CN103741326B - 一种耐磨的棉麻混纺面料的制备方法 - Google Patents

一种耐磨的棉麻混纺面料的制备方法 Download PDF

Info

Publication number
CN103741326B
CN103741326B CN201310688415.8A CN201310688415A CN103741326B CN 103741326 B CN103741326 B CN 103741326B CN 201310688415 A CN201310688415 A CN 201310688415A CN 103741326 B CN103741326 B CN 103741326B
Authority
CN
China
Prior art keywords
cotton
fabric
linen
blended spinning
wear
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310688415.8A
Other languages
English (en)
Other versions
CN103741326A (zh
Inventor
袁洪兵
陈红霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhuhai Useless Culture And Creative Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310688415.8A priority Critical patent/CN103741326B/zh
Publication of CN103741326A publication Critical patent/CN103741326A/zh
Application granted granted Critical
Publication of CN103741326B publication Critical patent/CN103741326B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种耐磨的棉麻面料的制备方法,包括以下步骤:(1)配制棉麻面料涂层,取聚酯树脂为3~5份、硅酸钙粉末为1~2份、二氧化硅粉末为1~2份,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在68℃~72℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.2mm~0.5mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻面料。

Description

一种耐磨的棉麻混纺面料的制备方法
技术领域
本发明涉及一种棉麻面料的制备方法,特别是涉及一种耐磨的棉麻混纺面料的制备方法。
背景技术
棉麻面料是人们在生活中最常遇到的一种混纺面料,棉麻面料在被用于一些常涉及到磨擦的环境当中时,如拖布、抹布等。对于棉麻面料的耐磨性能要求较高。未经过处理的棉麻面料,经过长时间的磨擦后,棉麻面料会产生一定的磨损,纤维会受到损坏,影响了棉麻面料的性能。提高棉麻面料的耐磨性能,降低其在多次磨擦后的损失,有多种方法,需要我们更加深入的进行研究。
发明内容
要解决的技术问题:普通的棉麻面料的耐磨擦性能差的问题。
技术方案:本发明公开了一种耐磨的棉麻混纺面料的制备方法,包括以下步骤:(1)配制棉麻面料涂层,取聚酯树脂为3~5份、硅酸钙粉末为1~2份、二氧化硅粉末为1~2份,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在68℃~72℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.2mm~0.5mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻面料。
其中,所述的聚酯树脂优选为3份。所述的二氧化硅粉末目数优选为330目。聚酯树脂的分子量优选为1000~10000。聚酯树脂的分子量更优选为3000~10000。有益效果:本发明的棉麻混纺面料在织物平模试验仪上磨擦300转后,重量损失率只有0.33%至0.41%,具有非常良好的耐磨性能。
具体实施方式
实施例1
(1)配制棉麻面料涂层,取聚酯树脂为3kg、硅酸钙粉末为1kg、二氧化硅粉末为2kg,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在68℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.2mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻混纺面料。
实施例2
(1)配制棉麻面料涂层,取聚酯树脂为4kg、硅酸钙粉末为2kg、二氧化硅粉末为1kg,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在72℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.4mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻混纺面料。
实施例3
(1)配制棉麻面料涂层,取聚酯树脂为5kg、硅酸钙粉末为1kg、二氧化硅粉末为1kg,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在70℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.5mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻混纺面料。
取实施例1、实施例2、实施例3的圆形棉麻面料,直径为150cm,使用圆盘织物平磨实验仪进行磨擦实验,重锤质量为400g,测定其磨擦300转后的重量损失率,结果如下表。
实施例1 实施例2 实施例3
重量损失率 0.37% 0.41% 0.33%
经过实验后,棉麻面料的重量损失率都很低,具备了很高的耐磨性能,可用于制备一些磨擦中常用的布料。

Claims (5)

1.一种耐磨的棉麻混纺面料的制备方法,其特征在于包括以下步骤:(1)配制棉麻面料涂层,取聚酯树脂为3~5份、硅酸钙粉末为1~2份、二氧化硅粉末为1~2份,加热后将三种成分混合均匀;(2)取圆形棉麻混纺面料,展开后喷洒蒸馏水到棉麻混纺面料上,再在68℃~72℃下烘干;(3)将涂层液均匀的刮涂在棉麻混纺面料的外层上,刮涂层的厚度为0.2mm~0.5mm;(4)最后将圆形棉麻混纺面料在通风的情况下,温度为80℃下烘干后保存,制备得耐磨的棉麻混纺面料。
2.根据权利要求1所述的一种耐磨的棉麻混纺面料的制备方法,其特征在于所述的聚酯树脂为3份。
3.根据权利要求1所述的一种耐磨的棉麻混纺面料的制备方法,其特征在于所述的二氧化硅粉末为330目。
4.根据权利要求1所述的一种耐磨的棉麻混纺面料的制备方法,其特征在于聚酯树脂的分子量为1000~10000。
5.根据权利要求1所述的一种耐磨的棉麻混纺面料的制备方法,其特征在于聚酯树脂的分子量为3000~10000。
CN201310688415.8A 2013-12-17 2013-12-17 一种耐磨的棉麻混纺面料的制备方法 Active CN103741326B (zh)