CN104370543B - 低温烧结超低介电常数微波介电陶瓷Ca3LaSmB4O12 - Google Patents
低温烧结超低介电常数微波介电陶瓷Ca3LaSmB4O12 Download PDFInfo
- Publication number
- CN104370543B CN104370543B CN201410627241.9A CN201410627241A CN104370543B CN 104370543 B CN104370543 B CN 104370543B CN 201410627241 A CN201410627241 A CN 201410627241A CN 104370543 B CN104370543 B CN 104370543B
- Authority
- CN
- China
- Prior art keywords
- microwave
- hours
- dielectric
- lasmb
- dielectric ceramic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (1)