CN103945025A - Method for manufacturing sterilization mobile-phone protecting shell - Google Patents

Method for manufacturing sterilization mobile-phone protecting shell Download PDF

Info

Publication number
CN103945025A
CN103945025A CN201410108660.1A CN201410108660A CN103945025A CN 103945025 A CN103945025 A CN 103945025A CN 201410108660 A CN201410108660 A CN 201410108660A CN 103945025 A CN103945025 A CN 103945025A
Authority
CN
China
Prior art keywords
pottery mud
composite particles
pottery
manufacture
crown cap
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410108660.1A
Other languages
Chinese (zh)
Other versions
CN103945025B (en
Inventor
郑景文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Jetech Electronics Technology Co ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410108660.1A priority Critical patent/CN103945025B/en
Publication of CN103945025A publication Critical patent/CN103945025A/en
Priority to CN201580002281.7A priority patent/CN105659572B/en
Priority to PCT/CN2015/072085 priority patent/WO2015143953A1/en
Application granted granted Critical
Publication of CN103945025B publication Critical patent/CN103945025B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A method for manufacturing a sterilization mobile-phone protecting shell comprises the following steps of bottom-shell manufacturing, covering-plate manufacturing and assembling. By means of manufacturing equipment of the sterilization mobile-phone protecting shell, metal materials are made into a metal shell and a metal cover, clay and husks or coconut shells are made into a composite particle clay plate, the composite particle clay plate is combined with the metal shell or the metal cover, the composite particle clay plate and the metal shell or the metal cover are sintered together, and therefore the sterilization mobile-phone protecting shell is obtained. The sterilization mobile-phone protecting shell has the functions, such as sterilization and absorption of formaldehyde and other harmful gases, of activated carbon. The void structure of the activated carbon of the sterilization mobile-phone protecting shell can be recovered by means of heat treatment. The functions of sterilization and absorption of formaldehyde and other harmful gases of the sterilization mobile-phone protecting shell are achieved again, and the sterilization mobile-phone protecting shell is capable of being be recycled and beneficial to physical health of people.

Description

The manufacture method of sterilization mobile phone protective case
Technical field
The present invention relates to a kind of manufacture method of mobile phone protective case, particularly the manufacture method of sterilization mobile phone protective case.
Background technology
At present, the mobile phone that people use contains bacterium, formaldehyde and other pernicious gases, be unfavorable for that people's is healthy, the mobile phone protective case that people use does not have sterilization yet, absorbs the function of formaldehyde and other pernicious gases, there is a sterilization mobile phone protective case for sterilization, absorption formaldehyde and other pernicious gases, need a kind of manufacturing equipment and manufacture method of sterilization mobile phone protective case.
Summary of the invention
The object of the invention is to overcome the deficiencies in the prior art, the manufacture method of sterilization mobile phone protective case is provided, for the manufacture of a kind of sterilization mobile phone protective case, utilize sterilization mobile phone protective case opponent machine carry out sterilization and absorb formaldehyde and other pernicious gases of mobile phone, safeguard that people's is healthy.
The technical solution adopted in the present invention is: sterilization mobile phone protective case include drain pan and cover plate, cover plate and drain pan are hinged; Drain pan includes metal shell, the first ceramic substrate and the first active carbon, the first ceramic substrate is fixedly connected with metal shell, the first active carbon is fixedly connected with the first ceramic substrate, and the first ceramic substrate is between metal shell and the first active carbon, and the first active carbon is positioned at the inside of drain pan; Cover plate includes crown cap, the second ceramic substrate and the second active carbon, the second ceramic substrate is fixedly connected with crown cap, the second active carbon is fixedly connected with the second ceramic substrate, and the second ceramic substrate is between crown cap and the second active carbon, and the second active carbon is positioned at the inside of cover plate.Drain pan and cover plate form by metal, pottery and active carbon are compound; The first active carbon is positioned at the first inner surface of drain pan, and the second active carbon is positioned at the second inner surface of cover plate; Metal shell, the first ceramic substrate and the first active carbon are combined with each other, and crown cap, the second ceramic substrate and the second active carbon are combined with each other; The first ceramic substrate and the first active carbon are sintered together, and the second ceramic substrate and the second active carbon are sintered together.
The flow process of the manufacture method of sterilization mobile phone protective case is: the manufacture → combination of drain pan manufacture → cover plate;
The flow process of drain pan manufacture is: the polishing of metal shell manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → metal shell composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → metal shell surface; The flow process of cover plate manufacture is: the surface finish of crown cap manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → crown cap composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → crown cap.
When the manufacture of sterilization mobile phone protective case: pottery mud material creates wet pottery mud by the mud manufacturing equipment of making pottery, controller control the flow work, conveying worm becomes the extruding of pottery mud the pottery mud strip of bar shaped, and pottery mud strip is transported to the first conveyer, pottery mud strip is delivered to two rod roller presses by the first conveyer, the roll extrusion of pottery mud strip is become the pottery mud lath being of the required size by two rod roller presses, and pottery mud lath is transported to second conveyor by two rod roller presses, pulverizer pulverizes shell or coconut husk for being transported to screening machine after particle, screening machine is by the pottery mud lath spreading to after particle screen selecting above second conveyor, make make pottery the upper surface covering last layer shell of mud lath or the particle of coconut husk, second conveyor is sent the pottery mud lath that is coated with particle into roller press, its particle is rolled into pottery mud lath by roller press 33, the mud lath that makes to make pottery becomes composite particles pottery mud lath, shearing machine delivered to by the composite particles mud lath of making pottery by controller control second conveyor, shearing machine becomes composite particles pottery mud plate by the composite particles mud lath of making pottery by dimensional requirement cutting, metallic plate is created metal shell or crown cap by punch press and diel, utilize staff or manipulator that metal shell or crown cap are put on the work mould of press, utilize staff or manipulator that the composite particles mud plate of making pottery is put into the groove of metal shell or crown cap, utilize press that make pottery mud plate and metal shell or crown cap of composite particles forced together, thereby produce the metal shell of composite particles pottery mud or the crown cap of composite particles pottery mud, the make pottery crown cap of the metal shell of mud or composite particles pottery mud of composite particles is sent into vacuum sintering furnace sintering and charing, after the crown cap sintering of the metal shell of composite particles pottery mud or composite particles pottery mud and charing, send into polishing machine polishing.
The invention has the beneficial effects as follows: a kind of manufacture method of sterilization mobile phone protective case, utilize the manufacturing equipment of sterilization mobile phone protective case, metal material is made to metal shell and crown cap, the mud of making pottery, shell or coconut husk are made composite particles pottery mud plate, by compound make pottery mud plate and metal shell or crown cap of composite particles, make pottery mud plate and metal shell or crown cap of composite particles is sintered together, thereby produce sterilization mobile phone protective case, make sterilization mobile phone protective case there is the sterilization of active carbon, absorb the function of formaldehyde and other pernicious gases, make sterilization mobile phone protective case can heat treatment recover the gap structure of its active carbon, recover the sterilization of sterilization mobile phone protective case, absorb the function of formaldehyde and other pernicious gases, sterilization mobile phone protective case can be recycled, be conducive to the healthy of people.
Brief description of the drawings
Fig. 1 is the structural representation of sterilization mobile phone protective case;
Fig. 2 is the manufacturing equipment schematic diagram of sterilization mobile phone protective case.
Embodiment
Below in conjunction with accompanying drawing, the present invention is further detailed:
The manufacturing equipment schematic diagram of the sterilization mobile phone protective case shown in structural representation and the Fig. 2 of the sterilization mobile phone protective case shown in Fig. 1;
Sterilization mobile phone protective case includes drain pan 1 and cover plate 2, and cover plate 2 is hinged with drain pan 1; Drain pan 1 includes metal shell 3, the first ceramic substrate 4 and the first active carbon 5, the first ceramic substrate 4 is fixedly connected with metal shell 3, the first active carbon 5 is fixedly connected with the first ceramic substrate 4, the first ceramic substrate 4 is between metal shell 3 and the first active carbon 5, and the first active carbon 5 is positioned at the inside of drain pan 1; Cover plate 2 includes crown cap 6, the second ceramic substrate 7 and the second active carbon 8, the second ceramic substrate 7 is fixedly connected with crown cap 6, the second active carbon 8 is fixedly connected with the second ceramic substrate 7, the second ceramic substrate 7 is between crown cap 6 and the second active carbon 8, and the second active carbon 8 is positioned at the inside of cover plate 2.
In order to implement being fixedly connected with of the first active carbon and the first ceramic substrate 4 and the second active carbon 8 and the second ceramic substrate 7, drain pan 1 and cover plate 2 form by metal, pottery and active carbon are compound; The first inner surface 22, the second active carbons 8 that the first active carbon 5 is positioned at drain pan 1 are positioned at the second inner surface 23 of cover plate 2; Metal shell 3, the first ceramic substrate 4 and the first active carbon 5 are combined with each other, and crown cap 6, the second ceramic substrate 7 and the second active carbon 8 are combined with each other; The first ceramic substrate 4 and the first active carbon 5 are sintered together, and the second ceramic substrate 7 and the second active carbon 8 are sintered together.
Manufacturing sterilization mobile phone protective case needs a kind of manufacturing equipment of sterilization mobile phone protective case, the manufacturing equipment of sterilization mobile phone protective case includes punch press 24, pottery mud manufacturing equipment 26, conveying worm 27, the first conveyer 28, two rod roller presses 29, second conveyor 30, pulverizer 31, screening machine 32, roller press 33, shearing machine 34, press 35, vacuum sintering furnace 36, polishing machine 37 and controller 38, it is characterized in that: described punch press 24, diel 25, pottery mud manufacturing equipment 26, conveying worm 27, the first conveyer 28, two rod roller presses 29, second conveyor 30, pulverizer 31, screening machine 32, roller press 33, shearing machine 34, press 35, vacuum sintering furnace 36, polishing machine 37 and controller 38 form streamline, for the manufacture of the manufacture method of sterilization mobile phone protective case, make the manufacture method of sterilization mobile phone protective case there is sterilization, absorb the function of formaldehyde and pernicious gas, pottery mud manufacturing equipment 26 is connected with conveying worm 27, conveying worm 27 is connected with the first conveyer 28, the first conveyer 28 is connected with two rod roller presses 29, two rod roller presses 29 are connected with second conveyor 30, pulverizer 31 is connected with vibrating screen 32, vibrating screen 32 is connected with second conveyor 30, vibrating screen 32 is positioned at the top of second conveyor 30, roller press 33 and shearing machine 34 are located on second conveyor 30, shearing machine 34 is positioned at the right of roller press 33, second conveyor 30 is connected with press 35, the side of press 35 is provided with punch press 24 and diel 25, press 35 and vacuum sintering furnace 36, vacuum sintering furnace 36 is connected with polishing machine 37.
The flow process of the manufacture method of sterilization mobile phone protective case is: the manufacture → combination of drain pan manufacture → cover plate;
The flow process of drain pan manufacture is: the polishing of metal shell manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → metal shell composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → metal shell surface;
The manufacture method of drain pan is specifically:
Metal shell is manufactured: design and manufacture its diel according to the size of metal shell 3 and shape, utilizing the diel of punch press 24 and metal shell 3 that sheet metal is processed into metal shell 3;
Pottery slurry manufacture: utilize pottery mud manufacturing equipment 26 and pottery mud material manufacture pottery mud;
Pottery mud lath is manufactured: utilize conveying worm 27 and strip extrusion die 40 will make pottery mud extruding for pottery mud strip; Utilize two rod roller presses 29 that the roll extrusion of pottery mud strip is become to the pottery mud lath being of the required size;
Particle is manufactured: utilizing pulverizer 31 is particle by shell or coconut husk pulverizing, utilizing screening machine 32 according to the dimensional requirement of its particle is the qualified shell of size or coconut husk particle by its particle screen selecting, and by qualified shell or coconut husk particle screen selecting to the surface of pottery mud lath;
Composite particles pottery mud lath is manufactured: utilize roller press 33 that the roll extrusion of pottery mud is become to pottery mud lath, utilize roller press that shell or the roll extrusion of coconut husk particle are embedded on pottery mud lath, thereby produce composite particles pottery mud lath;
Composite particles pottery mud lath cutting: utilize shearing machine 34 that the composite particles mud lath of making pottery is cut into the composite particles pottery mud plate of the size needing;
Metal shell composite particles pottery mud: the particle pottery mud plate that is compounded with that cuts out size is put into metal shell 3, and utilize press 35 that the composite particles mud plate of making pottery is pressed in to the inside of metal shell 3;
Vacuum-sintering: the make pottery metal shell 3 of mud plate of composite particles is put into vacuum sintering furnace 36, utilize vacuum sintering furnace that shell or coconut husk and pottery mud are sintered together, the particle charing of shell or coconut husk is become to active carbon simultaneously;
Activated carbon surface polishing: utilize polishing machine 37 by activated carbon surface polishing and clean clean;
Metal shell surface polishing: utilize polishing machine 37 by the surface finish of metal shell 3 and clean clean;
The flow process of cover plate manufacture is: the surface finish of crown cap manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → crown cap composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → crown cap;
The manufacture method of cover plate is specifically:
Crown cap is manufactured: according to the diel of the size of crown cap 6 and shape design and manufacture crown cap 6, utilize the diel of punch press 24 and crown cap 6 that sheet metal is processed into crown cap 6;
Pottery slurry manufacture: utilize pottery mud manufacturing equipment 26 and pottery mud material manufacture pottery mud;
Pottery mud lath is manufactured: utilize conveying worm 27 and strip extrusion die 40 will make pottery mud extruding for pottery mud strip; Utilize two rod roller presses 29 that the roll extrusion of pottery mud strip is become to the pottery mud lath being of the required size;
Particle is manufactured: utilizing pulverizer 31 is particle by shell or coconut husk pulverizing, utilizing screening machine 32 according to the dimensional requirement of its particle is the qualified shell of size or coconut husk particle by its particle screen selecting, and by qualified shell or coconut husk particle screen selecting to the surface of pottery mud lath;
Composite particles pottery mud lath is manufactured: utilize roller press 33 that the roll extrusion of pottery mud is become to pottery mud lath, utilize roller press that shell or the roll extrusion of coconut husk particle are embedded on pottery mud lath, thereby produce composite particles pottery mud lath;
Composite particles pottery mud lath cutting: utilize shearing machine 34 that the composite particles mud lath of making pottery is cut into the composite particles pottery mud plate of the size needing;
Crown cap composite particles pottery mud: the particle pottery mud plate that is compounded with that cuts out size is put into crown cap 6, and utilize press 35 that the composite particles mud plate of making pottery is pressed in to the inside of crown cap 6;
Vacuum-sintering: the make pottery crown cap 6 of mud plate of composite particles is put into vacuum sintering furnace 36, utilize vacuum sintering furnace that shell or coconut husk and pottery mud are sintered together, the particle charing of shell or coconut husk is become to active carbon simultaneously;
Activated carbon surface polishing: utilize polishing machine 37 by activated carbon surface polishing and clean clean;
Crown cap surface finish: utilize polishing machine 37 by the surface finish of crown cap 6 and clean clean;
Combination: polished metal shell 3 and polished crown cap 6 are combined, the hinge of cover plate 2 23 is inserted to the fraising 22 of drain pan 1, make metal shell 3 and crown cap 6 hinged.
In order to implement the combination of metal shell 3 and pottery mud, utilize metal shell to rush negative mold and punch press stamps out male and fomale(M&F) in the inner surface of metal shell 3; In order to implement the combination of crown cap 6 and pottery mud; The male and fomale(M&F) of metal shell 3 contacts with composite particles pottery mud, together with the male and fomale(M&F) of metal shell 3 is embedded in the male and fomale(M&F) of composite particles pottery mud; The inner surface of metal shell 3 contacts with the one side that there is no particle of composite particles pottery mud, and the male and fomale(M&F) of metal shell 3 and composite particles pottery mud do not have the male and fomale(M&F) close contact of particle one side.
In order to implement the combination of crown cap 6 and pottery mud, utilize crown cap to rush negative mold and punch press stamps out male and fomale(M&F) in the inner surface of crown cap 6; The male and fomale(M&F) of crown cap 6 and composite particles pottery mud close contact, together with the male and fomale(M&F) of crown cap 6 is embedded in the male and fomale(M&F) of composite particles pottery mud; The inner surface of crown cap 6 contacts with the one side that there is no particle of composite particles pottery mud, and the male and fomale(M&F) of crown cap 6 and composite particles pottery mud do not have the male and fomale(M&F) close contact of particle one side.
For the charing of sintering and shell and the coconut husk particle of the mud of implementing to make pottery, sintering and the carbonization temperature of composite particles pottery mud are 700 ° of C to 900 ° of C.

Claims (8)

1. the manufacture method of sterilization mobile phone protective case, sterilization mobile phone protective case includes drain pan (1) and cover plate (2), and cover plate (2) is hinged with drain pan (1); Drain pan (1) includes metal shell (3), the first ceramic substrate (4) and the first active carbon (5), the first ceramic substrate (4) is fixedly connected with metal shell (3), the first active carbon (5) is fixedly connected with the first ceramic substrate (4), the first ceramic substrate (4) is positioned between metal shell (3) and the first active carbon (5), and the first active carbon (5) is positioned at the inside of drain pan (1); Cover plate (2) includes crown cap (6), the second ceramic substrate (7) and the second active carbon (8), the second ceramic substrate (7) is fixedly connected with crown cap (6), the second active carbon (8) is fixedly connected with the second ceramic substrate (7), the second ceramic substrate (7) is positioned between crown cap (6) and the second active carbon (8), and the second active carbon (8) is positioned at the inside of cover plate (2); The first ceramic substrate (4) is sintered together with the first active carbon (5), and the second ceramic substrate (7) is sintered together with the second active carbon (8);
Manufacturing sterilization mobile phone protective case needs a kind of manufacturing equipment of sterilization mobile phone protective case, and the manufacturing equipment of sterilization mobile phone protective case includes punch press (24), pottery mud manufacturing equipment (26), conveying worm (27), the first conveyer (28), two rod roller presses (29), second conveyor (30), pulverizer (31), screening machine (32), roller press (33), shearing machine (34), press (35), vacuum sintering furnace (36), polishing machine (37) and controller (38), is characterized in that: described punch press (24), diel (25), pottery mud manufacturing equipment (26), conveying worm (27), the first conveyer (28), two rod roller presses (29), second conveyor (30), pulverizer (31), screening machine (32), roller press (33), shearing machine (34), press (35), vacuum sintering furnace (36), polishing machine (37) and controller (38) form streamline, for the manufacture of the manufacture method of sterilization mobile phone protective case, make the manufacture method of sterilization mobile phone protective case have sterilization, absorb the function of formaldehyde and pernicious gas, pottery mud manufacturing equipment (26) is connected with conveying worm (27), conveying worm (27) is connected with the first conveyer (28), the first conveyer (28) is connected with two rod roller presses (29), two rod roller presses (29) are connected with second conveyor (30), pulverizer (31) is connected with vibrating screen (32), vibrating screen (32) is connected with second conveyor (30), vibrating screen (32) is positioned at the top of second conveyor (30), roller press (33) and shearing machine (34) are located on second conveyor (30), shearing machine (34) is positioned at the right of roller press (33), second conveyor (30) is connected with press (35), the side of press (35) is provided with punch press (24) and diel (25), press (35) and vacuum sintering furnace (36), vacuum sintering furnace (36) is connected with polishing machine (37),
It is characterized in that: the flow process of the manufacture method of described sterilization mobile phone protective case is: the manufacture → combination of drain pan manufacture → cover plate;
The flow process of drain pan manufacture is: the polishing of metal shell manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → metal shell composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → metal shell surface;
The manufacture method of drain pan is specifically:
Metal shell is manufactured: design and manufacture its diel according to the size of metal shell (3) and shape, utilizing the diel of punch press (24) and metal shell (3) that sheet metal is processed into metal shell (3);
Pottery slurry manufacture: utilize pottery mud manufacturing equipment (26) and pottery mud material manufacture pottery mud;
Pottery mud lath is manufactured: utilize conveying worm (27) and strip extrusion die (40) will make pottery mud extruding for pottery mud strip; Utilize two rod roller presses (29) that the roll extrusion of pottery mud strip is become to the pottery mud lath being of the required size;
Particle is manufactured: utilize pulverizer (31) that shell or coconut husk are pulverized as particle, utilizing screening machine (32) according to the dimensional requirement of its particle is shell or the coconut husk particle that size is qualified by its particle screen selecting, and by qualified shell or coconut husk particle screen selecting to the surface of pottery mud lath;
Composite particles pottery mud lath is manufactured: utilize roller press (33) that the roll extrusion of pottery mud is become to pottery mud lath, utilize roller press that shell or the roll extrusion of coconut husk particle are embedded on pottery mud lath, thereby produce composite particles pottery mud lath;
Composite particles pottery mud lath cutting: utilize shearing machine (34) that the composite particles mud lath of making pottery is cut into the composite particles pottery mud plate of the size needing;
Metal shell composite particles pottery mud: the particle pottery mud plate that is compounded with that cuts out size is put into metal shell (3), and utilize press (35) that the composite particles mud plate of making pottery is pressed in to the inside of metal shell (3);
Vacuum-sintering: the make pottery metal shell (3) of mud plate of composite particles is put into vacuum sintering furnace (36), utilize vacuum sintering furnace that shell or coconut husk and pottery mud are sintered together, the particle charing of shell or coconut husk is become to active carbon simultaneously;
Activated carbon surface polishing: utilize polishing machine (37) by the surface finish of the first active carbon (5) and clean;
Metal shell surface polishing: utilize polishing machine (37) by the surface finish of metal shell (3) and clean clean;
The flow process of cover plate manufacture is: the surface finish of crown cap manufacture → pottery slurry manufacture → pottery mud lath manufacture → particle manufacture → composite particles pottery mud lath manufacture → composite particles pottery mud lath cutting → crown cap composite particles pottery mud → vacuum-sintering → activated carbon surface polishing → crown cap;
The manufacture method of cover plate is specifically:
Crown cap is manufactured: according to the diel of the size of crown cap (6) and shape design and manufacture crown cap (6), utilize the diel of punch press (24) and crown cap (6) that sheet metal is processed into crown cap (6);
Pottery slurry manufacture: utilize pottery mud manufacturing equipment (26) and pottery mud material manufacture pottery mud;
Pottery mud lath is manufactured: utilize conveying worm (27) and strip extrusion die (40) will make pottery mud extruding for pottery mud strip; Utilize two rod roller presses (29) that the roll extrusion of pottery mud strip is become to the pottery mud lath being of the required size;
Particle is manufactured: utilize pulverizer (31) that shell or coconut husk are pulverized as particle, utilizing screening machine (32) according to the dimensional requirement of its particle is shell or the coconut husk particle that size is qualified by its particle screen selecting, and by qualified shell or coconut husk particle screen selecting to the surface of pottery mud lath;
Composite particles pottery mud lath is manufactured: utilize roller press (33) that the roll extrusion of pottery mud is become to pottery mud lath, utilize roller press that shell or the roll extrusion of coconut husk particle are embedded on pottery mud lath, thereby produce composite particles pottery mud lath;
Composite particles pottery mud lath cutting: utilize shearing machine (34) that the composite particles mud lath of making pottery is cut into the composite particles pottery mud plate of the size needing;
Crown cap composite particles pottery mud: the particle pottery mud plate that is compounded with that cuts out size is put into crown cap (6), and utilize press (35) that the composite particles mud plate of making pottery is pressed in to the inside of crown cap (6);
Vacuum-sintering: the make pottery crown cap (6) of mud plate of composite particles is put into vacuum sintering furnace (36), utilize vacuum sintering furnace that shell or coconut husk and pottery mud are sintered together, the particle charing of shell or coconut husk is become to active carbon simultaneously;
Activated carbon surface polishing: utilize polishing machine (37) by the surface finish of the second active carbon (8) and clean;
Crown cap surface finish: utilize polishing machine (37) by the surface finish of crown cap (6) and clean clean;
Combination: polished metal shell (3) and polished crown cap (6) are combined, the hinge of cover plate (2) (23) is inserted to the fraising (22) of drain pan (1), make metal shell (3) and crown cap (6) hinged.
2. the manufacture method of sterilization mobile phone protective case according to claim 1, is characterized in that: described metal shell (3) manufacture method is: utilize metal shell to rush negative mold and punch press stamps out male and fomale(M&F) in the inner surface of metal shell (3).
3. the manufacture method of sterilization mobile phone protective case according to claim 1, is characterized in that: the manufacture method of described crown cap (6) is: utilize crown cap to rush negative mold and punch press stamps out male and fomale(M&F) in the inner surface of crown cap (6).
4. the manufacture method of sterilization mobile phone protective case according to claim 1, is characterized in that: the male and fomale(M&F) of described metal shell (3) contacts with composite particles pottery mud, together with the male and fomale(M&F) of metal shell (3) is embedded in the male and fomale(M&F) of composite particles pottery mud.
5. the manufacture method of sterilization mobile phone protective case according to claim 4, it is characterized in that: the inner surface of described metal shell (3) contacts with the one side that there is no particle of composite particles pottery mud, the male and fomale(M&F) of metal shell (3) and composite particles pottery mud do not have the male and fomale(M&F) close contact of particle one side.
6. the manufacture method of sterilization mobile phone protective case according to claim 1, is characterized in that: the male and fomale(M&F) of described crown cap (6) and composite particles pottery mud close contact, and together with the male and fomale(M&F) of crown cap (6) is embedded in the male and fomale(M&F) of composite particles pottery mud.
7. the manufacture method of sterilization mobile phone protective case according to claim 1, it is characterized in that: the inner surface of described crown cap (6) contacts with the one side that there is no particle of composite particles pottery mud, the male and fomale(M&F) of crown cap (6) and composite particles pottery mud do not have the male and fomale(M&F) close contact of particle one side.
8. the manufacture method of sterilization mobile phone protective case according to claim 1, is characterized in that: sintering and the carbonization temperature of described composite particles pottery mud are 700 ° of C to 900 ° of C.
CN201410108660.1A 2014-03-23 2014-03-23 The manufacture method of sterilization mobile phone protective case Expired - Fee Related CN103945025B (en)