CN104846415A - 一种用于处理汽车雨刮片主支架表面的方法 - Google Patents
一种用于处理汽车雨刮片主支架表面的方法 Download PDFInfo
- Publication number
- CN104846415A CN104846415A CN201510238584.0A CN201510238584A CN104846415A CN 104846415 A CN104846415 A CN 104846415A CN 201510238584 A CN201510238584 A CN 201510238584A CN 104846415 A CN104846415 A CN 104846415A
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- main support
- blade main
- wiper blade
- automobile wiper
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种用于处理汽车雨刮片主支架表面的方法,包括如下步骤,(1)不锈钢主支架表面进行表面本色白化处理,对不锈钢氧化皮处理采用化学法,使用一钟无污染酸洗钝化膏和常温无毒害的带有无机添加剂的清洗液进行浸洗,达到不锈钢本色的白化处理;(2)不锈钢主支架表面镜石光亮处理,根据不锈钢产品采用机械抛光或电化学抛光来达到镜石光泽。具有制作方便,效率高的特点。
Description
技术领域
本发明属于汽车配件技术领域,涉及用于处理汽车雨刮片主支架表面的方法。
背景技术
现在的车辆都配备有一个雨刷器,有骨雨刷的原理是通过骨架上的若干支撑点把雨刮片压在玻璃上的,使雨刮片上的各个支撑点的压力平均。雨天驾车行驶,不论雨是大是小,如果雨刷的故障无法排除,不能有效刮干净挡风玻璃上面的雨水,人的视线就会极度下降,安全就没有保障,无法继续行车。雨刷器一旦出现不能正常工作的情况,雨天会给行车带来很多不便,而雨刮片质量的好坏对雨刷乃至汽车的前挡风玻璃视线有直接影响,事关安全大事,需要给驾驶员提供一个明亮的视野十分重要。
发明内容
本发明旨在克服现有技术的缺陷,提供了一种用于处理汽车雨刮片主支架表面的方法,具有制作方便,效率高的特点。
本发明的目的通过以下技术方案来具体实现:
一种用于处理汽车雨刮片主支架表面的方法,包括如下步骤,(1)包括如下步骤,(1)不锈钢主支架表面进行表面本色白化处理,对不锈钢氧化皮处理采用化学法,使用一钟无污染酸洗钝化膏和常温无毒害的带有无机添加剂的清洗液进行浸洗,达到不锈钢本色的白化处理;(2)不锈钢主支架表面镜石光亮处理,根据不锈钢产品采用机械抛光或电化学抛光来达到镜石光泽。
进一步地,不锈钢雨刮片主支架表面着色处理,采用电化学法提高有雨刮片主支架的耐磨性。
进一步地,所述雨刮器主支架材质为AISI 304ES不锈钢雨刮片主支架。
与现有技术相比较,本发明具有如下的有益效果:
本发明具有制作方便,效率高的特点。耐磨性好,氧化皮取出干净,抛光整平性好,光泽保持时间长,产品质量好。
具体实施方式
以下对本发明的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本发明,并不用于限定本发明。
一种用于处理汽车雨刮片主支架表面的方法,包括如下步骤,(1)包括如下步骤,(1)不锈钢主支架表面进行表面本色白化处理,对不锈钢氧化皮处理采用化学法,使用一钟无污染酸洗钝化膏和常温无毒害的带有无机添加剂的清洗液进行浸洗,达到不锈钢本色的白化处理;(2)不锈钢主支架表面镜石光亮处理,根据不锈钢产品采用机械抛光或电化学抛光来达到镜石光泽。所述雨刮器主支架材质为AISI 304ES不锈钢雨刮片主支架。
优选地,不锈钢雨刮片主支架表面着色处理,采用电化学法提高有雨刮片主支架的耐磨性。
电化学法,是在特定溶液中,通过电化学氧化形成氧化膜的颜色。
最后应说明的是:以上所述仅为说明本发明的实施方式,并不用于限制本发明,对于本领域的技术人员来说,凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (3)
1.一种用于处理汽车雨刮片主支架表面的方法,其特征在于,包括如下步骤,(1)包括如下步骤,(1)不锈钢主支架表面进行表面本色白化处理,对不锈钢氧化皮处理采用化学法,使用一钟无污染酸洗钝化膏和常温无毒害的带有无机添加剂的清洗液进行浸洗,达到不锈钢本色的白化处理;(2)不锈钢主支架表面镜石光亮处理,根据不锈钢产品采用机械抛光或电化学抛光来达到镜石光泽。
2.如权利要求1所述汽车雨刮片主支架的处理方法,其特征在于,不锈钢雨刮片主支架表面着色处理,采用电化学法提高有雨刮片主支架的耐磨性。
3.如权利要求1所述汽车雨刮片主支架的处理方法,其特征在于,所述雨刮器主支架材质为AISI 304ES不锈钢雨刮片主支架。