CN103613968A - Modified durable waterproof paint - Google Patents
Modified durable waterproof paint Download PDFInfo
- Publication number
- CN103613968A CN103613968A CN201310505311.9A CN201310505311A CN103613968A CN 103613968 A CN103613968 A CN 103613968A CN 201310505311 A CN201310505311 A CN 201310505311A CN 103613968 A CN103613968 A CN 103613968A
- Authority
- CN
- China
- Prior art keywords
- parts
- paint
- paint provided
- waterproof
- waterproof paint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses modified durable waterproof paint. The paint is prepared from following raw materials by weight: 1.5-2.8 parts of 3-methyl-2-buten-1-ol, 5-8 parts of 4-tert-amylphenol, 1.5-2.7 parts of sodium polyacrylate, 2.3-4 parts of borax powder, 1.8-3.6 parts of calcium chloride, 2.5-6 parts of entirely hydrolysed polyvinyl alcohol, 0.8-1.7 parts of a phenol-urea-formaldehyde condensate sulfonate and 1.5-3.2 parts of an alkyltrimethylammonium salt type dodecyltrimethylammonium chloride. Compared with waterproof paint at present, the paint provided by the invention is suitable for waterproofing of basements, toilets, kitchens, pools, and other buildings. The paint provided by the invention can be used without being heated and can reduce environment pollution. The coat of the paint provided by the invention is low and application operation of the paint provided by the invention is simple. The paint provided by the invention can be applied on wet or dry bases of various materials. The paint provided by the invention has good waterproof property, no toxicity, no harm and long service lifetime, and is an ideal waterproof material.
Description
Technical field
The present invention relates to a kind of improved durable waterproof paint, belong to building material field.
Background technology
Due to advocating of environmental protection, water-borne coatings has become the hot product in market, and the development and application of China's waterproof paint started from for the 60's, once take in early days various chemical industry tankage as raw material development product, all because capability and performance is unstable, stops development.In the same period, China, for improve petroleum pitch configuration waterproof paint aspect with superpolymer, has also carried out relatively large work.There is chloroprene rubber in 60 mid-nineties 90s--asphalt waterproofing paint, and there is regenerated rubber in the initial stage in the 70's--asphalt waterproofing paint, and in engineering, obtain more successfully application.Steady progression along with China's synthesized polymer material industry, take the waterproof paint that various high-quality synthetic rubber and synthetic resins is raw material development, in the 80's, in succession come into operation: as the light waterproof paint of Two-component Waterproof Polyurethane Coating, esters of acrylic acid, cationic chloroprene latex asphalt waterproofing paint and silicon rubber waterproof coating etc., rubber asphalt class and synthetic high score subclass waterproof paint, in China's waterproofing work application, are just occupying increasing proportion.Take petroleum pitch as main, carry out the existing longer history of technological approaches , China of modification with superpolymer, its raw material sources is extensive, and cost is lower, the general waterproofing work of large light of the amount of being applicable to; Take synthesized polymer material as the main coating of making, and performance is more excellent, but price is higher.
Summary of the invention
The deficiency existing for prior art, technical problem to be solved by this invention is, a kind of improved durable waterproof paint is provided, steady quality, reduces environmental pollution, cheap.
For solving the problems of the technologies described above, the technical scheme that the present invention takes is, a kind of improved durable waterproof paint,
Raw material by following parts by weight is made: polyvinyl alcohol 2.5-6 part of 3-M2BOL 1.5-2.8 part, Pentaphen 5-8 part, polyacrylic acid sodium salt 1.5-2.7 part, borax powder 2.3-4 part, calcium chloride 1.8-3.6 part, complete hydrolysis, phenol-melocol condensate sulfonates 0.8-1.7 part and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride 1.5-3.2 part.
Optimize, above-mentioned improved durable waterproof paint, by the raw material of following parts by weight, made:
2.6 parts of 5.4 parts of the polyvinyl alcohol of 2.3 parts of 3-M2BOLs, 7 parts of Pentaphens, 1.6 parts of polyacrylic acid sodium salts, 3.2 parts, borax powder, 3.4 parts, calcium chloride, complete hydrolysis, 1.3 parts of phenol-melocol condensate sulfonates and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride.
The present invention compares with existing waterproof paint, the present invention is applicable to the waterproof of the buildings such as vault, toilet, kitchen, pond, during use without heating, reduce environmental pollution, have that cost is low, constructing operation is simple, can be on the basal plane of moist or dry various material construction waterproof functional, nontoxic, long service life is a kind of comparatively ideal water-proof material.
Embodiment
embodiment 1
The present invention is a kind of improved durable waterproof paint, by the raw material of following parts by weight, is made:
2.6 parts of 5.4 parts of the polyvinyl alcohol of 2.3 parts of 3-M2BOLs, 7 parts of Pentaphens, 1.6 parts of polyacrylic acid sodium salts, 3.2 parts, borax powder, 3.4 parts, calcium chloride, complete hydrolysis, 1.3 parts of phenol-melocol condensate sulfonates and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride.
embodiment 2
The present invention is a kind of improved durable waterproof paint, by the raw material of following parts by weight, is made:
1.5 parts of 2.5 parts of the polyvinyl alcohol of 1.5 parts of 3-M2BOLs, 5 parts of Pentaphens, 1.5 parts of polyacrylic acid sodium salts, 2.3 parts, borax powder, 1.8 parts, calcium chloride, complete hydrolysis, 0.8 part of phenol-melocol condensate sulfonates and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride.
embodiment 3
The present invention is a kind of improved durable waterproof paint, by the raw material of following parts by weight, is made:
3.2 parts of 6 parts of the polyvinyl alcohol of 2.8 parts of 3-M2BOLs, 8 parts of Pentaphens, 2.7 parts of polyacrylic acid sodium salts, 4 parts, borax powder, 3.6 parts, calcium chloride, complete hydrolysis, 1.7 parts of phenol-melocol condensate sulfonates and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride.
The present invention compares with existing waterproof paint, the present invention is applicable to the waterproof of the buildings such as vault, toilet, kitchen, pond, during use without heating, reduce environmental pollution, have that cost is low, constructing operation is simple, can be on the basal plane of moist or dry various material construction waterproof functional, nontoxic, long service life is a kind of comparatively ideal water-proof material.
Certainly, above-mentioned explanation is not limitation of the present invention, and the present invention is also not limited to above-mentioned giving an example; those skilled in the art; in essential scope of the present invention, the variation of making, remodeling, interpolation or replacement, all should belong to protection scope of the present invention.
Claims (2)
1. an improved durable waterproof paint, is characterized in that: the raw material by following parts by weight is made:
Polyvinyl alcohol 2.5-6 part of 3-M2BOL 1.5-2.8 part, Pentaphen 5-8 part, polyacrylic acid sodium salt 1.5-2.7 part, borax powder 2.3-4 part, calcium chloride 1.8-3.6 part, complete hydrolysis, phenol-melocol condensate sulfonates 0.8-1.7 part and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride 1.5-3.2 part.
2. improved durable waterproof paint according to claim 1, is characterized in that:
Raw material by following parts by weight is made: 2.6 parts of 5.4 parts of the polyvinyl alcohol of 2.3 parts of 3-M2BOLs, 7 parts of Pentaphens, 1.6 parts of polyacrylic acid sodium salts, 3.2 parts, borax powder, 3.4 parts, calcium chloride, complete hydrolysis, 1.3 parts of phenol-melocol condensate sulfonates and alkyl trimethyl ammonium salt type Dodecyl trimethyl ammonium chloride.