CN104841776A CN201510301703.2A CN201510301703A CN104841776A CN 104841776 A CN104841776 A CN 104841776A CN 201510301703 A CN201510301703 A CN 201510301703A CN 104841776 A CN104841776 A CN 104841776A
Authority
CN
China
Prior art keywords
bending
hydraulic
simmering
steel plates
mold
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510301703.2A
Other languages
English (en)
Inventor
彭雪峰
马魁
赵培勇
贺小锋
马军伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHAANXI CHEMICAL CONSTRUCTION CO Ltd
Original Assignee
SHAANXI CHEMICAL CONSTRUCTION CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHAANXI CHEMICAL CONSTRUCTION CO Ltd filed Critical SHAANXI CHEMICAL CONSTRUCTION CO Ltd
Priority to CN201510301703.2A priority Critical patent/CN104841776A/zh
Publication of CN104841776A publication Critical patent/CN104841776A/zh
Pending legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B21MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL
    • B21DWORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL
    • B21D37/00Tools as parts of machines covered by this subclass
    • B21D37/10Die sets; Pillar guides

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Bending Of Plates, Rods, And Pipes (AREA)

Abstract

本发明公开了一种用于接地母线平弯液压冷弯的液压煨弯模具,该模具包括中心顶、侧边模具卡,所述侧边模具卡设置在弯管架的左右两侧,所述中心顶设置在两侧的侧边模具卡中心位置的对立面上;所述中心顶包括钢板、圆弧弯夹,所述圆弧弯夹设置在两个钢板中间,所述两个钢板的一侧设置有用于与弯管机的液压柱塞连接的圆管;所述侧边模具卡包括中心柱、圆盘,所述中心柱上套设两个圆盘,所述两个圆盘之间设置有间隙。本发明将接地母线冷煨成镰刀弯,满足电气接地安装施工中平弯及镰刀弯的制作工艺,达到其操作方便,煨弯质量好,工作效率高,节约施工成本,防止破坏扁钢镀锌层等优点。

Description

用于接地母线平弯液压冷弯的液压煨弯模具
技术领域
本发明属于电气接地安装施工技术领域,具体涉及一种用于接地母线平弯液压冷弯的液压煨弯模具。
背景技术
在电气接地安装施工中,按照要求接地母线平弯需制作成镰刀弯,通常使用气焊将接地扁钢加热并配合榔头敲击煨制成90°平弯,这样使用火焰加热煨弯不仅破坏了接地扁钢上的镀锌层,而且煨弯比较费时费力。针对这种情况,在施工过程中根据以往的施工经验进行技术创新,发明一种液压煨弯设备,采用这种液压煨制机很轻松的将接地扁钢冷煨成镰刀弯。
发明内容
有鉴于此,本发明的主要目的在于提供一种用于接地母线平弯液压冷弯的液压煨弯模具。
为达到上述目的,本发明的技术方案是这样实现的:
本发明实施例提供一种用于接地母线平弯液压冷弯的液压煨弯模具,该模具包括中心顶、侧边模具卡,所述侧边模具卡设置在弯管架的左右两侧,所述中心顶设置在两侧的侧边模具卡中心位置的对立面上;所述中心顶包括钢板、圆弧弯夹,所述圆弧弯夹设置在两个钢板中间,所述两个钢板的一侧设置有用于与弯管机的液压柱塞连接的圆管;所述侧边模具卡包括中心柱、圆盘,所述中心柱上套设两个圆盘,所述两个圆盘之间设置有间隙。
上述方案中,所述中心顶与两侧的侧边模具卡之间设置用于放置待煨弯的接地母线的间隙,所述待煨弯的接地母线一侧设置在两侧侧边模具卡的间隙内,另一侧设置在圆弧弯夹的两个钢板内的圆弧弯夹上。
上述方案中,所述两个钢板用于焊接圆弧弯夹的间隙与两侧侧边模具卡的间隙处于同一水平面。
上述方案中,所述圆弧弯夹为一半径150~200mm的90°圆弧弯。
与现有技术相比,本发明的有益效果:
本发明将接地母线冷煨成镰刀弯,满足电气接地安装施工中平弯及镰刀弯的制作工艺,达到其操作方便,煨弯质量好,工作效率高,节约施工成本,防止破坏扁钢镀锌层等优点。
附图说明
图1为本发明实施例提供一种用于接地母线平弯液压冷弯的液压煨弯模具的结构示意图;
图2为本发明实施例提供一种用于接地母线平弯液压冷弯的液压煨弯模具的中心顶的结构示意图;
图3为本发明实施例提供一种用于接地母线平弯液压冷弯的液压煨弯模具的侧边模具卡的结构示意图。
具体实施方式
下面结合附图和具体实施方式对本发明进行详细说明。
本发明实施例提供一种用于接地母线平弯液压冷弯的液压煨弯模具,如图1所示,该模具包括中心顶1、侧边模具卡2,所述侧边模具卡2设置在弯管架5的左右两侧,所述中心顶1设置在两侧的侧边模具卡2中心位置的对立面上。
如图2所示,所述中心顶1包括钢板103、圆弧弯夹101,所述圆弧弯夹101设置在两个钢板103中间,所述两个钢板103的一侧设置有用于与弯管机的液压柱塞3连接的圆管102;所述圆弧弯夹101为一半径150~200mm的90°圆弧弯。
如图3所示,所述侧边模具卡2包括中心柱201、圆盘202,所述中心柱201上套设两个圆盘202,所述两个圆盘202之间设置有间隙。
所述中心顶1与两侧的侧边模具卡2之间设置用于放置待煨弯的接地母线的间隙,所述待煨弯的接地母线一侧设置在两侧侧边模具卡2的间隙内,另一侧设置在圆弧弯夹101的两个钢板103内的圆弧弯夹101上。
所述两个钢板103用于焊接圆弧弯夹101的间隙与两侧侧边模具卡2的间隙处于同一水平面,这样制作出来的镰刀弯也是水平的,左右侧边模具卡2必须放在弯管架5从中间到两边第三个孔上,即放置DN25弯管模具的位置;如果侧边模具卡2距离中心顶1较近,则在液压制作时两个侧边模具卡2会相互碰撞;如果两个侧边模具卡2距离中心顶1较远,则在液压制作时需要制作的接地母线会变形,制作出来的镰刀弯不在一个水平面上。
本发明的工作过程:
将待煨弯的接地母线放置好后,弯管机的液压柱塞3伸出带动中心顶1向两侧的侧边模具卡2中心位置靠近,逐步使得待煨弯的接地母线呈弯曲状,直到曲度符合要求时,所述弯管机的液压柱塞3收缩,取出已煨弯的接地母线。
以上所述,仅为本发明的较佳实施例而已,并非用于限定本发明的保护范围。

Claims (4)

1.一种用于接地母线平弯液压冷弯的液压煨弯模具,其特征在于,该模具包括中心顶(1)、侧边模具卡(2),所述侧边模具卡(2)设置在弯管架(5)的左右两侧,所述中心顶(1)设置在两侧的侧边模具卡(2)中心位置的对立面上;所述中心顶(1)包括钢板(103)、圆弧弯夹(101),所述圆弧弯夹(101设置在两个钢板(103)中间,所述两个钢板(103)的一侧设置有用于与弯管机的液压柱塞(3)连接的圆管(102);所述侧边模具卡(2)包括中心柱(201)、圆盘(202),所述中心柱(201)上套设两个圆盘(202),所述两个圆盘(202)之间设置有间隙。
2.根据权利要求1所述的用于接地母线平弯液压冷弯的液压煨弯模具,其特征在于:所述中心顶(1)与两侧的侧边模具卡(2)之间设置用于放置待煨弯的接地母线的间隙,所述待煨弯的接地母线一侧设置在两侧侧边模具卡(2)的间隙内,另一侧设置在圆弧弯夹(101)的两个钢板(103)内的圆弧弯夹(101)上。
3.根据权利要求1或2所述的用于接地母线平弯液压冷弯的液压煨弯模具,其特征在于:所述两个钢板(103)用于焊接圆弧弯夹(101)的间隙与两侧侧边模具卡(2)的间隙处于同一水平面。
4.根据权利要求3所述的用于接地母线平弯液压冷弯的液压煨弯模具,其特征在于:所述圆弧弯夹(101)为一半径150~200mm的90°圆弧弯。
CN201510301703.2A 2015-06-04 2015-06-04 用于接地母线平弯液压冷弯的液压煨弯模具 Pending CN104841776A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510301703.2A CN104841776A (zh) 2015-06-04 2015-06-04 用于接地母线平弯液压冷弯的液压煨弯模具

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510301703.2A CN104841776A (zh) 2015-06-04 2015-06-04 用于接地母线平弯液压冷弯的液压煨弯模具

Publications (1)

Publication Number Publication Date
CN104841776A true CN104841776A (zh) 2015-08-19

Family

ID=53841974

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510301703.2A Pending CN104841776A (zh) 2015-06-04 2015-06-04 用于接地母线平弯液压冷弯的液压煨弯模具

Country Status (1)

Country Link
CN (1) CN104841776A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105170796A (zh) * 2015-09-14 2015-12-23 山东双一科技股份有限公司 冷煨装置
CN106799415A (zh) * 2017-01-13 2017-06-06 中国化学工程第六建设有限公司 热镀锌扁钢弯头模具及应用其制作热镀锌扁钢弯头的方法

Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US2882952A (en) * 1958-02-06 1959-04-21 Carl Parten Die for use in bending flat metal stock and the like
CN101590497A (zh) * 2008-05-30 2009-12-02 中国二十冶建设有限公司 镀锌扁钢侧弯冷煨方法
CN201880767U (zh) * 2010-10-22 2011-06-29 中国华冶科工集团有限公司 带限位装置的液压煨弯机
CN203356289U (zh) * 2013-07-23 2013-12-25 胜利油田胜利石油化工建设有限责任公司 一种顶推式反变形液压冷弯成型机
CN204208947U (zh) * 2014-09-29 2015-03-18 中国化学工程第十四建设有限公司 一种接地扁钢弯头的制作工具
CN204747253U (zh) * 2015-06-04 2015-11-11 陕西化建工程有限责任公司 一种用于接地母线平弯液压冷弯的液压煨弯模具

Patent Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US2882952A (en) * 1958-02-06 1959-04-21 Carl Parten Die for use in bending flat metal stock and the like
CN101590497A (zh) * 2008-05-30 2009-12-02 中国二十冶建设有限公司 镀锌扁钢侧弯冷煨方法
CN201880767U (zh) * 2010-10-22 2011-06-29 中国华冶科工集团有限公司 带限位装置的液压煨弯机
CN203356289U (zh) * 2013-07-23 2013-12-25 胜利油田胜利石油化工建设有限责任公司 一种顶推式反变形液压冷弯成型机
CN204208947U (zh) * 2014-09-29 2015-03-18 中国化学工程第十四建设有限公司 一种接地扁钢弯头的制作工具
CN204747253U (zh) * 2015-06-04 2015-11-11 陕西化建工程有限责任公司 一种用于接地母线平弯液压冷弯的液压煨弯模具

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105170796A (zh) * 2015-09-14 2015-12-23 山东双一科技股份有限公司 冷煨装置
CN106799415A (zh) * 2017-01-13 2017-06-06 中国化学工程第六建设有限公司 热镀锌扁钢弯头模具及应用其制作热镀锌扁钢弯头的方法
CN106799415B (zh) * 2017-01-13 2018-05-08 中国化学工程第六建设有限公司 热镀锌扁钢弯头模具及应用其制作热镀锌扁钢弯头的方法

Similar Documents

Publication Publication Date Title
CN104841776A (zh) 用于接地母线平弯液压冷弯的液压煨弯模具
CN107069528B (zh) 电力施工用电线管弯管器及弯管方法
CN203863171U (zh) 一种电路快速拆焊工装
CN204747253U (zh) 一种用于接地母线平弯液压冷弯的液压煨弯模具
CN203530381U (zh) 薄壁圆环零件的热处理夹具
CN202180119U (zh) 弯扁钢装置
CN103521565A (zh) 一种大型角钢热弯方法及工装
CN103252391A (zh) 一种弯管器
CN203862780U (zh) 加热式的弯管机
CN203292386U (zh) 一种圆钢调直机
CN203330200U (zh) 电力铁塔钢管热弯装置
CN206986025U (zh) 一种热弯机
CN203457340U (zh) 中频感应电炉用磁轭
CN203818403U (zh) 加热装置
CN205911028U (zh) 一种运用于软硬一体铜排绝缘防护结构
CN204996990U (zh) 锻模预热管
CN206276754U (zh) 一种接地扁钢冷弯设备
CN204974844U (zh) 折弯器以及折弯结构
CN209901978U (zh) 便携式接地扁铁顶弯机装置
CN202868846U (zh) 一种水暖散热器
CN2840581Y (zh) 高精度电热平板
CN204093871U (zh) 一种船首折弯工装系统
CN204074867U (zh) 基于磁脉冲的贮箱箱底大倾斜角翻边孔成形装置
CN203550608U (zh) 适用于大型矿热炉炉台的冷却装置
CN204819412U (zh) 一种新型石英石定型装置

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
EXSB Decision made by sipo to initiate substantive examination
SE01 Entry into force of request for substantive examination
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20150819

WD01 Invention patent application deemed withdrawn after publication