CN103613929A - 一种复合橡胶电容器密封垫及其制备方法 - Google Patents

一种复合橡胶电容器密封垫及其制备方法 Download PDF

Info

Publication number
CN103613929A
CN103613929A CN201310549563.1A CN201310549563A CN103613929A CN 103613929 A CN103613929 A CN 103613929A CN 201310549563 A CN201310549563 A CN 201310549563A CN 103613929 A CN103613929 A CN 103613929A
Authority
CN
China
Prior art keywords
parts
rubber
mixing
sealing gasket
attapulgite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310549563.1A
Other languages
English (en)
Other versions
CN103613929B (zh
Inventor
江豪
李义
肖亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huijiawang Tianjin Technology Co ltd
Beijing Institute of Remote Sensing Equipment
Original Assignee
Anhui Jiangwei Precision Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Jiangwei Precision Manufacturing Co Ltd filed Critical Anhui Jiangwei Precision Manufacturing Co Ltd
Priority to CN201310549563.1A priority Critical patent/CN103613929B/zh
Publication of CN103613929A publication Critical patent/CN103613929A/zh
Application granted granted Critical
Publication of CN103613929B publication Critical patent/CN103613929B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种复合橡胶电容器密封垫,其特征在于,由下列重量份的原料制成:硅橡胶53-58、硬脂酸锌1-2、微晶石蜡6-8、巴西棕榈蜡4-5、氧化锌3-4、海藻多糖1-2、羧甲纤维素1-2、木质素磺酸钠2-3、羟基硅油5-8、四氧化三铁4-6、硫化剂TCY 0.7-0.9、促进剂Na-22 1-2、改性凹凸棒土12-15;本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明成本低,工艺简单,节约了加工时间,而且具有良好的耐油耐高温特性,前度大,综合性能优于普通橡胶。

Description

一种复合橡胶电容器密封垫及其制备方法
技术领域
本发明涉及橡胶复合材料加工领域,特别是一种复合橡胶电容器密封垫及其制备方法。
背景技术
电容器通常简称为电容,是电子设备中大量使用的电子元件之一,广泛应用于电路的隔直通交、耦合、旁路、滤波、调谐回路、能量转换、控制等方面。电容器由壳体、电容芯子、端盖及接线端子组成,电容器壳体内装有浸渍介质,浸渍介质一般为植物油或矿物油,电容器的密封部位均设有密封垫或密封圈,由于电容器的工作环境千差万别,有的电容器需要在恶劣的环境下工作,电容器密封垫需要耐高温、耐寒、耐酸碱、耐盐雾等有不同要求。
发明内容
本发明的目的是提供一种复合橡胶电容器密封垫及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种复合橡胶电容器密封垫,由下列重量份的原料制成:硅橡胶53-58、硬脂酸锌1-2、微晶石蜡6-8、巴西棕榈蜡4-5、氧化锌3-4、海藻多糖1-2、羧甲纤维素1-2、木质素磺酸钠2-3、羟基硅油5-8、四氧化三铁4-6、硫化剂TCY0.7-0.9、促进剂Na-221-2、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土30-35、1,6-己二异氰酸酯4-5、二缩三丙二醇二丙烯酸酯2-3、氧化锌5-6、玉石4-5、3-氨丙基三甲氧基硅烷2-3、氮化铝粉4-5、秸秆灰烬1-2、吗啉1-2、二甲基氧化锡1-2、茶多酚1-2;制备方法是将凹凸棒土、玉石混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述复合橡胶电容器密封垫,由以下具体步骤制成:将硅橡胶、硬脂酸锌、微晶石蜡、巴西棕榈蜡加入密炼机中,加热至30-40℃,混炼3-5min;然后升温至40-50℃,再加入氧化锌、海藻多糖、羧甲纤维素、木质素磺酸钠、羟基硅油、四氧化三铁,混炼6-8min,再加入硫化剂TCY、促进剂Na-22继续混炼4-6min;加入其余剩余成分混炼5-6min,即得本发明橡胶材料。
本发明的优异效果是:本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明成本低,工艺简单,节约了加工时间,而且具有良好的耐油耐高温特性,前度大,综合性能优于普通橡胶。
具体实施方式
下面通过具体实例对本发明进行详细说明。
一种复合橡胶电容器密封垫,由下列重量份(公斤)的原料制成:硅橡胶53、硬脂酸锌1、微晶石蜡6、巴西棕榈蜡4、氧化锌3、海藻多糖1、羧甲纤维素1、木质素磺酸钠2、羟基硅油5、四氧化三铁4、硫化剂TCY0.7、促进剂Na-221、改性凹凸棒土12;
所述改性凹凸棒土由下列重量份(公斤)的原料制成:凹凸棒土30、1,6-己二异氰酸酯4、二缩三丙二醇二丙烯酸酯2、氧化锌5、玉石4、3-氨丙基三甲氧基硅烷2、氮化铝粉4、秸秆灰烬1、吗啉1、二甲基氧化锡1、茶多酚1;制备方法是将凹凸棒土、玉石混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述复合橡胶电容器密封垫,由以下具体步骤制成:将硅橡胶、硬脂酸锌、微晶石蜡、巴西棕榈蜡加入密炼机中,加热至30-40℃,混炼3-5min;然后升温至40-50℃,再加入氧化锌、海藻多糖、羧甲纤维素、木质素磺酸钠、羟基硅油、四氧化三铁,混炼6-8min,再加入硫化剂TCY、促进剂Na-22继续混炼4-6min;加入其余剩余成分混炼5-6min,即得本发明橡胶材料。
用本发明的耐腐蚀橡胶密封垫与普通胶料物理性能对比如下表。
Figure BDA0000409430940000031
从表中可以看出用本发明的橡胶密封垫产品,综合性能比较好。

Claims (2)

1.一种复合橡胶电容器密封垫,其特征在于,由下列重量份的原料制成:硅橡胶 53-58、硬脂酸锌1-2、微晶石蜡6-8、巴西棕榈蜡4-5、氧化锌3-4、海藻多糖1-2、羧甲纤维素1-2、木质素磺酸钠2-3、羟基硅油 5-8、四氧化三铁4-6、硫化剂TCY 0.7-0.9、促进剂Na-22 1-2、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土30-35、1,6-己二异氰酸酯4-5、二缩三丙二醇二丙烯酸酯2-3、氧化锌5-6、玉石4-5、3-氨丙基三甲氧基硅烷2-3、氮化铝粉4-5、秸秆灰烬1-2、吗啉1-2、二甲基氧化锡1-2、茶多酚1-2;制备方法是将凹凸棒土、玉石混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
2.根据权利要求1所述复合橡胶电容器密封垫,其特征在于,由以下具体步骤制成:将硅橡胶、硬脂酸锌、微晶石蜡、巴西棕榈蜡加入密炼机中,加热至30-40℃,混炼3-5min;然后升温至40-50℃,再加入氧化锌、海藻多糖、羧甲纤维素、木质素磺酸钠、羟基硅油、四氧化三铁,混炼6-8min,再加入硫化剂TCY、促进剂Na-22继续混炼4-6min;加入其余剩余成分混炼5-6min,即得本发明橡胶材料。
CN201310549563.1A 2013-11-06 2013-11-06 一种复合橡胶电容器密封垫及其制备方法 Active CN103613929B (zh)