。该处理剂的生产过程是:(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;(2)磺甲基化剂与腐植酸钠进行反应;(3)在上述反应溶液中加入红矾反应,烘干制得。但是这种方法制得的磺化褐煤就有一个致命的缺陷,那就是这种磺化褐煤中含有铬,对水资源。人体大量吸入铬会中毒,且随着环保法的规范和更加严格,含铬的磺化褐煤在石油天然气钻探领域根本不敢再用。
发明内容
本发明目的在于提供一种不含铬的磺化褐煤。
一种钻井液用无铬磺化褐煤,其特征在于由以下步骤制得:
(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;
(2)磺甲基化剂与腐植酸钠按质量比1:10进行反应,混合物浓度控制在20%~30%,在常压下温度为80℃~90℃反应2h以上;
(3)将质量百分比浓度20%硫酸钛溶液,按照质量比腐植酸钠:硫酸钛为100:3喷淋到反应混合物中,反应温度控制在90℃~100℃,压力为常压,反应1h,最后烘干制得。
上述腐植酸钠由碱提取法制得。
这种不含铬的磺化褐煤经过检测,所有指标都能达标。
有益效果:本发明用钛离子取代了铬离子,产品中不含铬,避免了在钻井的过程中对水造成的铬污染。
具体实施方式
实施例1
一种钻井液用无铬磺化褐煤,由以下步骤制得:
(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;
(2)磺甲基化剂与腐植酸钠按质量比1:10进行反应,混合物浓度控制在20%,在常压下温度为80℃反应2h以上,所述腐植酸钠由碱提取法制得;
(3)将质量百分比浓度20%硫酸钛溶液,按照质量比腐植酸钠:硫酸钛为100:3喷淋到反应混合物中,反应温度控制在90℃,压力为常压,反应1h,最后烘干制得。
实施例2
一种钻井液用无铬磺化褐煤,由以下步骤制得:
(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;
(2)磺甲基化剂与腐植酸钠按质量比1:10进行反应,混合物浓度控制在30%,在常压下温度为90℃反应2h以上,所述腐植酸钠由碱提取法制得;
(3)将质量百分比浓度20%硫酸钛溶液,按照质量比腐植酸钠:硫酸钛为100:3喷淋到反应混合物中,反应温度控制在100℃,压力为常压,反应1h,最后烘干制得。
实施例3
一种钻井液用无铬磺化褐煤,由以下步骤制得:
(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;
(2)磺甲基化剂与腐植酸钠按质量比1:10进行反应,混合物浓度控制在25%,在常压下温度为85℃反应2h以上,所述腐植酸钠由碱提取法制得;
(3)将质量百分比浓度20%硫酸钛溶液,按照质量比腐植酸钠:硫酸钛为100:3喷淋到反应混合物中,反应温度控制在95℃,压力为常压,反应1h,最后烘干制得。
Claims (2)
1.一种钻井液用无铬磺化褐煤,其特征在于由以下步骤制得:
(1)用甲醛与焦亚硫酸钠反应制取磺甲基化剂;
(2)磺甲基化剂与腐植酸钠按质量比1:10进行反应,混合物浓度控制在20%~30%,在常压下温度为80℃~90℃反应2h以上;
(3)将质量百分比浓度20%硫酸钛溶液,按照质量比腐植酸钠:硫酸钛为100:3喷淋到反应混合物中,反应温度控制在90℃~100℃,压力为常压,反应1h,最后烘干制得。
2.根据权利要求1所述一种钻井液用无铬磺化褐煤,其特征在于:所述腐植酸钠由碱提取法制得。