CN105330897A - Sodium acrylate calcium carbonate activating agent - Google Patents

Sodium acrylate calcium carbonate activating agent Download PDF

Info

Publication number
CN105330897A
CN105330897A CN201510755979.8A CN201510755979A CN105330897A CN 105330897 A CN105330897 A CN 105330897A CN 201510755979 A CN201510755979 A CN 201510755979A CN 105330897 A CN105330897 A CN 105330897A
Authority
CN
China
Prior art keywords
parts
calcium carbonate
sodium acrylate
sodium
activating agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510755979.8A
Other languages
Chinese (zh)
Inventor
陶荣燕
杨毅
黄景诚
廖煜明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510755979.8A priority Critical patent/CN105330897A/en
Publication of CN105330897A publication Critical patent/CN105330897A/en
Pending legal-status Critical Current

Abstract

The invention discloses a sodium acrylate calcium carbonate activating agent. The sodium acrylate calcium carbonate activating agent is characterized by being prepared from, by weight, 5-8 parts of propylene glycol n-butyl ether, 3-8 parts of pentaerythritol rosin europium resin, 25-30 parts of coconut oil fatty acid diethanolamide, 5-8 parts of sodium carbonate, 3-5 parts of poly[(sodium acrylate)-co-(4-vinylpyridine)], 5-6 parts of glycerol triacetate, 10-12 parts of di-n-octyltin oxide, 3-5 parts of polyvinyl acetal resin, 25-30 parts of gamma-glycidoxy propyl trimethoxy silane, 3-5 parts of dodecyl dimethyl benzyl ammonium bromide, 20-30 parts of ethyl alcohol and 550-660 parts of water. The sodium acrylate calcium carbonate activating agent has the advantages of being scientific and reasonable in design, simple in process, safe, reliable, easy to control, convenient to prepare, suitable for large-scale production, low in production cost and the like.

Description

Sodium acrylate calcium carbonate activator
Technical field
The invention belongs to a kind of auxiliary agent producing non-metallic powder.
Background technology
At present, calcium carbonate is widely used in papermaking, plastics, plastics film, chemical fibre, rubber, tackiness agent, sealing agent, daily-use chemical industry, makeup, building materials, coating, paint, ink, putty, sealing wax, putty, carpet veneer is packed, medicine, food is (as chewing gum, chocolate), in feed, its effect has: increase small product size, reduce costs, improve processing characteristics (as adjusting viscosity, rheological property, curability), improve dimensional stability, reinforcement or half reinforcement, improve printing performance, improve physicals (as thermotolerance, extinction, wear resistance, flame retardant resistance, whiteness, glossiness) etc., for obtaining more superior performance, auxiliary agent is all adopted to carry out activation treatment.
Summary of the invention
The object of the invention is to; A kind of sodium acrylate calcium carbonate activator and preparation method thereof is proposed.
Sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3-8 part, cocoanut fatty acid diethanolamide 25-30 part, sodium carbonate 5-8 part, sodium acrylate-4-vinylpridine multipolymer 3-5 part, Vanay 5-6 part, di-n-octyltin oxide 10--12 part, polyvinyl acetal resin 3-5 part, γ-glycidyl ether oxygen propyl trimethoxy silicane 25-30 part, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms.
The preparation method of sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3-8 part, cocoanut fatty acid diethanolamide 25-30 part, sodium carbonate 5-8 part, sodium acrylate-4-vinylpridine multipolymer 3-5 part, Vanay 5-6 part, di-n-octyltin oxide 10--12 part, polyvinyl acetal resin 3-5 part, γ-glycidyl ether oxygen propyl trimethoxy silicane 25-30 part, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms, first with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
The present invention compared with prior art its beneficial effect is: have design science reasonable, and technique is simple, safe reliability, is easy to control, easy to operate, is applicable to scale operation, the advantages such as production cost is low.
Embodiment
Below in conjunction with embodiment, the invention will be further described, but embodiments of the present invention are not limited thereto.
All raw materials of the present invention can buy acquisition.
Embodiment 1
The preparation method of sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3-8 part, cocoanut fatty acid diethanolamide 25-30 part, sodium carbonate 5-8 part, sodium acrylate-4-vinylpridine multipolymer 3-5 part, Vanay 5-6 part, di-n-octyltin oxide 10--12 part, polyvinyl acetal resin 3-5 part, γ-glycidyl ether oxygen propyl trimethoxy silicane 25-30 part, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms, first with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
Embodiment 2
The preparation method of sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, is characterized in that: by weight, and its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3 parts, cocoanut fatty acid diethanolamide 25 parts, 5 parts, sodium carbonate, sodium acrylate-4-vinylpridine multipolymer 3 parts, Vanay 5 parts, dioctyl tin 10 parts, polyvinyl acetal resin 3 parts, glycidyl ether oxygen propyl trimethoxy silicane 25 parts, ethanol 20-30 part, water 550-600 part forms; First with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
Embodiment 3
The preparation method of sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 8 parts, cocoanut fatty acid diethanolamide 30 parts, 8 parts, sodium carbonate, sodium acrylate-4-vinylpridine multipolymer 5 parts, Vanay 6 parts, dioctyl tin 12 parts, polyvinyl acetal resin 5 parts, glycidyl ether oxygen propyl trimethoxy silicane 30 parts, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms; First with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
Embodiment 4
The preparation method of sodium acrylate calcium carbonate activator calcium carbonate activator of the present invention, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3 parts, cocoanut fatty acid diethanolamide 30 parts, 5 parts, sodium carbonate, sodium acrylate-4-vinylpridine multipolymer 5 parts, Vanay 5 parts, dioctyl tin 12 parts, polyvinyl acetal resin 3 parts, glycidyl ether oxygen propyl trimethoxy silicane 25 parts, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms; First with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
Product of the present invention, uses through production firm, and produce modified superfine water-ground limestone product, reaction effect is fine.
Part material illustrates:
Described rosin pentaerythritol ester europium resin, the method that can be preferably ZL201410078259.8 by the Chinese patent patent No. obtains.
γ-glycidyl ether oxygen propyl trimethoxy silicane
No. Cas: 2530-83-8
Molecular formula: C9H20O5Si molecular weight: 236.34
Another name: 3-(2,3-epoxy third oxygen) propyl trimethoxy silicane, 3-glycydoxy Trimethoxy silane
γ-glycidyl ether oxygen propyl trimethoxy silicane.

Claims (2)

1. a sodium acrylate calcium carbonate activator calcium carbonate activator, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3-8 part, cocoanut fatty acid diethanolamide 25-30 part, sodium carbonate 5-8 part, sodium acrylate-4-vinylpridine multipolymer 3-5 part, Vanay 5-6 part, di-n-octyltin oxide 10--12 part, polyvinyl acetal resin 3-5 part, γ-glycidyl ether oxygen propyl trimethoxy silicane 25-30 part, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms.
2. the preparation method of a sodium acrylate calcium carbonate activator calcium carbonate activator, it is characterized in that: by weight, its formula is by propylene glycol monobutyl ether 5-8 part, rosin pentaerythritol ester europium resin 3-8 part, cocoanut fatty acid diethanolamide 25-30 part, sodium carbonate 5-8 part, sodium acrylate-4-vinylpridine multipolymer 3-5 part, Vanay 5-6 part, di-n-octyltin oxide 10--12 part, polyvinyl acetal resin 3-5 part, γ-glycidyl ether oxygen propyl trimethoxy silicane 25-30 part, dodecyl dimethyl benzyl ammonium bromide 3-5 part, ethanol 20-30 part, water 550-600 part forms, first with ethanol by rosin europium resin dissolves, after adding water 550-600 part, add whole raw material and mix, at 85 ~ 95 DEG C, stir 20-30 minute, obtain product.
CN201510755979.8A 2015-11-07 2015-11-07 Sodium acrylate calcium carbonate activating agent Pending CN105330897A (en)