CN104120600A - Water cleaning process for artificial leather clothing - Google Patents
Water cleaning process for artificial leather clothing Download PDFInfo
- Publication number
- CN104120600A CN104120600A CN201410309716.XA CN201410309716A CN104120600A CN 104120600 A CN104120600 A CN 104120600A CN 201410309716 A CN201410309716 A CN 201410309716A CN 104120600 A CN104120600 A CN 104120600A
- Authority
- CN
- China
- Prior art keywords
- fur clothing
- saved
- drying
- artificial
- leather clothing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a water cleaning process for artificial leather clothing. The process comprises the following steps: putting the artificial leather clothing into a drying machine; heating and drying for 10-20 minutes at the temperature of 50-55 DEG C; uniformly spraying an aid solution onto the leather clothing by using a high-pressure water gun to moisten the leather clothing; closing a door of the drying machine to dry for 10-20 minutes; stopping the drying; beating by using cold air for 10-30 minutes. Compared with the conventional operating method, the water cleaning process for the artificial leather clothing has the advantages that high economical efficiency is realized, the number of needed equipment and personnel is small, labor force is saved, and the production cost is saved more importantly. The operating method has very remarkable economic benefits during production of 400,000 PU leather clothing, namely, water is saved by 236.8t, electricity is saved by 30,800 degrees, steam is saved by 375t, the cost is saved by 115,095.80 yuan, and the working efficiency is increased by 1.6 times.
Description
Technical field
The present invention relates to garment technology field, relate in particular to a kind of artificial fur clothing washing process.
Background technology
Artificial fur clothing washing is a step very important in artificial fur clothing production process, and the quality of its washing effect directly affects the quality of fur clothing.
The method of existing artificial fur clothing washing is: after clear water 15 minutes is fully moistening, then adds auxiliary agent and be warmed up to 55 degree, rerun out cylinder, dewatered drying, dries and need 2 hours, and temperature is controlled at 55 degree to 60 degree left and right.The consumption of water and not science of the consumption of steam, drying time length will be wasted heat energy, and also easily occur the high and low variable effect fur clothing of temperature surface quality, and temperature is high occurs the cortex surface scald of creasing, the low drying time of temperature is long, and cortex surface is causing that ash wound waits defect.Every of old maneuver need to water 6.25KG, needs electricity consumption 0.15 to spend, and uses steam 1.25kg, does for each person every day 750.Though can do, its water wasting, to take electricity, expense vapour, expense artificial.
Summary of the invention
In order to solve the deficiency of existing artificial fur clothing method for washing, the artificial fur clothing washing process that provides a kind of water-saving, power saving and saving artificial is provided the object of the invention.
The technical scheme that the present invention takes is:
The step of artificial fur clothing washing process of the present invention is as follows: first artificial fur clothing is put into dryer, then heating, drying 10-20min, bake out temperature is 50-55 DEG C, then with giant, compounding agent solution is evenly sprayed on fur clothing, make fur clothing moistening, shut again and dry gate and dry 10-20min, then stop drying, then beat 10-30min with cold wind.
Described dryer is roller dryer.
Preferably first artificial fur clothing is put into dryer, then heating, drying 15min.
Described auxiliary agent is ternary block silicone oil (SRS), and solubility is 25%.The spray flux of compounding agent solution is 5% of fur clothing weight.
After preferred fur clothing is moistening, then shut oven dry gate oven dry 15min.Cold wind is beaten 20min.
Good effect of the present invention is as follows:
The present invention has scientifically analyzed the emphasis of fur clothing washing, is to solve the consumption of water and the consumption of steam, and water is used to such an extent that more fumy consumption is just larger, while adjusting to a suitable crunode, will play the effect of water saving joint vapour.See the quality of product, outward appearance reaches cortex washing requirement again, and lining, under moist rollers running effect, can play the effect of washing equally.Requirement that also can be different according to client, adjustable oven dry or beat the wind time, reaches the requirement of client's washing, therefore method of the present invention meets this product requirement completely.And staff labor intensity obviously declines, origin operation method, needs tumbling-box washing machine, Water Extraction Machinery, and the equipment relating to is many, and the people who needs is just many, also needs employee to move into Water Extraction Machinery, after dehydration, takes out of from Water Extraction Machinery again, and the effort of taking a lot of work efficiency is low.
On artificial fur clothing washing process production cost of the present invention, have larger saving than old maneuver, adopt the equipment of the required use of New operating method few, the result that employee produces is just not identical yet.It every need electricity consumption 0.073 to spend, water 0.33kg, uses steam 0.3125kg, every day, everyone can do 1200.Origin operation method needs every 6.25kg of water and New operating method only needs 0.33kg, and using water wisely is more than 90%, and steam saves 75%, and improves the quality of products and save labour, and main is to have saved production cost.This maneuver, in 400,000 completed PU fur clothings are produced, produces economic benefit fairly obvious: using water wisely 236.8t, and using electricity wisely 30800 is spent, steam saving 375t, cost has been saved 115095.80 yuan, and operating efficiency improves 1.6 times.
Detailed description of the invention
The following examples are to describe in further detail of the present invention.
Embodiment 1
First artificial fur clothing is put into dryer, then heating, drying 10min, bake out temperature is 55 DEG C, then with giant, compounding agent solution is evenly sprayed on fur clothing, make fur clothing moistening, then shut oven dry gate oven dry 10min, then stop drying, then beat 10min with cold wind.
Described dryer is roller dryer.
Described auxiliary agent is ternary block silicone oil SRS., solubility is 25%.The spray flux of compounding agent solution is 5% of fur clothing weight.
Embodiment 2
First artificial fur clothing is put into dryer, then heating, drying 20min, bake out temperature is 50 DEG C, then with giant, compounding agent solution is evenly sprayed on fur clothing, make fur clothing moistening, then shut oven dry gate oven dry 20min, then stop drying, then beat 30min with cold wind.
Described dryer is roller dryer.
Described auxiliary agent is ternary block silicone oil SRS.The spray flux of compounding agent solution is 5% of fur clothing weight.
Embodiment 3
First artificial fur clothing is put into dryer, then heating, drying 15min, bake out temperature is 53 DEG C, then with giant, compounding agent solution is evenly sprayed on fur clothing, make fur clothing moistening, then shut oven dry gate oven dry 15min, then stop drying, then beat 20min with cold wind.
Described dryer is roller dryer.
Described auxiliary agent is ternary block silicone oil SRS.The spray flux of compounding agent solution is 5% of fur clothing weight.
Existing method: outward appearance is too bright, as artificial leather, be only limited to make sofa, family is spun, and is rarely used in garment material, due to hard without sub-light processing, surface, when oven dry, crease with breakage rate at 7-10% in surface.
Method of the present invention: the gloss that sub-light is completely the same with corium and outward appearance, feel, sales volume rises 10 times, due to sub-light processing, fabric softness, nothing crease and breakage rate in 1%.
Although illustrated and described embodiments of the invention, for the ordinary skill in the art, be appreciated that without departing from the principles and spirit of the present invention and can carry out multiple variation, amendment, replacement and modification to these embodiment, scope of the present invention is limited by claims and equivalent thereof.
Claims (7)
1. an artificial fur clothing washing process, it is characterized in that: the step of described technique is as follows: first artificial fur clothing is put into dryer, then heating, drying 10-20min, bake out temperature is 50-55 DEG C, then with giant, compounding agent solution is evenly sprayed on fur clothing, make fur clothing moistening, then shut oven dry gate oven dry 10-20min, then stop drying, then beat 10-30min with cold wind.
2. artificial fur clothing washing process as claimed in claim 1, is characterized in that: described dryer is roller dryer.
3. artificial fur clothing washing process as claimed in claim 1, is characterized in that: first artificial fur clothing is put into dryer, then heating, drying 15min.
4. artificial fur clothing washing process as claimed in claim 1, is characterized in that: described auxiliary agent is ternary block silicone oil.
5. artificial fur clothing washing process as claimed in claim 4, is characterized in that: the spray flux of compounding agent solution is 5% of fur clothing weight.
6. artificial fur clothing washing process as claimed in claim 4, is characterized in that: after fur clothing is moistening, then shut oven dry gate oven dry 15min.
7. artificial fur clothing washing process as claimed in claim 4, is characterized in that: cold wind is beaten 20min.