CN103757890B - A kind of western-style clothes finishing agent and preparation method thereof - Google Patents

A kind of western-style clothes finishing agent and preparation method thereof Download PDF

Info

Publication number
CN103757890B
CN103757890B CN201310751659.6A CN201310751659A CN103757890B CN 103757890 B CN103757890 B CN 103757890B CN 201310751659 A CN201310751659 A CN 201310751659A CN 103757890 B CN103757890 B CN 103757890B
Authority
CN
China
Prior art keywords
parts
western
finishing agent
style clothes
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201310751659.6A
Other languages
Chinese (zh)
Other versions
CN103757890A (en
Inventor
罗文亮
谭金安
邓红梅
周崇恩
赖琼华
邓波
卢光凤
庞建英
龙远生
周风华
谭翔宇
刘建兰
文明
黄结应
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hunan Dongfang Fashion Co., Ltd.
Original Assignee
HUNAN DONGFANG FASHION CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUNAN DONGFANG FASHION CO Ltd filed Critical HUNAN DONGFANG FASHION CO Ltd
Priority to CN201310751659.6A priority Critical patent/CN103757890B/en
Publication of CN103757890A publication Critical patent/CN103757890A/en
Application granted granted Critical
Publication of CN103757890B publication Critical patent/CN103757890B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of western-style clothes finishing agent and preparation method thereof, western-style clothes finishing agent is made up of according to weight ratio following composition: ethyoxyl aminopropyl dimethyl silicone polymer is 4 ~ 6 parts, ammonium dihydrogen phosphate (ADP) is 2 ~ 4 parts, calcium monohydrogen phosphate is 3 ~ 5 parts, sodium carboxymethylcellulose is 7 ~ 9 parts, mannosan is 5 ~ 6 parts, OPEO is 3 ~ 5 parts, ethanol is 35 ~ 55 parts, water is 210 ~ 220 parts.Carry out the heating of finishing agent composition by regulating after temperature, the step such as mixer carries out stirring, inflated with nitrogen, the refusing water, refuse oil of the western-style clothes finishing agent prepared, anti-wrinkle effect are better, western-style clothes can be allowed to possess and refuse water, refuse oil, crease-resistant performance.

Description

A kind of western-style clothes finishing agent and preparation method thereof
Technical field
The present invention relates to a kind of possess refuse water, refuse oil, the finishing agent of crease-resistant character and preparation method thereof, particularly relate to a kind of possess refuse water, refuse oil, the western-style clothes finishing agent of crease-resistant character and preparation method thereof.
Background technology
Western-style clothes is a kind of clothes that business people needs often dress.Western-style clothes material mostly is cotton, hair and silk etc.Western-style clothes is in wearing process, and water repellency, oil repellent energy, wrinkle resistance have important effect to it.Conventional Western-style clothes is after repeatedly wearing, and Western-style clothes there will be fold, affects the attractive in appearance of Western-style clothes.If when attending the dinner, when having oily matter to fall on Western-style clothes, the performance of oil refused by common Western-style clothes owing to not having, oily matter just can be adsorbed on western-style clothes, not easily removes.Aqueous substance drops and does not have on the western-style clothes of waterproofing function, makes troubles also can to the work of people.Therefore, be necessary to develop a kind of finishing agent, improve the wrinkle resistance of western-style clothes, water repellency, oil repellent energy.
Summary of the invention
The technical problem solved: common western-style clothes fold after repeatedly wearing is more, common western-style clothes is refused water and is refused the problem of oily poor-performing simultaneously.
Technical scheme: the invention discloses a kind of western-style clothes finishing agent and preparation method thereof, western-style clothes finishing agent is made up of according to weight ratio following composition: ethyoxyl aminopropyl dimethyl silicone polymer is 4 ~ 6 parts, ammonium dihydrogen phosphate (ADP) is 2 ~ 4 parts, calcium monohydrogen phosphate is 3 ~ 5 parts, sodium carboxymethylcellulose is 7 ~ 9 parts, mannosan is 5 ~ 6 parts, OPEO is 3 ~ 5 parts, ethanol is 35 ~ 55 parts, water is 210 ~ 220 parts.
A preparation method for western-style clothes finishing agent, preparation method comprises the following steps: (1) gets airtight reactor, temperature of reaction kettle is set as 66 DEG C ~ 70 DEG C; (2) airtight reactor is opened, in reactor, add that water is 210 ~ 220 parts, ethanol is 35 ~ 55 parts, ammonium dihydrogen phosphate (ADP) is 2 ~ 4 parts, calcium monohydrogen phosphate is 3 ~ 5 parts, sodium carboxymethylcellulose is 7 ~ 9 parts, stir with mixer, speed of agitator is 200r/min; (3) in reactor, add after stirring that ethyoxyl aminopropyl dimethyl silicone polymer is 4 ~ 6 parts, mannosan is 5 ~ 6 parts, OPEO is 3 ~ 5 parts again, stir with mixer, speed of agitator is 150r/min, stirs; (4) loaded in storage bucket by the finishing agent after stirring, after being filled with nitrogen, sealing is preserved.
The sodium carboxymethylcellulose added during preparation is preferably 9 parts.The calcium monohydrogen phosphate added during preparation is preferably 4 ~ 5 parts.The OPEO added during preparation is preferably 3 ~ 4 parts.
beneficial effect:cotton western-style clothes is after arranging through finishing agent of the present invention, and refusing water grade is 5 grades, and refuse wet goods level and be 6 to 7 grades, cotton western-style clothes also has good wrinkle resistance.
Detailed description of the invention
Embodiment 1
(1) get airtight reactor, temperature of reaction kettle is set as 70 DEG C; (2) open airtight reactor, add that water is 210kg, ethanol is 55kg, ammonium dihydrogen phosphate (ADP) is 4kg, calcium monohydrogen phosphate is 3kg, sodium carboxymethylcellulose is 9kg in reactor, stir with mixer, speed of agitator is 200r/min; (3) in reactor, add after stirring that ethyoxyl aminopropyl dimethyl silicone polymer is 4kg, mannosan is 6kg, OPEO is 3kg again, stir with mixer, speed of agitator is 150r/min, stirs; (4) loaded in storage bucket by the finishing agent after stirring, after being filled with nitrogen, sealing is preserved.
Embodiment 2
(1) get airtight reactor, temperature of reaction kettle is set as 66 DEG C; (2) open airtight reactor, add that water is 215kg, ethanol is 35kg, ammonium dihydrogen phosphate (ADP) is 3kg, calcium monohydrogen phosphate is 5kg, sodium carboxymethylcellulose is 7kg in reactor, stir with mixer, speed of agitator is 200r/min; (3) in reactor, add after stirring that ethyoxyl aminopropyl dimethyl silicone polymer is 5kg, mannosan is 5kg, OPEO is 4kg again, stir with mixer, speed of agitator is 150r/min, stirs; (4) loaded in storage bucket by the finishing agent after stirring, after being filled with nitrogen, sealing is preserved.
Embodiment 3
(1) get airtight reactor, temperature of reaction kettle is set as 68 DEG C; (2) open airtight reactor, add that water is 220kg, ethanol is 45kg, ammonium dihydrogen phosphate (ADP) is 2kg, calcium monohydrogen phosphate is 4kg, sodium carboxymethylcellulose is 8kg in reactor, stir with mixer, speed of agitator is 200r/min; (3) in reactor, add after stirring that ethyoxyl aminopropyl dimethyl silicone polymer is 6kg, mannosan is 6kg, OPEO is 5kg again, stir with mixer, speed of agitator is 150r/min, stirs; (4) loaded in storage bucket by the finishing agent after stirring, after being filled with nitrogen, sealing is preserved.
Soak 1h by the finishing agent being dipped into embodiment 1, embodiment 2, embodiment 3 under cotton western-style clothes room temperature, after a leaching one is rolled, pick-up is 65%, dries at 95 DEG C.Refusing water, refusing oily measure of merit standard is AATCC22-2010, AATCC118, and result is as following table.
Embodiment 1 Embodiment 2 Embodiment 3
Refuse water grade 5 grades 5 grades 5 grades
Refuse wet goods level 7 grades 7 grades 6 grades
Anti-wrinkle effect Fold is not had after wearing 5 times Fold is not had after wearing 3 times Fold is not had after wearing 4 times
Western-style clothes after finishing agent of the present invention arranges, has good water repellency and oil repellent energy, also has good anti-wrinkle effect simultaneously.

Claims (4)

1. a western-style clothes finishing agent, is characterized in that western-style clothes finishing agent is made up of according to weight ratio following composition: ethyoxyl aminopropyl dimethyl silicone polymer is 4 ~ 6 parts, ammonium dihydrogen phosphate (ADP) is 2 ~ 4 parts, calcium monohydrogen phosphate is 3 ~ 5 parts, sodium carboxymethylcellulose is 7 ~ 9 parts, mannosan is 5 ~ 6 parts, OPEO is 3 ~ 5 parts, ethanol is 35 ~ 55 parts, water is 210 ~ 220 parts;
The preparation method of described a kind of western-style clothes finishing agent, comprises the following steps: (1) gets airtight reactor, temperature of reaction kettle is set as 66 DEG C ~ 70 DEG C; (2) airtight reactor is opened, in reactor, add that water is 210 ~ 220 parts, ethanol is 35 ~ 55 parts, ammonium dihydrogen phosphate (ADP) is 2 ~ 4 parts, calcium monohydrogen phosphate is 3 ~ 5 parts, sodium carboxymethylcellulose is 7 ~ 9 parts, stir with mixer, speed of agitator is 200r/min; (3) in reactor, add after stirring that ethyoxyl aminopropyl dimethyl silicone polymer is 4 ~ 6 parts, mannosan is 5 ~ 6 parts, OPEO is 3 ~ 5 parts again, stir with mixer, speed of agitator is 150r/min, stirs; (4) loaded in storage bucket by the finishing agent after stirring, after being filled with nitrogen, sealing is preserved.
2. a kind of western-style clothes finishing agent according to claim 1, is characterized in that the sodium carboxymethylcellulose added when preparing is 9 parts.
3. a kind of western-style clothes finishing agent according to claim 1, is characterized in that the calcium monohydrogen phosphate added when preparing is 4 ~ 5 parts.
4. a kind of western-style clothes finishing agent according to claim 1, is characterized in that the OPEO added when preparing is 3 ~ 4 parts.
CN201310751659.6A 2013-12-31 2013-12-31 A kind of western-style clothes finishing agent and preparation method thereof Expired - Fee Related CN103757890B (en)