CN104276358A - 塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱 - Google Patents
塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱 Download PDFInfo
- Publication number
- CN104276358A CN104276358A CN201310293767.3A CN201310293767A CN104276358A CN 104276358 A CN104276358 A CN 104276358A CN 201310293767 A CN201310293767 A CN 201310293767A CN 104276358 A CN104276358 A CN 104276358A
- Authority
- CN
- China
- Prior art keywords
- porcelain
- mould
- plastic
- ceramic
- lath
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
集装箱使用寿命不过20年,都要进行焊接,价格也贵。塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱,先用塑料熔浆、陶瓷布烧制成塑瓷泡沫板,再将塑瓷泡沫板用螺栓组装各种塑瓷集装箱,不用焊接,不但节约成本,还提高制箱速度,及增强安全性能;塑瓷板用的陶瓷布为几元/M2,阻燃塑料万元/吨,令塑瓷泡沫板价格比钢板低。塑瓷泡沫板寿命百年,其塑料不会锈蚀,面层陶瓷布阻挡抗紫外线,保护第二层塑料;陶瓷布富有弹性提高其抗撞击力;其泡沫使它的抗弯比瓷玻板强几倍,而容重可小于0.3g/cm3。塑瓷集装箱百年寿命,价格低,各项性能都超过目前各种类的集装箱,所以塑瓷集装箱必然会,很快就占领钢板、铝板、玻璃钢板的集装箱市场。
Description
目前的集装箱用钢板、铝板、玻璃钢板生产,使用寿命不过20年,就算是玻璃钢集装箱,也要进行框架焊接,价格也贵。
本技术提出的塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱,简称塑瓷集装箱,不用钢板、铝板、玻璃钢板,能解决上述问题。塑为塑料,瓷为陶瓷布。
塑瓷集装箱,其有益效果是,无需焊接,降低成本,抗撞击,不用金属,百年使用,减轻重量,防水,抗酸碱,保温性能强。
塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱,其解决技术问题所采用的技术方案是,用机具使陶瓷布,或陶瓷布条通过塑料熔浆,塑料熔浆可有粘合剂,塑料可为阻燃塑料,令塑料熔浆穿过陶瓷布孔,刮除多余塑料熔浆,令塑料熔浆包襄陶瓷布成为塑料熔浆陶瓷布,或成为塑料熔浆陶瓷布条;多块塑料熔浆陶瓷布重叠粘成塑料熔浆陶瓷布板;多条塑料熔浆陶瓷布条重叠粘成塑料熔浆陶瓷布板条(1);冷却后获得塑瓷布板、塑瓷布板条;塑瓷板条等距离开窄缝(2),窄缝宽度等于板条厚度,窄缝长度等于板条宽度一半;将多条板条的窄缝对扦,用粘合剂粘成为板条框架(3);将板条框架放在塑瓷板上,再在板条框架上放塑瓷板,用粘合剂粘成为塑瓷泡沫板(4);板条框架与塑瓷板,或与塑瓷板条交错重叠,用粘合剂粘成塑瓷多层泡沫板(5),或粘成塑瓷多层泡沫板条;塑瓷多层泡沫板条,等距离放在塑瓷泡沫板上,用粘合剂粘成为柱式塑瓷泡沫板(6);将按设计开孔或不开孔的塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条,可放进炉加热令塑料粘紧,冷却后获得塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条;用塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条,代替钢板、铝板、玻璃钢板组装各种塑瓷集装箱(7):例如,a.取塑瓷多层泡沫板条用螺栓组装成框架,取柱式塑瓷泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为内柱式或外柱式塑瓷集装箱;b.取塑瓷多层泡沫板条用螺栓组装成框架,取塑瓷泡沫板做侧壁、端面、箱底、箱项、箱门,用螺栓组装在框架上,成为薄壳式塑瓷集装箱;c.取塑瓷多层泡沫板条用螺栓组装成框架,取塑瓷多层泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为玻璃钢式塑瓷集装箱;塑瓷集装箱进行装锁等相关工艺,从而使塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱得以运行。如图1
现结合原理介绍塑瓷集装箱:
陶瓷布耐1000℃高温,所以当塑料粉用300℃制成塑瓷板时,陶瓷布仍保持原来的抗拉性能,令塑瓷板不会断裂;在陶瓷布和塑料的比例上,以陶瓷布为主,塑料作为粘结剂使用,塑料粉厚度小于陶瓷布厚;塑料薄片具有弹性,当塑料薄片受到撞击时,撞击力就迅速传到陶瓷线条上,被陶瓷线条吸收,令塑瓷板保持完整不会断裂;塑料包裹陶瓷布构成塑料网络,塑料网络、陶瓷布网络互相紧密包裹,加强塑瓷板抗撞击力;塑料抗酸碱性,使塑瓷板防锈蚀性比钢铁强,只要不受过于强的撞击力,寿命百年;塑瓷泡沫板的保温隔热性能比玻璃钢强;重量相同时,塑瓷泡沫板抗弯比塑料板强几倍,而容重可小于0.3g/cm3。用粘合剂,使塑料熔浆不脱离陶瓷;用阻燃塑料,能提高塑瓷集装箱的阻燃性能。综上所述,用塑瓷泡沫板做集装箱,各项性能都比用钢板、铝板、玻璃钢板好很多。塑瓷泡沫板连接处可塾胶片,加强密封度。
塑瓷板用的陶瓷布为几元/M2,阻燃塑料粉万元/吨,令塑瓷泡沫板价格比钢板低几倍;塑瓷集装箱制作不用焊接,不但节约成本,还提高制箱速度,及增强安全性能。
说明书附图说明
图1、塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱
1塑料熔浆陶瓷布板条,2窄缝,3板条框架;4塑瓷泡沫板;5塑瓷多层泡沫板,6柱式塑瓷泡沫板,7塑瓷集装箱。
Claims (1)
1.塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱,其特征是,用机具使陶瓷布,或陶瓷布条通过塑料熔浆,塑料熔浆可有粘合剂,塑料可为阻燃塑料,令塑料熔浆穿过陶瓷布孔,刮除多余塑料熔浆,令塑料熔浆包裹陶瓷布成为塑料熔浆陶瓷布,或成为塑料熔浆陶瓷布条;多块塑料熔浆陶瓷布重叠粘成塑料熔浆陶瓷布板;多条塑料熔浆陶瓷布条重叠粘成塑料熔浆陶瓷布板条;冷却后获得塑瓷布板、塑瓷布板条;塑瓷板条等距离开窄缝,窄缝宽度等于板条厚度,窄缝长度等于板条宽度一半;将多条板条的窄缝对扦,用粘合剂粘成为板条框架;将板条框架放在塑瓷板上,再在板条框架上放塑瓷板,用粘合剂粘成为塑瓷泡沫板;板条框架与塑瓷板,或与塑瓷板条交错重叠,用粘合剂粘成塑瓷多层泡沫板,或粘成塑瓷多层泡沫板条;塑瓷多层泡沫板条,等距离放在塑瓷泡沫板上,用粘合剂粘成为柱式塑瓷泡沫板;将按设计开孔或不开孔的塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条,可放进炉加热令塑料粘紧,冷却后获得塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条;用塑瓷泡沫板、柱式塑瓷泡沫板、塑瓷多层泡沫板、塑瓷多层泡沫板条,代替钢板、铝板、玻璃钢板组装各种塑瓷集装箱:例如,a.取塑瓷多层泡沫板条用螺栓组装成框架,取柱式塑瓷泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为内柱式或外柱式塑瓷集装箱;b.取塑瓷多层泡沫板条用螺栓组装成框架,取塑瓷泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为薄壳式塑瓷集装箱;c.取塑瓷多层泡沫板条用螺栓组装成框架,取塑瓷多层泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为玻璃钢式塑瓷集装箱;塑瓷集装箱进行装锁等相关工艺,从而使塑料熔浆生产隔热防腐防水抗撞击寿命百年的塑瓷集装箱得以运行。