CN1748592A - Method for processing free ironing full cotton shirt - Google Patents
Method for processing free ironing full cotton shirt Download PDFInfo
- Publication number
- CN1748592A CN1748592A CN 200510061099 CN200510061099A CN1748592A CN 1748592 A CN1748592 A CN 1748592A CN 200510061099 CN200510061099 CN 200510061099 CN 200510061099 A CN200510061099 A CN 200510061099A CN 1748592 A CN1748592 A CN 1748592A
- Authority
- CN
- China
- Prior art keywords
- shirt
- ironing
- working solution
- full cotton
- processing method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The making process of no-ironing full cotton shirt includes the following treating steps: water washing, spraying no-ironing work fluid, dewatering, press-ironing to set, high temperature roasting, cooling and absorbing humidity, washing, stoving and air drying, finishing and packing. The present invention adopts press-ironing to set, rather than finishing-ironing to set, and the no-ironing work fluid is made to react with fiber for the primary setting, and this can greatly raise the shirt flatness degree grade.
Description
Technical field
The present invention relates to a kind of processing method of shirt, especially relate to a kind of processing method of free ironing full cotton shirt.
Background technology
In order to improve the flatness of cotton shirt, people adopt certain special processing method to make free ironing full cotton shirt.The processing method of existing free ironing full cotton shirt has certain defective, and the shirt that processes is difficult to reach flatness preferably.A kind of preparation method of 100 was disclosed in the disclosed No. 96120300.5 Chinese invention patent ublic specification of application as on February 11st, 1998, prop up cotton worsted fabric that high-accuracy yarn knits as raw material with height, it is carried out Liquid Ammonia Treatment, preshrunk processing, then lining is carried out cutting, clothing, the shirt of making is sprayed crease-resistant resin and oven dry processing, whole the scalding of high temperature finalized the design again, employing bakes forming machine and shirt is carried out HTHP bakes, clean shirt with warm water afterwards, at last packing.Wrinkle resistant effect of shirt that this invention is produced is better, non-ironingly is convinced naturally, and outward appearance is lasting for form.But this processing method also also has weak point, and the shirt flatness that processes is difficult to the rank that reaches higher.
Summary of the invention
Technical problem to be solved by this invention is the processing method that a kind of free ironing full cotton shirt is provided at above-mentioned prior art present situation, and the shirt flatness that processes can be up to state standards above.
The present invention solves the problems of the technologies described above the technical scheme that is adopted: a kind of processing method of free ironing full cotton shirt, the shirt ready-made clothes of making is carried out following processing to be handled: 1. washing, 2. spray and exempt to press working solution, 3. 4. dehydration is pressed and is scalded typing, and 5. high temperature bakes, 6. cool off moisture absorption, 7. clean, 8. oven dry hangs, 9. finishing and packing.
It is to be 150~180 ℃ in temperature that described pressure scalds that typing handles, and pressure is to scald having the pressure that the shirt of exempting to press working solution carries out each position under the condition of work of 2~4kg/cm, makes and exempts to press working solution and fiber-reactive, once finalizes the design.
Described high temperature bakes to be to use and bakes forming machine and baked 8~15 minutes pressing shirt after scalding to carry out high temperature under 110~150 temperature.
Compared with prior art, the invention has the advantages that will put in order boiling hot typing changes the boiling hot typing of pressure into, by under certain temperature condition, applying certain pressure the pressure that has the shirt of exempting to press working solution and carry out each position is scalded, make and exempt to press working solution and fiber-reactive, once finalize the design, can improve the rank of shirt flatness greatly, with respect to country formulate 〉=3.5 grades standard, use the flatness of the free ironing full cotton shirt of the inventive method processing can reach more than 4 grades, as shown in table 1.
The Main physical index of the free ironing full cotton shirt of table 1. the inventive method processing and national standard are relatively
The free ironing full cotton shirt of the inventive method processing | National standard | |
Flatness | 〉=4 grades | 〉=3.5 grades |
Content of formaldehyde | ≤50PPM | ≤75PPM |
Washing shrinkage | ≤±1% | ≤±2% |
The specific embodiment
Below in conjunction with embodiment the present invention is described in further detail.
Embodiment one: a kind of processing method of free ironing full cotton shirt, the 120S/2 that adopts accurate yarn to be made into
*120S/2 cotton worsted fabric is as raw material, by the lining cutting, be sewn into shirt ready-made clothes, the shirt ready-made clothes of making is carried out following processing to be handled: 1. clean the shirt ready-made clothes made from clear water, 2. exempting from of will preparing pressed working solution and is sprayed onto and cleans on back and the shirt, 3. dehydration, 4. it is 150 ℃ in temperature, pressure is to scald having the pressure that the shirt of exempting to press working solution carries out each position under the condition of work of 2kg/cm, make and exempt to press working solution and fiber-reactive, once finalize the design, 5. use to bake forming machine and baked 8 minutes, 6. cool off moisture absorption and placed 7. cleaned shirt 3 hours pressing shirt after scalding under 110 ℃ temperature, to carry out high temperature, 8. oven dry hangs, 9. finishing and packing.
Embodiment two:: a kind of processing method of free ironing full cotton shirt, the 100S/2 that adopts accurate yarn to be made into
*100S/2 cotton worsted fabric is as raw material, by the lining cutting, be sewn into shirt ready-made clothes, the shirt ready-made clothes of making is carried out following processing to be handled: 1. clean the shirt ready-made clothes made from clear water, 2. exempting from of will preparing pressed working solution and is sprayed onto and cleans on back and the shirt, 3. dehydration, 4. it is 165 ℃ in temperature, pressure is to scald having the pressure that the shirt of exempting to press working solution carries out each position under the condition of work of 3kg/cm, make and exempt to press working solution and fiber-reactive, once finalize the design, 5. use to bake forming machine and baked 12 minutes, 6. cool off moisture absorption and placed 7. cleaned shirt 4 hours pressing shirt after scalding under 130 temperature, to carry out high temperature, 8. oven dry hangs, 9. finishing and packing.
Embodiment three:: a kind of processing method of free ironing full cotton shirt, the 80S/2 that adopts accurate yarn to be made into
*80S/2 cotton worsted fabric is as raw material, by the lining cutting, be sewn into shirt ready-made clothes, the shirt ready-made clothes of making is carried out following processing to be handled: 1. clean the shirt ready-made clothes made from clear water, 2. exempting from of will preparing pressed working solution and is sprayed onto and cleans on back and the shirt, 3. dehydration, 4. it is 180 ℃ in temperature, pressure is to scald having the pressure that the shirt of exempting to press working solution carries out each position under the condition of work of 4kg/cm, make and exempt to press working solution and fiber-reactive, once finalize the design, 5. use to bake forming machine and baked 15 minutes, 6. cool off moisture absorption and placed 7. cleaned shirt 5 hours pressing shirt after scalding under 150 temperature, to carry out high temperature, 8. oven dry hangs, 9. finishing and packing.
Claims (3)
1, a kind of processing method of free ironing full cotton shirt is characterized in that the shirt ready-made clothes that will make carries out following processing and handles: 1. washing, and 2. spray and exempt to press working solution, 3. dehydration, 4. press and scald typing, 5. high temperature bakes, and 6. cools off moisture absorption, 7. clean, 8. oven dry hangs, 9. finishing and packing.
2, the processing method of a kind of free ironing full cotton shirt as claimed in claim 1 is characterized in that it is to be 150~180 ℃ in temperature that described pressure scalds that typing handles, and pressure is 2~4kg/cm
2Condition of work under scald having the pressure that the shirt of exempting to press working solution carries out each position, make and exempt to press working solution and fiber-reactive, once finalize the design.
3, the processing method of a kind of free ironing full cotton shirt as claimed in claim 1 is characterized in that described high temperature bakes to be to use to bake forming machine and baked 8~15 minutes pressing shirt after scalding to carry out high temperature under 110~150 temperature.