CN104924401A - 一种玉米皮防腐处理方法 - Google Patents
一种玉米皮防腐处理方法 Download PDFInfo
- Publication number
- CN104924401A CN104924401A CN201510312925.4A CN201510312925A CN104924401A CN 104924401 A CN104924401 A CN 104924401A CN 201510312925 A CN201510312925 A CN 201510312925A CN 104924401 A CN104924401 A CN 104924401A
- Authority
- CN
- China
- Prior art keywords
- maize peel
- parts
- corn bran
- water
- rinse
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种玉米皮防腐处理方法,包括以下步骤:(1)、将玉米皮在55℃条件下处理20h,然后将玉米皮使用1%的硝酸钾溶液在25℃下浸泡处理;(2)、将玉米皮使用清水冲洗干净,然后烘干至含水量为25%,使用质量浓度1%的氯化钠溶液浸泡2h;(3)、将玉米皮使用处理剂在28℃浸泡处理1.2h;(4)、将玉米皮使用0.5%的尿素水冲洗,然后将玉米皮使用处理液在25-30℃浸泡处理1h;(5)、将玉米皮使用0.5%的醋酸溶液浸泡3min,然后使用清水冲洗干净表面,在45℃下烘干即可。本发明制备的玉米皮防腐处理方法简单,处理后玉米皮的防腐、防霉能力明显增强。
Description
技术领域
本发明属于植物皮处理领域,具体涉及一种玉米皮防腐处理方法。
背景技术
在玉米种植过程中会产生大量的玉米皮,现在的玉米皮往往用于焚烧,利用价值低,而且容易产生污染,现在玉米皮可用于编织,编织各种工艺品,但是由于玉米皮较薄,防腐蚀性较差,而且玉米叶在编制过程中会造成玉米叶大面积出现折痕,影响制品的品质。
发明内容
本发明的目的是提供一种玉米皮处理方法,可以提高玉米皮的防腐蚀性能。
本发明通过以下技术方案实现:
一种玉米皮防腐处理方法,包括以下步骤:
(1)、将玉米皮在55℃、相对湿度15%条件下处理20h,然后将玉米皮使用质量分数为1%的硝酸钾溶液在25℃下浸泡处理10min;
(2)、将步骤(1)处理好的玉米皮使用清水冲洗干净,然后烘干至含水量为25%,使用质量浓度1%的氯化钠溶液浸泡2h,使用清水冲洗干净;
(3)、将步骤(2)处理好的玉米皮使用处理剂在28℃浸泡处理1.2h,所述处理剂按重量计由以下原料制备而成:水杨酸钠0.5份、鸡血藤1.2份、白蔹0.8份、酸枣叶1.2份、柏子仁0.8份、桃枝2.2份、水20份;
(4)、将步骤(3)处理好的玉米皮使用0.5%的尿素水冲洗,然后将玉米皮使用处理液在25-30℃浸泡处理1h,处理液按重量计由以下原料配制而成:尿素1.8份、甘油4份、水18份、小苏打0.9份;
(5)、将步骤(4)处理好的玉米皮使用质量分数0.5%的醋酸溶液浸泡3min,然后使用清水冲洗干净表面,在45℃下烘干即可。
处理剂制备时,将鸡血藤1.2份、白蔹0.8份、酸枣叶1.2份、柏子仁0.8份、桃枝2.2份、水20份混合,加热回流处理2h,然后取滤液,将滤液与水杨酸钠混合均匀,得到处理剂。
本发明的有益效果:本发明制备的玉米皮防腐处理方法简单,处理后玉米皮的防腐、防霉能力明显增强,可以保持其制品2-3年内不发霉、生虫,结合浸泡、清洗等步骤,各步骤结合使用可以使处理效果更好,处理更均匀,使玉米皮各部位的性能均衡,同时,处理后玉米皮的着色能力增强,便于玉米皮进行染色,便于后续进行染色处理。
具体实施方式
一种玉米皮防腐处理方法,包括以下步骤:
(1)、将玉米皮在55℃、相对湿度15%条件下处理20h,然后将玉米皮使用质量分数为1%的硝酸钾溶液在25℃下浸泡处理10min;
(2)、将步骤(1)处理好的玉米皮使用清水冲洗干净,然后烘干至含水量为25%,使用质量浓度1%的氯化钠溶液浸泡2h,使用清水冲洗干净;
(3)、将步骤(2)处理好的玉米皮使用处理剂在28℃浸泡处理1.2h,所述处理剂按重量计由以下原料制备而成:水杨酸钠0.5份、鸡血藤1.2份、白蔹0.8份、酸枣叶1.2份、柏子仁0.8份、桃枝2.2份、水20份;
(4)、将步骤(3)处理好的玉米皮使用0.5%的尿素水冲洗,然后将玉米皮使用处理液在25-30℃浸泡处理1h,处理液按重量计由以下原料配制而成:尿素1.8份、甘油4份、水18份、小苏打0.9份;
(5)、将步骤(4)处理好的玉米皮使用质量分数0.5%的醋酸溶液浸泡3min,然后使用清水冲洗干净表面,在45℃下烘干即可。
将霉菌在25℃、相对湿度40%的条件下接种霉菌到处理好的玉米皮上培养,结果显示,霉菌3h内失去活性。
Claims (1)
1.一种玉米皮防腐处理方法,其特征在于,包括以下步骤:
(1)、将玉米皮在55℃、相对湿度15%条件下处理20h,然后将玉米皮使用质量分数为1%的硝酸钾溶液在25℃下浸泡处理10min;
(2)、将步骤(1)处理好的玉米皮使用清水冲洗干净,然后烘干至含水量为25%,使用质量浓度1%的氯化钠溶液浸泡2h,使用清水冲洗干净;
(3)、将步骤(2)处理好的玉米皮使用处理剂在28℃浸泡处理1.2h,所述处理剂按重量计由以下原料制备而成:水杨酸钠0.5份、鸡血藤1.2份、白蔹0.8份、酸枣叶1.2份、柏子仁0.8份、桃枝2.2份、水20份;
(4)、将步骤(3)处理好的玉米皮使用0.5%的尿素水冲洗,然后将玉米皮使用处理液在25-30℃浸泡处理1h,处理液按重量计由以下原料配制而成:尿素1.8份、甘油4份、水18份、小苏打0.9份;
(5)、将步骤(4)处理好的玉米皮使用质量分数0.5%的醋酸溶液浸泡3min,然后使用清水冲洗干净表面,在45℃下烘干即可。