- CN104741406A CN104741406A CN201310751550.2A CN201310751550A CN104741406A CN 104741406 A CN104741406 A CN 104741406A CN 201310751550 A CN201310751550 A CN 201310751550A CN 104741406 A CN104741406 A CN 104741406A
- Authority
- CN
- China
- Prior art keywords
- patrix
- die
- upper die
- bridge
- hole
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B21—MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL
- B21C—MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES, OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B21C25/00—Profiling tools for metal extruding
- B21C25/02—Dies
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Extrusion Of Metal (AREA)
Abstract
本发明公开了一种结构改进的热挤压模具,包括能够前后叠加连接在一起的上模和下模,上模进料端设有导流板,导流板上设有若干桥位,各个桥位之间形成分流孔,下模自进料端到出料端依次设有连通的焊合室和出料孔,所述焊合室与上模的分流孔连通,上模的芯头插设于下模的成型孔内,所述上模的各个桥位沿上模径向方向呈曲线状态延伸,本发明将上模的桥位设计成曲线形结构,进入分流孔的材料经曲线形的分流孔进入焊合室,材料在焊合室内会形成紊流,使各个分流孔内流入焊合室内的材料充分焊合,材料经成型孔成型后的产品表面的焊合线也就呈螺旋曲线的方式延伸,其整体强度高,在弯折、冷拔和拉伸时不易开裂损坏。
Description
技术领域
本发明涉及一种挤压模具,特别涉及一种结构改进的热挤压模具。
背景技术
各种型材成型都通过热挤压模具来实现,一般热挤压模具由上模和下模组成,上模上设有导流板和芯头,导流板上设有桥位,材料经过各桥位间的分流孔进行分流后进入模具内,然后流入焊合室,进入焊合室后聚流,然后再进入由芯头和成型孔形成的成型空间内进行挤压成型,最终从出料孔排出,目前常见的桥位沿上模径向方向均为直线型,材料沿分流孔进入焊合室,材料在焊合室内聚流后进入成型孔内成型,然而由于桥位是直线型的,则材料沿分流孔直流入焊合室,各个分流孔内的材料难以很好的焊合,成型的产品表面就会产生沿其长度方向的直线型焊合线,这样就影响了产品的强度,产品在使用过程中容易出现开裂损坏。
发明内容
为了克服上述缺陷,本发明提供了一种结构改进的热挤压模具,该结构改进的热挤压模具结构简单,材料在经分流孔分流后在焊合室内紊流焊合,产品上焊合线沿其长度方向呈曲线,提高了产品的强度。
本发明为了解决其技术问题所采用的技术方案是:一种结构改进的热挤压模具,包括能够前后叠加连接在一起的上模和下模,上模进料端设有导流板,导流板上设有若干桥位,各个桥位之间形成分流孔,下模自进料端到出料端依次设有连通的焊合室和出料孔,所述焊合室与上模的分流孔连通,上模的芯头插设于下模的成型孔内,所述上模的各个桥位沿上模径向方向呈曲线状态延伸。
作为本发明的进一步改进,所述上模的各个桥位沿上模径向方向呈“S”形结构。
作为本发明的进一步改进,所述各个桥位的棱边均设有圆角。
作为本发明的进一步改进,所述各个桥位横截面位于出料端一侧沿其厚度方向呈两侧向中间收缩的尖形结构。
本发明的有益效果是:本发明将上模的桥位设计成曲线形结构,进入分流孔的材料经曲线形的分流孔进入焊合室,材料在焊合室内会形成紊流,使各个分流孔内流入焊合室内的材料充分焊合,材料经成型孔成型后的产品表面的焊合线也就呈螺旋曲线的方式延伸,其整体强度高,在弯折、冷拔和拉伸时不易开裂损坏。
附图说明
图1为本发明主视图;
图2为图1中A-A向剖视图;
图3为上模主视图;
图4为上模中B-B向剖视图。
具体实施方式
实施例:一种结构改进的热挤压模具,包括能够前后叠加连接在一起的上模1和下模2,上模1进料端设有导流板,导流板上设有若干桥位3,各个桥位3之间形成分流孔4,下模2自进料端到出料端依次设有连通的焊合室5和出料孔6,所述焊合室5与上模1的分流孔4连通,上模1的芯头插设于下模2的成型孔内,所述上模1的各个桥位3沿上模1径向方向呈曲线状态延伸,材料自上模1的分流孔4流入到下模2的焊合室5内,由于上模1的桥位3是曲线形的,分流孔4也呈相应的曲线形结构,材料沿曲线的分流孔4流入焊合室5内形成紊流,经过紊流的材料混合状态好,成型后产品上的焊合线沿产品长度方向呈螺旋曲线形延伸,提高了产品的强度,产品在使用过程中不易开裂损坏。
所述上模1的各个桥位3沿上模1径向方向呈“S”形结构,“S”形结构能够保证材料进入焊合室5内紊流强度,保证材料在焊合室5内充分融合,当然也可以是波浪形,圆弧形,弯折线形等等。
所述各个桥位3的棱边均设有圆角。
所述各个桥位3横截面位于出料端一侧沿其厚度方向呈两侧向中间收缩的尖形结构,这就使分流孔4的孔径自进料端向出料端逐渐增大,加大了流量,提高了材料的紊流性,保证其焊合良好。
Claims (4)
1.一种结构改进的热挤压模具,包括能够前后叠加连接在一起的上模(1)和下模(2),上模(1)进料端设有导流板,导流板上设有若干桥位(3),各个桥位(3)之间形成分流孔(4),下模(2)自进料端到出料端依次设有连通的焊合室(5)和出料孔(6),所述焊合室(5)与上模(1)的分流孔(4)连通,上模(1)的芯头插设于下模(2)的成型孔内,其特征在于:所述上模(1)的各个桥位(3)沿上模(1)径向方向呈曲线状态延伸。
2.根据权利要求1所述的结构改进的热挤压模具,其特征在于:所述上模(1)的各个桥位(3)沿上模(1)径向方向呈“S”形结构。
3.根据权利要求2所述的结构改进的热挤压模具,其特征在于:所述各个桥位(3)的棱边均设有圆角。
4.根据权利要求2所述的结构改进的热挤压模具,其特征在于:所述各个桥位(3)横截面位于出料端一侧沿其厚度方向呈两侧向中间收缩的尖形结构。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201310751550.2A CN104741406A (zh) | 2013-12-31 | 2013-12-31 | 结构改进的热挤压模具 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201310751550.2A CN104741406A (zh) | 2013-12-31 | 2013-12-31 | 结构改进的热挤压模具 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN104741406A true CN104741406A (zh) | 2015-07-01 |
Family
ID=53581986
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201310751550.2A Pending CN104741406A (zh) | 2013-12-31 | 2013-12-31 | 结构改进的热挤压模具 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN104741406A (zh) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN107931347A (zh) * | 2017-11-28 | 2018-04-20 | 福建省南平铝业股份有限公司 | 一种小开口大承压面遮挡式铝挤压模具 |
CN111330994A (zh) * | 2020-04-02 | 2020-06-26 | 南充市长远铝业有限公司 | 一种铝管挤压成型模具、装置及铝管 |
Citations (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN87204764U (zh) * | 1987-11-13 | 1988-08-17 | 长沙有色金属加工厂 | 一种分流组合模 |
CN2119278U (zh) * | 1991-08-08 | 1992-10-21 | 西南铝加工厂 | 一种新型搭接式平面分流组合模 |
JPH07185648A (ja) * | 1993-12-27 | 1995-07-25 | Yano Eng:Kk | 細孔を有する押出材の押出加工用ダイス |
CN1342531A (zh) * | 2000-09-12 | 2002-04-03 | 郭丽仪 | 生产铝合金无缝管材的方法和相应模具组 |
CN201482815U (zh) * | 2009-07-06 | 2010-05-26 | 西南铝业(集团)有限责任公司 | 一种平面分流模 |
CN203044558U (zh) * | 2012-11-28 | 2013-07-10 | 昆山捷安特轻合金科技有限公司 | 结构改进的挤压模具 |
CN203044556U (zh) * | 2012-11-28 | 2013-07-10 | 昆山捷安特轻合金科技有限公司 | 新型挤压模具用上模 |
CN203751017U (zh) * | 2013-12-31 | 2014-08-06 | 昆山捷安特轻合金科技有限公司 | 结构改进的热挤压模具 |
-
2013
- 2013-12-31 CN CN201310751550.2A patent/CN104741406A/zh active Pending
Patent Citations (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN87204764U (zh) * | 1987-11-13 | 1988-08-17 | 长沙有色金属加工厂 | 一种分流组合模 |
CN2119278U (zh) * | 1991-08-08 | 1992-10-21 | 西南铝加工厂 | 一种新型搭接式平面分流组合模 |
JPH07185648A (ja) * | 1993-12-27 | 1995-07-25 | Yano Eng:Kk | 細孔を有する押出材の押出加工用ダイス |
CN1342531A (zh) * | 2000-09-12 | 2002-04-03 | 郭丽仪 | 生产铝合金无缝管材的方法和相应模具组 |
CN201482815U (zh) * | 2009-07-06 | 2010-05-26 | 西南铝业(集团)有限责任公司 | 一种平面分流模 |
CN203044558U (zh) * | 2012-11-28 | 2013-07-10 | 昆山捷安特轻合金科技有限公司 | 结构改进的挤压模具 |
CN203044556U (zh) * | 2012-11-28 | 2013-07-10 | 昆山捷安特轻合金科技有限公司 | 新型挤压模具用上模 |
CN203751017U (zh) * | 2013-12-31 | 2014-08-06 | 昆山捷安特轻合金科技有限公司 | 结构改进的热挤压模具 |
Non-Patent Citations (1)
Title |
---|
李红英: "《金属塑性加工模具设计与制造》", 31 August 2009 * |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN107931347A (zh) * | 2017-11-28 | 2018-04-20 | 福建省南平铝业股份有限公司 | 一种小开口大承压面遮挡式铝挤压模具 |
CN111330994A (zh) * | 2020-04-02 | 2020-06-26 | 南充市长远铝业有限公司 | 一种铝管挤压成型模具、装置及铝管 |
CN111330994B (zh) * | 2020-04-02 | 2021-07-30 | 南充市长远铝业有限公司 | 一种铝管挤压成型模具及装置 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN208680203U (zh) | 一种用于大宽厚比型材连续挤压成型的组合式模腔 | |
CN201143522Y (zh) | 一种热挤压模具 | |
CN203044558U (zh) | 结构改进的挤压模具 | |
CN104741406A (zh) | 结构改进的热挤压模具 | |
CN203751017U (zh) | 结构改进的热挤压模具 | |
CN101837385B (zh) | 分级导流、多级分流的大型复杂截面模具 | |
CN204052415U (zh) | 一种一模双腔铝型材挤压模具 | |
CN201756587U (zh) | 一种生产镁牺牲阳极棒的双孔模具 | |
CN206184930U (zh) | 一种无缝管材的挤压模具 | |
CN204672719U (zh) | 一种管状铝型材挤压模具 | |
CN203751018U (zh) | 下模阻流结构改进的热挤压模具 | |
CN103101172A (zh) | 木塑钢芯共挤模具 | |
CN216420676U (zh) | 一种提高空芯工业型材焊合质量的热挤压模具 | |
CN104741405A (zh) | 下模阻流结构改进的热挤压模具 | |
CN209379676U (zh) | 一种异形铜管连续挤压设备 | |
CN104384226B (zh) | 矿山用空心导轨成型分流模具 | |
CN209395219U (zh) | 一种带钢衬的双层材料异型材挤出模具 | |
CN210475496U (zh) | 一种脆性钎料带的液态挤压成型装置 | |
CN203209463U (zh) | 一种小管径铝合金管材的无缝挤压模具 | |
CN219025440U (zh) | 一种冰箱把手热挤压模具 | |
CN103056186B (zh) | 一种挤压模具 | |
CN203209462U (zh) | 一种大管径铝合金管材无缝挤压模具 | |
CN203448647U (zh) | 一种生产铜扁线的模具 | |
CN203091448U (zh) | 超薄双面扣板铝型材挤压模具 | |
CN205413953U (zh) | 一种铝合金圆管热挤压模具 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20150701 |