CN103881402A - 一种彩色沥青及其制备方法 - Google Patents

一种彩色沥青及其制备方法 Download PDF

Info

Publication number
CN103881402A
CN103881402A CN201410088775.9A CN201410088775A CN103881402A CN 103881402 A CN103881402 A CN 103881402A CN 201410088775 A CN201410088775 A CN 201410088775A CN 103881402 A CN103881402 A CN 103881402A
Authority
CN
China
Prior art keywords
parts
asphalt
color asphalt
density polyethylene
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410088775.9A
Other languages
English (en)
Other versions
CN103881402B (zh
Inventor
林雨冬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shandong jiameitai New Material Co.,Ltd.
Original Assignee
JILIN JIARUI PITCH TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JILIN JIARUI PITCH TECHNOLOGY Co Ltd filed Critical JILIN JIARUI PITCH TECHNOLOGY Co Ltd
Priority to CN201410088775.9A priority Critical patent/CN103881402B/zh
Publication of CN103881402A publication Critical patent/CN103881402A/zh
Application granted granted Critical
Publication of CN103881402B publication Critical patent/CN103881402B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种彩色沥青及其制备方法,其按照重量份包括:40份-50份的芳香油、15份-20份的石油树脂、20份-30份的热塑性丁苯橡胶、10份-18份的低密度聚乙烯、1份-2份的抗老化剂与0.5份-1份的增粘助剂,及其制备方法。可以代替以往的黑色沥青路面及灰白色水泥路面,改善视觉,直接按照沥青路面的施工工艺,不需额外增加施工成本,并且其性能优良,不易脱落。

Description

一种彩色沥青及其制备方法
技术领域
本发明涉及彩色筑路高分子材料,尤其涉及一种彩色沥青及其制备方法。
背景技术
目前高分子材料和另外不同组成、不同形状、不同性质的物质复合粘结而成的多相固体材料,并且拥有界面的材料。高分子复合材料最大优点是博各种材料之长,如高强度、质轻、耐温、耐腐蚀、绝热、绝缘等性质,根据应用目的,选取高分子材料和其他具有特殊性质的材料,制成满足需要的复合材料。现有技术中常用的主要有用彩色陶瓷颗粒+聚氨酯粘合剂以及石油沥青脱色后再添加各种材料后染色的材料,彩色陶瓷颗粒+聚氨酯粘合剂的方式应用范围小,易脱落,而石油沥青脱色后再添加各种材料后染色的材料的方式,其工艺繁琐,成本高,指标低。
因此,现有技术还有待于更进一步的改进和发展。
发明内容
鉴于上述现有技术的不足,本发明的目的在于提供一种彩色沥青及其制备方法,降低其制造成本,拓展其应用空间。
本发明的技术方案如下:
一种彩色沥青,其按照重量份包括:
40份-50份的芳香油、15份-20份的石油树脂、20份-30份的热塑性丁苯橡胶、10份-18份的低密度聚乙烯、1份-2份的抗老化剂与0.5份-1份的增粘助剂。
所述的彩色沥青,其中,其按照重量份包括:30份的芳香油、20份的石油树脂、30的热塑性丁苯橡胶、15份的低密度聚乙烯、2份的抗老化剂与1份的增粘助剂。
一种所述彩色沥青的制备方法,其包括以下步骤:按照重量份依次将芳香油、石油树脂投入发育罐充分反应,然后再将热塑性丁苯橡胶、增粘助剂与抗老化剂投入所述发育罐内,最后将低密度聚乙烯投入所述发育罐内充分反应,制得所述彩色沥青。
本发明提供的一种彩色沥青及其制备方法,可以代替以往的黑色沥青路面及灰白色水泥路面,改善视觉,直接按照沥青路面的施工工艺,不需额外增加施工成本,并且其性能优良,不易脱落。
具体实施方式
本发明提供了一种彩色沥青及其制备方法,为使本发明的目的、技术方案及效果更加清楚、明确,以下对本发明进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定本发明。
本发明提供了一种彩色沥青,其按照重量份包括:40份-50份的芳香油、15份-20份的石油树脂、20份-30份的热塑性丁苯橡胶、10份-18份的低密度聚乙烯、1份-2份的抗老化剂与0.5份-1份的增粘助剂。
更进一步的,所述的彩色沥青按照重量份包括:30份的芳香油、20份的石油树脂、30的热塑性丁苯橡胶、15份的低密度聚乙烯、2份的抗老化剂与1份的增粘助剂。
本发明还提供了一种所述彩色沥青的制备方法,其包括以下步骤:按照重量份依次将芳香油、石油树脂投入发育罐充分反应,然后再将热塑性丁苯橡胶、增粘助剂与抗老化剂投入所述发育罐内,最后将低密度聚乙烯投入所述发育罐内充分反应,制得所述彩色沥青。
为了更进一步描述本发明,以下列举更详尽的实施例进行说明。
将50吨芳香油、18吨的石油树脂、25吨的热塑性丁苯橡胶、15吨的低密度聚乙烯、1吨的抗老化剂与0.5吨的增粘助剂,按照上述制备方法充分反应得到所述彩色沥青。其性能如表1与表2所示,
表1
Figure BDA0000475455180000031
表2
Figure BDA0000475455180000032
Figure BDA0000475455180000041
通过表1与表2的数据可以明显得出,本发明彩色沥青的性能远远高于现有技术中的彩色筑路高分子材料。
应当理解的是,本发明的应用不限于上述的举例,对本领域普通技术人员来说,可以根据上述说明加以改进或变换,所有这些改进和变换都应属于本发明所附权利要求的保护范围。

Claims (3)

1.一种彩色沥青,其按照重量份包括:
40份-50份的芳香油、15份-20份的石油树脂、20份-30份的热塑性丁苯橡胶、10份-18份的低密度聚乙烯、1份-2份的抗老化剂与0.5份-1份的增粘助剂。
2.根据权利要求1所述的彩色沥青,其特征在于,其按照重量份包括:30份的芳香油、20份的石油树脂、30的热塑性丁苯橡胶、15份的低密度聚乙烯、2份的抗老化剂与1份的增粘助剂。
3.一种如权利要求1所述彩色沥青的制备方法,其包括以下步骤:按照重量份依次将芳香油、石油树脂投入发育罐充分反应,然后再将热塑性丁苯橡胶、增粘助剂与抗老化剂投入所述发育罐内,最后将低密度聚乙烯投入所述发育罐内充分反应,制得所述彩色沥青。
CN201410088775.9A 2014-03-11 2014-03-11 一种彩色沥青及其制备方法 Active CN103881402B (zh)