CN104046227A - 一种改良型防水卷材 - Google Patents
一种改良型防水卷材 Download PDFInfo
- Publication number
- CN104046227A CN104046227A CN201410234854.6A CN201410234854A CN104046227A CN 104046227 A CN104046227 A CN 104046227A CN 201410234854 A CN201410234854 A CN 201410234854A CN 104046227 A CN104046227 A CN 104046227A
- Authority
- CN
- China
- Prior art keywords
- parts
- sulphur
- acrylate
- styrene
- hydrochloric acid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯7-18份,盐酸2-6份,石英砂20-40份,烷基苯磺酸钠3-6份,沥青15-35份,氢氧化钠3-7份,聚乙烯醇2-5份,对苯二胺5-15份,聚氧乙烯烷基胺15-25份,聚铣按20-35份,四氯化碳10-20份,弹性纤维6-10份,丁苯橡胶3-7份,三乙醇胺11-16份,膨胀珍珠岩9-17份,硫磺1-3份,本发明提供一种耐高温、不起泡、耐磨强度高,耐候性好,耐寒性强,回弹率高的改良型防水卷材。
Description
技术领域
本发明涉及建筑施工技术领域,具体涉及一种改良型防水卷材。
背景技术
目前,各类建筑物的防水作业是一个关键的问题。通常使用的防水材料多为各类防水卷材、防水涂料、防水胶泥等。防水卷材一般以热施工为主,多以火烤,主要不足是粘接不全面,有接缝,对一些特殊部位,诸如边角、管口等位置处不好处理,易渗水,渗水后不易维修。防水涂料一般冷施工,把防水涂料搅拌好后,一次进行涂刷,无接缝施工,粘接力强。改性沥青防水涂料运用高分子合成技术,加入了环氧树脂和树脂基团使本产品更具多功能与环保合一体,赋予新产品更具防水,防腐,防潮,防霉等功效。
发明内容
针对现有技术的不足,本发明所要解决的技术问题是,提供一种耐高温、不起泡、耐磨强度高,耐候性好,耐寒性强,回弹率高的改良型防水卷材。
为解决上述技术问题,本发明所采取的技术方案是:一种改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯7-18份,盐酸2-6份,石英砂20-40份,烷基苯磺酸钠3-6份,沥青15-35份,氢氧化钠3-7份,聚乙烯醇2-5份,对苯二胺5-15份,聚氧乙烯烷基胺15-25份,聚铣按20-35份,四氯化碳10-20份,弹性纤维6-10份,丁苯橡胶3-7份,三乙醇胺11-16份,膨胀珍珠岩9-17份,硫磺1-3份,电气石粉5-14份,硅酸钠 6-8份,钛白粉2-4份,石油烃9-20份,硬脂基三甲基氯化铵4-8份。
上述的改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯15份,盐酸4份,石英砂30份,烷基苯磺酸钠4份,沥青25份,氢氧化钠5份,聚乙烯醇4份,对苯二胺10份,聚氧乙烯烷基胺20份,聚铣按30份,四氯化碳15份,弹性纤维8份,丁苯橡胶5份,三乙醇胺14份,膨胀珍珠岩15份,硫磺2份,电气石粉10份,硅酸钠7份,钛白粉3份,石油烃15份,硬脂基三甲基氯化铵6份。
本发明改良型防水卷材优点是:
1、本发明改良型防水卷材,产品固含量 65-75%,表干 3-4h,实干 22-24h ;耐阳光照射,耐 90-110℃高温,100℃下 5h 不起泡不流淌 ; 0.1-0.2MPa、30min 不透水,粘度 175Pa·s ;产品耐磨强度高,耐候性好,耐寒性强,回弹率高,可以广泛生产并不断代替现有材料。
具体实施方式
下面结合实施例对本发明作进一步说明。
实施例1,一种改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯7份,盐酸2份,石英砂20份,烷基苯磺酸钠3份,沥青15份,氢氧化钠3份,聚乙烯醇2份,对苯二胺5份,聚氧乙烯烷基胺15份,聚铣按20份,四氯化碳10份,弹性纤维6份,丁苯橡胶3份,三乙醇胺11份,膨胀珍珠岩9份,硫磺1份,电气石粉5份,硅酸钠 6份,钛白粉2份,石油烃9份,硬脂基三甲基氯化铵4份。
实施例2,一种改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯15份,盐酸4份,石英砂30份,烷基苯磺酸钠4份,沥青25份,氢氧化钠5份,聚乙烯醇4份,对苯二胺10份,聚氧乙烯烷基胺20份,聚铣按30份,四氯化碳15份,弹性纤维8份,丁苯橡胶5份,三乙醇胺14份,膨胀珍珠岩15份,硫磺2份,电气石粉10份,硅酸钠7份,钛白粉3份,石油烃15份,硬脂基三甲基氯化铵6份。
实施例3,一种改良型防水卷材,由以下重量份数的原料制成:丙烯酸酯18份,盐酸6份,石英砂40份,烷基苯磺酸钠6份,沥青35份,氢氧化钠7份,聚乙烯醇5份,对苯二胺15份,聚氧乙烯烷基胺25份,聚铣按35份,四氯化碳20份,弹性纤维10份,丁苯橡胶7份,三乙醇胺16份,膨胀珍珠岩17份,硫磺3份,电气石粉14份,硅酸钠 8份,钛白粉4份,石油烃20份,硬脂基三甲基氯化铵8份。
当然,上述说明并非是对本发明的限制,本发明也并不限于上述举例,本技术领域的普通技术人员,在本发明的实质范围内,作出的变化、改变、添加或替换,都应属于本发明的保护范围。
Claims (2)
1.一种改良型防水卷材,其特征在于:由以下重量份数的原料制成:丙烯酸酯7-18份,盐酸2-6份,石英砂20-40份,烷基苯磺酸钠3-6份,沥青15-35份,氢氧化钠3-7份,聚乙烯醇2-5份,对苯二胺5-15份,聚氧乙烯烷基胺15-25份,聚铣按20-35份,四氯化碳10-20份,弹性纤维6-10份,丁苯橡胶3-7份,三乙醇胺11-16份,膨胀珍珠岩9-17份,硫磺1-3份,电气石粉5-14份,硅酸钠 6-8份,钛白粉2-4份,石油烃9-20份,硬脂基三甲基氯化铵4-8份。
2.根据权利要求1所述的改良型防水卷材,其特征是:由以下重量份数的原料制成:丙烯酸酯15份,盐酸4份,石英砂30份,烷基苯磺酸钠4份,沥青25份,氢氧化钠5份,聚乙烯醇4份,对苯二胺10份,聚氧乙烯烷基胺20份,聚铣按30份,四氯化碳15份,弹性纤维8份,丁苯橡胶5份,三乙醇胺14份,膨胀珍珠岩15份,硫磺2份,电气石粉10份,硅酸钠7份,钛白粉3份,石油烃15份,硬脂基三甲基氯化铵6份。