CN104669424A - 混凝土蒸养裂缝控制技术 - Google Patents
混凝土蒸养裂缝控制技术 Download PDFInfo
- Publication number
- CN104669424A CN104669424A CN201310632976.6A CN201310632976A CN104669424A CN 104669424 A CN104669424 A CN 104669424A CN 201310632976 A CN201310632976 A CN 201310632976A CN 104669424 A CN104669424 A CN 104669424A
- Authority
- CN
- China
- Prior art keywords
- concrete
- steam
- cured
- slab
- treatment technology
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及混凝土裂缝控制技术,公开了一种装配式住房预制钢筋混凝土板蒸养过程裂缝控制技术。在装配式住房预制钢筋混凝土板模具在自动行走轨道上依次经过按照指定工序制备,待上叶板的混凝土浇筑完成后,在进入蒸养窑蒸养之前,在模具向前行走过程中快速铺设一层薄膜材料,用以防止外层混凝土水分过快散发,从而有效防止裂缝。所述技术在流水线生产过程中完成对混凝土裂缝的处理,既不耽误生产线生产,又有效的控制了混凝土裂缝的产生。
Description
技术领域
本发明涉及一种混凝土裂缝控制技术,尤其涉及一种装配式住房预制钢筋混凝土板蒸养过程裂缝控制技术。
背景技术
混凝土裂缝是混凝土结构中普遍存在的一种现象。造成混凝土裂缝的主要原因有:
(1)混凝土浇筑后,大体积混凝土水化时产生的大量水化热得不到散发,使得外层混凝土与混凝土内部产生温度梯度,从而造成温度应力,出现裂缝;
(2)混凝土浇筑后,混凝土表面水分蒸发过快,造成毛细管中产生较大的负压而使混凝土体积急剧收缩,而此时混凝土强度低,不能抵抗这种变形应力而导致开裂;
(3)此外水泥或者粉砂用量过多,或者水灰比例不当,水中存在盐分和腐蚀酸等均可导致混凝土出现裂缝。
裂缝的存在不仅会影响建筑物的寿命、外形美观,还会使内部的钢筋或其他材料腐蚀,降低材料的稳定性从而影响建筑物的承载能力和抗渗能力。
预制钢筋混凝土板可构建成单层或者多层的装配式住房,若混凝土出现裂缝势必会导致装配式住房的美观和防水、稳定等功能受损,因此要在预制钢筋混凝土板制备过程中控制裂缝的产生。装配式住房预制钢筋混凝土板是自动生产线生产,一切工序均在自动行走轨道上操作完成,在预制板的混凝土浇筑完毕后进入蒸养窑之前,增加铺设一层薄膜材料,可有效控制混凝土裂缝产生。
发明内容
为了控制混凝土裂缝的产生,本发明提供了一种混凝土蒸养裂缝控制技术。采用铺设塑料薄膜的方法,即在装配式住房预制钢筋混凝土板的上叶板浇筑完毕后铺设一层薄膜材料,以控制预制板构件水分过快散发,有效控制混凝土裂缝。
为了实现上述目的,本发明是采用以下技术方法实现的:
一种混凝土蒸养裂缝处理技术,该技术是在装配式住房预制钢筋混凝土板模具在自动行走轨道上依次经过按照指定工序制备,待上叶板的混凝土浇筑完成后,在进入蒸养窑蒸养之前,在模具向前行走过程中快速铺设一层薄膜材料,用以防止外层混凝土水分过快散发,从而有效防止裂缝。
所述薄膜材料是厚度小于1mm的塑料薄膜,成卷状放置,其铺设方向与模具行走方向相反。塑料薄膜大小须大于模具内预制钢筋混凝土板的大小,借助刚刚浇筑的混凝土的水分塑料薄膜可与预制钢筋混凝土板紧密结合,边缘结合处须压实。
本发明的有益效果是,所述混凝土蒸养裂缝控制技术能够满足装配式住房预制钢筋混凝土板自动生产线生产,在流水线生产过程中完成对混凝土裂缝的处理,既不耽误生产线生产,又有效的控制了混凝土裂缝的产生。
附图说明
附图为混凝土蒸养裂缝控制技术的示意图。
附图中1为装配式住房预制钢筋混凝土板自动生产线自动行走轨道,2为预制钢筋混凝土板模具,3为塑料薄膜卷,4为蒸养窑。其中塑料薄膜卷铺设的方向与模板行走的方向相反。
具体实施方式
下面结合附图对本发明做进一步说明。
如附图所示,装配式住房预制钢筋混凝土板是模具在自动行走轨道上依次经过按照指定工序制备,待上叶板的混凝土浇筑完成后15-25min,在模具向前行走过程中快速铺设一层厚度小于1mm的塑料薄膜,其铺设方向与模具行走方向相反,塑料薄膜可借助新浇筑混凝土的水分与之紧密贴合,四周用力压实,塑料薄膜铺设完成后进入蒸养窑蒸养。塑料薄膜呈卷装放置,铺设完成一块预制板后,快速隔开,在进行下一块预制板塑料薄膜的铺设。
由以上步骤可知,混凝土经过塑料薄膜的覆盖有效阻止了水分的过快散发,从根本上解决了混凝土在蒸养过程中产生裂缝的问题。并且采用塑料薄膜卷沿模具行走反方向铺设的方法,可充分配合自动生产线工作。
Claims (7)
1.混凝土蒸养裂缝处理技术,是一种装配式住房预制钢筋混凝土板蒸养过程裂缝控制技术,其特征在于,采用铺设塑料薄膜的方法,即在装配式住房预制钢筋混凝土板制备的行走过程中,待上叶板混凝土浇筑完毕后进入蒸养窑之前铺设一层薄膜材料。
2.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的装配式住房预制钢筋混凝土板制备过程是在自动行走轨道上进行的。
3.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的上叶板混凝土浇筑完成后15-25min铺设薄膜材料。
4.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的薄膜材料铺设方向与预制钢筋混凝土板行走方向相反。
5.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的铺设薄膜材料的大小须大于钢筋混凝土板的大小。
6.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的薄膜材料通过上叶板混凝土的水分与之紧密结合,四周用力压实。
7.如权利要求1所述的混凝土蒸养裂缝处理技术,其特征在于,所述的薄膜材料为厚度小于1mm的塑料薄膜,呈卷状放置。