CN1037691C - 水性防水剂 - Google Patents
水性防水剂 Download PDFInfo
- Publication number
- CN1037691C CN1037691C CN 94112116 CN94112116A CN1037691C CN 1037691 C CN1037691 C CN 1037691C CN 94112116 CN94112116 CN 94112116 CN 94112116 A CN94112116 A CN 94112116A CN 1037691 C CN1037691 C CN 1037691C
- Authority
- CN
- China
- Prior art keywords
- water
- agent
- watery
- proofing agent
- present
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了一种建筑用的水性防水剂,按重量计它含有氧化沥青15-25%,澄清油10-25%,膨润土8-15%,滑石粉0-3%,水40-60%,十二烷基硫酸钠0.02-0.05%,聚甲基丙酸钠盐0-0.2%。本发明可适用于屋面防水和地下建筑物防水,可可作粘结剂,防锈剂,堵漏胶。
Description
本发明涉及一种建筑防水涂料,具体地说明是水性防水剂。
国内屋面防水,一般都用传统的老方法,即“三油二毡”或称热粘法,即使用熔融的热沥青粘结油毡,此法粘结力强,施工麻烦。该法每平方米造价17元左右。另外屋面防水也用冷粘法,使用溶剂型冷胶粘剂或水乳型冷胶粘剂,涂于屋面,再敷上无纺布,再涂上一层冷胶粘剂,再敷上一层无纺布,最后涂上一层冷胶粘剂。此法粘结性能劣于热粘法,且有50%左右溶剂挥发,对环境污染比热粘法更加严重。该法每平方米造价13.7元。地下防水,即用于地下池、浴池、游泳池、隧道、地下工程、矿井等。通常用于地下工程防水剂为聚氨酯型,其性能较好,但其原料为二异氰酸酯,大多靠国外进口,使用时为两组组分混合,适用期一般只有20分钟,超过时间就不能用,同时价格昂贵。本溪某化工厂生产一种固体防水剂,其成份为增水性的高分子聚合物,以及加少量的交联剂,加水泥,滑石粉作为填充物,该固体防水剂施工麻烦,造价高。国内以往用传统水乳型改良沥青防水涂料,即用沥青乳液与橡胶乳液按一定比例混合而成,由于存在此涂层薄,强度不过关,涂层厚,延伸性和低温韧性不过关,因此使用很困难,易发生质量事故。武汉大学有机建材研究所研制一种SBR改良沥青厚质防水涂料,解决了以上问题,但是此新产品存在原料来源困难,价格高,使用涂层厚、费用大,且产品只能储存一年,怕冻。中国专利局1987年11月18日公告,申请号为87102242,名为“一种建筑防水涂料”,该发明特征是在分散相中增加三类物质,即增韧剂、增容剂和增强剂。对改善建筑防水涂料性能起积极作用。从上看来,国内对防水剂研究是在不断创新。
本发明的目的在于提供一种使用方便效果好,成本低,原料易得,无三废,成品无污染,便于长期保管的优质水性防水剂。
为了实现述目的,本发明采用如下技术方案:一种水性防水剂,其特征在于按重量计它含有:氧化沥青15-25%,澄清油10-25%,膨润土8-15%,滑石粉0-3%,水40-60%,十二烷基硫酸钠0.02-0.05%,聚甲基丙烯酸钠盐0-0.2%。
本发明与已有技术相比,具有显而易见优点:原料来源广,成本较低;溶剂为水介质,无污染,制造时无三废;防水性能好;该产品使用方便,可以喷、涂、刷均可,不怕冻,储存期六年以上性能仍良好;可作粘结剂,粘结强度达8.3mpa;加入酒精或醋酸乙酯,即可作溶剂型防锈剂,堵漏胶。
以下结合实施例对本发明做进一步说明:
实施例一、一利水性防水剂,用于屋面防水剂,按重量计它含有:氧化沥青24%,澄清油13%,膨润土11%,滑石粉2%,水50%,十二烷基硫酸钠0.03%,聚甲基丙烯酸钠盐0.02%。
实施例二、一种水性防水剂,用于地下工程防水剂,按重量计它含有氧化沥青25%,澄清油16%,膨润土13%,滑石粉1%,水45%,十二烷基硫酸钠0.03%,聚甲基丙烯酸钠0.02%。
屋面防水要求增加涂层的硬度,有一定粘着力与柔韧性,因此增加氧化沥青与滑石粉。地下防水要求增加粘结力与柔韧性,因此增加澄清油、减少滑石粉,为了增加浓度,因此减少水。
操作条件,将水温40℃-60℃与膨润土加滑石粉调成糊状,在不断搅拌情况下,依次分批加入水、十二烷基硫酸钠,聚甲基丙烯酸钠盐,然后分数批加入已混合好的氧化沥青和澄清油混合物,维持50℃-90℃,反应3-5小时左右,最后产品呈黑褐色分散微颗粒物,即为成品。
附表1是本发明水性防水剂的试验数据。
附表2是本发明水性防水剂抗拉强度检验数据。
附表1
名称 | 延伸性(无处理)不小于 | 柔韧性℃ | 耐热性℃ | 粘结力mpa | 不透水性mpa | 冷冻性次 |
水性防水剂 | 7.5 | -20 | 80 | 8.3 | 0.1(30分) | 20 |
附表2
名 称 | 螺丝 | 木条 | 纸条 | 瓷砖 | 延伸率 |
水性防水剂 | 23.1mpa | 2.60mpa | 2.73mpa | 1.47mpa | 7.5% |
Claims (1)
1.一种水性防水剂,其特征在于按重量计它含有:
氧化沥青 15-25%
澄清油 10-25%
膨润土 8-15%
滑石粉 0-3%
水 40-60%
十二烷基硫酸钠 0.02-0.05%
聚甲基丙烯酸钠盐 0-0.2%。