一种水处理用碱式硫酸铁混凝剂的生产方法 Download PDFInfo
- Publication number
- CN1046923C CN1046923C CN89109236A CN89109236A CN1046923C CN 1046923 C CN1046923 C CN 1046923C CN 89109236 A CN89109236 A CN 89109236A CN 89109236 A CN89109236 A CN 89109236A CN 1046923 C CN1046923 C CN 1046923C
- Authority
- CN
- China
- Prior art keywords
- sulfate
- ferric sulfate
- water
- basic ferric
- water treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
一种用于水处理的三价铁混凝剂-碱式硫酸铁,是一种特殊硫酸盐。本发明以硫酸亚铁为原料,用空气中的氧气作氧化剂,经催化加工而成,成品是固体,这种混凝剂生产工艺流程简单,生产成本低廉。其具有三价铁混凝剂的各种优点:生成的矾花重、沉淀快,受水温(特别是低温)影响小,适用的pH值范围宽且不潮解,所以运输、贮存、使用都很方便。其可广泛应用于生活饮用水等各种给水和各种工业废水处理。
Description
本发明涉及一种适用于饮用水处理的新型三价铁盐混凝剂-碱式硫酸铁混凝剂的生产方法,此混凝剂也适用于工业给水、工业废水和生活污水处理。
采用地面水源的城市自来水厂,水处理时必须投加混凝剂。无机混凝剂有铝盐混凝剂和铁盐混凝剂两大类。铝是一种慢性毒物,城市自来水厂用铝盐混凝剂净水会增大自来水中的铝含量,由此产生对广大人民群众身体健康的危害。与铝盐混凝剂相比,铁盐混凝剂不仅卫生安全性好,混凝处理性能也好:生成的矾花密实,比重大,沉淀快;适用的PH值范围和水温范围宽;除有机物的性能好。所以城市自来水厂改用三价铁盐混凝剂有重要意义。问题是符合卫生质量要求的三价铁盐混凝剂产量少,货源缺。传统的三价铁盐混凝剂有氯化铁、硫酸铁、氯化硫酸铁等数种,由于种种原因,只有无水氯化铁在给水处理中得到了较多应用。生产无水氯化铁时氯气用量大,由于受到氯气货源的限制,所以产量不多。聚合硫酸铁混凝剂有货源,因其含有致癌物质亚硝酸盐,故城市自来水厂不能使用。
英国专利GB-1469193,专利名称为《生产碱式硫酸铁的方法和设备》。采用一台倾斜设置的回转管窑,窑管上缠电阻丝,用于加热窑内的物料和空气。硫酸亚铁从管窑上端加入,随着管窑的旋转逐渐下移,碱式硫酸铁产品从管窑下端排出。热空气从管窑下端送入,废气从上端排出。管窑内的空气温度上端最低为46℃,下端最高许可达480℃。该专利中未讲产品的用途和碱式硫酸铁产品的成分,仅从其举的两个例子中得知,产品内总铁[Fe(Ⅱ)+Fe(Ⅲ)]中Fe(Ⅲ)占89-91%,这Fe(Ⅲ)中有一部分是α-Fe2O3(铁红)。此产品溶解于水时,在浓度1%(以产品重量计)、PH=2的溶液中水不溶物量占产品重量的11%,这水不溶物应是铁红。由此可见,Fe(Ⅲ)内相当多一部分是Fe2O3,以Fe(OH)SO4存在的Fe(Ⅲ)要比89-91%小不少。从这些数据可知,这样质量的产品是不能用作净水剂的,谅必有其他用途。此生产方法存在的问题是,因窑管温度很高,而硫酸亚铁七水物的熔点是64℃,故硫酸亚铁进入窑中后会熔化烧结,而一旦烧结,硫酸亚铁颗粒内部的分子就难于与空气接触,产品中残余的Fe(Ⅱ)就多。管窑下端处温度在300℃以上,最高达480℃,根据化学手册,硫酸亚铁水合物变成无水物的温度是300℃,而硫酸亚铁一旦变成了无水物,就难于转
化成碱式硫酸铁了。此外,在这样高的温度下,碱式硫酸铁还会分解成Fe2O3。由于上述原因,此法生产出来的碱式硫酸铁产品纯度低。所以这种生产方法和设备不适用于碱式硫酸铁混凝剂的生产。
本发明的目的是提供一种生产成本低、使用效果好的碱式硫酸铁混凝剂的生产方法。参照无水氯化铁国家标准GB1621-79,用硫酸亚铁作原料生产碱式硫酸铁混凝剂时,硫酸亚铁中Fe2+的氧化率必须大于95%。
本发明的技术方案是:将硫酸亚铁用加热或日晒法进行脱水干燥,使其脱去部分结晶水变成疏松体;将疏松体在≤250℃的氧化温度下与空气中的氧气进行氧化反应,制成碱式硫酸铁。
本发明的效果:由于硫酸亚铁是在固体状态下用空气中的氧气进行氧化,所以工艺流程简单,生产成本低。此混凝剂在水处理工艺上不仅具有现有三价铁盐混凝剂的各种优点,如生成的矾花重、沉淀快,不受水温影响(特别是低温),适用PH值范围宽,而且此混凝剂是固体,没有潮解性,因此运输、贮存、使用方便。用此种方法生产的碱式硫酸铁混凝剂,产品质量安全可靠,可在生活饮用水等给水、污水和工业废水澄清及去色处理中广泛使用。
Claims (1)
1.一种水处理用碱式硫酸铁混凝剂的生产方法,其特征在于:
①将硫酸亚铁用加热或日晒法进行脱水干燥,使其脱去部分结晶水变成疏松体;
②将硫酸亚铁疏松体在≤250℃的氧化温度下与空气中的氧气进行氧化反应,制成碱式硫酸铁。