CN105693146A - Environmentally friendly building material - Google Patents
Environmentally friendly building material Download PDFInfo
- Publication number
- CN105693146A CN105693146A CN201410683806.5A CN201410683806A CN105693146A CN 105693146 A CN105693146 A CN 105693146A CN 201410683806 A CN201410683806 A CN 201410683806A CN 105693146 A CN105693146 A CN 105693146A
- Authority
- CN
- China
- Prior art keywords
- building material
- environmentally friendly
- parts
- friendly building
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an environmentally friendly building material. The environmentally friendly building material is prepared through mixing 60-80 parts of crushed straws, 10-15 parts of cement, 8-12 parts of fly ash, 2-5 parts of a water reducer, 2-4 parts of an adhesive and a proper amount of water. A preparation method of the environmentally friendly building material comprises the following steps: crushing above proportion of the straws to the granularity of 10-20mm, adding all components to the proper amount of water, uniformly mixing the components, adding the obtained mixture to a stirrer, stirring the mixture, adding the stirred mixture to a die, carrying out molding pressurization, and maintaining the pressurized mixture for 24h. Compared with building materials in the prior art, the environmentally friendly building material has the advantages of small product investment scale, short preparation cycle, abundant resources, strong pressure resistance and stable quality, and reaches use requirements of building materials. The environmentally friendly building material can be widely applied to building material preparation technologies.
Description
Technical field:
The present invention relates to building material technical field, especially a kind of environmental-friendly construction material。
Background technology:
At present, along with China's chemurgy progress faster, a large amount of straws of annual generation, burn and pile up, taking up room, serious environment pollution。Polluting for eliminating, a lot of areas adopt straws to manufacture construction materials to be improved, but all because fail to reach building requirements and cannot large-scale production。
Summary of the invention:
It is an object of the invention to provide a kind of straw and produce environmental-friendly construction material, its production cost is relatively low, meets the environmental-friendly construction material of building instructions for use。
The present invention adopts the following technical scheme that: a kind of environmental-friendly construction material, by the raw material of following weight proportioning and prepared by method: mixed in right amount formed by crushing straw 60-80 part, cement 10-15 part, flyash 8-12, water reducer 2-5 part, adhesive 2-4 part, water;Its preparation method is to be 10-20mm by the crushed stalk in said ratio to granularity, each component adds appropriate water and mixes and stir into blender, enter modeling pressurization, maintenance 24 hours。
The present invention has product-specific investments small scale compared to existing technology, and the manufacturing cycle is short, aboundresources, and product compressive resistance is strong, and steady quality reaches the technical characterstic of the instructions for use of construction material。Can be widely applied to construction material manufacturing technology。
Detailed description of the invention:
Below in conjunction with embodiment, the present invention will be further described:
A kind of environmental-friendly construction material, takes crushing straw 60-80 part, cement 10-15 part, flyash 8-12, water reducer 2-5 part, adhesive 2-4 part, water mix composition in right amount;Its preparation method is to be 10-20mm by the crushed stalk in said ratio to granularity, each component adds appropriate water and mixes and stir into blender, enter modeling pressurization, maintenance 24 hours。
Claims (1)
1. an environmental-friendly construction material, by the raw material of following weight proportioning and prepared by method: crushing straw 60-80 part, cement 10-15 part, flyash 8-12, water reducer 2-5 part, adhesive 2-4 part, water mix in right amount and forms;Its preparation method is to be 10-20mm by the crushed stalk in said ratio to granularity, each component adds appropriate water and mixes and stir into blender, enter modeling pressurization, maintenance 24 hours。