CN105503111A - Method for preparing waterproof material - Google Patents
Method for preparing waterproof material Download PDFInfo
- Publication number
- CN105503111A CN105503111A CN201510948929.1A CN201510948929A CN105503111A CN 105503111 A CN105503111 A CN 105503111A CN 201510948929 A CN201510948929 A CN 201510948929A CN 105503111 A CN105503111 A CN 105503111A
- Authority
- CN
- China
- Prior art keywords
- weight part
- component
- parts
- mixed
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for preparing a waterproof material. The method comprises the following steps: 1, uniformly mixing, by weight, 1-2 parts of ethanediol, 1.8 parts of diethyl toluenediamine, 3.1 parts of alcohol ethoxide carboxylate, 7.6 parts of silicone acrylic emulsion and 13 parts of water, so that a component A is obtained; 2, uniformly mixing, by weight, 1.4 parts of dihydrate gypsum, 0.8 part of aluminum hydroxide, 1.7 parts of calcium chloride, 1.2 parts of polyethylene glycol and 8.8 parts of quartz sand, so that a component B is obtained; 3, mixing, by weight, 3.8 parts of the component A with 5.9 parts of the component B, heating the mixture to 56 DEG C, then stirring the mixture uniformly, and conducting natural cooling, so that the waterproof material is obtained. The waterproof material prepared through the method for preparing the waterproof material has good flexibility, waterproofness and crack resistance and is suitable for producing kitchen and toilet products.
Description
Technical field
The present invention relates to the method for the preparation of water-proof material.
Background technology
Existing kitchen products, its snappiness, water-repellancy, crack resistence performance have much room for improvement.
Summary of the invention
The object of the present invention is to provide a kind of method for the preparation of water-proof material, the water-proof material of preparation has good snappiness, water-repellancy, crack resistence, is applicable to preparing kitchen products.
For achieving the above object, technical scheme of the present invention is a kind of method for the preparation of water-proof material of design, comprises the steps:
1) 1 ~ 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
Preferably, for the preparation of the method for water-proof material, comprise the steps:
1) 1 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
Preferably, for the preparation of the method for water-proof material, comprise the steps:
1) 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
Advantage of the present invention and beneficial effect are: provide a kind of method for the preparation of water-proof material, and the water-proof material of preparation has good snappiness, water-repellancy, crack resistence, is applicable to preparing kitchen products.
Embodiment
Below in conjunction with embodiment, the specific embodiment of the present invention is further described.Following examples only for technical scheme of the present invention is clearly described, and can not limit the scope of the invention with this.
The technical scheme that the present invention specifically implements is:
Embodiment 1
For the preparation of a method for water-proof material, comprise the steps:
1) 1 ~ 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
Embodiment 2
For the preparation of the method for water-proof material, comprise the steps:
1) 1 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
Embodiment 3
For the preparation of the method for water-proof material, comprise the steps:
1) 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
The above is only the preferred embodiment of the present invention; it should be pointed out that for those skilled in the art, under the prerequisite not departing from the technology of the present invention principle; can also make some improvements and modifications, these improvements and modifications also should be considered as protection scope of the present invention.
Claims (3)
1. for the preparation of the method for water-proof material, it is characterized in that, comprise the steps:
1) 1 ~ 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
2. the method for the preparation of water-proof material according to claim 1, is characterized in that, comprise the steps:
1) 1 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.
3. the method for the preparation of water-proof material according to claim 1, is characterized in that, comprise the steps:
1) 2 weight part ethylene glycol, 1.8 weight part diethyl toluene diamines, 3.1 weight part alcohol b-oxide carboxylate salts, 7.6 weight part organosilicon crylic acid latexs, 13 weight parts waters are mixed, obtained component A;
2) 1.4 weight part dihydrate gypsums, 0.8 weight part aluminium hydroxide, 1.7 weight part calcium chloride, 1.2 weight part polyoxyethylene glycol, 8.8 weight part quartz sands are mixed, obtained B component;
3) 3.8 weight part component A are mixed with 5.9 weight part B component, be heated to 56 DEG C, then stir, naturally cooling, obtained water-proof material.