CN104614944B - A kind of negative pressure drying silk-screen manufacturing method of screen - Google Patents

A kind of negative pressure drying silk-screen manufacturing method of screen Download PDF

Info

Publication number
CN104614944B
CN104614944B CN201510019859.1A CN201510019859A CN104614944B CN 104614944 B CN104614944 B CN 104614944B CN 201510019859 A CN201510019859 A CN 201510019859A CN 104614944 B CN104614944 B CN 104614944B
Authority
CN
China
Prior art keywords
halftone
negative pressure
screen
silk
photosensitive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201510019859.1A
Other languages
Chinese (zh)
Other versions
CN104614944A (en
Inventor
何忠亮
丁华
赖灶钦
张�林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Dinghua Xintai Technology Co ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510019859.1A priority Critical patent/CN104614944B/en
Publication of CN104614944A publication Critical patent/CN104614944A/en
Application granted granted Critical
Publication of CN104614944B publication Critical patent/CN104614944B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of production methods of negative pressure drying silk-screen halftone: forming uniform pressure to photosensitive matter to be dried on halftone using atmospheric pressure under negative pressure state, rapid draing forms the photosensitive matter face of hither plane under the effect of this pressure, to obtain good halftone printing face;The problems such as silk-screen halftone made using the present invention, graphic edge is neat, smooth, no sawtooth, dog tooth, printed pattern is apparent, accurate.

Description

A kind of negative pressure drying silk-screen manufacturing method of screen
[technical field]
The present invention relates to the production method of silk-screen manufacturing method of screen more particularly to a kind of negative pressure drying silk-screen halftone and Use the silk-screen halftone of high precision made by this method.
[background technique]
High-accuracy halftone is needed to support in current accurate silk-screen industry, silk-screen high-precision product.It is coated in halftone Emulsion or after attaching photographic film, in the drying process emulsion or photographic film can because of the volatilization of moisture content and solvent, And shrinkage phenomenon is generated, photosensitive matter layer 13 and printing face 12 deform after dewatering as shown in Figure 1:, and film data details is caused to lose It loses, causes 11 figure of print material on stock 10 irregular, the problems such as graphic edge distortion, sawtooth occur.
[summary of the invention]
To solve the above problems, the technical solution adopted by the present invention are as follows: using atmospheric pressure under negative pressure state on halftone to Dry photosensitive matter forms uniform pressure, and rapid draing forms the photosensitive matter face of hither plane under the effect of this pressure, to obtain Obtain good halftone printing face.
Device of the present invention includes the level table for carrying halftone, the component of drying and negative pressure;
Production method of the invention, including following steps:
Step 1) prepares the silk-screen halftone to be dried of a blank adhering sense light quality;
Its printing is placed on the level table of the component of drying and negative pressure by step 2) up, heating, drying halftone;
Step 3) coats photosensitive matter in printing face again;
Its printing is placed on the level table of the device of drying and negative pressure by step 4) down, is applied to photosensitive matter negative Pressure, heating, drying;
If the photosensitive matter thickness of step 5) is insufficient, then dries to after the photosensitive matter of halftone coating through step 4;
Halftone is exposed, is developed by step 6), then is dried through step 4;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the level table of the carrying halftone is thermally conductive or passes Hot material;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the level table of the carrying halftone has release characteristic;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the drying, negative pressure component include: seal frame, close Sealing skin, ventilating interlayer, air extractor, heating device;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the stripper rubber, ventilating interlayer have release characteristic;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the ventilating interlayer is gas permeable material, in negative pressure state It is lower to be easy to exclude air;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the heating device is infrared heating device;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the heating device is hot plate heating device;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the photosensitive matter is emulsion;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein the photosensitive matter is photographic film;
The method of above-mentioned negative pressure drying silk-screen halftone, wherein when the described photosensitive matter thickness deficiency, then apply photosensitive Matter, number are 2 times or 2 times or more.
[Detailed description of the invention]
It is described in detail referring to following attached drawing to made by non-limiting case study on implementation by reading, other spies of the invention Sign, objects and advantages will become more apparent upon.
It is the halftone of conventional method production shown in Fig. 1, the section view of halftone and its printing product after exposure, development, drying Figure.
It is the structure chart of negative pressure drying silk-screen halftone equipment of the present invention shown in Fig. 2.
It is the flow chart of negative pressure drying silk-screen manufacturing method of screen of the present invention shown in Fig. 3.
It is the halftone made using the present invention and its cross-sectional view for printing product shown in Fig. 4.
Label declaration in attached drawing
10 stock, 11 print material, 12 printing face, 13 15 printing surface of photosensitive 14 grenadine of matter, 20 seal frame, 21 sealant 26 air extractor of skin 22 ventilating interlayer, 23 halftone, 24 level table, 25 heating device, 27 body fuselage
[specific embodiment]
Case study on implementation one
Fig. 3 gives a kind of production method flow chart of negative pressure drying silk-screen halftone of the invention, and Fig. 2 gives by this hair The structure of the negative pressure drying equipment of bright production 2,3 is illustrated with reference to the accompanying drawing:
As shown in figure 3, a kind of production method detailed process of negative pressure drying silk-screen halftone is as follows:
1) prepare the silk-screen halftone S1 to be dried of a blank attachment emulsion;2) its printing has been placed on up The level table of the device of drying and negative pressure, heating, drying S2;3) emulsion S3 is coated in printing face;4) its printing is faced Under be placed on drying and negative pressure device level table, to emulsion apply negative pressure, heating, drying S4;If 5) emulsion Thickness degree is insufficient, then applies emulsion, dries S5 through step 4;6) by halftone exposure, development S6;6) it is dried again through step 4 S7。
In S1, the silk-screen halftone for selecting blank clean, first oil removing degreasing keeps the cleanliness of grenadine;It is roasting with low temperature afterwards 45-55 DEG C of case is dried for standby.
Then emulsion is coated on clean halftone, the coated area on halftone is unilateral 2cm bigger than stock.
In S2, start the infrared heating device 25 of negative pressure drying machine, after 24 temperature of level table reaches 50 DEG C, by net 23 printings of version are placed on up on the level table of negative pressure drying machine, are dried 3-5 minutes;
In S3, emulsion is coated again in 23 printing face of halftone;
In S4,23 printing of halftone is placed on down on the level table 24 of negative pressure drying machine, then there is release characteristic Ventilating interlayer 22 be placed on 23 printing surface of halftone, after seal frame 20 is covered to and is started negative pressure device 26, coat thoughts at this time For the grenadine of X-ray emulsion X under 21 negative pressure pressure of stripper rubber, moisture content and solvent in emulsion run through ventilating interlayer 22 It is discharged by the pipeline of negative pressure device, the emulsion after 3-4 minutes on halftone is dry to be completed, and is closed negative pressure device 26, is opened close It seals frame 20 and takes out halftone 23.
In S5, if sensitive emulsion layer thickness not up to requires, just come again by S3-S4 one time, until emulsion thickness Until degree reaches requirement.
In S6, emulsion will be coated with and dried halftone exposure, development.
In S7, after negative pressure drying machine level table temperature reaches 50 DEG C, 23 printing of halftone is placed on negative pressure downwards On the level table 24 of drying machine, then there is the ventilating interlayer 22 of release characteristic to be placed on screen painting face, after by seal frame 20 It covers and starts negative pressure device 26, develop has the halftone of figure under 21 negative pressure pressure of stripper rubber at this time, on halftone, schemes The moisture content in shape area runs through ventilating interlayer 22 and is discharged by the pipeline of negative pressure device, and halftone is dry after 8-10 minutes completes, and closes Negative pressure device 26 opens seal frame and takes out halftone 23.
Thus the problems such as product of the screen painting of case study on implementation production, graphic edge is neat, smooth, no sawtooth, dog tooth, It is apparent using printed pattern, accurate.Referring to attached drawing 4.
Case study on implementation two
In Fig. 3, a kind of production method process of negative pressure drying silk-screen halftone also gives second of case study on implementation, under Face is illustrated in conjunction with attached drawing 2, Fig. 3:
The difference of the implementation case and case study on implementation one is the difference of photosensitive material, and requires no S2, S3 and S5.
In S1, the silk-screen halftone for selecting blank clean, first oil removing degreasing keeps the cleanliness of grenadine;It is roasting with low temperature afterwards 45-55 DEG C of case is dried for standby.
Then in cleaning and dried halftone, one layer of water mist is sprayed, uniformly moistens grenadine, then the net in printing face Yarn attaches photographic film, and photographic film area is unilateral 2cm bigger than stock.
In S4, start the infrared heating device 25 of negative pressure drying machine, after 24 temperature of level table reaches 50 DEG C, by net The printing of version 23 is placed on down on the level table 24 of negative pressure drying machine, then ventilating interlayer 22 is placed on screen painting face, after Seal frame 20 is covered and starts negative pressure device 26, is pasted with the grenadine of photographic film at this time in 21 negative pressure pressure of stripper rubber Under, the moisture content in photographic film runs through ventilating interlayer 22 and is discharged by the pipeline of negative pressure device, after 3-4 minutes on halftone Photographic film is dry to be completed, and negative pressure device 26 is closed, and is opened seal frame and is taken out halftone 23.
S5 is required no, directly carries out operation by the S6 of case study on implementation one.
Thus the problems such as product of the screen painting of case study on implementation production, graphic edge is neat, smooth, no sawtooth, dog tooth, It is apparent using printed pattern, accurate.Referring to attached drawing 4.
The halftone cross-sectional view made shown in Fig. 4 of method of the invention, from fig. 4, it can be seen that the emulsion of this halftone Or the graphic edge of photographic film production is neat, smoothly.
Specific embodiments of the present invention are described above.It is to be appreciated that the invention is not limited to above-mentioned Particular implementation, devices and structures not described in detail herein should be understood as gives reality with the common mode in this field It applies;Those skilled in the art can make various deformations or amendments within the scope of the claims, this has no effect on of the invention Substantive content.

Claims (6)

1. a kind of production method of negative pressure drying silk-screen halftone, it is characterised in that:
The method forms uniform pressure to photosensitive matter to be dried on halftone using atmospheric pressure under negative pressure state, in this pressure The photosensitive matter face that lower rapid draing forms hither plane is acted on, to obtain good halftone printing face;
The method is made of following step:
Step 1) prepares the silk-screen halftone to be dried of a blank adhering sense light quality: the silk-screen halftone for selecting blank clean, first Oil removing degreasing keeps the cleanliness of grenadine;Afterwards with low temperature oven 45-55 DEG C be dried for standby;
Its printing is placed on the level table of dry and negative pressure component by step 2) up, heating, dry halftone;Its In, the level table is thermally conductive or heat-transfer matcrial and the level table has release characteristic, the group of the drying and negative pressure Part includes: seal frame, stripper rubber, ventilating interlayer, air extractor, heating device;The stripper rubber, ventilating interlayer have Release characteristic;The ventilating interlayer is poromerics, is easy to exclude air under negative pressure state;
Step 3) coats photosensitive matter in printing face again;
Its printing is placed on the level table of dry and negative pressure component by step 4) down, then there is the saturating of release characteristic Air-casing is placed on the printing surface of halftone, applies negative pressure, heat drying to photosensitive matter using the component of the drying and negative pressure;
If the photosensitive matter thickness of step 5) is insufficient, then to dry through step 4 after the photosensitive matter of halftone coating;
Halftone is exposed, is developed by step 6), then dry through step 4.
2. according to the method described in claim 1, it is characterized by: the heating device is infrared heating device.
3. according to the method described in claim 1, it is characterized by: the heating device is hot plate heating device.
4. according to the method described in claim 1, it is characterized by: the photosensitive matter is emulsion in step 1).
5. according to the method described in claim 1, it is characterized by: the photosensitive matter is photographic film in step 1).
6. according to the method described in claim 1, it is characterized by: in step 5), when the described photosensitive matter thickness deficiency, then Photosensitive matter is applied, number is 2 times or more.
CN201510019859.1A 2015-01-15 2015-01-15 A kind of negative pressure drying silk-screen manufacturing method of screen Active CN104614944B (en)