CN103666096B - 一种固化快且环保的uv固化油墨及其制备方法 - Google Patents

一种固化快且环保的uv固化油墨及其制备方法 Download PDF

Info

Publication number
CN103666096B
CN103666096B CN201310601034.1A CN201310601034A CN103666096B CN 103666096 B CN103666096 B CN 103666096B CN 201310601034 A CN201310601034 A CN 201310601034A CN 103666096 B CN103666096 B CN 103666096B
Authority
CN
China
Prior art keywords
phenyl
butyl
environmental protection
acetone
hydroxy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310601034.1A
Other languages
English (en)
Other versions
CN103666096A (zh
Inventor
陈可夏
陈可亮
潮建平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Hengji Ink Technology Co ltd
Original Assignee
Tongling Founder Plastics Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tongling Founder Plastics Technology Co Ltd filed Critical Tongling Founder Plastics Technology Co Ltd
Priority to CN201310601034.1A priority Critical patent/CN103666096B/zh
Publication of CN103666096A publication Critical patent/CN103666096A/zh
Application granted granted Critical
Publication of CN103666096B publication Critical patent/CN103666096B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种固化快且环保的UV固化油墨,其特征在于,由下列重量份的原料制备制成:有机颜料1-3、二甲基硅油3-5、柠檬酸三丁酯2-3、高岭土1-2、水滑石粉2-3、二氧化钛1-2、聚丙烯酸丁酯12-14、脂肪酸聚乙二醇酯11-15、二缩三丙二醇二丙烯酸酯16-19、2-羟基-2-甲基-1-苯基-1-丙酮(1173)4-5、UV环氧丙烯酸酯12-15、2-氨基-5-(对-甲氧基苯基)-1,3,4-噻二唑镧2-3、三(2,4-二叔丁基苯基)亚磷酸酯4-5、助剂4-5;本发明的原料和制备方法所得的油墨固化快、生产周期短、操作简单方便、无溶剂污染,对环境友好。

Description

一种固化快且环保的UV固化油墨及其制备方法
技术领域
本发明涉及一种油墨及其制备方法,特别是一种固化快且环保的UV固化油墨及其制备方法。
背景技术
紫外光固化(UV)油墨是指在紫外线照射下,利用不同波长和能量的紫外光使油墨成膜和干燥的油墨。利用不同紫外光谱,可产生不同能量,将不同油墨连结料中的单体聚合成聚合物,所以UV油墨的色膜具有良好的机械和化学性能。UV油墨的主要优点有:(1)不用溶剂;(2)干燥速度快,耗能少;(3)光泽好,色彩鲜艳;(4)耐水、耐溶剂,耐磨性能好。UV油墨中光引发剂是一种易受光激发的化合物,在吸收光照后激发成自由基,能量转移给感光性分子或光交联剂,使UV墨发生光固化反应。目前UV墨已成为一种较成熟的油墨技术,其污染物排放几乎为零,不会污染大气,印刷品几乎无臭。
发明内容
本发明的目的是提供一种固化快且环保的UV固化油墨及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种固化快且环保的UV固化油墨,由下列重量份的原料制备制成:有机颜料1-3、二甲基硅油3-5、柠檬酸三丁酯2-3、高岭土1-2、水滑石粉2-3、二氧化钛1-2、聚丙烯酸丁酯12-14、脂肪酸聚乙二醇酯11-15、二缩三丙二醇二丙烯酸酯16-19、2-羟基-2-甲基-1-苯基-1-丙酮(1173)4-5、UV环氧丙烯酸酯12-15、2-氨基-5-(对-甲氧基苯基)-1,3,4-噻二唑镧2-3、三(2,4-二叔丁基苯基)亚磷酸酯4-5、助剂4-5;
所述助剂由下列重量份的原料制备而成:纳米硅藻土粉0.2-0.3、纳米云母粉0.2-0.3、硅烷偶联剂KH-5502-3、茶多酚2-3、新戊二醇5-7、对叔丁基苯甲酸1-2、抗氧剂10351-2、2-丁氧基-乙醇3-4、交联剂TAC2-3、乙氧基化三羟甲基丙烷三丙烯酸酯10-12、没食子酸丙酯2-3、薏仁油1-2;其制备方法是将各物料混合,加热至60-70℃,搅拌反应30-40分钟,即得。
本发明所述固化快且环保的UV固化油墨,由以下具体步骤制成:首先加入有机颜料、二甲基硅油、柠檬酸三丁酯、高岭土、水滑石粉、二氧化钛、聚丙烯酸丁酯、脂肪酸聚乙二醇酯、二缩三丙二醇二丙烯酸酯搅拌混匀,加热至80-90℃,搅拌25-35分钟;然后加入除2-羟基-2-甲基-1-苯基-1-丙酮(1173)之外的其余剩余成分,搅拌反应3-5小时;最后降温至60-70℃,加入2-羟基-2-甲基-1-苯基-1-丙酮(1173),搅拌反应40-50分钟,冷却后,研磨得到20-40μm浆料,即得。
本发明的有益效果是:本发明的原料和制备方法所得的油墨固化快、生产周期短、操作简单方便、无溶剂污染,对环境友好。
具体实施方案
下面通过具体实例对本发明进行详细说明。
一种固化快且环保的UV固化油墨,由下列重量份(公斤)的原料制备制成:有机颜料1、二甲基硅油3、柠檬酸三丁酯2、高岭土1、水滑石粉2、二氧化钛1、聚丙烯酸丁酯12、脂肪酸聚乙二醇酯11、二缩三丙二醇二丙烯酸酯16、2-羟基-2-甲基-1-苯基-1-丙酮(1173)4、UV环氧丙烯酸酯12、2-氨基-5-(对-甲氧基苯基)-1,3,4-噻二唑镧2、三(2,4-二叔丁基苯基)亚磷酸酯4、助剂4;
所述助剂由下列重量份(公斤)的原料制备而成:纳米硅藻土粉0.2、纳米云母粉0.2、硅烷偶联剂KH-5502、茶多酚2、新戊二醇5、对叔丁基苯甲酸1、抗氧剂10351、2-丁氧基-乙醇3、交联剂TAC2、乙氧基化三羟甲基丙烷三丙烯酸酯10、没食子酸丙酯2、薏仁油1;其制备方法是将各物料混合,加热至60-70℃,搅拌反应30-40分钟,即得。
本发明所述固化快且环保的UV固化油墨,由以下具体步骤制成:首先加入有机颜料、二甲基硅油、柠檬酸三丁酯、高岭土、水滑石粉、二氧化钛、聚丙烯酸丁酯、脂肪酸聚乙二醇酯、二缩三丙二醇二丙烯酸酯搅拌混匀,加热至80-90℃,搅拌25-35分钟;然后加入除2-羟基-2-甲基-1-苯基-1-丙酮(1173)之外的其余剩余成分,搅拌反应3-5小时;最后降温至60-70℃,加入2-羟基-2-甲基-1-苯基-1-丙酮(1173),搅拌反应40-50分钟,冷却后,研磨得到20-40μm浆料,即得。
所得的油墨,使用划格法牛皮胶带剥离,划格间距1mm,100%附着;使用浸有酒精的棉球,300克压力擦拭50次,无异状;浸泡于色拉油中(常温)8小时,无异状;使用浸有盐水的棉球,300克压力擦拭50次,无异状。

Claims (2)

1.一种固化快且环保的UV固化油墨,其特征在于,由下列重量份的原料制成:有机颜料1-3、二甲基硅油3-5、柠檬酸三丁酯2-3、高岭土1-2、水滑石粉2-3、二氧化钛1-2、聚丙烯酸丁酯12-14、脂肪酸聚乙二醇酯11-15、二缩三丙二醇二丙烯酸酯16-19、2-羟基-2-甲基-1-苯基-1-丙酮(1173)4-5、UV环氧丙烯酸酯12-15、2-氨基-5-(对-甲氧基苯基)-1,3,4-噻二唑镧2-3、三(2,4-二叔丁基苯基)亚磷酸酯4-5、助剂4-5;所述助剂由下列重量份的原料制备而成:纳米硅藻土粉0.2-0.3、纳米云母粉0.2-0.3、硅烷偶联剂KH-5502-3、茶多酚2-3、新戊二醇5-7、对叔丁基苯甲酸1-2、抗氧剂10351-2、2-丁氧基乙醇3-4、交联剂TAC2-3、乙氧基化三羟甲基丙烷三丙烯酸酯10-12、没食子酸丙酯2-3、薏仁油1-2;其制备方法是将各物料混合,加热至60-70℃,搅拌反应30-40分钟,即得。
2.根据权利要求1所述固化快且环保的UV固化油墨,其特征在于,由以下具体步骤制成:首先加入有机颜料、二甲基硅油、柠檬酸三丁酯、高岭土、水滑石粉、二氧化钛、聚丙烯酸丁酯、脂肪酸聚乙二醇酯、二缩三丙二醇二丙烯酸酯搅拌混匀,加热至80-90℃,搅拌25-35分钟;然后加入除2-羟基-2-甲基-1-苯基-1-丙酮(1173)之外的其余剩余成分,搅拌反应3-5小时;最后降温至60-70℃,加入2-羟基-2-甲基-1-苯基-1-丙酮(1173),搅拌反应40-50分钟,冷却后,研磨得到20-40μm浆料,即得。
CN201310601034.1A 2013-11-25 2013-11-25 一种固化快且环保的uv固化油墨及其制备方法 Active CN103666096B (zh)