CN103643516B - 一种玻璃纤维壁布涂层的制备方法 - Google Patents

一种玻璃纤维壁布涂层的制备方法 Download PDF

Info

Publication number
CN103643516B
CN103643516B CN201310630650.XA CN201310630650A CN103643516B CN 103643516 B CN103643516 B CN 103643516B CN 201310630650 A CN201310630650 A CN 201310630650A CN 103643516 B CN103643516 B CN 103643516B
Authority
CN
China
Prior art keywords
coating
appropriate
cold water
gelatinized starch
crosslinking agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310630650.XA
Other languages
English (en)
Other versions
CN103643516A (zh
Inventor
尤晓明
李洋
刘国华
张兰鹏
葛汝海
燕纪祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Rizhao Jingying Media Technology Co ltd
Original Assignee
Shandong Yongtai Chemical Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shandong Yongtai Chemical Group Co Ltd filed Critical Shandong Yongtai Chemical Group Co Ltd
Priority to CN201310630650.XA priority Critical patent/CN103643516B/zh
Publication of CN103643516A publication Critical patent/CN103643516A/zh
Application granted granted Critical
Publication of CN103643516B publication Critical patent/CN103643516B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种玻璃纤维壁布涂层的制备方法,涉及高分子涂料及建筑建材领域。本发明是通过以下技术方案实现的,一种玻璃纤维壁布涂层,包括以下质量份数的原料制备而成:丙烯酸酯乳液50~100;冷水糊化淀粉25~30;增稠剂2~5;交联剂3~5;杀菌剂适量;消泡剂适量;钛白膏适量;水350~400本发明的技术特点及优良效果如下:采用对淀粉交联防水效果明显的碳酸锆铵和聚酰胺聚脲树脂(PAPU)作为交联剂,促进淀粉与聚丙烯酸酯之间的交联,形成网状体系,大幅提高防水性能;原料冷水糊化淀粉价格低廉,来源丰富;涂层制备工艺简单、操作性及实用性强。

Description

一种玻璃纤维壁布涂层的制备方法
技术领域
本发明涉及一种玻璃纤维壁布涂层的制备方法,涉及高分子涂料及建筑建材领域。
背景技术
玻璃纤维壁布又叫海吉布,是以定长玻璃纤维纱或玻璃纤维变形纱的机织物为基材,经表面涂覆处理而成,是一种天然环保型绿色建材,用于建筑内墙装饰装修。具有耐潮防霉、耐撞击、耐腐蚀、耐水洗、无毒不燃、防水透气等优点,还可以有效加固墙面,起到防止墙面开裂的作用。同时变化多端的织造手法衍生出数以千计富有质感的花纹图案,还可根据个人喜好随意改变外观色彩,实现意想不到的装饰效果,符合当今社会追求健康、环保、安全、舒适的潮流,是星级酒店、高档写字楼、机场、餐厅、影剧院、地铁等场所的理想装饰装修材料。
玻璃纤维机织物进行表面涂覆主要是为了减少织物表面的毛羽,使壁布挺括定型,便于施工,同时赋予壁布与墙面、涂料良好的亲和性。目前国内玻璃纤维壁布涂层的主要成分包括:热水糊化淀粉、丙烯酸酯乳液、消泡剂、杀菌剂等。典型的工艺如下:将预糊化淀粉在热水中搅拌糊化,并加入磷酸等助剂调整浆料粘度,调整pH值后然后加入丙烯酸酯乳液,搅拌均匀后加入杀菌剂、消泡剂等助剂后过滤出料;涂料经涂布机涂在玻璃纤维坯布上,再经200°C左右烘干定型。玻璃纤维壁布在使用时要先在背面涂胶,然后平整的粘附在墙壁上,这对涂层的耐水性及柔软性要求很高。上述工艺可以通过调整丙烯酸酯乳液的Tg来调整柔软性,Tg越低,壁布的柔软性就越好。但是由于亲水性物质淀粉的存在,壁布的耐水性很差,涂层经胶水短时间浸泡后即失去粘结能力,造成玻璃织物松散,影响花纹图案。
美国专利US20060036014A1提供了一种玻璃纤维壁布涂层的制备方法,也是国外玻璃纤维壁布涂层的代表性工艺。本专利采用冷水糊化磷酸酯淀粉、丙烯酸酯乳液、钛白粉、交联剂、增稠剂、杀菌剂、消泡剂等为原料,高速搅拌混合均匀后即可涂覆。交联剂的存在可以提高涂层的耐水性,但是效果还是不太理想;冷水糊化磷酸酯淀粉的采用简化了工艺流程,对柔软性及光泽也有改善,但是冷水糊化磷酸酯淀粉成本较高,国内没有规模化生产厂家,该工艺难以在国内推广。
发明内容
本发明旨在克服以上种种不足,提供一种成本低廉、耐水性好、工艺简单的玻璃纤维壁布涂层的制备方法。
本发明是通过以下技术方案实现的,一种玻璃纤维壁布涂层,包括以下质量份数的原料制备而成:
丙烯酸酯乳液50~100
冷水糊化淀粉25~30
增稠剂2~5
交联剂3~5
杀菌剂适量
消泡剂适量
钛白膏适量
水350~400。
所指的丙烯酸酯乳液Tg为-40~20°C,优选的该丙烯酸酯乳液为纯丙乳液,即共聚单体中不含苯乙烯及有机硅氟类单体,Tg为-30~10°C;
所指的冷水糊化淀粉是指未经化学改性的普通淀粉,优选的该淀粉为土豆及木薯冷水糊化淀粉;
所指的增稠剂为纤维素类增稠剂、聚丙烯酸类增稠剂及缔合型聚氨酯类增稠剂,如羧甲基纤维素、羟丙基甲基纤维素、水溶性聚丙烯酸盐等,优选的该增稠剂为羟丙基甲基纤维素和水溶性聚丙烯酸盐;
所指的交联剂为碳酸锆铵、聚酰胺聚脲树脂(PAPU)、氮丙啶、乙二醛水溶液等,优选的该交联剂为碳酸锆铵和聚酰胺聚脲树脂(PAPU)。
一种玻璃纤维壁布涂层,制备方法如下:
先将冷水糊化淀粉、钛白膏加入到水中,高速搅拌使其分散均匀;再加入丙烯酸酯乳液,继续搅拌均匀;持续搅拌下缓慢加入交联剂,再加入增稠剂溶液调整至适宜粘度;最后加入适量消泡剂和杀菌剂,搅拌均匀后出料。
本发明的技术特点及优良效果如下:
1、采用对淀粉交联防水效果明显的碳酸锆铵和聚酰胺聚脲树脂(PAPU)作为交联剂,促进淀粉与聚丙烯酸酯之间的交联,形成网状体系,大幅提高防水性能;
2、原料冷水糊化淀粉价格低廉,来源丰富;
3、涂层制备工艺简单、操作性及实用性强。
具体实施方式
下面结合具体实施例对本发明作更进一步的说明,以便本领域的技术人员更了解本发明,但并不因此限制本发明。
实施例1
涂层原料及质量份数如下:
纯丙乳液(Tg-30°C)50kg
冷水糊化木薯淀粉25kg
羟丙基甲基纤维素4.8kg
PAPU(50%固含量)5kg
杀菌剂适量
消泡剂适量
钛白膏适量
水400kg。
先将冷水糊化木薯淀粉、钛白膏加入到水中,高速搅拌使其分散均匀;再加入纯丙乳液,继续搅拌均匀;持续搅拌下缓慢加入PAPU溶液,再加入羟丙基甲基纤维素溶液调整至粘度为2500cP;最后加入适量消泡剂和杀菌剂,搅拌均匀后出料。
该玻璃纤维织物涂层光泽鲜艳,柔软性好,将水滴在壁布上有荷叶效应,防水性能优良。
实施例2
涂层原料及质量份数如下:
纯丙乳液(Tg10°C)100kg
冷水糊化土豆淀粉30kg
聚丙烯酸盐2kg
碳酸锆铵(30%固含量)5kg
杀菌剂适量
消泡剂适量
钛白膏适量
水400kg。
先将冷水糊化木薯淀粉、钛白膏加入到水中,高速搅拌使其分散均匀;再加入纯丙乳液,继续搅拌均匀;持续搅拌下缓慢加入碳酸锆铵溶液,再加入聚丙烯酸盐溶液调整至粘度为2200cP;最后加入适量消泡剂和杀菌剂,搅拌均匀后出料。
该玻璃纤维织物涂层光泽鲜艳,柔软性良好,同样有荷叶效应,防水性能优良。
最后应说明的是,以上实施例仅用以说明本发明而并非限制本发明所描述的技术方案。一切不脱离本发明的精神和范围的技术方案及其改进,其均应涵盖在本发明的权利要求范围中。

Claims (1)

1.一种玻璃纤维壁布涂层,包括以下质量份数的原料制备而成::
丙烯酸酯乳液50~100
冷水糊化淀粉25~30
增稠剂2~5
交联剂3~5
杀菌剂适量
消泡剂适量
钛白膏适量
水350~400;所述的丙烯酸酯乳液为纯丙乳液,Tg为-30~10℃,
所述的冷水糊化淀粉为土豆或木薯冷水糊化淀粉;所述的增稠剂为羟丙基甲基纤维素和水溶性聚丙烯酸盐;所述的交联剂为碳酸锆铵和聚酰胺聚脲树脂(PAPU);
制备方法如下:先将冷水糊化淀粉、钛白膏加入到水中,高速搅拌使其分散均匀;再加入丙烯酸酯乳液,继续搅拌均匀;持续搅拌下缓慢加入交联剂,再加入增稠剂溶液调整至适宜粘度;最后加入适量消泡剂和杀菌剂,搅拌均匀后出料。
CN201310630650.XA 2013-12-02 2013-12-02 一种玻璃纤维壁布涂层的制备方法 Active CN103643516B (zh)