CN103882680B - 一种真丝织物挂练练漂的方法 - Google Patents

一种真丝织物挂练练漂的方法 Download PDF

Info

Publication number
CN103882680B
CN103882680B CN201410127728.0A CN201410127728A CN103882680B CN 103882680 B CN103882680 B CN 103882680B CN 201410127728 A CN201410127728 A CN 201410127728A CN 103882680 B CN103882680 B CN 103882680B
Authority
CN
China
Prior art keywords
real silk
groove
washing
silk fabric
bleaching
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410127728.0A
Other languages
English (en)
Other versions
CN103882680A (zh
Inventor
钱英莺
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Money Emperor Network Polytron Technologies Inc
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410127728.0A priority Critical patent/CN103882680B/zh
Publication of CN103882680A publication Critical patent/CN103882680A/zh
Application granted granted Critical
Publication of CN103882680B publication Critical patent/CN103882680B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种真丝织物挂练练漂的方法,预处理:将真丝织物浸泡在1号挂练槽中,槽中纯碱1-2g/L,渗透剂JFC0.2-0.5g/L;精练:再将真丝织物放入2号挂练槽中,槽中真丝精练剂8-15g/L,合成洗涤剂1-3g/L,液体泡花碱1-3g/L,液体烧碱0.2-0.5g/L;水洗:再将精练好的真丝织物放入3号挂练槽中水洗;酶练:再将水洗后的真丝织物放入4号挂练槽中,槽中碱性蛋白酶0.4-1g/L,乙二胺四乙酸二钠0.5-1g/L,纯碱1-3g/L;漂白:再将酶练后的真丝织物放入5号挂练槽中,槽中过硫酸盐6-10g/L,焦磷酸钠2-4g/L;反复水洗,晾干或烘干,完成真丝织物的挂练练漂。

Description

一种真丝织物挂练练漂的方法
技术领域
本发明涉及一种真丝织物生产方法,特别涉及一种真丝织物挂练练漂的方法。
背景技术
真丝除了纤维的主体丝素外,还含有丝胶、蜡质、色素、无机物和碳水化合物等天然杂质,以及因织造所需添加的浸渍助剂等人为杂质。这些杂质的存在不仅有损于丝绸柔软、光亮和洁白等优良品质,而且会影响真丝织物的后续染整加工。因此,真丝织物需要经过精练和漂白处理。真丝挂练常用的工艺有皂碱法、专用丝绸精练剂法、酶-合成洗涤剂法及合成洗涤剂碱法。皂碱法精练易产生白雾、皂迹、出水不清等病疵,专用精练剂法脱胶速度慢,织物毛效略差,酶-合成洗涤剂法织物手感略差,绉效应差,合成洗涤剂碱法手感略差,绉效应差。精练后丝绸产品为除去色素,一般采用保险粉或者双氧水漂白。保险粉气味较大、易自燃,运输和存储要求高,生产效率较低,双氧水漂白织物易带红光,影响丝绸品质及后续染整加工。
发明内容
本发明所要解决的技术问题是,针对现有生产技术的不足,生产效率低下等问题,提供一种真丝织物挂练练漂的方法。
为了实现上述目的,本发明所采取的措施:
一种真丝织物挂练练漂的方法,步骤一:预处理:将真丝织物浸泡在60℃-70℃的1号挂练槽中,槽中纯碱1-2g/L,渗透剂JFC0.2-0.5g/L,浸泡时间为60-90分钟;步骤二:精练:将步骤一中预处理好的的真丝织物放入2号挂练槽中,槽中真丝精练剂8-15g/L,合成洗涤剂1-3g/L,液体泡花碱1-3g/L,液体烧碱0.2-0.5g/L,真丝精练剂由聚丙烯酸钠、乙二胺四乙酸二钠和表面活性剂组成,精练溶液的pH为10-11.5,温度90-95℃,浸泡时间为40-60min;步骤三:水洗:将步骤二中精练好的真丝织物放入3号挂练槽中水洗,水洗温度60-70℃,时间10min;步骤四:酶练:将步骤三中水洗后的真丝织物放入4号挂练槽中,槽中碱性蛋白酶0.4-1g/L,乙二胺四乙酸二钠0.5-1g/L,纯碱1-3g/L,酶练溶液pH为9-11,温度40-45℃,酶练时间为50-60min;步骤五:漂白:将步骤四中酶练后的真丝织物放入5号挂练槽中,槽中过硫酸盐6-10g/L,焦磷酸钠2-4g/L,漂白溶液的pH为7-8,温度60-70℃,漂白时间为50-70min;步骤六:水洗:将步骤五中漂白的真丝织物放入6号挂练槽中水洗,水洗温度60-70℃,水洗时间为20min-30min;步骤七:水洗:将步骤六中水洗后的真丝织物放入7号挂练槽中水洗,水洗温度40-50℃,时间20min-30min;步骤八:水洗:将步骤七中水洗后的真丝织物放入8号挂练槽中,室温水洗20min-30min,晾干或烘干,完成真丝织物的挂练练漂。
所述的步骤五中过硫酸盐为过硫酸钾或过硫酸钠。
所述的渗透剂JFC为脂肪醇聚氧乙烯醚。
本发明的有益效果:提高了生产效率,生产出的真丝织物手感好,光泽度好,提高了真丝织物的质量。
具体实施方式
一种真丝织物挂练练漂的方法,步骤一:预处理:将真丝织物浸泡在60℃-70℃的1号挂练槽中,槽中纯碱1-2g/L,渗透剂JFC0.2-0.5g/L,浸泡时间为60-90分钟;步骤二:精练:将步骤一中预处理好的的真丝织物放入2号挂练槽中,槽中真丝精练剂8-15g/L,合成洗涤剂1-3g/L,液体泡花碱1-3g/L,液体烧碱0.2-0.5g/L,真丝精练剂由聚丙烯酸钠、乙二胺四乙酸二钠和表面活性剂组成,精练溶液的pH为10-11.5,温度90-95℃,浸泡时间为40-60min;步骤三:水洗:将步骤二中精练好的真丝织物放入3号挂练槽中水洗,水洗温度60-70℃,时间10min;步骤四:酶练:将步骤三中水洗后的真丝织物放入4号挂练槽中,槽中碱性蛋白酶0.4-1g/L,乙二胺四乙酸二钠0.5-1g/L,纯碱1-3g/L,酶练溶液pH为9-11,温度40-45℃,酶练时间为50-60min;步骤五:漂白:将步骤四中酶练后的真丝织物放入5号挂练槽中,槽中过硫酸盐6-10g/L,焦磷酸钠2-4g/L,漂白溶液的pH为7-8,温度60-70℃,漂白时间为50-70min;步骤六:水洗:将步骤五中漂白的真丝织物放入6号挂练槽中水洗,水洗温度60-70℃,水洗时间为20min-30min;步骤七:水洗:将步骤六中水洗后的真丝织物放入7号挂练槽中水洗,水洗温度40-50℃,时间20min-30min;步骤八:水洗:将步骤七中水洗后的真丝织物放入8号挂练槽中,室温水洗20min-30min,晾干或烘干,完成真丝织物的挂练练漂。
所述的步骤五中过硫酸盐为过硫酸钾或过硫酸钠。
所述的渗透剂JFC为脂肪醇聚氧乙烯醚。
步骤一中的预处理采用中温长时间浸泡,有效地克服了脱胶不匀、减少了灰伤,改善了产品手感,步骤二中精练时间相应缩短。碱性精练过程采用真丝精练剂和合成洗涤剂,脱胶速度快,精练过后进一步采用酶练,提升了练后织物的手感和绉效应。
采用过硫酸盐漂白真丝织物,漂白条件温和,节能降耗,漂白产品白度好,色光正,提升了产品质量和稳定性。

Claims (2)

1.一种真丝织物挂练练漂的方法,其特征在于:步骤一:预处理:将真丝织物浸泡在60℃-70℃的1号挂练槽中,槽中纯碱1-2g/L,渗透剂JFC0.2-0.5g/L,浸泡时间为60-90分钟;步骤二:精练:将步骤一中预处理好的的真丝织物放入2号挂练槽中,槽中真丝精练剂8-15g/L,合成洗涤剂1-3g/L,液体泡花碱1-3g/L,液体烧碱0.2-0.5g/L,真丝精练剂由聚丙烯酸钠、乙二胺四乙酸二钠和表面活性剂组成,精练溶液的pH为10-11.5,温度90-95℃,浸泡时间为40-60min;步骤三:水洗:将步骤二中精练好的真丝织物放入3号挂练槽中水洗,水洗温度60-70℃,时间10min;步骤四:酶练:将步骤三中水洗后的真丝织物放入4号挂练槽中,槽中碱性蛋白酶0.4-1g/L,乙二胺四乙酸二钠0.5-1g/L,纯碱1-3g/L,酶练溶液pH为9-11,温度40-45℃,酶练时间为50-60min;步骤五:漂白:将步骤四中酶练后的真丝织物放入5号挂练槽中,槽中过硫酸盐6-10g/L,焦磷酸钠2-4g/L,漂白溶液的pH为7-8,温度60-70℃,漂白时间为50-70min;步骤六:水洗:将步骤五中漂白的真丝织物放入6号挂练槽中水洗,水洗温度60-70℃,水洗时间为20min-30min;步骤七:水洗:将步骤六中水洗后的真丝织物放入7号挂练槽中水洗,水洗温度40-50℃,时间20min-30min;步骤八:水洗:将步骤七中水洗后的真丝织物放入8号挂练槽中,室温水洗20min-30min,晾干或烘干,完成真丝织物的挂练练漂。
2.根据权利要求1所述的一种真丝织物挂练练漂的方法,其特征在于:所述的步骤五中过硫酸盐为过硫酸钾或过硫酸钠。
CN201410127728.0A 2014-04-01 2014-04-01 一种真丝织物挂练练漂的方法 Active CN103882680B (zh)