CN103721857B - 一种硅锌矿物捕收剂的制备方法 - Google Patents
一种硅锌矿物捕收剂的制备方法 Download PDFInfo
- Publication number
- CN103721857B CN103721857B CN201310751000.0A CN201310751000A CN103721857B CN 103721857 B CN103721857 B CN 103721857B CN 201310751000 A CN201310751000 A CN 201310751000A CN 103721857 B CN103721857 B CN 103721857B
- Authority
- CN
- China
- Prior art keywords
- willemite
- collecting agent
- thing
- seedlings
- roots
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
一种硅锌矿物捕收剂的制备方法,包括如下步骤:以大豆、蓖麻耔、茶树耔和茶树树皮中的两种或三种为原料。经烘干、粉碎和过筛,按质量比取:果树皮粉末:三乙醇胺:水=5~8:2~4:5~10,加热至120~130℃,通入氮气搅拌反应2~3h,再升温至150~160℃,通入氮气搅拌反应2~3h,冷却至60℃以下,取滤液用离心沉淀机进行2~3次离心分离。上层清液进行减压蒸馏,得深黄色浓缩液,在60~70℃水浴中加热,将溶剂蒸干,完全干燥后得到黄色粉末即为硅锌矿矿物的捕收剂。采用本发明所述捕收剂能够有效捕收泥化、含白云石的硅锌矿物。
Description
一、技术领域
本发明涉及一种硅锌矿矿物的捕收剂,特别是对于含泥和含白云石脉石的硅锌矿。
二、背景技术
氧化锌矿种类繁多,常见的有工业价值的氧化锌矿物是菱锌矿(ZnC03)和异极矿[ZnSi2O7·(OH)2·H2O]、硅锌矿(ZnSiO3)、水锌矿[3Zn(OH)2·2ZnCO3]、红锌矿(ZnO)等。菱锌矿和异极矿的回收,目前最有效的方法是硫化胺浮选法。硅锌矿往往与菱锌矿共存,长期以来,由于硅锌矿物难捕收,在回收氧化锌矿时常常不能有效回收,造成了极大的资源浪费。
三、发明内容
本发明的目的在于提供一种硅锌矿物捕收剂的制备方法,制备得的捕收剂能够有效捕收泥化、含白云石的硅锌矿物,药剂用量少,无毒无污染。
本发明采用以下技术方案达到上述目的:一种硅锌矿物捕收剂的制备方法,包括如下步骤:以植物果实、果皮或树皮为原料,洗净后低温烘干、粉碎,过100目筛,按质量比取:果树皮粉末:三乙醇胺:水=5~8:2~4:5~10,加热至120~130℃,通入氮气搅拌反应2~3h,再升温至150~160℃,通入氮气搅拌反应2~3h,冷却至60℃以下,过滤3~5次,取滤液用离心沉淀机进行2~3次离心分离,上层清液进行减压蒸馏,得深黄色浓缩液,在60~70℃水浴中加热,将溶剂蒸干,得到的粘稠液体在温度为60℃的真空干燥箱中干燥,得到黄褐色粘稠固体,完全干燥后得到黄色粉末即为硅锌矿矿物的捕收剂。
所述果树皮原料为蓖麻耔、茶油耔、大豆和茶树树皮中的两种或三种。
浮选时,矿浆pH值为12~13,浮选过程中,将矿石磨矿至矿物单体解离后,加入分散剂、抑制剂和活化剂,按1000~1500g/t加入所述捕收剂,然后再加起泡剂。
使用时,将所述抑制剂先配制成质量百分浓度为1~3%的水溶液。
药剂总用量为:1000~1500g/t。
本发明的具体优点在于:
1、采用本发明制备的捕收剂能够对含泥、白云石脉石矿物硅锌矿进行较好的捕收作用,使有用矿物获得较好的回收率和精矿品位。
2、药剂用量少,无毒无污染。
四、具体实施方式
以下通过具体实施例对本发明的技术方案作进一步描述。
实施例1
本发明所述硅锌矿物捕收剂的制备方法的一个实例,包括以下步骤:
以茶树耔、蓖麻耔和茶树树皮为原料,洗净后低温烘干、粉碎,过100目筛,得所述果皮粉末,按质量比取:果皮粉末:三乙醇胺:水=6:4:10,加热至120℃,通入氮气搅拌反应2h,再升温至150~160℃,通入氮气搅拌反应2~3h,用冷水浴冷却至60℃以下,用纱布过滤5次,取滤液用离心沉淀机进行2~3次离心分离,上层清液收集于圆底烧瓶中进行减压蒸馏,得深黄色浓缩液,在温度为60~70℃水浴中加热,将溶剂蒸干,得到的粘稠液体在真空干燥箱中干燥,温度60℃左右,将溶剂蒸干,得到的粘稠液体在温度60℃的真空干燥箱中干燥,得到黄褐色粘稠固体,完全干燥后得到有特殊香味的黄色粉末即为硅锌矿物的捕收剂。
实施例2
本发明所述硅锌矿物捕收剂的制备方法的一个实例,包括以下步骤:
以大豆、蓖麻耔和茶树树皮为原料,洗净后低温烘干、粉碎,过100目筛,得所述果皮粉末,按质量比取:果皮粉末:三乙醇胺:水=6:4:10,加热至120℃,通入氮气搅拌反应保持2h,再升温至150~160℃,通入氮气搅拌反应2~3h,用冷水浴冷却至60℃以下,用纱布过滤5次,取滤液用离心沉淀机进行2~3次离心分离,上层清液收集于圆底烧瓶中进行减压蒸馏,得深黄色浓缩液,在温度为60~70℃水浴中加热,将溶剂蒸干,得到的粘稠液体在温度为60℃的真空干燥箱中干燥,将溶剂蒸干,得到黄褐色粘稠固体,完全干燥后得到有特殊香味的黄色粉末即为硅锌矿物的捕收剂。
实施例3
本实施例为所述硅锌矿物捕收剂在硅锌矿矿物浮选中的应用实例。
1、矿物原料:
原料矿石中硅锌矿中锌含量为10.2%,铁3.17%,铁主要以褐铁矿形式存在,矿石泥化严重。物相分析表明锌主要是以硅锌矿形式存在。
2、药剂制度及操作条件:用碳酸钠调矿浆pH到12~13、按六偏磷酸钠2000g/t,硫酸铜200g/t,捕收剂用量1200g/t,2号油60g/t药剂用量进行了一年100t/d工业扩大试验,结果表明采用以上工艺和药剂条件能够有效将泥化硅锌矿浮选回收,在给矿锌品位为10.2%条件下,经过一次粗选两次扫选及二次精选,浮选精矿锌品位可以达到45.8%,回收率达到80.25%。
实施例4
本实施例为所述硅锌矿物捕收剂在硅锌矿矿物浮选中的应用实例。
1、矿物原料
原料矿石中硅锌矿中锌含量为8.2%,白云石8.24%,铁主要以褐铁矿形式存在,矿石泥化严重。物相分析表明锌主要是以硅锌矿形式存在。
2、药剂制度及操作条件:碳酸钠调矿浆pH到12~13.5,按照捕收剂1300g/t,六偏磷酸钠3000g/t,硫酸铜200g/t,2号油80g/t的药剂用量进行了八个月200t/d的工业试验,结果表明采用上述工艺和药剂条件能够有效回收硅锌矿物,经过一次粗选两次扫选及二次精选,得到铅锑品位达到43.65%,回收率达到81.26%的浮选精矿。
Claims (4)
1.一种硅锌矿物捕收剂的制备方法,其特征在于,包括如下步骤:以植物果实、果皮或树皮为原料,洗净后低温烘干、粉碎,过100目筛,按质量比取:果树皮粉末:三乙醇胺:水=5~8:2~4:5~10,加热至120~130℃,通入氮气搅拌反应2~3h,再升温至150~160℃,通入氮气搅拌反应2~3h,冷却至60℃以下,过滤3~5次,取滤液用离心沉淀机进行2~3 次离心分离,上层清液进行减压蒸馏,得深黄色浓缩液,在60~70℃水浴中加热, 将溶剂蒸干, 得到的粘稠液体在温度为60℃的真空干燥箱中干燥, 得到黄褐色粘稠固体, 完全干燥后得到黄色粉末即为硅锌矿矿物的捕收剂。
2.根据权利要求1所述的硅锌矿物捕收剂的制备方法,其特征在于,所述果树皮原料为蓖麻耔、茶油耔、大豆和茶树树皮中的两种或三种。
3.权利要求1所述硅锌矿物捕收剂的应用,其特征在于,浮选时用碳酸钠调矿浆pH值为12~13,浮选过程中,将矿石磨矿至矿物单体解离后,加入分散剂、抑制剂和活化剂,按捕收剂用量为1000~1500 g/t加入所述捕收剂,然后再加起泡剂。
4.根据权利要求3所述硅锌矿物捕收剂的应用,其特征在于,使用时,将所述抑制剂先配制成质量百分浓度为1~3%的水溶液。