CN103602196A - Non-toxic waterproof coating material - Google Patents

Non-toxic waterproof coating material Download PDF

Info

Publication number
CN103602196A
CN103602196A CN201310580541.1A CN201310580541A CN103602196A CN 103602196 A CN103602196 A CN 103602196A CN 201310580541 A CN201310580541 A CN 201310580541A CN 103602196 A CN103602196 A CN 103602196A
Authority
CN
China
Prior art keywords
parts
coating material
waterproof coating
waterproof
toxic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310580541.1A
Other languages
Chinese (zh)
Other versions
CN103602196B (en
Inventor
王玉庆
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Kun Macao Building Materials Co ltd
Original Assignee
QINGDAO GUANGLIANDA PRECISION MACHINERY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO GUANGLIANDA PRECISION MACHINERY Co Ltd filed Critical QINGDAO GUANGLIANDA PRECISION MACHINERY Co Ltd
Priority to CN201310580541.1A priority Critical patent/CN103602196B/en
Publication of CN103602196A publication Critical patent/CN103602196A/en
Application granted granted Critical
Publication of CN103602196B publication Critical patent/CN103602196B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a non-toxic waterproof coating material. The non-toxic waterproof coating material is prepared from the following raw materials in parts by weight: 2.5-3.3 parts of tetrabutyl phosphorus chloride, 3.5-4.8 parts of acrylate acrylic copolymer emulsion, 0.8-1.6 parts of methylstyrene linear dimer, 1.2-2.3 parts of tartaric acid, 0.6-1.5 parts of xylene, 2.3-3.5 parts of phenethyl diphenol polyoxyethylene ether, 1.3-3.3 parts of dipolyglycerol and 1.6-2.8 parts of dibutyl phthalate. Compared with the existing waterproof coating materials, the waterproof coating material has the advantages that the waterproof coating material is applicable to the waterproofing of buildings, such as basements, toilets, kitchens, pools and the like and does not need heating during use, so that the environmental pollution is reduced; the waterproof coating material is low in construction cost, simple in construction operation and strong in binding power and is cracking-resistant, and the waterproof effect is improved; the waterproof coating material is good in waterproof performance and long in service life, is non-toxic and harmless and can be applied to wet or dry base faces of a variety of materials, so that the waterproof coating material is a relatively ideal waterproof material.

Description

A kind of nontoxic waterproof paint
Technical field
The present invention relates to a kind of nontoxic waterproof paint, belong to building material field.
Background technology
Due to advocating of environmental protection, water-borne coatings has become the hot product in market, and the development and application of China's waterproof paint started from for the 60's, once take in early days various chemical industry tankage as raw material development product, all because capability and performance is unstable, stops development.In the same period, China, for improve petroleum pitch configuration waterproof paint aspect with superpolymer, plays chess and has carried out relatively large work.There is chloroprene rubber in 60 mid-nineties 90s--asphalt waterproofing paint, and there is regenerated rubber in the initial stage in the 70's--asphalt waterproofing paint, and in engineering, obtain more successfully application.Steady progression along with China's synthesized polymer material industry, take the waterproof paint that various high-quality synthetic rubber and synthetic resins is raw material development, in the 80's, in succession come into operation: as the light waterproof paint of Two-component Waterproof Polyurethane Coating, esters of acrylic acid, cationic chloroprene latex asphalt waterproofing paint and silicon rubber waterproof coating etc., rubber asphalt class and synthetic high score subclass waterproof paint, in China's waterproofing work application, are just occupying increasing proportion.Take petroleum pitch as main, carry out the existing longer history of technological approaches , China of modification with superpolymer, its raw material sources is extensive, and cost is lower, the general waterproofing work of large light of the amount of being applicable to; Take synthesized polymer material as the main coating of making, and performance is more excellent, but price is higher; Due to building distortion, thereby body of wall be full of cracks causes coating surface cracking, reduces waterproof effect.
Summary of the invention
The deficiency existing for prior art, technical problem to be solved by this invention is, a kind of nontoxic waterproof paint is provided, and cohesive force is strong, and cracking resistance reduces environmental pollution, and cost is low.
For solving the problems of the technologies described above, the technical scheme that the present invention takes is, a kind of nontoxic waterproof paint,
Raw material by following parts by weight is made: tetrabutyl phosphorus chloride 2.5-3.3 part, acrylate acrylate copolymer emulsion 3.5-4.8 part, vinyl toluene linear dimeric 0.8-1.6 part, tartrate 1.2-2.3 part, dimethylbenzene 0.6-1.5 part, styroyl xenol Soxylat A 25-7 2.3-3.5 part, two Polyglycerine 1.3-3.3 parts and dibutyl phthalate 1.6-2.8 part.
Optimize, above-mentioned nontoxic waterproof paint, by the raw material of following parts by weight, made:
2.7 parts of 2.8 parts, tetrabutyl phosphorus chloride, 4.2 parts of acrylate acrylate copolymer emulsions, 1.5 parts of vinyl toluene linear dimerics, 1.6 parts, tartrate, 1.2 parts of dimethylbenzene, 2.6 parts of styroyl xenol Soxylat A 25-7s, 3.1 parts of two Polyglycerine and dibutyl phthalates.
The present invention compares with existing waterproof paint, and the present invention is applicable to the waterproof of the building such as vault, toilet, kitchen, pond, during use, without heating, reduces environmental pollution, has that cost is low, constructing operation is simple; Cohesive force is strong, and cracking resistance has improved waterproof effect; Can be on the basal plane of moist or dry various material construction waterproof functional, nontoxic, long service life, is a kind of comparatively ideal water-proof material.
Embodiment
embodiment 1
The present invention is a kind of nontoxic waterproof paint, by the raw material of following parts by weight, is made:
2.7 parts of 2.8 parts, tetrabutyl phosphorus chloride, 4.2 parts of acrylate acrylate copolymer emulsions, 1.5 parts of vinyl toluene linear dimerics, 1.6 parts, tartrate, 1.2 parts of dimethylbenzene, 2.6 parts of styroyl xenol Soxylat A 25-7s, 3.1 parts of two Polyglycerine and dibutyl phthalates.
embodiment 2
The present invention is a kind of nontoxic waterproof paint, by the raw material of following parts by weight, is made:
1.6 parts of 2.5 parts, tetrabutyl phosphorus chloride, 3.5 parts of acrylate acrylate copolymer emulsions, 0.8 part of vinyl toluene linear dimeric, 1.2 parts, tartrate, 0.6 part of dimethylbenzene, 2.3 parts of styroyl xenol Soxylat A 25-7s, 1.3 parts of two Polyglycerine and dibutyl phthalates.
embodiment 3
The present invention is a kind of nontoxic waterproof paint, by the raw material of following parts by weight, is made:
2.8 parts of 3.3 parts, tetrabutyl phosphorus chloride, 4.8 parts of acrylate acrylate copolymer emulsions, 1.6 parts of vinyl toluene linear dimerics, 2.3 parts, tartrate, 1.5 parts of dimethylbenzene, 3.5 parts of styroyl xenol Soxylat A 25-7s, 3.3 parts of two Polyglycerine and dibutyl phthalates.
The present invention compares with existing waterproof paint, and the present invention is applicable to the waterproof of the building such as vault, toilet, kitchen, pond, during use, without heating, reduces environmental pollution, has that cost is low, constructing operation is simple; Cohesive force is strong, and cracking resistance has improved waterproof effect; Can be on the basal plane of moist or dry various material construction waterproof functional, nontoxic, long service life, is a kind of comparatively ideal water-proof material.
Certainly, above-mentioned explanation is not limitation of the present invention, and the present invention is also not limited to above-mentioned giving an example; those skilled in the art; in essential scope of the present invention, the variation of making, remodeling, interpolation or replacement, all should belong to protection scope of the present invention.

Claims (2)

1. a nontoxic waterproof paint, is characterized in that: the raw material by following parts by weight is made:
Tetrabutyl phosphorus chloride 2.5-3.3 part, acrylate acrylate copolymer emulsion 3.5-4.8 part, vinyl toluene linear dimeric 0.8-1.6 part, tartrate 1.2-2.3 part, dimethylbenzene 0.6-1.5 part, styroyl xenol Soxylat A 25-7 2.3-3.5 part, two Polyglycerine 1.3-3.3 parts and dibutyl phthalate 1.6-2.8 part.
2. nontoxic waterproof paint according to claim 1, is characterized in that:
Raw material by following parts by weight is made: 2.7 parts of 2.8 parts, tetrabutyl phosphorus chloride, 4.2 parts of acrylate acrylate copolymer emulsions, 1.5 parts of vinyl toluene linear dimerics, 1.6 parts, tartrate, 1.2 parts of dimethylbenzene, 2.6 parts of styroyl xenol Soxylat A 25-7s, 3.1 parts of two Polyglycerine and dibutyl phthalates.
CN201310580541.1A 2013-11-19 2013-11-19 A kind of nontoxic waterproof paint Expired - Fee Related CN103602196B (en)