CN104249866A - 玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱 - Google Patents
玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱 Download PDFInfo
- Publication number
- CN104249866A CN104249866A CN201310289240.3A CN201310289240A CN104249866A CN 104249866 A CN104249866 A CN 104249866A CN 201310289240 A CN201310289240 A CN 201310289240A CN 104249866 A CN104249866 A CN 104249866A
- Authority
- CN
- China
- Prior art keywords
- glass
- cotton
- glass powder
- powder paste
- asbestos cloth
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
集装箱用钢板、铝板、玻璃钢板生产,使用寿命不过20年,都要进行焊接,价格也贵。玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱,先用玻璃粉浆、石棉布烧制成玻棉泡沫板,再将玻棉泡沫板用螺栓组装各种玻棉集装箱,不用焊接,不但节约成本,还提高制箱速度,及增强安全性能;玻棉板用的耐高温石棉布为1元/m2,玻璃粉每吨千元,令玻棉泡沫板价格比钢板低几倍。玻棉泡沫板寿命百年,其玻璃坚硬耐磨、不会锈蚀、抗紫外线;石棉布富有弹性提高其抗撞击力;其泡沫使它的抗弯比陶瓷板强几倍,而容重可小于0.3g/cm3。玻棉集装箱百年寿命,价格低,各项性能都超过目前各种类的集装箱,所以玻棉集装箱必然会,很快就占领钢板、铝板、玻璃钢板的集装箱市场。
Description
目前的集装箱,用钢板、铝板、玻璃钢板生产,使用寿命不过20年,就算是玻璃钢集装箱,也要进行框架焊接,价格也贵。
本技术提出的玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱,简称玻棉集装箱,不用钢铁、铝、玻璃钢,能解决上述问题。玻为玻璃,棉为石棉布。
玻棉集装箱,其有益效果是,无需焊接,降低成本,抗撞击,不用金属,百年使用,减轻重量,防水,抗酸碱,保温性能强。
玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱,其解决技术问题所采用的技术方案是,用机具使石棉布,或石棉布条通过玻璃粉浆,玻璃粉浆可加粘合剂,令玻璃粉浆穿过石棉布孔,刮除多余玻璃粉浆,令玻璃粉浆包裹石棉布成为玻璃粉浆石棉布,或成为玻璃粉浆石棉布条;多块玻璃粉浆石棉布重叠粘成玻璃粉浆石棉布板;多条玻璃粉浆石棉布条重叠粘成玻璃粉浆石棉布板条(1),玻璃粉浆石棉布板条等距离开窄缝(2),窄缝宽度等于板条厚度,窄缝长度等于板条宽度一半;将多条板条的窄缝对扦,粘成为板条框架(3);将板条框架放在玻璃粉浆石棉布板上,再在板条框架上放玻璃粉浆石棉布板,粘成为玻璃粉浆石棉布泡沫板(4);板条框架与玻璃粉浆石棉布板,或与玻璃粉浆石棉布板条交错重叠,粘成玻璃粉浆石棉布多层泡沫板(5),或粘成玻璃粉浆石棉布多层泡沫板条;玻璃粉浆石棉布多层泡沫板条,等距离放在玻璃粉浆石棉布泡沫板上,粘成为柱式玻璃粉浆石棉布泡沫板(6);将按设计开孔或不开孔的玻璃粉浆石棉布泡沫板、柱式玻璃粉浆石棉布泡沫板、玻璃粉浆石棉布多层泡沫板、玻璃粉浆石棉布多层泡沫板条,干燥后放进窑炉烧制,令玻璃粉熔粘,冷却后获得玻棉泡沫板、柱式玻棉泡沫板(7)、玻棉多层泡沫板、玻棉多层泡沫板条;用玻棉泡沫板、柱式玻棉泡沫板、玻棉多层泡沫板、玻棉多层泡沫板条,代替钢板、铝板、玻璃钢板组装各种玻棉集装箱(8):例如,a.取玻棉多层泡沫板条用螺栓组装成框架,取柱式玻棉泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为内柱式或外柱式玻棉集装箱;b.取玻棉多层泡沫板条用螺栓组装成框架,取玻棉泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为薄壳式玻棉集装箱;c.取玻棉多层泡沫板条用螺栓组装成框架,取玻棉多层泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为玻璃钢式玻棉集装箱;玻棉集装箱进行装锁等相关工艺,从而使玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱得以运行。如图1
现结合原理介绍玻棉集装箱:
石棉布耐1200℃高温,所以当玻璃粉经700℃制成玻棉板时,石棉布仍保持原来的抗拉性能,令玻棉板不会断裂;在石棉布和玻璃的比例上,以石棉布为主,玻璃作为粘结剂使用,玻璃浆厚度小于石棉布厚;玻璃薄片具有弹性,当玻璃薄片受到撞击时,撞击力就迅速传到石棉线条上,被石棉线条吸收,令玻棉板保持完整不会断裂;玻璃包裹石棉布构成玻璃网络,玻璃网络、石棉布网络互相紧密包裹,加强玻棉板抗撞击力;玻璃抗酸碱性,硬度比钢铁高,使玻棉板抗磨性、防锈蚀性比钢铁强,只要不受过于强的撞击力,寿命千年;玻棉泡沫板的保温隔热性能比玻璃钢强;重量相同时,玻棉泡沫板抗弯比玻璃板强几倍,而容重可小于0.3g/cm3。玻璃粉浆加粘合剂,使玻璃粉浆不脱离石棉布;综上所述,用玻棉泡沫板做集装箱,各项性能都比用钢板、铝板、玻璃钢板好很多。玻棉泡沫板连接处可塾胶片,加强密封度。
玻棉板用的耐高温石棉布为1元/M2,玻璃粉每吨千元,令玻棉泡沫板价格比钢板低几倍;玻棉集装箱制作不用焊接,不但节约成本,还提高制箱速度,及增强安全性能。
说明书附图说明
图1、玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱
1玻璃粉浆石棉布板条,2窄缝,3板条框架,4玻璃粉浆石棉布泡沫板,5玻璃粉浆石棉布多层泡沫板,6柱式玻璃粉浆石棉布泡沫板,7柱式玻棉泡沫板,8玻棉集装箱。
Claims (1)
1.玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱,其特征是,用机具使石棉布,或石棉布条通过玻璃粉浆,玻璃粉浆可加粘合剂,令玻璃粉浆穿过石棉布孔,刮除多余玻璃粉浆,令玻璃粉浆包裹石棉布成为玻璃粉浆石棉布,或成为玻璃粉浆石棉布条;多块玻璃粉浆石棉布重叠粘成玻璃粉浆石棉布板;多条玻璃粉浆石棉布条重叠粘成玻璃粉浆石棉布板条,玻璃粉浆石棉布板条等距离开窄缝,窄缝宽度等于板条厚度,窄缝长度等于板条宽度一半;将多条板条的窄缝对扦,粘成为板条框架;将板条框架放在玻璃粉浆石棉布板上,再在板条框架上放玻璃粉浆石棉布板,粘成为玻璃粉浆石棉布泡沫板;板条框架与玻璃粉浆石棉布板,或与玻璃粉浆石棉布板条交错重叠,粘成玻璃粉浆石棉布多层泡沫板,或粘成玻璃粉浆石棉布多层泡沫板条;玻璃粉浆石棉布多层泡沫板条,等距离放在玻璃粉浆石棉布泡沫板上,粘成为柱式玻璃粉浆石棉布泡沫板;将按设计开孔或不开孔的玻璃粉浆石棉布泡沫板、柱式玻璃粉浆石棉布泡沫板、玻璃粉浆石棉布多层泡沫板、玻璃粉浆石棉布多层泡沫板条,干燥后放进窑炉烧制,令玻璃粉熔粘,冷却后获得玻棉泡沫板、柱式玻棉泡沫板、玻棉多层泡沫板、玻棉多层泡沫板条;用玻棉泡沫板、柱式玻棉泡沫板、玻棉多层泡沫板、玻棉多层泡沫板条,代替钢板、铝板、玻璃钢板组装各种玻棉集装箱:例如,a.取玻棉多层泡沫板条用螺栓组装成框架,取柱式玻棉泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为内柱式或外柱式玻棉集装箱;b.取玻棉多层泡沫板条用螺栓组装成框架,取玻棉泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为薄壳式玻棉集装箱;c.取玻棉多层泡沫板条用螺栓组装成框架,取玻棉多层泡沫板做侧壁、端面、箱底、箱顶、箱门,用螺栓组装在框架上,成为玻璃钢式玻棉集装箱;玻棉集装箱进行装锁等相关工艺,从而使玻璃粉生产隔热防腐防水抗撞击寿命百年的玻棉集装箱得以运行。