CN1041012C - 闸盘的制造方法 - Google Patents
闸盘的制造方法 Download PDFInfo
- Publication number
- CN1041012C CN1041012C CN 94107623 CN94107623A CN1041012C CN 1041012 C CN1041012 C CN 1041012C CN 94107623 CN94107623 CN 94107623 CN 94107623 A CN94107623 A CN 94107623A CN 1041012 C CN1041012 C CN 1041012C
- Authority
- CN
- China
- Prior art keywords
- brake disc
- chemically stable
- mentioned
- carried out
- pellicle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Images
Landscapes
- Braking Arrangements (AREA)
- Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP338040/93 | 1993-12-28 | ||
| JP33804093 | 1993-12-28 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| CN1110767A CN1110767A (zh) | 1995-10-25 |
| CN1041012C true CN1041012C (zh) | 1998-12-02 |
Family
ID=18314363
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CN 94107623 Expired - Fee Related CN1041012C (zh) | 1993-12-28 | 1994-12-27 | 闸盘的制造方法 |
Country Status (2)
| Country | Link |
|---|---|
| CN (1) | CN1041012C (enExample) |
| TW (1) | TW290591B (enExample) |
-
1994
- 1994-12-17 TW TW83111813A patent/TW290591B/zh active
- 1994-12-27 CN CN 94107623 patent/CN1041012C/zh not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| CN1110767A (zh) | 1995-10-25 |
| TW290591B (enExample) | 1996-11-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6183570B1 (en) | Surface treatment process of metallic material and metallic material obtained thereby | |
| TWI488974B (zh) | 複合螺絲的製造方法 | |
| CN106011736A (zh) | 一种汽车刹车盘及其表面改性方法 | |
| CN1096937C (zh) | 金属表面精整的方法及其制品 | |
| CN1041012C (zh) | 闸盘的制造方法 | |
| KR100613157B1 (ko) | 마그네슘 또는 마그네슘 합금 하우징 및 그 제조 방법 | |
| JP3587180B2 (ja) | 耐汚れ性と耐食性に優れたステンレス鋼板とその製造方法。 | |
| US7138066B2 (en) | Gear surface treatment procedure | |
| CN106702310A (zh) | 一种不锈钢氮化处理方法 | |
| CN115478237B (zh) | 一种热镀锌钢卷及其生产工艺 | |
| KR100855358B1 (ko) | 마그네슘 합금용 화성 처리액과 이를 이용한 마그네슘합금의 환경 친화적 표면처리방법 및 그에 따른 마그네슘합금 기재 | |
| JPH07233826A (ja) | ブレーキディスクの製造方法 | |
| JP4532438B2 (ja) | 異形断面線の製造方法 | |
| KR20140106938A (ko) | 마그네슘용 화성처리 조성물 및 이를 이용한 마그네슘 및 마그네슘 합금 소재의 표면처리방법 | |
| CN101161862A (zh) | 镁合金材料的表面处理溶液及处理镁合金材料表面的工艺 | |
| JP2000087259A (ja) | ステンレス鋼板およびその製造方法 | |
| CN107502854A (zh) | 一种增强汽车冲压件使用特性的处理方法 | |
| EP3415659B1 (en) | Alkaline conversion treatment composition for magnesium and magnesium alloy, and method for performing surface treatment on magnesium and magnesium alloy material by using same | |
| JPH049597A (ja) | 熱交換器用アルミニウムフィン用材及びその製造方法 | |
| JP5436782B2 (ja) | アルミホイールの製造方法、およびアルミホイール | |
| JP3664538B2 (ja) | 塗膜密着性に優れたフェライト系ステンレス鋼板およびその製造方法 | |
| CN111254381A (zh) | 一种提高不锈钢材料性能的改性方法 | |
| JPH07173635A (ja) | 金属の表面処理方法 | |
| KR20030089201A (ko) | 래디칼 질화처리된 핀커터의 제조방법 | |
| CN117358558A (zh) | 一种中厚板表面防护处理方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| C10 | Entry into substantive examination | ||
| SE01 | Entry into force of request for substantive examination | ||
| C10 | Entry into substantive examination | ||
| SE01 | Entry into force of request for substantive examination | ||
| C06 | Publication | ||
| PB01 | Publication | ||
| C14 | Grant of patent or utility model | ||
| GR01 | Patent grant | ||
| C19 | Lapse of patent right due to non-payment of the annual fee | ||
| CF01 | Termination of patent right due to non-payment of annual fee | ||
| C17 | Cessation of patent right | ||
| CF01 | Termination of patent right due to non-payment of annual fee |
Granted publication date: 19981202 |