CN103834278A - 一种安全环保耐磨紫外光固化涂料及其制备方法 - Google Patents
一种安全环保耐磨紫外光固化涂料及其制备方法 Download PDFInfo
- Publication number
- CN103834278A CN103834278A CN201410075434.8A CN201410075434A CN103834278A CN 103834278 A CN103834278 A CN 103834278A CN 201410075434 A CN201410075434 A CN 201410075434A CN 103834278 A CN103834278 A CN 103834278A
- Authority
- CN
- China
- Prior art keywords
- parts
- bamboo charcoal
- minute
- nano
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (2)