Prior art keywords
graphite coating
delivery track
coating device
coating machine
graphite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310129251.5A
Other languages
English (en)
Inventor
许峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
RIXING METAL PRODUCT (SHANGHAI) Co Ltd
Original Assignee
RIXING METAL PRODUCT (SHANGHAI) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by RIXING METAL PRODUCT (SHANGHAI) Co Ltd filed Critical RIXING METAL PRODUCT (SHANGHAI) Co Ltd
Priority to CN201310129251.5A priority Critical patent/CN104096789A/zh
Publication of CN104096789A publication Critical patent/CN104096789A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Forging (AREA)

Abstract

本发明涉及金属挤压加工设备领域,具体为一种用于温锻作业的石墨喷涂装置及其使用方法。一种用于温锻作业的石墨喷涂装置,包括锻压机(1),其特征是:还包括石墨喷涂机(2),石墨喷涂机(2)的出料口设于锻压机(1)的进料口前。一种用于温锻作业的石墨喷涂装置的使用方法,包括预热、喷涂和锻压。本发明结构简单,使用方便,延长模具使用寿命。

Description

用于温锻作业的石墨喷涂装置及其使用方法
技术领域
本发明涉及金属挤压加工设备领域,具体为一种用于温锻作业的石墨喷涂装置及其使用方法。
背景技术
传统法兰盘成型时石墨喷涂在模具表面,喷涂模具表面不充分,模具磨损较快,更换模具频繁,模具制造成本高。
发明内容
为了克服现有技术的缺陷,提供一种结构简单、使用方便、产品质量高的挤压加工辅助设备,本发明公开了一种用于温锻作业的石墨喷涂装置及其使用方法。
本发明通过如下技术方案达到发明目的:
一种用于温锻作业的石墨喷涂装置,包括锻压机,其特征是:还包括石墨喷涂机,石墨喷涂机的出料口设于锻压机的进料口前。
所述的用于温锻作业的石墨喷涂装置,其特征是:还包括输送轨道、夹辊式进料机和预热感应炉,石墨喷涂机设于锻压机进料口前的两侧,石墨喷涂机内设有输送轨道,输送轨道从石墨喷涂机的进料口穿入,石墨喷涂机外的输送轨道依次连接夹辊式进料机和预热感应炉,石墨喷涂机内的输送轨道呈波浪型。
所述的用于温锻作业的石墨喷涂装置的使用方法,其特征是:将零件由夹辊式进料机夹持后经输送轨道送入预热感应炉内预热至300℃,随后再由零件输送轨道送入石墨喷涂机内,石墨喷涂机向零件的外表面喷涂石墨,喷涂时间不长于3sec,喷涂完毕后零件由输送轨道从预热感应炉送至锻压机,再加热至900℃以上后实施锻压。
本发明使用时,零件加热后先经输送轨道送入石墨喷涂机内,由于输送轨道呈波浪型,因此可以使喷涂时石墨在零件表面粘附得更均匀,喷涂完后零件送入锻压机锻压。由于先喷涂后锻压,石墨起到更好的保护作用,零件表面脱落的杂质少,可使模具具有更长的连续使用时间,延长了使用寿命。
本发明的有益效果是:结构简单,使用方便,延长模具使用寿命3倍以上,提高模具的反复利用率,减少模具成本,减少生产过程中的模具更换时间。
附图说明
图1是本发明的结构示意图。
具体实施方式
以下通过具体实施例进一步说明本发明。
实施例1
一种用于温锻作业的石墨喷涂装置,包括锻压机1、石墨喷涂机2、输送轨道21、夹辊式进料机3和预热感应炉4,如图1所示,具体结构是:
石墨喷涂机2设于锻压机1进料口前的两侧,石墨喷涂机2内设有输送轨道21,输送轨道21从石墨喷涂机2的进料口穿入,石墨喷涂机2外的输送轨道21依次连接夹辊式进料机3和预热感应炉4,石墨喷涂机2内的输送轨道21呈波浪型。
本实施例使用时,按如下步骤依次进行:
将零件由夹辊式进料机3夹持后经输送轨道21送入预热感应炉4内预热至300℃,随后再由零件输送轨道21送入石墨喷涂机2内,石墨喷涂机2向零件的外表面喷涂石墨,喷涂时间不长于3sec,喷涂完毕后零件由输送轨道21从预热感应炉4送至锻压机1,再加热至900℃以上后实施锻压。

Claims (3)

1.一种用于温锻作业的石墨喷涂装置,包括锻压机(1),其特征是:还包括石墨喷涂机(2),石墨喷涂机(2)的出料口设于锻压机(1)的进料口前。
2.如权利要求1所述的用于温锻作业的石墨喷涂装置,其特征是:还包括输送轨道(21)、夹辊式进料机(3)和预热感应炉(4),石墨喷涂机(2)设于锻压机(1)进料口前的两侧,石墨喷涂机(2)内设有输送轨道(21),输送轨道(21)从石墨喷涂机(2)的进料口穿入,石墨喷涂机(2)外的输送轨道(21)依次连接夹辊式进料机(3)和预热感应炉(4),石墨喷涂机(2)内的输送轨道(21)呈波浪型。
3.如权利要求2所述的用于温锻作业的石墨喷涂装置的使用方法,其特征是:
将零件由夹辊式进料机(3)夹持后经输送轨道(21)送入预热感应炉(4)内预热至300℃,随后再由零件输送轨道(21)送入石墨喷涂机(2)内,石墨喷涂机(2)向零件的外表面喷涂石墨,喷涂时间不长于3sec,喷涂完毕后零件由输送轨道(21)从预热感应炉(4)送至锻压机(1),再加热至900℃以上后实施锻压。
CN201310129251.5A 2013-04-15 2013-04-15 用于温锻作业的石墨喷涂装置及其使用方法 Pending CN104096789A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310129251.5A CN104096789A (zh) 2013-04-15 2013-04-15 用于温锻作业的石墨喷涂装置及其使用方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310129251.5A CN104096789A (zh) 2013-04-15 2013-04-15 用于温锻作业的石墨喷涂装置及其使用方法

Publications (1)

Publication Number Publication Date
CN104096789A true CN104096789A (zh) 2014-10-15

Family

ID=51665555

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310129251.5A Pending CN104096789A (zh) 2013-04-15 2013-04-15 用于温锻作业的石墨喷涂装置及其使用方法

Country Status (1)

Country Link
CN (1) CN104096789A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110421112A (zh) * 2019-07-23 2019-11-08 诸暨市润拓机械自动化科技有限公司 全自动下料锻压设备
CN111135971A (zh) * 2019-12-20 2020-05-12 安徽禹锋数据科技有限公司 一种温锻作业的石墨喷涂装置及其使用方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110421112A (zh) * 2019-07-23 2019-11-08 诸暨市润拓机械自动化科技有限公司 全自动下料锻压设备
CN111135971A (zh) * 2019-12-20 2020-05-12 安徽禹锋数据科技有限公司 一种温锻作业的石墨喷涂装置及其使用方法

Similar Documents

Publication Publication Date Title
CN102398146A (zh) 截齿齿靴锻造工艺
CN102941240A (zh) 一种铜卷排或铜带生产工艺
CN104889286B (zh) 合页页片轴位模具加工机械
CN104096789A (zh) 用于温锻作业的石墨喷涂装置及其使用方法
CN104148431A (zh) 一种挤压铜合金的连续挤压装置
CN204430260U (zh) 一种铝锭连续铸造生产线
CN105312349A (zh) 一种增大金属反挤压筒形件筒底变形量的方法
CN205967318U (zh) 一种铝碳化硅生产用热室压铸组件
CN203265501U (zh) 用于温锻作业的石墨喷涂装置
CN205128837U (zh) 一种二次冷镦加工自动上料机
CN102501007B (zh) 一种焊缝后移风口前帽的压力加工方法
CN204449289U (zh) 一种原料补偿式粉末冶金填料模具
CN203409162U (zh) 钛合金棒冷镦成形润滑剂涂覆装置
CN202824505U (zh) 半轴法兰成套生产设备
CN105057614A (zh) 一种连续式高铁接触线高效制坯装置
CN202556644U (zh) 一种模具冷却系统
CN202779784U (zh) 一种使用电磁加热的粉末冶金模具
CN204817989U (zh) 一种精密压铸件的压铸模具
CN204220660U (zh) 二片式结构热挤压模具
CN100393437C (zh) 利用单轮槽连续挤压机生产挤压产品的方法及其装置
CN202377261U (zh) 加工镁合金板的热轧装置
CN210023530U (zh) 一种轮辋成型自动上料装置
CN103357802B (zh) 钛合金棒冷镦成形润滑剂涂覆装置
CN107442589B (zh) 一种大型带凸耳镁合金构件成形模具
CN204074781U (zh) 组合式氧枪喷头上部喉管一体挤压成型模具

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20141015